Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MARTENSITE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,603 records · Page 89

Elevated Temperature Corrosion Studies of AlCrN and TiAlN Coatings by PAPVD on T91 Boiler Steel

The present investigation discusses the hot corrosion behavior of AlCrN and TiAlN nano-coatings on T91 boiler steel by PAPVD process subjected to molten salt of Na{sub 2}SO{sub 4}-60%V{sub 2}O{sub 5} at 900 °C for 50 cycles. Surface and cross-sectional studies were performed by AFM, SEM/EDS and XRD techniques to understand the corrosion kinetics and mechanism. T91 bare boiler steel as well as TiAlN-coated specimen has shown higher internal oxidation as well as weight gain. The better corrosion resistance of AlCrN-coated specimen has been observed by virtue of higher availability of Cr and Al in the oxide scale as well as adherent and dense coating. The betterment of AlCrN coating can be attributed to low internal oxidation as well as movement of Cr and Al toward oxide scale to form protective corrosion barriers.

36 MATERIALS SCIENCE↗

Effect of Y/Zr Ratio on Inclusions and Mechanical Properties of 9Cr-RAFM Steel Fabricated by Vacuum Melting

This study investigates the inclusions, microstructures, tensile properties, and impact toughness of reduced-activation ferritic/martensitic (RAFM) steels with different Y/Zr ratio contents. An optical microscope and a scanning electron microscope (SEM) were employed to determine the size and number of inclusions, and SEM and transmission electron microscope were employed to examine the inclusion types. The increase in Y/Zr ratio influenced the prior austenite grain size owing to the pinning effect of the inclusions. The result of this examination showed that the mechanical properties of the steel are closely related to the refinement of prior austenite grain size and as well as the fine submicron-sized inclusions. The average prior austenite grain sizes of the alloys were 14.5, 13.5, and 13.4 μm for the steels with different Y/Zr ratio contents (i.e., 1/2, 5/3, and 11/2, respectively). Moreover, the submicron-sized inclusions in the alloys achieved densities of 4.71 × 10{sup 16}, 4.49 × 10{sup 16}, and 3.84 × 10{sup 16}/m{sup 3}. The ductile-to-brittle transition temperature (DBTT) decreases when the Y/Zr ratio increases to 5/3. However, the DBTT increases when the Y/Zr ratio reaches 11/2 owing to inclusion coarsening. The RAFM steel with Y content of approximately 0.005 wt.% and Zr content of 0.002 wt.% was verified to exhibit an optimized combination of microstructures, tensile properties, and impact toughness.

36 MATERIALS SCIENCE↗

Ductile-to-Brittle Transition in Low-Alloy Steel: A Combined Experimental and Numerical Investigation

Ductile-to-brittle transition in a low-alloy bainitic steel used as reactor pressure vessel material coincided with the change in brittle facet plane normal(s). Experimentally, it changed from ~ {100} facets at low temperatures to off-{100} planes at the higher temperatures. And such a change was also associated with brittle-to-ductile transition in the fracture mode. Molecular dynamics simulations, however, showed that the intrinsic cleavage plane remained {100} at all temperatures. Activation of atomistic mechanisms of crack kinking and dislocation pile-up, at higher temperatures, followed by the creation of atomistic ledges at the free surface resulted in the appearance of off-{100} facets.

36 MATERIALS SCIENCE↗

Application of X-ray Technique to Study the Structure of Ultrafine-Grained Ferritic/Martensitic Steel

In this work, x-ray diffraction and transmission electron microscopy (TEM) analyses have been applied to study the structure of ultrafine-grained (UFG) ferritic/martensitic steel as compared to coarse-grained samples subjected to standard treatment. The x-ray phase analysis of diffraction patterns taken in the “transmission” mode allowed determining the volume fraction and phase composition of particles in the UFG samples. The lattice parameter, the size of coherent scattering domains, the averaged dislocation density, and the fraction of edge and screw dislocations of the ferritic phase in steel were determined according to the diffraction patterns taken in the “reflection” mode. The small-angle x-ray scattering (SAXS) technique was used to study the quantitative characteristics of the size, shape, and distribution of precipitates in the UFG samples. The TEM investigations were performed on the same foils to confirm the results of SAXS. The quantitative evaluations of dispersion and dislocation hardenings in ferritic/martensitic steel were conducted on the basis of the results obtained.

36 MATERIALS SCIENCE↗

Simultaneously achieved large reversible elastocaloric and magnetocaloric effects and their coupling in a magnetic shape memory alloy

Large reversible caloric effects covering a broad temperature region are essential for high-efficiency and environment-friendly solid-state caloric refrigeration that can potentially replace the traditional vaporcompression-based cooling technology. Here, we report the simultaneously achieved large reversible magnetocaloric and elastocaloric effects in a Ni 43 Co 6 Mn 40 Sn 11 magnetic shape memory alloy. A reversible near-room-temperature magnetic entropy change Δ S m of as high as 19.3 J kg –1 K –1 under 5 T was experimentally obtained and the corresponding adiabatic temperature change Δ T ad was estimated to be 7.7 K. Meanwhile, a large reversible elastocaloric effect with a directly measured Δ T ad up to 7.1 K was attained. The elastocaloric effect exhibits high cyclic stability with no apparent degradation during 380 cycles of loading and unloading. Furthermore, we propose and demonstrate the utilization of the multicaloric approach under the coupled uniaxial stress and magnetic field to enlarge the refrigeration temperature region of reversible caloric effects. By combining the reversible magnetocaloric and elastocaloric effects and the reversible multicaloric effect under the coupling of uniaxial stress and magnetic field in the hysteresis region, large reversible caloric effects covering a broad temperature region from 257 K to 383 K can be obtained. Finally, this study may pave the way for designing advanced caloric materials with cyclically stable and reversible large caloric effects and wide refrigeration temperature region for solid-state refrigeration.

36 MATERIALS SCIENCE↗

A phase-field model for non-isothermal phase transformation and plasticity in polycrystalline yttria-stabilized tetragonal zirconia

Here we propose an elastoplastic phase-field (PF) model to investigate the mechanics of tetragonal-to-monoclinic phase transformation (TMPT) and elastoplastic deformation of polycrystalline yttria-stabilized tetragonal zirconia (YSTZ). A Landau polynomial with non-vanishing chemical energy at the equilibrium temperature is introduced to account for the actual formation energies of the phases. The effects of different grain orientations, latent heat, and temperature on TMPT and deformation mechanisms are considered. The suppressive transformation effects of the grain boundaries (GBs) is modeled using an inhomogeneous kinetic coefficient in the bulk and GBs. The simulation results for single crystals demonstrate the capability of the model to reproduce the orientation-dependent compressive deformation of YSTZ similar to atomistic simulations and micropillar experiments. The single crystal with [100] crystallographic orientation along the loading direction (SC[100]) displays both TMPT and plasticity, SC[101] experiences only phase transformation, while SC[001] undergoes only plastic yielding. The TMPT induced by compressive loading exhibits shape memory effect (SME) below the equilibrium transformation temperature and pseudoelasticity above it, while the critical transformation stress increases with increasing loading temperature. The irrecoverable plastic strain is found to trap a part of the monoclinic phase, which prevents a complete reverse transformation. The polycrystalline cases also display SME and PE at low and high temperatures, respectively. Due to the orientation differences between grains and the stress concentrations at geometric nonlinearities, plastic deformation occurs in polycrystalline YSTZ for an applied load less than the yield stress. The results suggest a possible limitation of plasticity and an improvement of the shape recovery of YSTZ if one can control the orientation of the grains and/or increase the density of stacking faults at the GBs during material processing.

36 MATERIALS SCIENCE↗

An overview of the US DCLL ITER-TBM program

Under the US Fusion Nuclear Science and Technology program, we selected the Dual Coolant Lead Lithium (DCLL) concept as our primary Test Blanket Module (TBM) for testing in ITER. The DCLL blanket concept has the potential to be a high-performance DEMO blanket design with a projected thermal efficiency of >40%. Reduced activation ferritic/martensitic (RAF/M) steel is used as the structural material. Helium is used to cool the first wall and blanket structure, and the self-cooled Pb-17Li breeder is circulated for power conversion and for tritium extraction. A SiC-based flow channel insert (FCI) is used as an electrical insulator for magnetohydrodynamic pressure drop reduction from the circulating Pb-17Li and as a thermal insulator to separate the high-temperature Pb-17Li (~650–700 °C) from the RAF/M structure, which has a corrosion temperature limit of ~480 °C. The RAF/M material must also operate at temperatures above 350 °C but less than 550 °C. We are continuing the development of the mechanical design and performing neutronics, structural and thermal hydraulics analyses of the DCLL TBM module. Prototypical FCI structures were fabricated and further attention was paid to MHD effects and the design of the inboard blanket for DEMO. We are also making progress on related R&D needs to address key areas. Finally, this paper is a summary report on the progress and results of recent DCLL TBM development activities.

Wong, C. P. C.↗

Predicting Failure Modes and Ductility of Dual Phase Steels Using Plastic Strain Localization

Ductile failure of metals is often treated as the result of void nucleation, growth and coalescence. Various criteria have been proposed to capture this failure mechanism for various materials. In this study, ductile failure of dual phase steels is predicted in the form of plastic strain localization resulting from the incompatible deformation between the harder marternsite phase and the softer ferrite matrix. Microstructure-level inhomogeneity serves as the initial imperfection triggering the instability in the form of plastic strain localization during the deformation process. Failure modes and ultimate ductility of two dual phase steels are analyzed using finite element analyses based on the actual steel microstructures. The plastic work hardening properties for the constituent phases are determined by the in-situ synchrotron-based high-energy X-ray diffraction technique. Under different loading conditions, different failure modes and ultimate ductility are predicted in the form of plastic strain localization. It is found that the local failure mode and ultimate ductility of dual phase steels are closely related to the stress state in the material. Under plane stress condition with free lateral boundary, one dominant shear band develops and leads to final failure of the material. However, if the lateral boundary is constrained, splitting failure perpendicular to the loading direction is predicted with much reduced ductility. On the other hand, under plane strain loading condition, commonly observed necking phenomenon is predicted which leads to the final failure of the material. These predictions are in reasonably good agreement with experimental observations.

36 MATERIALS SCIENCE↗

Temperature-dependence of superelastic stress in nanocrystalline NiTi with complete transformation capability

Nanocrystalline (NC) NiTi were previously reported to obtain non-hysteretic superelasticity and nearly zero temperature-dependence of superelastic stresses. However, the influence of the non-transforming regions in the specimens was not ruled out. In this study, we fabricate NC NiTi specimens with grain size down to 15 nm by wire drawing and annealing. Our specimens have no detectable non-transforming regions and thus are of complete transformation capability. We demonstrate that the hysteretic superelasticity is observed in all specimens of different grain sizes and that the minimum temperature-dependence of superelastic stresses is 4.7 MPa/K. Possible reasons for the discrepancy have been discussed.

36 MATERIALS SCIENCE↗

Determination of the stretch tensor for structural transformations

Structural transformations in crystalline solids are increasingly the basis of the functional behavior of materials. Both low hysteresis and reversibility of phase transformations have been linked to the satisfaction of the nongeneric conditions of compatibility between phases in diverse alloy systems. According to the Cauchy–Born rule, these conditions are expressed as properties of transformation stretch tensor. The transformation stretch tensor is difficult to measure directly due to the lack of knowledge about the exact transforming pathway during the structural change, and the complicating effects of microstructure. In this paper we give a rigorous algorithmic approach for determining the transformation stretch tensor from X-ray measurements of structure and lattice parameters. For some traditional and emerging phase transformations, the results given by the algorithm suggest unexpected transformation mechanisms.

42 ENGINEERING↗

Extended continuous cooling transformation diagram for 410 stainless steel encompassing δ → γ and γ → αʹ transformations determined by dilatometry

In this study, we use dilatometry to construct an extended Continuous Cooling Transformation (CCT) diagram for 410 stainless steel, capturing both δ → γ and γ → αʹ transformations specifically for directed energy deposition (DED) additive manufacturing (AM) applications. To ensure that the findings are representative of AM specific microstructures and compositions, dilatometry coupons were extracted from a wire arc DED wall, thereby preserving the inherent microstructural and compositional variability within the material. The on-heating phase transformations, including A c1 , A c3 , and γ → δ, were found to be essentially location independent, despite the typical heterogeneity associated with AM. Conversely, increasing cooling rates were observed to shift the start and finish temperatures of both δ → γ and γ → αʹ transformations to lower values. The resulting extended CCT diagram offers a more complete depiction of phase transformation behavior in the system, enabling accurate microstructure evolution modeling and residual stress predictions specifically for directed energy deposition additive manufacturing applications.

Additive manufacturing↗

Microstructural evolution in NF616 (P92) and Fe–9Cr–0.1C-model alloy under heavy ion irradiation

In this comparative study, in situ investigations of the microstructure evolution in a Fee9Cr ferritic emartensitic steel, NF616, and a Fee9Cre0.1C-model alloy with a similar ferriticemartensitic microstructure have been performed. NF616 and Fee9Cre0.1C-model alloy were irradiated to high doses (up to ~10 dpa) with 1 MeV Kr ions between 50 and 673 K. Defect cluster density increased with dose and saturated in both alloys. The average size of defect clusters in NF616 was constant between 50 and 573 K, on the other hand average defect size increased with dose in Fee9Cre0.1C-model alloy around ~1 dpa. At low temperatures (50e298 K), alignment of small defect clusters resulted in the formation of extensive defects in Fee9Cre0.1C-model alloy around ~2e3 dpa, while similar large defects in NF616 started to form at a high temperature of 673 K around ~5 dpa. Interaction of defect clusters with the lath boundaries were found to be much more noticeable in Fee9Cre0.1C-model alloy. Differences in the microstructural evolution of NF616 and Fee9Cre0.1C-model alloy are explained by means of the defect cluster trapping by solute atoms which depends on the solute atom concentrations in the alloys.

Ferritic-martensitic alloys↗

Investigation of mechanical and microstructural properties of Zircaloy-4 under different experimental conditions

Here two types of Zircaloy-4 (alpha-annealed and beta-quenched) were investigated in their different forms. It was found that mechanical properties of Zircaloy-4 are affected significantly by welding and hydrogen-charging followed by neutron irradiation. Evaluation of microstructural properties of samples showed that these changes are mainly due to the formation of secondary phases such as hydrides—mostly along grain boundaries, dislocation channeling and their disruptions, and the increase in the type dislocation loops.

36 MATERIALS SCIENCE↗

Microchemical evolution of irradiated additive-manufactured HT9

The microstructural responses under 5 MeV Fe2 + single-ion-beam irradiation of three conditions of additive-manufactured (AM) HT9 steel using a powder-based directed energy deposition (DED) technique with and without postbuild heat treatments were investigated. Besides the observed dislocation loop formation and the absence of cavities at the irradiation condition of 50 dpa at 460 °C, Ni/Si/Mn-rich precipitates are found to form in all three conditions of AM-HT9, whereas Cu-rich clusters that arise from Cu uptake from the DED process are only observed in the heat-treated conditions, and not in the as-built (ASB) condition. Coprecipitation of the Cu- and Ni/Si/Mn-rich clusters occur near defect sinks such as line dislocations and grain boundaries in the heat-treated AM-HT9. The variation in microchemical evolution can be directly linked to the starting sink strength of the three AM-HT9 conditions, and the ASB condition with higher sink strength suppressed the responses observed in the postbuild heat-treated specimens.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effects of aging on the characteristics of TiNiPd shape memory alloy thin films

TiNiPd thin films have been deposited on glass substrate using R.F. magnetron sputtering. Effects of annealing and aging on the microstructure, phase transformation behaviors and shape memory effects of these thin films have been studied by X-ray diffractometry, differential scanning calorimeter, tensile tests and internal friction characteristics. The TiNiPd thin films annealed at 750 deg. C exhibit uniform martensite/austenite transformations and shape memory effect. Aging at 450 deg. C for 1 h improved the uniformity of transformations and shape memory effect. Long time aging decreased transformation temperatures and increased the brittleness of TiNiPd thin films.

36 MATERIALS SCIENCE↗

Effects of strain amplitude and temperature on the damping capacity of an Fe-19Mn alloy with different microstructures

The influences of strain amplitude (10{sup -5}-10{sup -4}) and temperature (25 deg. C-500 deg. C) on the internal friction of a cold-drawn and solution treated Fe-19Mn alloy were investigated. The internal friction was measured using reversal torsion pendulum and multifunction internal friction equipment. The microstructure was observed using scanning electron microscopy. The phase transformation temperatures were determined using differential scanning calorimetry. The results indicated that the internal friction of the solution treated alloy was related to strain amplitude, which could be explained using the movement of Shockley partial dislocations (bowing out and breaking away). But the internal friction of the cold-drawn alloy was independent of strain amplitude because of high density dislocations formed by cold forming. Moreover, when the temperature was changed between 25 deg. C and 500 deg. C, the internal friction of the cold-drawn alloy increased slowly from 25 deg. C to 375 deg. C, and then increased quickly from 375 deg. C to 500 deg. C. However, for the solution treated alloy, there was an internal friction peak at about 210 deg. C in the heating process (from 25 deg. C to 500 deg. C), and there was another internal friction peak at about 150 deg. C in the cooling process. These peaks could be explained using the heat-assisted movement of dislocations. - Research Highlights: {yields}Internal friction of solution treated Fe-19Mn alloy is related to strain amplitude. {yields}Internal friction of cold-drawn Fe-19Mn alloy is independent of strain amplitude. {yields}IF of cold-drawn alloy increases from RT to 500 deg. C. {yields}There is an IF peak of solution treated alloy in heating and cooling process separately. {yields}The results can be explained using the movement of dislocations.

36 MATERIALS SCIENCE↗

Microstructural evolution of P92 ferritic/martensitic steel under argon ion irradiation

Microstructural evolution of P92 ferritic/martensitic steel irradiated by Ar{sup +} ion beams at doses from 0.6 to 230 displacements per atom (dpa) at room temperature was investigated with conventional transmission electron microscope technique. Selected-area electron diffraction combined with bright-field and dark-field contrast image indicated that carbide/matrix interfaces were more easily damaged. The carbide peripheries became partly amorphous at irradiation dose of 2.3 dpa and were almost complete amorphous at the dose of 11.5 dpa. The small carbides would re-precipitate in matrices at 34.5 dpa. Energy dispersive X-ray analysis revealed that segregation of Cr and W and depletion of Fe in carbides occurred under irradiation. With the irradiation dose increasing, the irradiation induced segregation and depletion became more severe, which would influence mechanical properties of the steel. - Research Highlights: {yields} Carbide/matrix interfaces in P92 ferritic/martensitic steel were easily damaged. {yields} Small carbides re-precipitated in matrices after higher dose irradiation. {yields} Segregation of Cr and W and depletion of Fe in carbides occurred after irradiation.

36 MATERIALS SCIENCE↗