The study of flow pattern and phase-change problem in die casting process

The flow pattern and solidification phenomena in die casting process have been investigated in the first phase study. The flow pattern in filling process is predicted by using a VOF (volume of fluid) method. A good agreement with experimental observation is obtained for filling the water into a die cavity with different gate geometry and with an obstacle in the cavity. An enthalpy method has been applied to solve the solidification problem. By treating the latent heat implicitly into the enthalpy instead of explicitly into the source term, the CPU time can be reduced at least 20 times. The effect of material properties on solidification fronts is tested. It concludes that the dependence of properties on temperature is significant. The influence of the natural convection over the diffusion has also been studied. The result shows that the liquid metal solidification phenomena is diffusion dominant, and the natural convection can affect the shape of the interface. In the second phase study, the filling and solidification processes will be considered simultaneously.

Wang, T. S.↗

To the Die Smartly: Heavy Ion Testing of PEMs on COTS Boards Through the Plastic

Seven commercial off the shelf (COTS) boards containing electronic devices (all in plastic packages, PEMS), under consideration for use in a spacecraft subsystem, were exposed to beams of very high energy ions at the National Superconducting Cyclotron Laboratory (MSU). The ion energies were high enough that an entire board could be exposed in air, and it could still penetrate through the plastic and reach the silicon die. A total of about 300 runs were made, and for each, the LET of the ion entering the silicon die had to be determined, based on the thickness of the plastic lid and the thickness of overlaying materials (e.g., aluminum degraders). Single event latchup (SEL) and functional interrupt (SEFI) were determined during each run, the SEFI by means of simple programs being continuously written to and read from the boards to monitor functionality, while each part was being exposed to the heavy ions.

Wert, J. L.↗

Microstructure, Mechanical Properties, Hot-Die Forming, and Joining of 47XD Gamma TiAl Rolled Sheets

The microstructure and mechanical properties, along with the hot-die forming and joining of Ti-47Al-2Nb-2Mn-0.8 vol% TiB, sheets (known as 47XD), produced by a low-cost rolling process, were evaluated. A near-gamma microstructure was obtained in the as-rolled condition. The microstructures of heat-treated sheets ranged from a recrystallized equiaxed near-gamma microstructure at 1,200 to 1,310 C, to a duplex microstructure at 1,350 C, to a fully lamellar microstructure at 1,376 C. Tensile behavior was determined for unidirectionally rolled and cross-rolled sheets for room temperature (RT) to 816 C. Yield stress decreased gradually with increasing deformation temperature up to 704 C; above 704 C, it declined rapidly. Ultimate tensile strength exhibited a gradual decrease up to 537 C before peaking at 704 C, followed by a rapid decline at 816 C. The modulus showed a gradual decrease with temperature, reaching approximately 72% of the RT value at 816 C. Strain to failure increased slowly from RT to 537 C; between 537 C and 704 C it exhibited a phenomenal increase, suggesting that the ductile-brittle transition temperature was below 704 C. Fracture mode changed from transgranular fracture at low temperature, to a mixture of transgranular and intergranular fracture at intermediate temperature, to ductile fracture at 816 C, coupled with dynamic recrystallization at large strains. Creep rupture response was evaluated between 649 and 816 C over the stress range of 69 to 276 MPa. Deformation parameters for steady-state creep rate and time-to-rupture were similar: activation energies of approximately 350 kJ/mol and stress exponents of approximately 4.5. Hot-die forming of sheets into corrugations was done at elevated temperatures in vacuum. The process parameters to join sheets by diffusion bonding and brazing with TiCuNi 70 filler alloy were optimized for test coupons and successfully used to fabricate large truss-core and honeycomb structures. Nondestructive evaluation methods, e.g., ultrasonic C-scans and thermography along with metallography, were used to characterize bond quality. Microstructural evaluation during heat treatment, identification of phases at the braze/matrix interface, determination of shear strengths of brazed joints, and deformation mechanisms during tensile and creep processes will be discussed.

Das, G.↗

Optimization of combined delayed neutron and differential die-away prompt neutron signal detection for characterization of spent nuclear fuel assemblies

The Next Generation Safeguards Initiative (NGSI) of the U.S. Department of Energy (DOE) has funded multiple laboratories and universities to develop a means to accurately quantify the Plutonium (Pu) mass in spent nuclear fuel assemblies and ways to also detect potential diversion of fuel pins. Delayed Neutron (DN) counting provides a signature somewhat more sensitive to {sup 235}U than Pu while Differential Die-Away (DDA) is complementary in that it has greater sensitivity to Pu. The two methods can, with care, be combined into a single instrument which also provides passive neutron information. Individually the techniques cannot robustly quantify the Pu content but coupled together the information content in the signatures enables Pu quantification separate to the total fissile content. The challenge of merging DN and DDA, prompt neutron (PN) signal, capabilities in the same design is the focus of this paper. Other possibilities also suggest themselves, such as a direct measurement of the reactivity (multiplication) by either the boost in signal obtained during the active interrogation itself or by the extension of the die-away profile. In an early study, conceptual designs have been modeled using a neutron detector comprising fission chambers or 3He proportional counters and a {approx}14 MeV neutron Deuterium-Tritium (DT) generator as the interrogation source. Modeling was performed using the radiation transport code Monte Carlo N-Particles eXtended (MCNPX). Building on this foundation, the present paper quantifies the capability of a new design using an array of {sup 3}He detectors together with fission chambers to optimize both DN and PN detections and active characterization, respectively. This new design was created in order to minimize fission in {sup 238}U (a nuisance DN emitter), to use a realistic neutron generator, to reduce the cost and to achieve near spatial interrogation and detection of the DN and PN, important for detection of diversion, all within the constraints of a single practical instrument. Both DN and PN detections are active techniques using the signal from the most prominent fissile isotopes of spent nuclear fuel that respond the best to a slow neutron interrogation, {sup 235}U, {sup 239}U and {sup 241}PU. The performance is characterized against a library of 64 assemblies and 40 diversion scenarios at different burnup (BU), cooling-time (CT) and initial enrichment (IE) in fresh water.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Architecture for on-die interconnect

In an embodiment, an apparatus includes: a plurality of islands configured on a semiconductor die, each of the plurality of islands having a plurality of cores; and a plurality of network switches configured on the semiconductor die and each associated with one of the plurality of islands, where each network switch includes a plurality of output ports, a first set of the output ports are each to couple to the associated network switch of an island via a point-to-point interconnect and a second set of the output ports are each to couple to the associated network switches of a plurality of islands via a point-to-multipoint interconnect. Other embodiments are described and claimed.

97 MATHEMATICS AND COMPUTING↗

Architecture for on-die interconnect

In an embodiment, an apparatus includes: a plurality of islands configured on a semiconductor die, each of the plurality of islands having a plurality of cores; and a plurality of network switches configured on the semiconductor die and each associated with one of the plurality of islands, where each network switch includes a plurality of output ports, a first set of the output ports are each to couple to the associated network switch of an island via a point-to-point interconnect and a second set of the output ports are each to couple to the associated network switches of a plurality of islands via a point-to-multipoint interconnect. Other embodiments are described and claimed.

42 ENGINEERING↗

An Experimental Investigation of Multilayer Flow in a Slide Die Coating Process

Roll-to-roll coating technology has been actively applied not only for conventional film production but also for emerging energy devices such as organic solar cells, organic light emitting diodes, batteries, smart windows, and fuel cells. The devices are multilayer structures requiring several coating and drying steps when implemented in a serial fashion, which increases capital costs and energy consumption. Simultaneous multilayer (ML) coating technologies present an opportunity for cost reductions and improved process efficiency by reducing equipment footprint and the number of process steps. In this talk, we experimentally investigate ML slide die coating flow for the manufacturing of fuel cell membrane electrode assemblies (MEAs). For ML slide coating, understanding fluid properties such as density, surface tension, and viscosity are necessary for stable flows and limiting intermixing of the miscible layers. Here, we utilize a design-of-experiment methodology - Box-Behnken design (BBD) - to correlate ink formulation parameters to fluid properties. Using the ink properties obtained from the BBD, we performed numerical flow simulations to obtain a proper process conditions to guide experimental coating trials. Finally, experimental verification is performed on a ML slide die and a degree of miscibility was observed for various ink formulation conditions.

28 EE - Advanced Manufacturing Office (EE-5A)↗

Accelerating the Scalability of PrintCast structures using High Pressure Die Casting

PrintCast composites are fabricated by infiltrating a metal mesh or preform (e.g., an additively-manufactured 316L lattices) with molten metal of a lower melting temperature (e.g., A380 aluminum). The resulting PrintCast composite has been shown in the literature to produce diverse and unique mechanical properties that are controllable at the local or global level by adjusting volume-fraction and/or topology of the preforms geometry and overall volume fraction. Although promising mechanical and thermal properties have been achieved at the laboratory scale level, the scalability from laboratory to full scale components has been limited using conventional casting infiltration. This work highlights how using high pressure die casting can significantly advance the development and eventual deployment of PrintCast approaches at large scales. We have successfully produced 9-inch by 6-inch by 1-inch thick PrintCast 316L stainless steel/A380 aluminum “bricks” via high pressure die casting. Initial findings show excellent infiltration and production capability. The resulting approach demonstrates the scalability and manufacturability of hybrid cost effective metal-metal matrix composites at larger length scales with high quality infiltration results.

Splitter, Derek↗

In Situ Structure Characterization in Slot-Die-Printed All-Polymer Solar Cells with Efficiency Over 9%

Herein, high-performance printed all-polymer solar cells (all-PSCs) based on a bulk-heterojunction (BHJ) blend film are demonstrated using PTzBI as the donor and N2200 as the acceptor. A slot-die process is used to prepare the BHJ blend, which is a cost-effective, high-throughput approach to achieve large-area photovoltaic devices. The real-time crystallization of polymers in the film drying process is investigated by in situ grazing incidence wide-angle X-ray scattering characterization. Printing is found to significantly improve the crystallinity of the polymer blend in comparison with spin coating. Moreover, printing with 1,8-diiodooctane as the solvent additive enhances the polymer aggregation and crystallization during solvent evaporation, eventually leading to multi-length-scale phase separation, with PTzBI-rich domains in-between the N2200 crystalline fibers. This unique morphology achieved by printing fabrication results in an impressively high power conversion efficiency of 9.10%, which is the highest efficiency reported for printed all-PSCs. Finally, these findings provide important guidelines for controlling film drying dynamics for processing all-PSCs.

14 SOLAR ENERGY↗

Microstructure and Properties of A356 Alloy Wheels Fabricated by Low-Pressure Die Casting with Local Squeeze

The low-pressure die-casting process (LPDC) is widely used in fabricating aluminum alloy automotive wheels. With good castability and mechanical properties, A356 alloys are important and common materials for LPDC wheels. However, in practical casting process, defects often appear, especially porosities in the wheel thick-walled parts (i.e., spoke) due to inadequate interdendritic feeding, which greatly decreases the mechanical properties. In this investigation, to deal with this problem, local squeeze (LS) was added in conventional LPDC to enhance the interdendritic feeding. The practical A356 alloy wheel castings were fabricated with different LS velocities and times. The quantitative characteristics of α-Al cells, Si particles, and porosities with and without the LS analyzed by optical microscope, scanning electron microscope, and 3D x-ray computed tomography were compared. Their effects on the tensile and impact properties were discussed. The results have shown that the LS can increase the cooling rate and feed shrinkage of spoke parts, hence resulting in finer grains and denser microstructure. In result, the properties of spoke parts were improved with the LS.

36 MATERIALS SCIENCE↗

The investigation of die-pressing and sintering behavior of ITP CP-Ti and Ti-6Al-4V powders

This paper investigated the die-pressing and sintering behavior of the low-cost CP-Ti and Ti-6Al- 4V powders made by the Armstrong Process . The Armstrong powders have an irregular coral like, dendritic morphology, with a dendrite size of approximately 2-5 m. As-received as well as milled powders were uniaxially pressed at designated pressures up to 690 MPa to form disk samples with different aspect ratios. In the studied pressure range, an empirical powder compaction equation was applied to linearize the green density pressure relationship, and powder compaction parameters were obtained. The Armstrong Ti-64 powder exhibited a significantly higher sinterability than the CP-Ti powder. This was explained to be due to the higher diffusivity of V at the sintering temperature. The Ti-64 samples with a green density of 71.0% increased to 99.6% after sintering at 1300oC for 1 hour. An ex-situ technique was used to track the powder morphology change before and after sintering.

36 MATERIALS SCIENCE↗

Enhanced toughness and tear resistance of thin-walled High-Pressure Die-Cast aluminum alloys through Friction stir processing

In this study, we investigate the toughness and resistance to tear of thin-wall high-pressure die-cast (HPDC) aluminum alloys in two different orientations following the implementation of friction stir processing (FSP). The FSP technique was applied to two different HPDC Al-Si alloys: the recyclable-grade, high iron, A380 alloy and the premium-quality, low iron, Aural-5 alloy. Our findings reveal significant tear resistance and strength enhancements for both alloys after FSP modification. Specifically, FSPed A380 alloy requires 126% higher energy to tear, and it has 49% higher tear strength than the HPDC counterpart. Similarly, the tear energy and tear strength of the Aural-5 alloy witness enhancements of 69% and 21%, respectively. In conclusion, these results highlight the potential of FSP as a viable method for augmenting the mechanical properties of HPDC aluminum alloys, thereby opening up new avenues for their utilization in diverse engineering applications for crack obstruction.

36 MATERIALS SCIENCE↗

Friction stir processing: A thermomechanical processing tool for high pressure die cast Al-alloys for vehicle light-weighting

This study uses friction stir processing (FSP) for thermomechanical processing of high-pressure die-casting (HPDC) to modify microstructure and improve mechanical properties. FSP is carried out on two different HPDC aluminum alloys: (a) general-purpose, high-iron, HPDC A380 alloy and (b) premium quality, low-iron HPDC Aural-5 alloy in thin wall, flat plate geometry. Subsequent mechanical testing shows ~30 % and ~65 % enhancement in yield strength and tensile ductility. In addition, FSP leads to ~10 times improvement in fatigue life for A380 alloy and ~70 % improvement in fracture toughness for Aural-5 alloy. These findings emphasize the capability of FSP to modify the microstructure of HPDC Al-alloys-based structural components so that they can demonstrate a good combination of strength, ductility, fracture toughness, and high fatigue properties for long-term durability and reliability.

36 MATERIALS SCIENCE↗

Simulation of differential die-away instrument’s response to asymmetrically burned spent nuclear fuel

Here, previous simulation studies of Differential Die–Away (DDA) instrument’s response to active interrogation of spent nuclear fuel from a pressurized water reactor (PWR) yielded promising results in terms of its capability to accurately measure or estimate basic spent fuel assembly (SFA) characteristics, such as multiplication, initial enrichment (IE) and burn-up (BU) as well as the total plutonium content. These studies were however performed only for a subset of idealized SFAs with a symmetric BU with respect to its longitudinal axis. Therefore, to complement the previous results, additional simulations have been performed of the DDA instrument’s response to interrogation of asymmetrically burned spent nuclear fuel in order to determine whether detailed assay of SFAs from all 4 sides will be necessary in real life applications or whether a cost and time saving single sided assay could be used to achieve results of similar quality as previously reported in case of symmetrically burned SFAs.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Rapid scalable fabrication of roll-to-roll slot-die coated flexible perovskite solar cells using intense pulse light annealing

Perovskite solar cells have achieved high efficiencies at the lab scale using batch processes that often may not be scalable. Processes that can be integrated into a continuous manufacturing platform, such as roll-to-roll, where several processes can be carried out sequentially are necessary to develop a new cost-competitive solar technology. In this work, intense pulsed light thermal post-processing is coupled with scalable slot-die coating and air knife evaporation in a high-speed roll-to-roll process of up to 2 m min –1 . The optimization of IPL energy parameters, web speeds, solution flow rates, and concentration of precursor inks yielded a champion power conversion efficiency of 11.24% for a 1 cm 2 roll-to-roll coated device. The overall processing time for a single layer in this process is reduced from minutes to seconds and the overall footprint of the manufacturing process is decreased. Furthermore, this demonstrates the promising capabilities for intensed pulsed light to reduce manufacturing costs and paves a roadmap for scalable and efficient PSCs on a roll-to-roll platform.

14 SOLAR ENERGY↗

Formation of blade and slot die coated small molecule multilayers for OLED applications studied theoretically and by XPS depth profiling

Slot die coaters especially designed for low material consumption and doctor blades were used to process small molecule solutions for organic light-emitting diodes (OLEDs). Optimum process parameters were developed for the large-scale coating techniques to generate stable single and multiple layers only a few nanometers thick. Achieving a multilayer architecture for solution-processed OLEDs is the most challenging step. X-ray photoelectron spectroscopy sputter depth profiling was performed to determine defined interfaces between coated organic layers. Commercially available small molecules NPB (N,N’-Di(1-naphthyl)-N,N’-diphenyl-(1,1’-biphenyl)-4,4’-diamine) and BAlq (Bis(8-hdroxy-2methylquinoline)-(4-phenylphenoxy)aluminum), originally developed for vacuum deposition, were used as hole, respectively electron transport material. Defined double-layers were processed with both scalable coating methods using the orthogonal solvent approach. The use of non-orthogonal solvents resulted in complete intermixing of the material. The results are explained by calculations of solubilities and simulating drying and diffusion kinetics of the small molecule solutions.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Design of Premoderated Pulsed-Neutron Die-Away Experiments for Validating Beryllium Thermal Neutron Scattering Laws

Accurate thermal scattering laws (TSLs) are essential for reliable neutron transport simulations, particularly for systems with low-energy neutrons. Pulsed-neutron die-away (PNDA) experiments provide a highly sensitive platform for TSL validation but face challenges from fast neutron leakage and material constraints in nonhydrogenous targets such as beryllium. This work investigates the use of high-density polyethylene (HDPE) as a premoderator to reduce leakage, improve thermalization, and shorten experimental run times while preserving sensitivity to the Be TSL. Here, three premoderated configurations, encapsulation, slab, and interstitial, were evaluated using MCNP6.3® simulations with ENDF/B-VIII.0 nuclear data. The effects of the Be TSL was quantified by comparing decay constants from simulations with and without 𝑆⁡(𝛼,𝛽) treatments for both beryllium and HDPE. The results show that premoderation enables the use of as little as 5.20% of the beryllium volume required for an unreflected geometry, achieving uncertainties below 0.5% and reducing run time by up to 72.2% in the studied configurations. The interstitial configuration achieved the best balance between low statistical uncertainty and high TSL sensitivity, outperforming the slab and encapsulation designs. These findings demonstrate that carefully optimized premoderation can significantly enhance the efficiency, feasibility, and precision of PNDA experiments for Be TSL validation.

Integral Experiments↗

Spaced Orthocyclic Winding Pattern for Improved Die Compressed Coils

Winding fill, coil fill, or packing factor, is critical to the performance of many types of electromagnetic devices from electric machines to actuators, transformers, inductors, etc. One technique to increase the packing of conductors in the winding area is to compress round magnet wire conductors in a die, so that they deform and air voids between coil turns are removed. The winding layout of the coil turns on a bobbin before compression has a direct impact on the achievable coil fill and the damage to the coil insulation or conductors after compression. It is thought that winding the turns in an orthocyclic pattern on the bobbin before compression would minimize damage to the turns. This however causes turns to displace during the winding compression process. A new pre-compression winding pattern is proposed, a spaced orthocyclic winding, to minimize turn displacement and damage. A design of experiments study has been carried out to optimize this winding method and to compare it to the traditional orthocyclic winding.

33 ADVANCED PROPULSION SYSTEMS↗