Resorption of Ca{sub 3–} {sub x}M{sub 2x}(PO{sub 4}){sub 2} (M = Na, K) Calcium Phosphate Bioceramics in Model Solutions
The resorbability of bioceramics in the Ca{sub 3}(PO{sub 4}){sub 2}–CaNaPO{sub 4}–CaKPO{sub 4} system is evaluated in an approach involving thermodynamic assessment of solubility and investigation of the dissolution kinetics in model media, in particular in citric acid solutions. Thermodynamic calculation indicates high solubility of the Ca{sub 5}Na{sub 2}(PO{sub 4}){sub 4}, α-CaМPO{sub 4}, β-CaKPO{sub 4}, and β-СаK{sub 0.6}Na{sub 0.4}PO{sub 4} phases. Investigation of the dissolution kinetics of ceramics has made it possible to identify two distinct types of behavior of resorbable materials in weakly acidic solutions: with fast resorption kinetics in the case of the phases based on nagelschmidtite solid solutions and α-CaМPO{sub 4} disordered high-temperature solid solutions, and with a nearly constant, relatively low dissolution rate and a high solubility limit in the case of β-СaK{sub 1–} {sub x}Na{sub x}-based phases.