Magnetic and structural properties of BiFeO{sub 3} thin films grown epitaxially on SrTiO{sub 3}/Si substrates
The integration of oxides with semiconductors is important for the technological advancement of the next generation electronics. Concomitant ferroelectric and antiferromagnetic (AF) behavior is demonstrated in single crystal BiFeO{sub 3} (BFO) films grown on 20 nm SrTiO{sub 3} (STO) virtual substrates on Si(100) using molecular beam epitaxy (MBE). STO thin films are grown in an oxide MBE chamber by co-deposition of Sr, Ti, and molecular O{sub 2}. Careful control of the O{sub 2} during nucleation produced commensurate growth of STO on Si. The sequence of the steps allows for the suppression of an amorphous SiO{sub 2} layer. This STO(20 nm)/Si structure was used as a virtual substrate for MBE deposition of BFO on Si without breaking vacuum. BFO was deposited using Fe and O{sub 2} plasma with an overpressure of Bi flux, the growth rate was controlled by the incoming Fe flux. The reflection high energy electron diffraction image shows a 2-D growth front with a 6-fold surface reconstruction under optimized O{sub 2} pressure of 5 Multiplication-Sign 10{sup -8} mbar. Cross-sectional transmission electron microscopy (TEM) confirms the high crystallinity of the films and shows sharp, atomically flat interfaces. The selected area diffraction pattern (SADP) reveals that BFO grows in a distorted rhombohedral crystal structure. X-ray diffraction does not show formation of second phases and is consistent with the TEM and SADP results. The BFO films show AF behavior with a Neel temperature that exceeds 350 K, as expected (T{sub N} = 673 K) and with a residual ferromagnetic behavior that decreases with film thickness and is consistent with the G-type AF due to the canted spins. The saturation magnetization per unit volume for a 40 nm thick film was 180 emu/cm{sup 3} at an in-plane magnetic field of 8 kOe. The ferroelectric behavior of the films was verified using piezoresponse force microscopy.