The comparison of microstructures and mechanical properties between 14Cr-Al and 14Cr-Ti ferritic ODS alloys

In this study, two kinds of 14Cr ODS alloys (14Cr-Al and 14Cr-Ti) were investigated to reveal the different effects between Al and Ti on the microstructures and mechanical properties of 14Cr ferritic ODS alloys. The microstructure information such as grains, minor phases of these two alloys has been investigated by high-energy X-ray diffraction and transmission electron microscopy (TEM). The in situ synchrotron X-ray diffraction tensile test was applied to investigate the mechanical properties of these two alloys. The lattice strains of different phases through the entire tensile deformation process in these two alloys were analyzed to calculate their elastic stresses. From the comparison of elastic stress, the strengthening capability of Y 2 Ti 2 O 7 is better than TiN in 14Cr-Ti, and the strengthening capability of YAH is much better than YAM and AlN in 14Cr-Al ODS. The dislocation densities of 14Cr-Ti and 14Cr-Al ODS alloys during tensile deformation were also examined by modified Williamson-Hall analyses of peak broadening, respectively. In conclusion, the different increasing speed of dislocation density with plastic deformation reveals the better strengthening effect of Y-Ti-O particles in 14Cr-Ti ODS than that of Y-Al-O particles in 14Cr-Al ODS alloy.

36 MATERIALS SCIENCE↗

Microstructural characterization of amorphous and nanocrystalline boron nitride prepared by high-energy ball milling

Microstructural parameters like crystallite size, lattice strain, stacking faults and dislocation density were evaluated from the X-ray diffraction data of boron nitride (BN) powder milled in a high-energy vibrational ball mill for different length of time (2-120 h), using different model based approaches like Scherrer analysis, integral breadth method, Williamson-Hall technique and modified Rietveld technique. From diffraction line-broadening analysis of the successive patterns of BN with varying milling time, it was observed that overall line broadening was an operative cause for crystallite size reduction at lower milling time ({approx}5 h), whereas lattice strains were the prominent cause of line broadening at higher milling times (>19 h). For intermediate milling time (7-19 h), both crystallite size and lattice strain influence the profile broadening although their relative contribution vary with milling time. Microstructural information showed that after long time milling (>19 h) BN becomes mixture of nanocrystalline and amorphous BN. The accumulations of defects cause this crystalline to amorphous transition. It has been found that twin fault ({beta}') and deformation fault ({alpha}) significantly contributed to BN powder as synthesized by a high-energy ball-milling technique. Present study consider only three ball-milled (0, 2 and 3 h) BN powder for faults calculation because fault effected reflections (1 0 1, 1 0 2, 1 0 3) disappear with milling time (>3 h). The morphology and particle size of the BN powders before and after ball milling were also observed in a field emission scanning electron microscope (FESEM)

36 MATERIALS SCIENCE↗

Effects of surfactants on the microstructure of porous ceramic scaffolds fabricated by foaming for bone tissue engineering

A porous scaffold comprising a {beta}-tricalcium phosphate matrix and bioactive glass powders was fabricated by foaming method and the effects of surfactants as foaming agent on microstructure of scaffolds were investigated. Foaming capacity and foam stability of different surfactants in water firstly were carried out to evaluate their foam properties. The porous structure and pore size distribution of the scaffolds were systematically characterized by scanning electron microscopy (SEM) and an optical microscopy connected to an image analyzer. The results showed that the foam stability of surfactant has more remarkable influence on their microstructure such as pore shape, size and interconnectivity than the foaming ability of one. Porous scaffolds fabricated using nonionic surfactant Tween 80 with large foam stability exhibited higher open and total porosities, and fully interconnected porous structure with a pore size of 750-850 {mu}m.

36 MATERIALS SCIENCE↗

Dopant induced variations in microstructure and optical properties of CeO{sub 2} nanoparticles

Research highlights: {yields} Dopant (Zr{sup 4+}, La{sup 3+}, and Ca{sup 2+}) induced phase stability, and changes in microstructure and optical properties of CeO{sub 2} nanoparticles have been studied. {yields} The nanoparticles were prepared by hydrothermal synthesis of nitrate solutions. {yields} The results show modification of the unit cell parameter by -0.39, +0.83 and +0.16% for doping of 20% Zr{sup 4+}, La{sup 3+}, and Ca{sup 2+}, respectively. {yields} For each batch prepared, nanoparticles with a narrow size distribution of 5-15 nm have been obtained. These particles are single crystals mostly having polygonal two-dimensional projections. {yields} UV-visible spectra of doped particles exhibit shift of the absorption edge and absorption peak with respect to those of the undoped ones and has been attributed to compensation of Ce{sup 3+} and decreasing crystallite size as result of doping. -- Abstract: Nanocrystalline CeO{sub 2} particles doped in the range of 0-20% of Ca{sup 2+}, La{sup 3+}, and Zr{sup 4+} have been prepared from hydrothermal synthesis of nitrate solutions at 200 {sup o}C and the influences of the dopants on microstructure and optical properties of the nanoparticles have been investigated. The unit cell parameter is found to be modified by -0.39, +0.83 and +0.16% for doping of 20% Zr{sup 4+}, La{sup 3+}, and Ca{sup 2+}, respectively. For each batch prepared, nanoparticles with a narrow size distribution of 5-15 nm have been obtained. A high-resolution transmission electron microscopy investigation reveals that these particles are single crystals mostly having hexagonal, square or circular two-dimensional projections. UV-visible spectra of doped powders exhibit shift of the absorption edge and absorption peak with respect to those of the undoped CeO{sub 2} particles and has been attributed to compensation of Ce{sup 3+} and decreasing crystallite size as result of doping.

36 MATERIALS SCIENCE↗

Solution-deposited GdCeO{sub x} thin films: Microstructure, band structure, and dielectric property

Highlights: ► Microstructural and electrical properties of sol–gel-deposited GdCeO{sub x} thin films with different mixing ratios. ► Ce incorporation enhanced crystallization and refractive index, reduced hysteresis, and increased dielectric constant. ► Bandgap gradually decreased with increasing Ce, which was primarily affected by VBO reduction. -- Abstract: The microstructural and electrical properties of solution-deposited GdCeO{sub x} dielectric thin films with different mixing ratios were studied. The Ce incorporation enhanced the degree of crystallization and the refractive index of the Gd{sub 2}O{sub 3} film, reduced the hysteresis and increased the dielectric constant. According to reflective electron energy loss spectroscopy and X-ray photoelectron spectroscopy analyses, the bandgap of the GdCeO{sub x} film gradually decreased with increasing Ce/(Gd + Ce) atomic ratio, which was primarily affected by the reduction of the valence band offset.

36 MATERIALS SCIENCE↗

Microstructure and optical properties of CdI{sub 2} doped silver vanadate glass-nanocomposites

Graphical abstract: TEM micrograph for 0.20CdI{sub 2}–0.80(0.60Ag{sub 2}O–0.40V{sub 2}O{sub 5}) and SAED pattern (shown right inset) from the selected area. High resolution image for a particle along with its FFT pattern is also shown in left inset. Highlights: ► CdI{sub 2} doped silver vanadate glass nanocomposites have been prepared. ► Microstructure of the compositions has been investigated. ► Nanocrystalline phases (β-AgI, Cd{sub 2}V{sub 2}O{sub 7}, etc.) are distributed in the glass matrix. ► Volume fraction of these crystalline phases increases with increase of CdI{sub 2} content. ► Formation of Cd{sub 2}V{sub 2}O{sub 7} and β-AgI phase confirms the Cd–Ag exchange in the samples. -- Abstract: Microstructure and optical properties of glass-nanocomposites of compositions xCdI{sub 2}–(1 − x)(0.60Ag{sub 2}O–0.40V{sub 2}O{sub 5})(x = 0.0–0.20) have been reported in this paper. X-ray diffraction patterns show the amorphous nature for the compositions x = 0 and 0.05. However, nanocrystalline phases have been observed in these compositions in electron microscopic studies. X-ray diffraction and electron microscopic studies reveal formation of different nanocrystalline phases such as β-AgI, Cd{sub 2}V{sub 2}O{sub 7}, Ag{sub 4}V{sub 2}O{sub 7} distributed within the amorphous matrix for the compositions x = 0.05–0.20. The presence of Cd{sub 2}V{sub 2}O{sub 7} and β-AgI phase for x = 0.05–0.20 confirms the exchange of coordination between Cd and Ag in these samples. The crystalline volume fraction increases with the increase of CdI{sub 2} content in these compositions. The average size of the nanocrystalline phases was estimated from the transmission and scanning electron microscopic studies. The network structure of the glass nanocomposites has been studied using Fourier transform infrared spectroscopy. Differential scanning calorimetric results show that the embedded nanocrystals decrease the glass transition temperature.

36 MATERIALS SCIENCE↗

The charge transfer transition phenomenon and microstructure of Eu{sup 3+}-doped NaCaPO{sub 4} phosphors sintered with NH{sub 4}Cl flux via solid-state reaction

Graphical abstract: This paper describes: The charge transfer transition phenomenon and microstructure of Eu{sup 3+}-doped NaCaPO{sub 4} phosphors sintered with NH{sub 4}Cl flux via solid-state reaction. The emission intensity of NaCa{sub 0.95}PO{sub 4}:0.05Eu{sup 3+} phosphors with 2 wt.% NH{sub 4}Cl flux is enhanced as the sintering temperature was increased from 800 °C to 1000 °C and reveals the maximum value at 1000 °C. Photoluminescence emission spectra of NaCa{sub 0.95}PO{sub 4}:0.05Eu{sup 3+} phosphors with 2 wt.% NH{sub 4}Cl flux sintered at various sintering temperature for 3 h via solid state reaction method (λ{sub ex} = 270 nm). Highlights: ► NH{sub 4}Cl flux is helpful for enhancing the crystallization degree and decreasing surface defects. ► A single phase of NaCaPO{sub 4}:Eu{sup 3+} phosphor was observed as the sintering temperature was increased from 800 °C to 1000 °C. ► The intensity of the excitation peaks displays a maximum value at 1000 °C. ► The NaCaPO{sub 4} host added with NH{sub 4}Cl flux and sintered at the different temperature can affect the morphology. ► The NaCaPO{sub 4} host added with NH{sub 4}Cl flux and sintered at the different temperature can affect fluorescent properties. - Abstract: NaCa{sub 0.95}PO{sub 4}:0.05Eu{sup 3+} phosphors with 2 wt.% NH{sub 4}Cl flux sintered at various sintering temperature (800, 900, 1000, 1100 °C) for 3 h under air atmosphere were synthesized successfully via solid state reaction method. It is found that the addition of NH{sub 4}Cl flux and different sintering temperatures can affect the morphology and fluorescent properties of NaCa{sub 0.95}PO{sub 4}:0.05Eu{sup 3+} phosphor. The X-ray diffractions show a single phase and the microstructure observations show uniform morphologies for NaCa{sub 0.95}PO{sub 4}:0.05Eu{sup 3+} phosphors sintered at the range from 900 °C to 1000 °C, indicating that addition of 2 wt.% NH{sub 4}Cl flux is helpful for enhancing the crystallization, thus improving the luminescence intensity of the charge transfer transition. The intensity of the excitation peaks displayed a maximum value at 1000 °C. The chromaticity (x, y) is in the orange-red region (0.54, 0.39) and the lifetime value is about 2.1 ms, suitable for the remote phosphor packages.

36 MATERIALS SCIENCE↗

Effect of oxygen partial pressure on microstructural and optical properties of titanium oxide thin films prepared by pulsed laser deposition

Graphical abstract: - Highlights: • Microstructural and optical properties are studied systematically. • The optical properties are studied by UV–visible and photoluminescence. • The PL spectra shows two peaks correspond to bandgap of anatase and rutile. • The maximum refractive index of 2.73 is obtained for rutile phase of titania. - Abstract: Nanocrystalline titanium oxide (TiO{sub 2}) thin films were deposited on silicon (1 0 0) and quartz substrates at various oxygen partial pressures (1 × 10{sup −5} to 3.5 × 10{sup −1} mbar) with a substrate temperature of 973 K by pulsed laser deposition. The microstructural and optical properties were characterized using Grazing incidence X-ray diffraction, atomic force microscopy, UV–visible spectroscopy and photoluminescence. The X-ray diffraction studies indicated the formation of mixed phases (anatase and rutile) at higher oxygen partial pressures (3.5 × 10{sup −2} to 3.5 × 10{sup −1} mbar) and strong rutile phase at lower oxygen partial pressures (1 × 10{sup −5} to 3.5 × 10{sup −3} mbar). The atomic force microscopy studies showed the dense and uniform distribution of nanocrystallites. The root mean square surface roughness of the films increased with increasing oxygen partial pressures. The UV–visible studies showed that the bandgap of the films increased from 3.20 eV to 3.60 eV with the increase of oxygen partial pressures. The refractive index was found to decrease from 2.73 to 2.06 (at 550 nm) as the oxygen partial pressure increased from 1.5 × 10{sup −4} mbar to 3.5 × 10{sup −1} mbar. The photoluminescence peaks were fitted to Gaussian function and the bandgap was found to be in the range ∼3.28–3.40 eV for anatase and 2.98–3.13 eV for rutile phases with increasing oxygen partial pressure from 1 × 10{sup −5} to 3.5 × 10{sup −1} mbar.

36 MATERIALS SCIENCE↗

Investigation of the role of deposition rate on optical, microstructure and ethanol sensing characteristics of nanostructured Sn doped In2O3 films

Highlights: • Deposition rate can play an important role in gas sensing of In{sub 2}O{sub 3}:Sn films. • The crystallite size and linear defects of the films is estimated by eCMWP method. • The correlation between the optical, microstructure and gas sensing properties is studied. • The size distribution behavior of samples is in agreement with the results of porosity. • Optimum deposition rate for In{sub 2}O{sub 3}:Sn films is 0.2 nm/s. - Abstract: In this paper, Sn doped In{sub 2}O{sub 3} (In{sub 2}O{sub 3}:Sn) nanostructured films as metal oxide semiconductor material which is very important in optoelectronics and gas sensing industries, were prepared by thermal evaporation technique. It is discussed how different deposition rate (0.1, 0.2, 0.3 and 0.4 nm/s) affects the optical, electrical, microstructural and ethanol gas sensing characteristics of In{sub 2}O{sub 3}:Sn films and must be precisely monitored. The gas sensing performance of the films was evaluated in terms of gas concentration and operating temperature. A correlation between the crystallite size, porosity, dislocation density, outer cut-off radius of dislocation, optical band gap, activation energy and sensitivity of the films was established. The results demonstrate that the maximum sensitivity to ethanol vapors can be obtained for the sample grown at deposition rate of 0.2 nm/s. The response and recovery times of this sensor exposed to 100 ppm of ethanol vapors were determined and found to be 9.0 s and 3.9 s, respectively.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure manipulation via machining and heat treatments in hybrid manufacturing of 316L stainless steel

Hybrid manufacturing combines additive and subtractive (machining) processes in a single platform to reduce the total time to fabricate a component in its final form. Here we show that if sufficient plastic deformation can be imparted to the material during machining, recrystallization can be triggered during post-fabrication heat treatment. This can enable highly localized microstructure control. Additionally, we show that stainless steel 316L, when machined without coolant accumulates significant plastic strain compared to when machined with coolant that results in faster recrystallization kinetics during heat treatment. These effects are limited to the surface while the bulk microstructure remains unaffected.

316L stainless steel↗

Microstructure Optimization of Austenitic Alloy 800H (Fe-21Cr-32Ni)

The microstructural evolution, specifically of grain boundaries, precipitates, and dislocations in thermomechanically processed (TMP) Alloy 800H samples was characterized by scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDS), electron backscattered diffraction (EBSD), transmission electron microscopy (TEM), and atomic force microscopy (AFM). The TMP not only significantly increased the fraction of low-{Sigma} coincidence site lattice boundaries, but also introduced nanoscale precipitates in the matrix and altered the distribution of dislocations. Statistical analysis indicates that the morphology and distribution of grain boundary precipitates were dependent on grain boundary types. The microstructure optimization played a synergistic effect on the significantly increased strength with comparable ductility and enhanced intergranular corrosion resistance and creep-fatigue life compared to the as-received samples.

36 MATERIALS SCIENCE↗

Microstructure-based prediction of thermal aging strength reduction factors for grade 91 ferritic-martensitic steel

This study aimed to develop a microstructure-based mechanistic approach to address the long-term thermal aging effect on yield stress and ultimate tensile strength and to provide a physical basis for developing thermal aging factors for G91 for a design life of 60 years. Several heats of G91 steel were examined. Controlled aging experiments were conducted on two heats at temperatures of 550, 600, and 650 °C for times up to ~64,000 h. Specimens were also taken from archived creep-tested specimens of G91 and from a tube removed from the Kingston coal-fired power plant to obtain data that cover a wide range of temperatures and for aging times up to 155,000 h. Thermal aging caused significant subgrain recovery, coarsening of M 23 C 6 carbides at subgrain boundaries and MX carbonitrides within subgrains. The intermetallic Laves phase forms during aging and grows rapidly. The growth rate of the subgrain width and MX mean size during thermal aging were described by kinetic models. Thermal aging results in the reductions in the yield stress and the ultimate tensile strength of G91. The effects of thermal aging on the reductions in yield stress and ultimate tensile strength were well described by the microstructure-strength model that considers three superimposed strengthening mechanisms, namely, sub-boundary strengthening, MX precipitation hardening, and Mo solid solution strengthening. Furthermore, the model was independently validated by the ASME Code values and is being used by the ASME to develop the aging-induced strength reduction factors for G91 steel for a design life of 60 years.

36 MATERIALS SCIENCE↗

Solid state welding of medium-entropy CrCoNi with heterogeneous, partially recrystallized microstructures

We report that heterogeneous, partially recrystallized (PRX) microstructures have recently been used to improve strength-ductility combinations in high-entropy alloys. However, these microstructures are incompatible with conventional joining processes that require melting or prolonged exposure to elevated temperatures. This work presents an initial exploration of solid state joining in this challenging condition using vaporizing foil actuator welding (VFAW) applied to PRX equiatomic alloy CrCoNi.

36 MATERIALS SCIENCE↗

Solid-state reaction mediated microstructural evolution in a spark plasma sintered in situ Ti–B 4 C composite

For this study, a novel porosity-free in situ Ti–B 4 C composite was fabricated via spark plasma sintering (SPS). Detailed analysis of the phase evolution, coupling results from XRM, XRD and SEM-EBSD-EDS, indicate that primarily TiB 2 precipitates formed due to the in-situ reactions between the boron-carbide and titanium powders. The precipitation of TiB 2 resulted in the formation of a graphitic C-rich thin layer circumscribing the partially reacted B 4 C particles. Further progression of the in-situ reaction leads to the out-diffusion of the excess carbon from the B 4 C particles, across the graphite and TiB 2 phases, forming TiC upon reacting with the titanium matrix. Therefore, the final microstructure primarily consisted of TiB 2 , TiC, and partially reacted B 4 C phases, with small amounts of TiB, α-Ti, and graphite. Furthermore, the microstructure in these SPS processed in situ composites appeared to be the product of a solid-state Ti–B 4 C diffusion couple, substantially different from their fusion-based additively manufactured counterparts. Nano-indentation tests revealed a remarkably high average hardness of ~25 GPa for this SPS-processed Ti–B 4 C composite and comparable (with literature) phase-specific hardness and modulus values for the constituent TiB 2 , TiC, and B 4 C phases.

36 MATERIALS SCIENCE↗

Interfacial microstructure and mechanical properties of rotary inertia friction welded dissimilar 422 martensitic stainless steel to 4140 low alloy steel joints

In this work, dissimilar rotary inertia friction welds between 422 martensitic stainless steel and 4140 martensitic low-alloy steel were made to fabricate prototype heavy-duty diesel engine pistons. The influence of the inertia friction welding process and post weld heat treatment (PWHT) temperature on the interfacial microstructure evolutions and corresponding effects on mechanical properties of the 422/4140 welds were evaluated in detail. Carbon diffused from the 4140 side to the 422 side during PWHT at 650 °C for 1.5 h, causing the formation of a hard carbide-rich layer on the 422 side, and a softer but discontinuous C-depleted layer the 4140 side. PWHT at 700 °C for 1.5 h greatly accelerated C diffusion across the interface relative to 650 °C, resulting in a thicker hard carbide-rich layer and a relatively thick and continuous layer of coarse C-depleted grains (ferrite) on the 4140 side. In addition, the PWHT temperature greatly influenced the tensile properties and fracture behavior of the welds, with the 650 °C PWHT-ed samples failing predominately in a ductile manner in the 4140 heat affected zone during tensile testing. Conversely, the 700 °C PWHT specimens exhibited a strength reduction compared with the 650 °C PWHT specimens because of additional coarsening of the interfacial ferrite layer and softening of the base materials during PWHT, with brittle fracture between the hard and soft layers the predominate failure mechanism. Based on the findings, a reduced PWHT temperature and/or time, minimizing the hardness differential of the base metals, and pre-heating the 422 steel prior to welding are the potential pathways to achieve a more optimal balance between desirable tempering and stress relief of the weld microstructure and undesirable C migration across the weld interface, and to reduce the strength mismatch across the weld.

36 MATERIALS SCIENCE↗

Friction surface layer deposition of triple-phase Al 10 Cr 12 Fe 35 Mn 23 Ni 20 high entropy alloy: Process optimization and microstructural evolution

A high-strength Co-free triple-phase Al 10 Cr 12 Fe 35 Mn 23 Ni 20 high-entropy alloy (HEA) was successfully fabricated using Friction Surface Layer Deposition (FSLD), a bulk manufacturing method. Multiple single-layer deposits were produced by varying forging force (F) and traverse speeds (T r ) to optimize the process parameters. The optimized conditions (F = 40 kN & T r = 200 mm/min) were then applied to manufacture a scaled-up multi-layer specimen. The initial microstructure of the HEA consisted of coarse grains of the soft FCC-phase, long columnar dendrites of the hard BCC-phase, and small precipitates of the harder B2-phase within the BCC-dendrites. During FSLD, the FCC-matrix underwent continuous dynamic recrystallization due to high-temperature severe plastic deformation, forming finer equiaxed grains. Simultaneously, the BCC-dendrites fractured into smaller fragments, some of which experienced partial growth and coarsening under applied stress, resulting in an hourglass morphology. In contrast, the small B2-precipitates within the BCC-fragments dissolved during the elevated temperatures of FSLD and reprecipitated as substantially finer precipitates during continuous cooling post-FSLD. Additionally, the orientation relationships between the FCC and BCC/B2 phases were completely destroyed by the severe thermoplastic deformation inherent to FSLD. The microstructural refinements led to a substantial improvement in hardness from 177 HV to 283 HV, driven by Hall-Petch strengthening. The increased number of interfaces, including coherent BCC-B2 interfaces, potentially enhances the sink strength and radiation tolerance of the HEA, making it a promising candidate for nuclear applications. In conclusion, this study also highlights FSLD as a versatile technique for achieving tunable properties in HEAs, with detailed schematics illustrating the complex mechanisms of phase transformations during processing.

Additive Manufacturing↗

Linking microstructure to creep behavior in vertically and horizontally built LPBF Haynes 282 compared with wrought material via θ -projection

Laser Powder Bed Fusion (LPBF) has emerged as a promising route for fabricating intricate geometries in high-performance alloys. Haynes 282 (H282) is a strong candidate for applications such as heat exchangers or engines due to its excellent creep strength and thermal stability; however, the long-term creep behavior of LPBF-processed H282 remains poorly understood. In this study, the θ -projection method is used to analyze and extrapolate the creep behavior of vertically built LPBF, horizontally built LPBF, compared to wrought H282 tested at 816 °C. Vertically built LPBF H282 exhibits the lowest minimum creep rate (MCR), while the horizontally built condition shows a higher MCR comparable to that of wrought H282. Despite these differences, both LPBF conditions exhibit significantly shorter rupture life and reduced rupture strain than the wrought material, with the most severe degradation observed in the horizontal builds, consistent with an earlier onset of tertiary creep and accelerated strain-rate evolution. Microstructural characterization reveals that both LPBF and wrought H282 exhibit abundant twin-related boundary character; however, their grain boundary topologies differ markedly. The wrought alloy contains a higher fraction of low-angle grain boundaries and continuous twin lamellae, whereas the LPBF microstructure is characterized by a suppressed low-angle boundary population and fragmented twin-related boundaries embedded within irregular high-angle grain boundary networks. Fractographic analysis further reveals predominantly intergranular cracking in LPBF H282, accompanied by grain-boundary-decorated carbides, Al 2 O 3 inclusions, and high-aspect-ratio pores. These results demonstrate that grain boundary topology, rather than minimum creep rate alone, plays a critical role in governing creep damage accumulation and rupture behavior in LPBF and wrought H282.

Creep↗

Microstructural evolution, defect mitigation, and precipitation behavior in AA6061 via laser powder bed fusion with high-temperature substrate heating

Defects, particularly solidification cracking, remain persistent challenges in the laser powder bed fusion (LPBF) processing of AA6061 aluminum alloy. This study systematically investigates defect mitigation, microstructural evolution, and mechanical properties associated with high-temperature substrate preheating at 500 °C. Comprehensive microstructural analyses, including characterization of defects, grain structures, and precipitation behavior, were performed on samples in both as-built and T6 heat-treated states. Elevated preheating substantially reduced solidification cracking across a wide processing window, while demonstrating decreased crack sensitivity to laser parameters. Columnar cracks along the build direction were observed despite substrate preheating. Lack-of-fusion and keyhole porosity were effectively eliminated, though gas-induced microporosity persisted at higher powers. In-depth characterization of two distinct laser power and speed conditions confirmed the formation of micron-sized, non-coherent Mg 2 Si precipitates under heated substrate conditions, alongside α-AlFeCrMnSi intermetallic phases indicative of in-situ thermal effects during fabrication. Subsequent T6 heat treatment revealed the formation of fine, coherent needle-shaped β″ strengthening precipitates. Despite substantial differences in processing parameters, comparable mechanical properties were measured in the as-built samples (∼52 MPa yield strength, ∼130 MPa tensile strength), primarily due to reduced strain hardening effects and consistent precipitation characteristics. Meanwhile, the T6 heat treatment led to significant improvement in properties, enhancing yield strength by over 400%, aligning closely with the performance of conventional wrought AA6061-T6. These findings underscore that high-temperature substrate preheating offers an effective means to suppress cracks, control precipitation, and enhance mechanical performance in LPBF-processed AA6061.