Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Bonding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Adhesive Bonding Characterization of Composite Joints for Cryogenic Usage

The development of polymer composite cryogenic tanks is a critical step in creating the next generation of launch vehicles. Future reusable launch vehicles need to minimize the gross liftoff weight (GLOW). This weight reduction is possible due to the large reduction in weight that composite materials can provide over current aluminum technology. In addition to composite technology, adhesively bonded joints potentially have several benefits over mechanically fastened joints, such as weight savings and cryogenic fluid containment. Adhesively bonded joints may be used in several areas of these cryogenic tanks, such as in lobe-to-lobe joints (in a multi-lobe concept), skirt-to-tank joint, strut-to-tank joint, and for attaching stringers and ring frames. The bonds, and the tanks themselves, must be able to withstand liquid cryogenic fuel temperatures that they contain. However, the use of adhesively bonded composite joints at liquid oxygen and hydrogen temperatures is largely unknown and must be characterized. Lockheed Martin Space Systems Company, Michoud Operations performed coupon-level tests to determine effects of material selection, cure process parameters, substrate surface preparation, and other factors on the strength of these composite joints at cryogenic temperatures. This led to the selection of a material and process that would be suitable for a cryogenic tank. KEY WORDS: Composites, Adhesive Bonding, Cryogenics

Graf, Neil A.↗

Wood Bond Testing

A joint development program between Hartford Steam Boiler Inspection Technologies and The Weyerhaeuser Company resulted in an internal bond analyzer (IBA), a device which combines ultrasonics with acoustic emission testing techniques. It is actually a spinoff from a spinoff, stemming from a NASA Lewis invented acousto-ultrasonic technique that became a system for testing bond strength of composite materials. Hartford's parent company, Acoustic Emission Technology Corporation (AET) refined and commercialized the technology. The IBA builds on the original system and incorporates on-line process control systems. The IBA determines bond strength by measuring changes in pulsar ultrasonic waves injected into a board. Analysis of the wave determines the average internal bond strength for the panel. Results are displayed immediately. Using the system, a mill operator can adjust resin/wood proportion, reduce setup time and waste, produce internal bonds of a consistent quality and automatically mark deficient products.

Source record↗

Shearography for Non-destructive Inspection with applications to BAT Mask Tile Adhesive Bonding and Specular Surface Honeycomb Panels

The applicability of shearography techniques for non-destructive evaluation in two unique application areas is examined. In the first application, shearography is used to evaluate the quality of adhesive bonds holding lead tiles to the B.4T gamma ray mask for the NASA Swift program. Using a vibration excitation, the more poorly bonded tiles are readily identifiable in the shearography image. A quantitative analysis is presented that compares the shearography results with a destructive pull test measuring the force at bond failure. The second application is to evaluate the bonding between the skin and core of a honeycomb structure with a specular (mirror-like) surface. In standard shearography techniques, the object under test must have a diffuse surface to generate the speckle patterns in laser light, which are then sheared. A novel configuration using the specular surface as a mirror to image speckles from a diffuser is presented, opening up the use of shearography to a new class of objects that could not have been examined with the traditional approach. This new technique readily identifies large scale bond failures in the panel, demonstrating the validity of this approach.

Lysak, Daniel B.↗

Shearography for Non-Destructive Evaluation with Applications to BAT Mask Tile Adhesive Bonding and Specular Surface Honeycomb Panels

In this report we examine the applicability of shearography techniques for nondestructive inspection and evaluation in two unique application areas. In the first application, shearography is used to evaluate the quality of adhesive bonds holding lead tiles to the BAT gamma ray mask for the NASA Swift program. By exciting the mask with a vibration, the more poorly bonded tiles can be distinguished by their greater displacement response, which is readily identifiable in the shearography image. A quantitative analysis is presented that compares the shearography results with a destructive pull test measuring the force at bond failure. Generally speaking, the results show good agreement. Further investigation would be useful to optimize certain test parameters such as vibration frequency and amplitude. The second application is to evaluate the bonding between the skin and core of a honeycomb structure with a specular (mirror-like) surface. In standard shearography techniques, the object under test must have a diffuse surface to generate the speckle patterns in laser light, which are then sheared. A novel configuration using the specular surface as a mirror to image speckles from a diffuser is presented, opening up the use of shearography to a new class of objects that could not have been examined with the traditional approach. This new technique readily identifies large scale bond failures in the panel, demonstrating the validity of this approach. For the particular panel examined here, some scaling issues should be examined further to resolve the measurement scale down to the very small size of the core cells. In addition, further development should be undertaken to determine the general applicability of the new approach and to establish a firm quantitative foundation.

Lysak, Daniel B.↗

Effect of Environments on Degradation of Molding Compound and Wire Bonds in PEMs

Degradation of wire bonds (WBs) is one of the major factors limiting reliability of plastic encapsulated microcircuits (PEMs) at high temperatures. Use of PEMs in military and aerospace applications requires extended and thorough evaluation of encapsulating materials and reliability of packages in harsh environments. However, the effect of environmental conditions on characteristics of molding compounds (MCs) and reliability of wire bonds has not been studied sufficiently to date. In this work, two types of PEMs in QFP-style packages have been stored in different environments at temperatures from 130 C to 225 C for up to 4,500 hours in some cases. To assess the effect of oxygen, the parts were aged at 198 C in air and vacuum chambers. The effect of humidity was evaluated during long-term highly accelerated temperature and humidity stress testing (HAST) at temperatures of 130 C and 150 C. Thermo-mechanical and thermo-gravimetrical analyses were used to evaluate the effect of environment on characteristics of molding compound used. Measurements of contact resistances of wire bonds and their mechanical strength were employed to monitor degradation of wire bonds throughout the testing. Correlation between degradation of MC and WB failures has been analyzed. The effect of environmental conditions on accelerating factors of WB failures has been assessed, and the mechanism of wire bond degradation due to the presence of moisture and oxygen is discussed.

Teverosky, Alexander↗

Diffusion Bonding of Silicon Carbide for MEMS-LDI Applications

A robust joining approach is critically needed for a Micro-Electro-Mechanical Systems-Lean Direct Injector (MEMS-LDI) application which requires leak free joints with high temperature mechanical capability. Diffusion bonding is well suited for the MEMS-LDI application. Diffusion bonds were fabricated using titanium interlayers between silicon carbide substrates during hot pressing. The interlayers consisted of either alloyed titanium foil or physically vapor deposited (PVD) titanium coatings. Microscopy shows that well adhered, crack free diffusion bonds are formed under optimal conditions. Under less than optimal conditions, microcracks are present in the bond layer due to the formation of intermetallic phases. Electron microprobe analysis was used to identify the reaction formed phases in the diffusion bond. Various compatibility issues among the phases in the interlayer and substrate are discussed. Also, the effects of temperature, pressure, time, silicon carbide substrate type, and type of titanium interlayer and thickness on the microstructure and composition of joints are discussed.

Halbig, Michael C.↗

Development and Characterization of the Bonding and Integration Technologies Needed for Fabricating Silicon Carbide Based Injector Components

Advanced ceramic bonding and integration technologies play a critical role in the fabrication and application of silicon carbide based components for a number of aerospace and ground based applications. One such application is a lean direct injector for a turbine engine to achieve low NOx emissions. Ceramic to ceramic diffusion bonding and ceramic to metal brazing technologies are being developed for this injector application. For the diffusion bonding technology, titanium interlayers (coatings and foils) were used to aid in the joining of silicon carbide (SiC) substrates. The influence of such variables as surface finish, interlayer thickness, and processing time were investigated. Electron microprobe analysis was used to identify the reaction formed phases. In the diffusion bonds, an intermediate phase, Ti5Si3Cx, formed that is thermally incompatible in its thermal expansion and caused thermal stresses and cracking during the processing cool-down. Thinner interlayers of pure titanium and/or longer processing times resulted in an optimized microstructure. Tensile tests on the joined materials resulted in strengths of 13-28 MPa depending on the SiC substrate material. Nondestructive evaluation using ultrasonic immersion showed well formed bonds. For the joining technology of brazing Kovar fuel tubes to silicon carbide, preliminary development of the joining approach has begun. Various technical issues and requirements for the injector application are addressed.

Halbig,Michael C.↗

Shape Bonding method

The present invention is directed to a method of bonding at least two surfaces together. The methods step of the present invention include applying a strip of adhesive to a first surface along a predefined outer boundary of a bond area and thereby defining a remaining open area there within. A second surface, or gusset plate, is affixed onto the adhesive before the adhesive cures. The strip of adhesive is allowed to cure and then a second amount of adhesive is applied to cover the remaining open area and substantially fill a void between said first and second surfaces about said bond area. A stencil may be used to precisely apply the strip of adhesive. When the strip cures, it acts as a dam to prevent overflow of the subsequent application of adhesive to undesired areas. The method results in a precise bond area free of undesired shapes and of a preferred profile which eliminate the drawbacks of the prior art bonds.

Pontius, James T.↗

Bonding Thin Mirror Segments Without Distortion for the International X-Ray Observatory

The International X-Ray Observatory (IXO) uses thin glass optics to maximize large effective area and precise low angular resolution. The thin glass mirror segments must be transferred from their fabricated state to a permanent structure without imparting distortion. IXO will incorporate about fourteen thousand thin mirror segments to achieve the mission goal of 3.0 square meters of effective area at 1.25 keV with an angular resolution of five arcseconds. To preserve figure and alignment, the mirror segment must be bonded with sub-micron movement at each corner. Recent advances in technology development have produced significant x-ray test results of a bonded pair of mirrors. Three specific bonding cycles will be described highlighting the improvements in procedure, temperature control, and precision bonding. This paper will highlight the recent advances in alignment and permanent bonding as well as the results they have produced.

Evans, Tyler C.↗

Quasi-Monolithic Structures for Spaceflight Using Hydroxide-Catalysis Bonding

Future space-based missions will take measurements of the universe with unprecedented results. To do this, these missions will require materials and bonding techniques with ever-increasing stability in order to make their measurements. As an example, the Laser Interferometer Space Antenna (LISA) will detect and observe gravitational waves in the 0.1 mHz to 1 Hz frequency range with strain sensitivities on the order of 10(exp -21) at its most sensitive frequency. To make these measurements, critical components such as the optical bench or telescope support structure, will need to have path-length stabilities of better than 1 pm/(square root)Hz. The baseline construction method for the LISA optical bench is to affix fused silica optical components to a Zerodur baseplate using hydroxide-catalysis bonding (HCB). HCB is a recently developed technique that allows the bonding of glasses, some metals, and silicon carbide with significant strength and stability with a bond thickness of less than a few micrometers. In addition, a wide range of surface profiles can be bonded using only a small amount of hydroxide solution. These characteristics make HCB ideal for adhering optical components in complex optical systems. In addition to being used to construct the LISA optical bench, the HCB technique shows great promise for constructing other structures such as hollow retroreflectors to be used for lunar laser ranging, or a visible nulling coronograph to be used for exo-planet detection. Here we present construction techniques that could be used to make an optical bench, hollow retroreflector, nulling coronograph, or other quasi-monolithic structures using HCB. In addition, we present dimensional stability results of an optical bench that was made using HCB, as well as HCB strength measurements.

Preston, Alix↗

Supersonic Retropulsion Surface Preparation of Carbon Fiber Reinforced Epoxy Composites for Adhesive Bonding

Surface preparation is widely recognized as a key step to producing robust and predictable bonds in a precise and reproducible manner. Standard surface preparation techniques, including grit blasting, manual abrasion, and peel ply, can lack precision and reproducibility, which can lead to variation in surface properties and subsequent bonding performance. The use of a laser to ablate composite surface resin can provide an efficient, precise, and reproducible means of preparing composite surfaces for adhesive bonding. Advantages include elimination of physical waste (i.e., grit media and sacrificial peel ply layers that ultimately require disposal), reduction in process variability due to increased precision (e.g. increased reproducibility), and automation of surface preparation, all of which improve reliability and process control. This paper describes a Nd:YAG laser surface preparation technique for composite substrates and the mechanical performance and failure modes of bonded laminates thus prepared. Additionally, bonded specimens were aged in a hot, wet environment for approximately one year and subsequently mechanically tested. The results of a one year hygrothermal aging study will be presented.

Palmieri, Frank L.↗

James Webb Space Telescope (JWST) Integrated Science Instruments Module (ISIM) Electronics Compartment (IEC) Conformal Shields Composite Bond Structure Qualification Test Method

The JWST IEC conformal shields are mounted onto a composite frame structure that must undergo qualification testing to satisfy mission assurance requirements. The composite frame segments are bonded together at the joints using epoxy, EA 9394. The development of a test method to verify the integrity of the bonded structure at its operating environment introduces challenges in terms of requirements definition and the attainment of success criteria. Even though protoflight thermal requirements were not achieved, the first attempt in exposing the structure to cryogenic operating conditions in a thermal vacuum environment resulted in approximately 1 bonded joints failure during mechanical pull tests performed at 1.25 times the flight loads. Failure analysis concluded that the failure mode was due to adhesive cracks that formed and propagated along stress concentrated fillets as a result of poor bond squeeze-out control during fabrication. Bond repairs were made and the structures successfully re-tested with an improved LN2 immersion test method to achieve protoflight thermal requirements.

Thermal Vacuum Testing Chamber↗

Laser Surface Preparation of Epoxy Composites for Secondary Bonding: Optimization of Ablation Depth

Surface preparation has been identified as one of the most critical aspects of attaining predictable and reliable adhesive bonds. Energetic processes such as laser ablation or plasma treatment are amenable to automation and are easily monitored and adjusted for controlled surface preparation. A laser ablation process was developed to accurately remove a targeted depth of resin, approximately 0.1 to 20 micrometers, from a carbon fiber reinforced epoxy composite surface while simultaneously changing surface chemistry and creating micro-roughness. This work demonstrates the application of this process to prepare composite surfaces for bonding without exposing or damaging fibers on the surface. Composite panels were prepared in an autoclave and had a resin layer approximately 10 micrometers thick above the fiber reinforcement. These composite panels were laser surface treated using several conditions, fabricated into bonded panels and hygrothermally aged. Bond performance of aged, experimental specimens was compared with grit blast surface treated specimens using a modified double cantilever beam test that enabled accelerated saturation of the specimen with water. Comparison of bonded specimens will be used to determine how ablation depth may affect average fracture energies and failure modes.

Palmieri, Frank L.↗

TEM Analysis of Diffusion-Bonded Silicon Carbide Ceramics Joined Using Metallic Interlayers

SiC fiber-bonded ceramics (SA-Tyrannohex: SA-THX) diffusion-bonded with TiCu metallic interlayers were investigated. Thin samples of the ceramics were prepared with a focused ion beam (FIB) and the interfacial microstructure of the prepared samples was studied by transmission electron microscopy (TEM) and scanning TEM (STEM). In addition to conventional microstructure observation, for detailed analysis of reaction compounds in diffusion-bonded area, we performed STEM-EDS measurements and selected area electron diffraction (SAD) experiments. The TEM and STEM experiments revealed the diffusion-bonded area was composed of only one reaction layer, which was characterized by TiC precipitates in Cu-Si compound matrix. This reaction layer was in good contact with the SA-THX substrates, and it is concluded that the joint structure led to the excellent bonding strength.

Ceramics↗

Alignment and Bonding of Silicon Mirrors for High-Resolution X-Ray Optics

How to align and bond sub-arc second silicon mirrors? (1) Description of the alignment and bonding process. (2) Technical challenges and advances in aligning and bonding precise silicon mirrors. (a) Precise mirror placement (b) Measurement of focusing (c) Method of spacer adjustment (d) Bonding distortion and displacement (e) Co-alignment and bonding of subsequent mirrors.

Chan, Kai-Wing↗

Reliability improvement of 1 mil aluminum wire bonds for semiconductors, technical performance summary

The reliability of semiconductor devices as influenced by the reliability of wire bonds used in the assembly of the devices is investigated. The specific type of failure dealt with involves fracture of wire bonds as a result of repeated flexure of the wire at the heel of the bond when the devices are operated in an on-off mode. The mechanism of failure is one of induced fracture of the wire. To improve the reliability of a chosen transistor, one-mil diameter wires of aluminum with various alloy additions were studied using an accelerated fatigue testing machine. In addition, the electroprobe was used to study the metallurgy of the wires as to microstructure and kinetics of the growth of insoluble phases. Thermocompression and ultrasonic bonding techniques were also investigated.

Source record↗

Non-classical adhesive-bonded joints in practical aerospace construction

Solutions are derived for adhesive-bonded joints of non-classical geometries. Particular attention is given to bonded doublers and to selective reinforcement by unidirectional composites. Non-dimensionalized charts are presented for the efficiency limit imposed on the skin as the result of the eccentricity in the load path through the doubler. It is desirable to employ a relativly large doubler to minimize the effective eccentricity in the load path. The transfer stresses associated with selective reinforcement of metal structures by advanced composites are analyzed. Reinforcement of bolt holes in composites by bonded metal doublers is covered quantitatively. Also included is the adhesive joint analysis for shear flow in a multi-cell torque box, in which the bond on one angle becomes more critical sooner than those on the others, thereby restricting the strength to less than the total of each maximum strength when acting alone. Adhesive plasticity and adherend stiffness and thermal imbalances are included. A simple analysis/design technique of solution in terms of upper and lower bounds on an all-plastic adhesive analysis is introduced.

Hart-Smith, L. J.↗

Polyimide weld bonding for titanium alloy joints

Two weld bonding processes were developed for joining titanium alloy; one process utilizes a weld-through technique and the other a capillary-flow technique. The adhesive used for the weld-through process is similar to the P4/A5F system. A new polyimide laminating resin, BFBI/BMPM, was used in the capillary-flow process. Static property information was generated for weld-bonded joints over the temperature range of 219 K (-65 F) to 561 K (+550 F) and fatigue strength information was generated at room temperature. Significant improvement in fatigue strength was demonstrated for weld-bonded joints over spot-welded joints. A demonstration was made of the applicability of the weld-through weld-bonding process for fabricating stringer stiffened skin panels.

Vaughan, R. W.↗