Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FIB”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Intermetallics Based on Sodium Chalcogenides Promote Stable Electrodeposition–Electrodissolution of Sodium Metal Anodes

Sodiophilic micro-composite films of sodium-chalcogenide intermetallics (Na 2 Te and Na 2 S) and Cu particles are fabricated onto commercial copper foam current collectors (Na 2 Te@CF and Na 2 S@CF). For the first time a controllable capacity thermal infusion process is demonstrated. Enhanced wetting by the metal electrodeposition leads to state-of-the-art electrochemical performance. For example, Na 2 Te@CF-based half-cells demonstrate stable cycling at 6 mA cm -2 and 6 mAh cm -2 , corresponding to 54 µm of Na electrodeposited/electrodissolved by geometric area. Sodium metal batteries with Na 3 V 2 (PO 4 ) 3 cathodes are stable at 30C (7 mA cm -2 ) and for 10 000 cycles at 5C and 10C. Cross-sectional cryogenic focused ion beam (cryo-FIB) microscopy details deposited and remnant dissolved microstructures. Sodium metal electrodeposition onto Na 2 Te@CF is dense, smooth, and free of dendrites or pores. On unmodified copper foam, sodium grows in a filament-like manner, not requiring cycling to achieve this geometry. Substrate–metal interaction critically affects the metal–electrolyte interface, namely the thickness and morphology of the solid electrolyte interphase. Density functional theory and mesoscale simulations provide insight into support-adatom energetics, nucleation response, and early-stage morphological evolution. On Na 2 Te sodium atomic dispersion is thermodynamically more stable than isolated clusters, leading to conformal adatom coverage of the surface.

36 MATERIALS SCIENCE↗

Tuned Reactivity at the Lithium Metal–Argyrodite Solid State Electrolyte Interphase

Thin intermetallic Li 2 Te–LiTe 3 bilayer (0.75 µm) derived from 2D tellurene stabilizes the solid electrolyte interphase (SEI) of lithium metal and argyrodite (LPSCl, Li 6 PS 5 Cl) solid-state electrolyte (SSE). Tellurene is loaded onto a standard battery separator and reacted with lithium through single-pass mechanical rolling or transferred directly to SSE surface by pressing. State-of-the-art electrochemical performance is achieved, e.g., symmetric cell stable for 300 cycles (1800 h) at 1 mA cm -2 and 3 mAh cm -2 (25% DOD, 60 µm foil). Cryo-stage focused ion beam (Cryo-FIB) sectioning and Raman mapping demonstrate that the Li 2 Te–LiTe 3 bilayer impedes SSE decomposition. The unmodified Li–LPSCl interphase is electrochemically unstable with a geometrically heterogeneous reduction decomposition reaction front that extends deep into the SSE. Decomposition drives voiding in Li metal due to its high flux to the reaction front, as well as voiding in the SSE due to the associated volume changes. Analysis of cycled SSE found no evidence for pristine (unreacted) lithium metal filaments/dendrites, implying failure driven by decomposition phases with sufficient electrical conductivity that span electrolyte thickness. In conclusion, DFT calculations clarify thermodynamic stability, interfacial adhesion, and electronic transport properties of interphases, while mesoscale modeling examines interrelations between reaction front heterogeneity (SEI heterogeneity), current distribution, and localized chemo-mechanical stresses.

25 ENERGY STORAGE↗

Mechanical Milling – Induced Microstructure Changes in Argyrodite LPSCl Solid-State Electrolyte Critically Affect Electrochemical Stability

Microstructure of argyrodite solid-state electrolyte (SSE) critically affects lithium metal electrodeposition/dissolution. While the stability of unmodified SSE is mediocre, once optimized state-of-the-art electrochemical performance is achieved (symmetric cells, full cells with NMC811) without secondary interlayers or functionalized current collectors. Planetary mechanical milling in wet media (m-xylene) is employed to alter commercial Li 6 PS 5 Cl (LPSCl) powder. Quantitative stereology demonstrates how milling progressively refines grain and pore size/distribution in the SSE compact, increases its density, and geometrically smoothens the SSE-Li interface. Mechanical indentation demonstrates that these changes lead to reduced site-to-site variation in the compact's hardness. Milled microstructures promote uniform early-stage electrodeposition on foil collectors and stabilize solid electrolyte interphase (SEI) reactivity. Analysis of half-cells with bilayer electrolytes demonstrates the importance of microstructure directly contacting current collector, with interface roughness due to pore and grain size distribution being key. For the first time, short-circuiting Li metal dendrite is directly identified, employing 1.5 mm diameter “mini” symmetrical cell and cryogenic focused ion beam (cryo-FIB) electron microscopy. The branching sheet-like dendrite traverses intergranularly, filling the interparticle voids and forming an SEI around it. Importantly, mesoscale modeling reveals the relationship between Li-SSE interface morphology and the onset of electrochemical instability, based on underlying reaction current distribution.

25 ENERGY STORAGE↗

Mitigating Battery Cell Failure: Role of Ag‐Nanoparticle Fillers in Solid Electrolyte Dendrite Suppression

Abstract The development of solid‐state batteries (SSBs) with lithium Li metal anodes holds significant promise for enhancing the energy density and safety of next‐generation energy storage systems. However, their commercialization is hindered by challenges related to Li dendrite formation, which can lead to short circuits and battery failure. In this study, the role of Ag nanoparticles embedded within solid electrolytes (SE) is investigated in suppressing dendrite propagation. The results demonstrate that Ag nanoparticles effectively mitigate two key failure mechanisms: (1) dendrite growth within porous networks at low current densities and (2) stress intensification‐induced SE fracture at higher current densities (12 mA cm −2 ). Ex situ characterization using focused‐ion beam – scanning electron microscopy (FIB–SEM) and energy dispersive X‐ray spectroscopy (EDS,) reveals that Ag nanoparticles migrate alongside advancing Li dendrites, promoting homogeneous dendrite growth and reducing the likelihood of localized stress concentrations. Additionally, the incorporation of Ag nanoparticles is shown to facilitate a more uniform Li distribution toward the anode side, which can potentially enable the use of higher charging rates in SSBs. This study provides a new perspective on Li dendrite suppression and presents new opportunities for enhancing the performance and safety of SSBs.

Diallo, Mouhamad Said↗

Influence of Potassium Metal‐Support Interactions on Dendrite Growth

Abstract Combined synchrotron X‐ray nanotomography imaging, cryogenic electron microscopy (cryo‐EM) and modeling elucidate how potassium (K) metal‐support energetics influence electrodeposit microstructure. Three model supports are employed: O‐functionalized carbon cloth (potassiophilic, fully‐wetted), non‐functionalized cloth and Cu foil (potassiophobic, nonwetted). Nanotomography and focused ion beam (cryo‐FIB) cross‐sections yield complementary three‐dimensional (3D) maps of cycled electrodeposits. Electrodeposit on potassiophobic support is a triphasic sponge, with fibrous dendrites covered by solid electrolyte interphase (SEI) and interspersed with nanopores (sub‐10 nm to 100 nm scale). Lage cracks and voids are also a key feature. On potassiophilic support, the deposit is dense and pore‐free, with uniform surface and SEI morphology. Mesoscale modeling captures the critical role of substrate‐metal interaction on K metal film nucleation and growth, as well as the associated stress state.

Liu, Pengcheng↗

Interdependence of Support Wettability ‐ Electrodeposition Rate‐ Sodium Metal Anode and SEI Microstructure

Abstract This study examines how current collector support chemistry (sodiophilic intermetallic Na 2 Te vs. sodiophobic baseline Cu) and electrodeposition rate affect microstructure of sodium metal and its solid electrolyte interphase (SEI). Capacity and current (6 mAh cm −2 , 0.5–3 mA cm −2 ) representative of commercially relevant mass loading in anode‐free sodium metal battery (AF‐SMBs) are analyzed. Synchrotron X‐ray nanotomography and grazing‐incidence wide‐angle X‐ray scattering (GIWAXS) are combined with cryogenic ion beam (cryo‐FIB) microscopy. Highlighted are major differences in film morphology, internal porosity, and crystallographic preferred orientation e.g. (110) vs. (100) and (211) with support and deposition rate. Within the SEI, sodium fluoride (NaF) is more prevalent with Te−Cu versus sodium hydride (NaH) and sodium hydroxide (NaOH) with baseline Cu. Due to competitive grain growth the preferred orientation of sodium crystallites depends on film thickness. Mesoscale modeling delineates the role of SEI (ionic conductivity, morphology) on electrodeposit growth and onset of electrochemical instability.

Lo, Chang‐An↗

Influence of Potassium Metal-Support Interactions on Dendrite Growth

We report combined synchrotron X-ray nanotomography imaging, cryogenic electron microscopy (cryo-EM) and modeling elucidate how potassium (K) metal-support energetics influence electrodeposit microstructure. Three model supports are employed: O-functionalized carbon cloth (potassiophilic, fully-wetted), non-functionalized cloth and Cu foil (potassiophobic, nonwetted). Nanotomography and focused ion beam (cryo-FIB) cross-sections yield complementary three-dimensional (3D) maps of cycled electrodeposits. Electrodeposit on potassiophobic support is a triphasic sponge, with fibrous dendrites covered by solid electrolyte interphase (SEI) and interspersed with nanopores (sub-10 nm to 100 nm scale). Lage cracks and voids are also a key feature. On potassiophilic support, the deposit is dense and pore-free, with uniform surface and SEI morphology. Mesoscale modeling captures the critical role of substrate-metal interaction on K metal film nucleation and growth, as well as the associated stress state.

36 MATERIALS SCIENCE↗

Alumina – Stabilized SEI and CEI in Potassium Metal Batteries

Aluminum oxide (Al 2 O 3 ) nanopowder is spin-coated onto both sides of commercial polypropene separator to create artificial solid-electrolyte interphase (SEI) and artificial cathode electrolyte interface (CEI) in potassium metal batteries (KMBs). Here, this significantly enhances the stability, including of KMBs with Prussian Blue (PB) cathodes. For example, symmetric cells are stable after 1,000 cycles at 0.5 mA/cm 2 –0.5 mAh/cm 2 and 3.0 mA/cm 2 –0.5 mAh/cm 2 . Alumina modified separators promote electrolyte wetting and increase ionic conductivity (0.59 vs. 0.2 mS/cm) and transference number (0.81 vs. 0.23). Cryo-stage focused ion beam (cryo-FIB) analysis of cycled modified anode demonstrates dense and planar electrodeposits, versus unmodified baseline consisting of metal filaments (dendrites) interspersed with pores and SEI. Alumina-modified CEI also suppresses elemental Fe crossover and reduces cathode cracking. Mesoscale modeling of metal – SEI interactions captures crucial role of intrinsic heterogeneities, illustrating how artificial SEI affects reaction current distribution, conductivity and morphological stability.

25 ENERGY STORAGE↗

3D‐Printed Carbon Nanoneedle Electrodes for Dopamine Detection in Drosophila

In vivo electrochemistry in small brain regions or synapses requires nanoelectrodes with long straight tips for submicron scale measurements. Nanoelectrodes can be fabricated using a Nanoscribe two-photon printer, but annealed tips curl if they are long and thin. We propose a new pulling-force strategy to fabricate a straight carbon nanoneedle structure. A micron-width bridge is printed between two blocks. The annealed structure shrinks during pyrolysis, and the blocks create a pulling force to form a long, thin, and straight carbon bridge. Parameterization study and COMSOL modeling indicate changes in the block size, bridge size and length affect the pulling force and bridge shrinkage. Electrodes were printed on niobium wires, insulated with aluminum oxide, and the bridge cut with focused ion beam (FIB) to expose the nanoneedle tip. Annealed needle diameters ranged from 400 nm to 5.25 μm and length varied from 50.5 μm to 146 μm. The electrochemical properties are similar to glassy carbon, with good performance for dopamine detection with fast-scan cyclic voltammetry. Nanoelectrodes enable biological applications, such as dopamine detection in a specific Drosophila brain region. Long and thin nanoneedles are generally useful for other applications such as cellular sensing, drug delivery, or gas sensing.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Interdependence of Support Wettability - Electrodeposition Rate- Sodium Metal Anode and SEI Microstructure

Here, this study examines how current collector support chemistry (sodiophilic intermetallic Na 2 Te vs. sodiophobic baseline Cu) and electrodeposition rate affect microstructure of sodium metal and its solid electrolyte interphase (SEI). Capacity and current (6 mAh cm -2 , 0.5–3 mA cm -2 ) representative of commercially relevant mass loading in anode-free sodium metal battery (AF-SMBs) are analyzed. Synchrotron X-ray nanotomography and grazing-incidence wide-angle X-ray scattering (GIWAXS) are combined with cryogenic ion beam (cryo-FIB) microscopy. Highlighted are major differences in film morphology, internal porosity, and crystallographic preferred orientation e.g. (110) vs. (100) and (211) with support and deposition rate. Within the SEI, sodium fluoride (NaF) is more prevalent with Te-Cu versus sodium hydride (NaH) and sodium hydroxide (NaOH) with baseline Cu. Due to competitive grain growth the preferred orientation of sodium crystallites depends on film thickness. Mesoscale modeling delineates the role of SEI (ionic conductivity, morphology) on electrodeposit growth and onset of electrochemical instability.

36 MATERIALS SCIENCE↗

Ternary Potassium‐Bismuth‐Telluride Intermetallic Support Promotes Electrochemical Stability in Potassium Metal Anodes

We employed accumulative roll bonding to fabricate self‐standing metallurgical composite of in situ formed alkaline potassium‐bismuth‐telluride intermetallic K 2 (Bi 2/6 Te 3/6 Vac 1/6 ) embedded in potassium metal. This newly discovered thermodynamically stable potassiophilic crystal, termed “KBT”, is fcc antifluorite with K 2 Te archetype. Symmetric cells achieve 880 h of cycling at 0.5 mA cm −2 and 0.5 mAh cm −2 . Potassium metal battery (KMB) with Prussian blue (PB) cathode in carbonate electrolyte retains 80% capacity after 200 cycles at 1C. In ether‐based electrolyte with organic cathode, it achieves 80% retention after 900 cycles at 2C. Combined synchrotron X‐ray nano‐tomography, cryogenic‐focused ion beam microscopy (Cryo‐FIB) and sputter‐down X‐ray photoelectron spectroscopy (XPS) demonstrate uniform electrodeposits, versus baseline of potassium filaments intermixed with pores and coarse SEI. Binary K 3 Bi‐K and K 2 Te‐K intermetallic supports also provide improved electrochemical performance, albeit to lesser extent. Multiscale simulation provides insight into role of support structure in adatom energetics, film nucleation, early‐stage SEI morphology and interfacial stability.

36 MATERIALS SCIENCE↗

Working Principle of an Ionic Liquid Interlayer During Pressureless Lithium Stripping on Li 6.25 Al 0.25 La 3 Zr 2 O 12 (LLZO) Garnet‐Type Solid Electrolyte

Abstract Solid‐state‐batteries employing lithium metal anodes promise high theoretical energy and power densities. However, morphological instability occurring at the lithium/solid–electrolyte interface when stripping and plating lithium during cell cycling needs to be mitigated. Vacancy diffusion in lithium metal is not sufficiently fast to prevent pore formation at the interface above a certain current density during stripping. Applied pressure of several MPa can prevent pore formation, but this is not conducive to practical application. This work investigates the concept of ionic liquids as “self‐adjusting” interlayers to compensate morphological changes of the lithium anode while avoiding the use of external pressure. A clear improvement of the lithium dissolution process is observed as it is possible to continuously strip more than 70 μm lithium (i. e., 15 mAh cm −2 charge) without the need for external pressure during assembly and electrochemical testing of the system. The impedance of the investigated electrodes is analyzed in detail, and contributions of the different interfaces are evaluated. The conclusions are corroborated with morphology studies using cryo‐FIB‐SEM and chemical analysis using XPS. This improves the understanding of the impedance response and lithium stripping in electrodes employing liquid interlayers, acting as a stepping‐stone for future optimization.

Fuchs, Till↗

Inhibition of Micro-pitting by Tribofilm-Forming ZrO 2 Nanocrystal Lubricant Additives: A Micro-pitting Rig and Transmission Electron Microscope Study

The drive to reduce fuel consumption in transportation has encouraged the emergence of low viscosity lubricants to reduce viscous losses in the engine, drivetrain, and other components. However, viscosity reduction increases the risk of surface damage, thus motivating the development of new anti-wear (AW) additives. Capped ZrO 2 nanocrystals (NCs) in base oils have been shown to form AW tribofilms within microscale sliding contacts. However, the potential of ZrO 2 NCs to protect surfaces subjected to rolling-sliding contact from macroscale damage, such as micro-pitting, remains unexplored. Here, we explore the ability of ZrO 2 NCs to form protective tribofilms under harsh conditions using a micro-pitting rig (MPR), consisting of a three ring-on-roller configuration. The experiments were conducted in polyalphaolephin (PAO) base oil, with and without 5 nm diameter ZrO 2 NCs, at two levels of slide-to-roll ratio (SRR) (30% and 0%) and at variable test durations up to long durations (119 h). MPR results showed the use of ZrO 2 NCs gives rise to the formation of a tribofilm covering the roller surfaces and decreases the initiation and propagation of micro-pits compared to tests in pure PAO base stock. Transmission electron microscopy (TEM) performed on focused ion beam (FIB) milled cross-sectional samples of the roller surfaces revealed the growth of dense and 50–100 nm thick ZrO 2 -based tribofilms independent of (SRR), indicating the potential for robust micro-pitting fatigue protection. Nevertheless, small cracks localized within the near surface region of the roller tested at the most severe conditions (30% SRR and 119 h) were observed. The initiation of these cracks was directly related to the presence of manganese sulphide (MnS) inclusions in the steel, revealed using TEM combined with energy dispersive spectroscopy (EDS). Furthermore, the results highlight the benefits of the protective tribofilms formed by ZrO 2 NCs and suggest approaches for further optimizing their use.

36 MATERIALS SCIENCE↗

In-situ re-crystallization of heavily-irradiated Gd 2 Ti 2 O 7

Gadolinium titanate (Gd 2 Ti 2 O 7 , or GTO) and other lanthanide pyrochlores are interesting candidates for actinide waste disposal and fast ion conduction because the relevant material properties are intimately dependent on local cation structure. Therefore, a deep understanding of the kinetics associated with cation ordering and disordering is required if such material properties are to be tuned for specific device designs. To this end, single crystals of GTO were irradiated with 190 keV helium ions to a total fluence of 1 × 10 17 ions/cm 2 , amorphizing the sample surface to a depth of ~1 μm and resulting in significant He bubble accumulation. FIB lamellae lifted out from the irradiated sections were examined during heat treatment in the (scanning) transmission electron microscope. Two distinct stages of the re-crystallization of the amorphized material were observed. The material near the end of the ions’ range transformed first and with the same orientation as the pristine material. This was due to the close proximity of the pristine material and the presence of small defect fluorite seeds, but the propagation of this growth front was frustrated by the large pores (formerly bubbles) in the He accumulation layer. This was followed by heterogeneous nucleation of new crystallites at random orientations at the top of the He accumulation layer, which is attributed to the high surface area associated with the many small He bubbles in that region. Finally, it is inferred that the kinetics of grain growth in this material are significantly faster than the kinetics of grain nucleation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Transformations of Ti-5Al-5V-5Cr-3Mo powder due to reuse in laser powder bed fusion: A surface analytical approach

Reactive Ti-5Al-5 V-5Cr-3Mo (Ti5553) alloy feedstock powder is used in laser powder-bed fusion (LPBF). Due to the large quantity of powder necessary for LPBF, powder is reused numerous times under oxidizing environments. Transformations to the powder’s native surface oxide may impact the LPBF process and lead to deviations from expected behavior of printed parts. In this work, we present a multimodal characterization of new and reused powder by combining X-ray photoelectron spectroscopy (XPS), time-of-flight secondary ion mass spectrometry (ToF-SIMS), and transmission electron microscopy (TEM) of focused ion beam (FIB)-prepared cross sections of individual powder particles to understand how the surface oxide composition changes, grows, and becomes hydroxylated and hydrated due to reuse. We show that the native oxide film of Ti5553 powder is a hydroxylated mixed oxide composed of TiO 2 and Al 2 O 3 that grows from 5.6 +/- 0.7 nm to 8.3 +/- 1.1 nm due to reuse. Al oxide regions of the surface oxide become more hydroxylated during reuse in comparison to Ti oxide regions. This indicates that an outer oxide of pure TiO 2 may enhance recyclability of Ti5553 powder while the presence of Al oxides may decrease recyclability. Further characterization of surface transformations due to recyclability may eliminate unnecessary variation in LPBF.

36 MATERIALS SCIENCE↗

Probing Heterogeneity in Bovine Enamel Composition through Nanoscale Chemical Imaging using Atom Probe Tomography

Objective: The aim of this study was to determine the heterogeneity in chemical composition of bovine enamel using atom probe tomography, and thereby evaluate the suitability of bovine enamel as a substitute for human enamel in in vitro dental research. Design: Enamel samples from extracted bovine incisor teeth were first sectioned using a diamond saw and then milled into needle-like samples (<100 nm diameter) by focused ion beam (FIB) coupled with a scanning electron microscope (SEM). The samples were then analyzed in the atom probe to acquire three-dimensional (3D) images and quantify the atomic chemistry and distribution in bovine enamel. Results: For the first time, the atomic-level composition and clustering of major constituents and impurities within bovine enamel were determined and imaged. We discovered that the chemical composition of bovine enamel is spatially inhomogeneous at the atomic scale. The average bulk Ca/P ratio, ~1.4, was in agreement with previously reported literature values from alternative conventional methods. When assessed locally at the atomic scale, the Ca/P ratio varied between 1.1 and 2.03. We also discovered that the Mg impurities were significantly segregated throughout the enamel, and such clustering influenced the variation of Ca/P ratios. The increase in Mg concentrations, near the Mg clusters, correlated with increased Ca and decreased P concentrations. Conclusion: In conclusion, the presented findings of variability in local composition should be taken into account when interpreting dental research results from bovine enamel.

59 BASIC BIOLOGICAL SCIENCES↗

Multimodal imaging and machine learning to enhance microscope images of shale

A machine learning based image processing workflow is presented to enhance shale source rock microscopic images obtained using diverse imaging platforms. Images were acquired from a 30 μm diameter cylindrical Vaca Muerta shale sample using both nondestructive Transmission X-Ray Microscopy (TXM, alternately referred to as nano computed tomography) and destructive Focused Ion Beam-Scanning Electron Microscopy (FIB-SEM). Output cross-sectional images from each modality were aligned using a combination of manual and automated registration techniques to create a registered image dataset. We then apply this dataset for two image processing tasks: prediction of image cross sections with SEM-like resolution from nondestructive TXM data and repair of charged region artifacts (localized accumulation of electrons) within SEM images. The image processing algorithms for both tasks use deep learning models, specifically image-to-image Convolutional Neural Networks (CNNs) and conditional Generative Adversarial Networks (cGANs). In the image enhancement tasks, we are able to achieve significant qualitative and quantitative improvement in TXM images. Here, the best model reaches an average Peak Signal to Noise Ratio (PSNR) of 15.8 dB. Conditioning on TXM data is also shown to reduce artifacts from SEM charging, achieving an average PSNR of 25.8 dB. Furthermore, our results suggest that properly trained and validated networks are capable of significant enhancement of images obtained using nondestructive techniques, thereby improving interpretation of two- and three-dimensional images while preserving samples for future use.

58 GEOSCIENCES↗