Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CMC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Architectures for High-Performance Ceramic Composites Being Improved

A major thrust of the Ultra-Efficient Engine Technology (UEET) Program at the NASA Glenn Research Center is to develop advanced hot-section engine components using SiC/SiC ceramic matrix composites (CMC's) with thermostructural capability to 2400 F (1315 C). In previous studies, UEET determined that the higher the ultimate tensile strength (UTS) of the as-fabricated CMC, the greater its structural performance at 2400 F. Thus efforts have been ongoing within UEET to understand and develop fiber architecture approaches that can improve the UTS of SiC/SiC CMC's. Under UEET, SiC/SiC test panels and demonstration engine components are currently produced by the multi-ply layup of two-dimensional fabric pieces. The fabric is typically formed of multifilament tows containing high-performance Sylramic (Dow Corning) SiC fiber that is woven into two-dimensional five-harness satin fabric with 20 ends per inch in the 0 degree and 90 degree directions. In some cases, fabric pieces containing woven Sylramic fiber tows are thermally treated at NASA to form Sylramic-iBN fibers that contain a very thin in-situ-grown boron nitride layer on their surfaces. The final SiC/SiC panels and components are fabricated at the CMC vendor by compressing the fabric pieces in tools and then depositing a thin BN interphase coating on the fibers by chemical vapor deposition. The last step at the vendor is to infiltrate the BN-coated fiber architecture with SiC and silicon matrix constituents to form a dense product. Because the as-produced Sylramic fiber tows are sized with a thin polymer coating to facilitate handling and weaving, the individual fibers within the tows and fabric are in close contact with each other. This contact is further increased during fabric compression. One important recent finding is that increasing Sylramic fiber tow width in a fabric increases the UTS of the final SiC/SiC CMC. This effect is presumably related to minimizing fiber/fiber contact, which can be detrimental to CMC strength because of the boron-rich chemistry and roughness of the Sylramic fiber surface. Tows can be spread by mechanically agitating the Sylramic fabric prior to CMC fabrication or by simply thermally treating the Sylramic fabric as in the formation of the Sylramic-iBN fibers. However, CMC's with the treated Sylramic-iBN fabric are even stronger than CMC's with mechanically spread Sylramic tows. The extra strength capability is presumably related to the in situ BN on the fiber surface, which adds compliance to the fiber surfaces and is more resistant to oxygen impurities introduced during the chemical vapor deposition BN process. As shown, another important finding is that the use of fabric with tows having less than the standard of 20 ends per inch provides advantages in terms of reduced ply height and increased ply and CMC strength. The reduced ply height provides more control of part thickness by allowing more plies for a given thickness and by reducing interlaminar residual stresses between plies. The increased ply strength is presumably related to a reduced number of interlaced 90 tows, which, in turn, reduces the crimp angle on the high-modulus fibers in the 0 degree tows. Also, as shown, although fabric with fewer ends per inch reduced the maximum fiber fraction in an eight-ply CMC panel; CMC UTS actually increased because of increased ply strength. Thus, using fabric with fewer ends per inch has several advantages, including providing a significantly higher strength per fiber fraction in the CMC. Consequently, ongoing UEET efforts will attempt to use architectural approaches for components that minimize fiber-fiber contacts and fiber bending within the final composite microstructure.

Yun, Hee Mann↗

Constituent-Based Life Models Being Developed for SiC/SiC Composites

For the successful utilization of ceramic matrix composites (CMC) as hot-section components in advanced aeropropulsion engines, the CMC constituents will need to be tailored and optimized to meet all the critical property demands of each component. Under the High-Speed Research (HSR) and Advanced High-Temperature Engine Materials Technology (HITEMP) Programs, the NASA Glenn Research Center at Lewis Field initiated research to develop mechanistic models for key CMC thermostructural properties. These models would describe the effects of different constituent factors (composition, geometry, and volume fraction) and of potential application conditions (stress, time, temperature, and environment) on these properties. Particular focus was placed on both analytical and numerical modeling of state-of-the-art SiC/SiC composites where the primary load-bearing constituents are stoichiometric SiC fibers in a complex multiphase SiC matrix produced by chemical vapor infiltration and melt infiltration. Recent studies have resulted in computer-based numerical models for the elastic modulus, thermal expansion, and thermal conductivity properties of the SiC/SiC system. Additional studies have generated analytical and empirical models for the time dependence of composite rupture strength at temperatures above 2200 F (1200 C), where CMC's have an important thermostructural advantage over current nickel-based superalloys. These life models utilize thermal activation theory and fiber stress-rupture results measured at Glenn to generate Larson-Miller (L M) plots of fiber rupture strength versus q, a single time- and temperature-dependent parameter. Assuming a worse case in which the SiC matrix is cracked, rupture is then controlled by the time-dependent fracture characteristics of the fiber bundles bridging the matrix cracks. With this as the controlling mechanism, one can then use simple composite theory and the fiber L M plots to predict CMC rupture strength versus the q parameter. The dashed line shows the predicted rupture strength of a SiC/SiC composite that is reinforced by a state-of-the-art stoichiometric SiC fiber. For the q parameter, time is in hours and temperature in degrees kelvin. To generate these predictions, a two-dimensional 0 /90 composite with approximately 16 percent fiber in the applied stress direction and an air test environment were assumed. As such, it is possible to compare the model predictions against limited stress-rupture data for this CMC as shown by the data points. The good agreement confirms the rupture model at least for the selected CMC and test conditions. Thus for this particular SiC/SiC composite, one can estimate a 1000-hr rupture strength of approximately 12 ksi at 2400 F (T = 1588 K and q = 39 700 K). At lower CMC application stresses, the SiC matrix is typically uncracked, so both the fiber and matrix constituents share the composite load. In this case, CMC rupture is controlled by the constituent with the longest rupture time based on the creep rate of the composite. Measured Monkman-Grant plots of rupture time versus creep rate for the two SiC constituents have been used to develop CMC life models for this important application condition. NASA and DOD are currently using this information to establish application and material goals for more advanced CMC's that can be used at even higher temperatures.

DiCarlo, James A.↗

Hybrid Thermally Efficient Core (HyTEC) HyTEC Phase 1 – Combustor Final Report

The objective of the HyTEC – Combustor Technology project is to develop technology for a compact, low emissions, rich-burn combustor that maintains a high-level of durability. To accomplish this, the combustor will incorporate CMC liners and a CMC Dome to enable improved air utilization for mixing and NOx reduction. In particular, three technology areas were matured: metallic swirler attachment to the CMC dome, Nickel diffusion in CMC, and EBC advancements with improved durability. The maturation of these technology areas is critical to successfully designing a combustor for an engine intended to demonstrate increased thermal efficiency with integrated high-power density-core engine technologies. As part of the project, multiple swirler attachment architectures were matured through the design process, manufactured, and tested in simulated engine conditions. These architectures utilized two different approaches to attachment: a pressure loaded approach and a clamped approach. Each approach required testing at simulated engine conditions to mature the technology. These tests were developed to ensure that the probable failure mechanisms for each architecture were assessed relative to its long-term durability. After successfully testing both approaches, the pressure loaded approach was chosen based on its simplicity and its similarity to the attachment approach used on lean burn combustors. Finally, this successful testing resulted in the swirler attachment technology achieving TRL 4 status. Another aspect of concern with the metallic swirler attachment is the potential for nickel diffusion into the CMC to cause durability shortfalls. A series of tests were completed to understand both the amount of nickel that is expected to diffuse into the CMC and the effect this diffusion will have on mechanical properties of the CMC. After successfully completing this testing, the reduction in local mechanical properties was found to not have an impact on the overall durability of the CMC Dome. To further improve the overall durability, three different EBC coating architectures were also studied. One of these coatings being the current state of the art for CMC liners with the other two being proposed improvements. Coupons were produced using each coating and subjected to a series of laboratory testing. One coating was found to have an overall superior durability in laboratory testing and survived rig testing without indication of degradation. This successful testing resulted in the EBC technology achieving TRL 5 status. Overall, a design approach was successfully down-selected that achieves both the TPM requirements and the need for TRL 4+ status. This design incorporates a pressure loaded swirler attachment with an improved EBC coating (Architecture 1). This combination allows the continued use of a CMC dome and results in an improved durability for the proposed compact core combustor.

CMC↗

Determination of the critical micelle concentration in simulations of surfactant systems

Alternative methods for determining the critical micelle concentration (cmc) are investigated using canonical and grand canonical Monte Carlo simulations of a lattice surfactant model. A common measure of the cmc is the “free” (unassociated) surfactant concentration in the presence of micellar aggregates. Many prior simulations of micellizing systems have observed a decrease in the free surfactant concentration with overall surfactant loading for both ionic and nonionic surfactants, contrary to theoretical expectations from mass-action models of aggregation. In the present study, we investigate a simple lattice nonionic surfactant model in implicit solvent, for which highly reproducible simulations are possible in both the canonical (NVT) and grand canonical (μVT) ensembles. We confirm the previously observed decrease of free surfactant concentration at higher overall loadings and propose an algorithm for the precise calculation of the excluded volume and effective concentration of unassociated surfactant molecules in the accessible volume of the solution. We find that the cmc can be obtained by correcting the free surfactant concentration for volume exclusion effects resulting from the presence of micellar aggregates. We also develop an improved method for determination of the cmc based on the maximum in curvature for the osmotic pressure curve determined from μVT simulations. Excellent agreement in cmc and other micellar properties between NVT and μVT simulations of different system sizes is observed. The methodological developments in this work are broadly applicable to simulations of aggregating systems using any type of surfactant model (atomistic/coarse grained) or solvent description (explicit/implicit)

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Development of a material property database on selected ceramic matrix composite materials

Ceramic Matrix Composites, with fiber/whisker/particulate reinforcement, possess the attractive properties of ceramics such as high melting temperature, high strength and stiffness at high temperature, low density, excellent environmental resistance, combined with improved toughness and mechanical reliability. These unique properties have made these composites an enabling technology for thermomechanically demanding applications in high temperature, high stress and aggressive environments. On a broader scale, CMC's are anticipated to be applicable in aircraft propulsion, space propulsion, power and structures, in addition to ground based applications. However, it is also true that for any serious commitment of the material toward any of the intended critical thermo-mechanical applications to materialize, vigorous research has to be conducted for a thorough understanding of the mechanical and thermal behavior of CMC's. The high technology of CMC'S is far from being mature. In view of this growing need for CMC data, researchers all over the world have found themselves drawn into the characterization of CMC's such as C/SiC, SiC/SiC, SiC/Al203, SiC/Glass, SiC/C, SiC/Blackglas. A significant amount of data has been generated by the industries, national laboratories and educational institutions in the United States of America. NASA/Marshall Space Flight Center intends to collect the 'pedigreed' CMC data and store those in a CMC database within MAPTIS (Materials and Processes Technical Information System). The task of compilation of the CMC database is a monumental one and requires efforts in various directions. The project started in the form of a summer faculty fellowship in 1994 and has spilled into the months that followed and into the summer faculty fellowship of 1995 and has the prospect of continuing into the future for a healthy growth, which of course depends to a large extent on how fast CMC data are generated. The 10-week long summer fellowship has concentrated, basically, on establishing the procedure for a smooth transfer of data into a CMC database on MAPTIS which is a vital part of the following broader picture of the project.

Mahanta, Kamala↗

Synthesis and characterization of carboxymethyl cellulose from office waste paper: A greener approach towards waste management

Highlights: • Carboxymethyl cellulose (CMC) was successfully prepared from waste paper. • CMC had maximum degree of substitution (DS) 1.07. • Rheological studies of CMC (DS, 1.07) showed non-Newtonian pseudoplastic behavior. • Characterization of CMC was done by FT-IR and NMR techniques. • Morphology of prepared CMC was studied by SEM. - Abstract: In the present study, functionalization of mixed office waste (MOW) paper has been carried out to synthesize carboxymethyl cellulose, a most widely used product for various applications. MOW was pulped and deinked prior to carboxymethylation. The deinked pulp yield was 80.62 ± 2.0% with 72.30 ± 1.50% deinkability factor. The deinked pulp was converted to CMC by alkalization followed by etherification using NaOH and ClCH{sub 2}COONa respectively, in an alcoholic medium. Maximum degree of substitution (DS) (1.07) of prepared CMC was achieved at 50 °C with 0.094 M and 0.108 M concentrations of NaOH and ClCH{sub 2}COONa respectively for 3 h reaction time. The rheological characteristics of 1–3% aqueous solution of optimized CMC product showed the non-Newtonian pseudoplastic behavior. Fourier transform infra red (FTIR), nuclear magnetic resonance (NMR) and scanning electron microscope (SEM) study were used to characterize the CMC product.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Evaluation of Ceramic Matrix Composite Technology for Aircraft Turbine Engine Applications

The goals of the NASA Environmentally Responsible Aviation (ERA) Project are to reduce the NO(x) emissions, fuel burn, and noise from turbine engines. In order to help meet these goals, commercially-produced ceramic matrix composite (CMC) components and environmental barrier coatings (EBCs) are being evaluated as parts and panels. The components include a CMC combustor liner, a CMC high pressure turbine vane, and a CMC exhaust nozzle as well as advanced EBCs that are tailored to the operating conditions of the CMC combustor and vane. The CMC combustor (w/EBC) could provide 2700 F temperature capability with less component cooling requirements to allow for more efficient combustion and reductions in NOx emissions. The CMC vane (w/EBC) will also have temperature capability up to 2700 F and allow for reduced fuel burn. The CMC mixer nozzle will offer reduced weight and improved mixing efficiency to provide reduced fuel burn. The main objectives are to evaluate the manufacturability of the complex-shaped components and to evaluate their performance under simulated engine operating conditions. Progress in CMC component fabrication, evaluation, and testing is presented in which the goal is to advance from the proof of concept validation (TRL 3) to a system/subsystem or prototype demonstration in a relevant environment (TRL 6).

Halbig, Michael C.↗

Fast patient-specific Monte Carlo brachytherapy dose calculations via the correlated sampling variance reduction technique

Purpose: To demonstrate potential of correlated sampling Monte Carlo (CMC) simulation to improve the calculation efficiency for permanent seed brachytherapy (PSB) implants without loss of accuracy. Methods: CMC was implemented within an in-house MC code family (PTRAN) and used to compute 3D dose distributions for two patient cases: a clinical PSB postimplant prostate CT imaging study and a simulated post lumpectomy breast PSB implant planned on a screening dedicated breast cone-beam CT patient exam. CMC tallies the dose difference, {Delta}D, between highly correlated histories in homogeneous and heterogeneous geometries. The heterogeneous geometry histories were derived from photon collisions sampled in a geometrically identical but purely homogeneous medium geometry, by altering their particle weights to correct for bias. The prostate case consisted of 78 Model-6711 {sup 125}I seeds. The breast case consisted of 87 Model-200 {sup 103}Pd seeds embedded around a simulated lumpectomy cavity. Systematic and random errors in CMC were unfolded using low-uncertainty uncorrelated MC (UMC) as the benchmark. CMC efficiency gains, relative to UMC, were computed for all voxels, and the mean was classified in regions that received minimum doses greater than 20%, 50%, and 90% of D{sub 90}, as well as for various anatomical regions. Results: Systematic errors in CMC relative to UMC were less than 0.6% for 99% of the voxels and 0.04% for 100% of the voxels for the prostate and breast cases, respectively. For a 1 x 1 x 1 mm{sup 3} dose grid, efficiency gains were realized in all structures with 38.1- and 59.8-fold average gains within the prostate and breast clinical target volumes (CTVs), respectively. Greater than 99% of the voxels within the prostate and breast CTVs experienced an efficiency gain. Additionally, it was shown that efficiency losses were confined to low dose regions while the largest gains were located where little difference exists between the homogeneous and heterogeneous doses. On an AMD 1090T processor, computing times of 38 and 21 sec were required to achieve an average statistical uncertainty of 2% within the prostate (1 x 1 x 1 mm{sup 3}) and breast (0.67 x 0.67 x 0.8 mm{sup 3}) CTVs, respectively. Conclusions: CMC supports an additional average 38-60 fold improvement in average efficiency relative to conventional uncorrelated MC techniques, although some voxels experience no gain or even efficiency losses. However, for the two investigated case studies, the maximum variance within clinically significant structures was always reduced (on average by a factor of 6) in the therapeutic dose range generally. CMC takes only seconds to produce an accurate, high-resolution, low-uncertainly dose distribution for the low-energy PSB implants investigated in this study.

61 RADIATION PROTECTION AND DOSIMETRY↗

Enabling Technologies for Ceramic Hot Section Components

Silicon-based ceramics are attractive materials for use in gas turbine engine hot sections due to their high temperature mechanical and physical properties as well as lower density than metals. The advantages of utilizing ceramic hot section components include weight reduction, and improved efficiency as well as enhanced power output and lower emissions as a result of reducing or eliminating cooling. Potential gas turbine ceramic components for industrial, commercial and/or military high temperature turbine applications include combustor liners, vanes, rotors, and shrouds. These components require materials that can withstand high temperatures and pressures for long duration under steam-rich environments. For Navy applications, ceramic hot section components have the potential to increase the operation range. The amount of weight reduced by utilizing a lighter gas turbine can be used to increase fuel storage capacity while a more efficient gas turbine consumes less fuel. Both improvements enable a longer operation range for Navy ships and aircraft. Ceramic hot section components will also be beneficial to the Navy's Growth Joint Strike Fighter (JSF) and VAATE (Versatile Affordable Advanced Turbine Engines) initiatives in terms of reduced weight, cooling air savings, and capability/cost index (CCI). For DOE applications, ceramic hot section components provide an avenue to achieve low emissions while improving efficiency. Combustors made of ceramic material can withstand higher wall temperatures and require less cooling air. Ability of the ceramics to withstand high temperatures enables novel combustor designs that have reduced NO{sub x}, smoke and CO levels. In the turbine section, ceramic vanes and blades do not require sophisticated cooling schemes currently used for metal components. The saved cooling air could be used to further improve efficiency and power output. The objectives of this contract were to develop technologies critical for ceramic hot section components for gas turbine engines. Significant technical progress has been made towards maturation of the EBC and CMC technologies for incorporation into gas turbine engine hot-section. Promising EBC candidates for longer life and/or higher temperature applications relative to current state of the art BSAS-based EBCs have been identified. These next generation coating systems have been scaled-up from coupons to components and are currently being field tested in Solar Centaur 50S engine. CMC combustor liners were designed, fabricated and tested in a FT8 sector rig to demonstrate the benefits of a high temperature material system. Pretest predictions made through the use of perfectly stirred reactor models showed a 2-3x benefit in CO emissions for CMC versus metallic liners. The sector-rig test validated the pretest predictions with >2x benefit in CO at the same NOx levels at various load conditions. The CMC liners also survived several trip shut downs thereby validating the CMC design methodology. Significant technical progress has been made towards incorporation of ceramic matrix composites (CMC) and environmental barrier coatings (EBC) technologies into gas turbine engine hot-section. The second phase of the program focused on the demonstration of a reverse flow annular CMC combustor. This has included overcoming the challenges of design and fabrication of CMCs into 'complex' shapes; developing processing to apply EBCs to 'engine hardware'; testing of an advanced combustor enabled by CMCs in a PW206 rig; and the validation of performance benefits against a metal baseline. The rig test validated many of the pretest predictions with a 40-50% reduction in pattern factor compared to the baseline and reductions in NOx levels at maximum power conditions. The next steps are to develop an understanding of the life limiting mechanisms in EBC and CMC materials, developing a design system for EBC coated CMCs and durability testing in an engine environment.

33 ADVANCED PROPULSION SYSTEMS↗

Factors Controlling Stress Rupture of Fiber-Reinforced Ceramic Composites

The successful application of fiber-reinforced ceramic matrix composites (CMC) depends strongly on maximizing material rupture life over a wide range of temperatures and applied stresses. The objective of this paper is to examine the various intrinsic and extrinsic factors that control the high-temperature stress rupture of CMC for stresses below and above those required for cracking of the 0 C plies (Regions I and II, respectively). Using creep-rupture results for a variety of ceramic fibers and rupture data for CMC reinforced by these fibers, it is shown that in those cases where the matrix carries little structural load, CMC rupture conditions can be predicted very well from the fiber behavior measured under the appropriate test environment. As such, one can then examine the intrinsic characteristics of the fibers in order to develop design guidelines for selecting fibers and fiber microstructures in order to maximize CMC rupture life. For those cases where the fiber interfacial coatings are unstable in the test environment, CMC lives are generally worse than those predicted by fiber behavior alone. For those cases where the matrix can support structural load, CMC life can even be greater provided matrix creep behavior is properly controlled. Thus the achievement of long CMC rupture life requires understanding and optimizing the behavior of all constituents in the proper manner.

DiCarlo, J. A.↗

Goals and Progress for Mil Handbook 17, Vol. 5 on Ceramic Matrix Composites: Testing and Characterization

The initial edition of the Mil Handbook 17, Vol. 5 on ceramic matrix composites (CMCs) was recently published. Part C of this CMC volume describes procedures for characterization of the thermal, physical, and mechanical properties of CMCs and subsequent data analysis procedures. As is the case for entire CMC volume, this chapter is a "work in progress" with sections on recommended test plans and matrices, data reduction, and test methods. This presentation will describe the current status in development of this section of the CMC volume and will highlight examples of critical issues that will be addressed in this volume. CMC systems are a different class of material than metals or polymer matrix composite with different mechanical response and failure modes, design rules, test methods, and characterization techniques. The CMC test protocols need to include guidance on how to generate enough reliable data in order to estimate, with reasonable confidence, the lower bounds of performance properties, such as strength and life. Strength data sets on two material systems, C/SiC and Nicalon/SiNC, and a creep rupture data set on C/SiC, will be presented to highlight this issue. The structural properties of CMC parts can sometimes be significantly different than those obtained from flat panels because of changes in fiber architecture often required to make shapes and spatial and lot-to-lot variations in processing conditions. To illustrate an example, the hoop tensile properties of SiC/SiC cylinders will be compared to properties obtained from flat panels fabricated from the same composites. These CMC testing-design issues are being defined and documented in the Mil Handbook 17 CMC volume.

Verrilli, Michael J.↗

Influence of Carboxymethyl Cellulose as a Thickening Agent for Glauber’s Salt-Based Low Temperature PCM

This work is focused on a novel, promising low temperature phase change material (PCM), based on the eutectic Glauber’s salt composition. To allow phase transition within the refrigeration range of temperatures of +5 °C to +12 °C, combined with a high repeatability of melting–freezing processes, and minimized subcooling, the application of three variants of sodium carboxymethyl cellulose (Na-CMC) with distinct molecular weights (700,000, 250,000, and 90,000) is considered. The primary objective is to optimize the stabilization of this eutectic PCM formulation, while maintaining the desired enthalpy level. Preparation methods are refined to ensure repeatability in mixing components, thereby optimizing performance and stability. Additionally, the influence of Na-CMC molecular weight on stabilization is examined through differential scanning calorimetry (DSC), T-history, and rheology tests. The PCM formulation of interest builds upon prior research in which borax, ammonium chloride, and potassium chloride were used as additives to sodium sulfate decahydrate (Glauber’s salt), prioritizing environmentally responsible materials. The results reveal that CMC with molecular weights of 250 kg/mol and 90 kg/mol effectively stabilize the PCM without phase separation issues, slowing crystallization kinetics. Conversely, CMC of 700 kg/mol proved ineffective due to the disruption of gel formation at its low gel point, hindering higher concentrations. Calculations of ionic concentration indicate higher Na ion content in PCM stabilized with 90 kg/mol CMC, suggesting increased ionic interactions and gel strength. A tradeoff is discovered between the faster crystallization in lower molecular weight CMC and the higher concentration required, which increases the amount of inert material that does not participate in the phase transition. After thermal cycling, the best formulation had a latent heat of 130 J/g with no supercooling, demonstrating excellent performance. This work advances PCM’s reliability as a thermal energy storage solution for diverse applications and highlights the complex relationship between Na-CMC molecular weight and PCM stabilization.

25 ENERGY STORAGE↗

Adsorption of rare earth elements in carboxylated mesoporous carbon

The separation of Rare Earth Elements (REEs) from various non-conventional sources is critically important to maintain the supply–demand balance of REEs in the western world. Here, in this research, we have investigated coal Fly Ash (CFA) as the non-conventional source of REEs. In order to recover REEs, we have synthesized carboxylate-functionalized mesoporous carbon (CMC) to harness the chelation-induced adsorption of REEs. These adsorbents were characterized with pore textural properties, FTIR spectroscopy, and SEM-EDX mapping. In the initial study with single-component La(III) Dy(III) and Lu(III), it was revealed that CMC can adsorb those REEs 2–4 times more than that of pristine mesoporous carbon confirming the effective role of the carboxylate group in the REE separation. Furthermore, the affiliation of the carboxylate group towards heavier REEs (Lu>Dy>La, when present is equal amounts) provides an added benefit of this adsorbent owing to the high demand for heavier REEs in the technology sectors. The leachate solution produced from CFA contained sixteen REEs in the range of 50–200 ppb for most of the REEs. It was revealed that CMC can extract 80–90% of all the REEs thereby further confirming the success of the CMC as an effective REE sorbent. Three successive cycles of adsorption and desorption of REEs with the same CMC revealed the consistent adsorption capacity of REEs. In-situ X-ray Absorption Near Edge Spectroscopy (XANES) analysis confirmed the +3 oxidation states of La, Dy, and Lu within CMC. In-situ Extended X-ray Absorption Fine Structure (EXAFS) analysis revealed the shortening of mean La-O, Dy-O, and Lu-O bond distance by 0.03–0.05 Å thereby confirming the coordination of these REEs with carboxylate groups present on CMC.

36 MATERIALS SCIENCE↗

Cast Metals Coalition Technology Transfer and Program Management Final Report

The Cast Metals Coalition (CMC) partnership program was funded to ensure that the results of the Department of Energy's (DOE) metalcasting research and development (R&D) projects are successfully deployed into industry. Specifically, the CMC program coordinated the transfer and deployment of energy saving technologies and process improvements developed under separately funded DOE programs and projects into industry. The transition of these technologies and process improvements is a critical step in the path to realizing actual energy savings. At full deployment, DOE funded metalcasting R&D results are projected to save 55% of the energy used by the industry in 1998. This closely aligns with DOE's current goal of driving a 25% reduction in industrial energy intensity by 2017. In addition to benefiting DOE, these energy savings provide metalcasters with a significant economic advantage. Deployment of already completed R&D project results and those still underway is estimated to return over 500% of the original DOE and industry investment. Energy savings estimates through December 2008 from the Energy-Saving Melting and Revert Reduction Technology (E-SMARRT) portfolio of projects alone are 12 x 1012 BTUs, with a projection of over 50 x 1012 BTUs ten years after program completion. These energy savings and process improvements have been made possible through the unique collaborative structure of the CMC partnership. The CMC team consists of DOE's Office of Industrial Technology, the three leading metalcasting technical societies in the U.S: the American Foundry Society; the North American Die Casting Association; and the Steel Founders Society of America; and the Advanced Technology Institute (ATI), a recognized leader in distributed technology management. CMC provides collaborative leadership to a complex industry composed of approximately 2,100 companies, 80% of which employ less than 100 people, and only 4% of which employ more than 250 people. Without collaboration, new technologies enabling energy efficiencies and environment-friendly improvements are slow to develop, and have trouble obtaining a broad application. The CMC team was able to effectively and efficiently transfer the results of DOE's metalcasting R&D projects to industry by utilizing and delivering the numerous communication vehicles identified in the proposal. The three metalcasting technical associations achieved significant technology transition results under this program. In addition to reaching over 23,000 people per year through Modern Casting and 28,000 through Engineered Casting Solutions, AFS had 84 national publications and reached over 1,200 people annually through Cast Metals Institute (CMI) education courses. NADCA's education department reached over 1,000 people each year through their courses, in addition to reaching over 6,000 people annually through Die Casting Engineer, and publishing 58 papers. The SFSA also published 99 research papers and reached over 1,000 people annually through their member newsletters. In addition to these communication vehicles, the CMC team conducted numerous technical committee meetings, project reviews, and onsite visits. All of these efforts to distribute the latest metalcasting technologies contributed to the successful deployment of DOE's R&D projects into industry. The DOE/CMC partnership demonstrated significant success in the identification and review of relevant and easy-to-implement metalcasting energy-saving processes and technologies so that the results are quickly implemented and become general practice. The results achieved in this program demonstrate that sustained technology transfer efforts are a critical step in the deployment of R&D projects to industry.

36 MATERIALS SCIENCE↗

Self-degradable Cementitious Sealing Materials

A self-degradable alkali-activated cementitious material consisting of a sodium silicate activator, slag, Class C fly ash, and sodium carboxymethyl cellulose (CMC) additive was formulated as one dry mix component, and we evaluated its potential in laboratory for use as a temporary sealing material for Enhanced Geothermal System (EGS) wells. The self-degradation of alkali-activated cementitious material (AACM) occurred, when AACM heated at temperatures of {ge}200 C came in contact with water. We interpreted the mechanism of this water-initiated self-degradation as resulting from the in-situ exothermic reactions between the reactants yielded from the dissolution of the non-reacted or partially reacted sodium silicate activator and the thermal degradation of the CMC. The magnitude of self-degradation depended on the CMC content; its effective content in promoting degradation was {ge}0.7%. In contrast, no self-degradation was observed from CMC-modified Class G well cement. For 200 C-autoclaved AACMs without CMC, followed by heating at temperatures up to 300 C, they had a compressive strength ranging from 5982 to 4945 psi, which is {approx}3.5-fold higher than that of the commercial Class G well cement; the initial- and final-setting times of this AACM slurry at 85 C were {approx}60 and {approx}90 min. Two well-formed crystalline hydration phases, 1.1 nm tobermorite and calcium silicate hydrate (I), were responsible for developing this excellent high compressive strength. Although CMC is an attractive, as a degradation-promoting additive, its addition to both the AACM and the Class G well cement altered some properties of original cementitious materials; among those were an extending their setting times, an increasing their porosity, and lowering their compressive strength. Nevertheless, a 0.7% CMC-modified AACM as self-degradable cementitious material displayed the following properties before its breakdown by water; {approx}120 min initial- and {approx}180 min final-setting times at 85 C, and 1825 to 1375 psi compressive strength with 51.2 to 55.0% porosity up to 300 C.

15 GEOTHERMAL ENERGY↗

Factors Affecting Fiber Design and Selection for Advanced Ceramic Composites

Structural Ceramic Matrix Composites (CMC) have the potential for application in the hot sections of a variety of advanced propulsion and power systems. It is therefore necessary to have a general understanding of the key properties of CMC and Reinforcing Fibers. This need is complicated by the wide variety of application conditions and structural requirements for which CMC's will be used, and the proprietary concerns of the design engineers. CMC's, to be successful, must display properties which are competitive with the currently used high temperature structural materials: (i.e., Iron and Nickel based superalloys, tough monolithic ceramics, and carbon/carbon composites.) Structural CMC offers several areas of competition: (1) performance, (i.e., strength and strength retention, creep resistance, and thermal conductivity), (2) reliability (i.e., environmental durability, and damage tolerance) and (3) processing (i.e., capability for varying sizes and shapes, and cost effective fabrication). The presentation further discusses, and illustrates with fiber and CMC data the key fiber properties and processes which strongly affect each CMC area of competition. The presentation further discusses the current knowledge of the important factors which control the key fiber properties. A design guidelines for the optimum fiber characteristics is developed, and the currently available fibers are compared against those guidelines.

DiCarlo, James A.↗

Large thermal protection system panel

A protective panel for a reusable launch vehicle provides enhanced moisture protection, simplified maintenance, and increased temperature resistance. The protective panel includes an outer ceramic matrix composite (CMC) panel, and an insulative bag assembly coupled to the outer CMC panel for isolating the launch vehicle from elevated temperatures and moisture. A standoff attachment system attaches the outer CMC panel and the bag assembly to the primary structure of the launch vehicle. The insulative bag assembly includes a foil bag having a first opening shrink fitted to the outer CMC panel such that the first opening and the outer CMC panel form a water tight seal at temperatures below a desired temperature threshold. Fibrous insulation is contained within the foil bag for protecting the launch vehicle from elevated temperatures. The insulative bag assembly further includes a back panel coupled to a second opening of the foil bag such that the fibrous insulation is encapsulated by the back panel, the foil bag, and the outer CMC panel. The use of a CMC material for the outer panel in conjunction with the insulative bag assembly eliminates the need for waterproofing processes, and ultimately allows for more efficient reentry profiles.

Myers, Franklin K.↗

Post Test Evaluation of HSCT Nozzle Acoustic Liner Subcomponents Subjected to a Hot Acoustic Durability Test

The acoustic liner system designed for use in the High Speed Civil Transport (HSCT) was tested in a thermal-acoustic environment. Five ceramic matrix composite (CMC) acoustic tile configurations, five bulk acoustic absorbers, and one thermal protection system design were tested. The CMC acoustic tiles were subjected to two 2 3/4 hr ambient temperature acoustic exposures to measure their dynamic response. One exposure was conducted on the tiles alone and the second exposure included the tiles and the T-foam bulk absorber. The measured tile RMS strains were small. With or without the T-foam absorber, the dynamic strains were below strain levels that would cause damage during fatigue loading. After the ambient exposure, a 75-hr durability test of the entire acoustic liner system was conducted using a thermal-acoustic cycle that approximated the anticipated service cycle. Acoustic loads up to 139 dB/Hz and temperatures up to 1670 F (910 C) were employed during this 60 cycle test. During the durability test, the CMC tiles were exposed to temperatures up to 1780 F and a transient through thickness gradient up to 490 F. The TPS peak temperatures on the hot side of the panels ranged from 750 to 1000 F during the 60 cycles. The through thickness delta T ranged from 450 to 650 F, varying with TPS location and cycle number. No damage, such as cracks or chipping, was observed in the CMC tiles after completion of the testing. However, on tile warped during the durability test and was replaced after 43 or 60 cycles. No externally observed damage was found in this tile. No failure of the CMC fasteners occurred, but damage was observed. Cracks and missing material occurred, only in the fastener head region. No indication of damage was observed in the T-foam acoustic absorbers. The SiC foam acoustic absorber experienced damage after about 43 cycles. Cracking in the TPS occurred around the attachment holes and under a vent. In spite of the development of damage, the TPS maintained its insulative capability throughout the durability test. The durability test results demonstrate damage-tolerant CMC tile, CMC fastener, TPS, and T-foam absorber designs for the combined thermal and acoustic engine nozzle environment.

Verrilli, Michael J.↗