Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “DISLOCATIONS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,603 records · Page 89

A comparison of EBSD based strain indicators for the study of Fe-3Si steel subjected to cyclic loading

The current work aims at proposing an EBSD-based indicator for fatigue damage of a Fe-3Si steel. At the same time direct observation of dislocation structures is provided by electron channelling contrast imaging (ECCI). The investigation consisted in processing the EBSD data from patterns collected on specimen subjected to low cycle fatigue. It revealed two different regimes depending on the applied total strain variation which is explained by the identification of the dislocations structures and their evolution. At low strain variation, strain accommodation occurs by planar glide of dislocations uniformly distributed throughout the grains. No misorientation evolution is observed. At higher strain variation, the vein-channel structure is observed within the grain and the wall-channel structure in the vicinity of grain boundaries. The misorientation between these two dislocation structures is evaluated at about 0.7° which is detected by the EBSD analyses and explains the increase of the different misorientation based criteria. The EBSD study enables also the prediction of crack initiation mode. Finally, this study points out the limits of the EBSD technique as no misorientation evolution is detected at small strain variation. Indeed, the lattice distortion is too weak to be detected by conventional EBSD. - Highlights: • Microstructure investigation of the fatigue behaviour of an iron-silicon steel • Use of cECCI to investigate the fatigue dislocations structures • Characterisation of local plastic accommodation through EBSD misorientation criteria.

36 MATERIALS SCIENCE↗

On the tungsten single crystal coatings achieved by chemical vapor transportation deposition

The tungsten single crystal has many excellent properties, namely a high melting point, high anti-creeping strength. Chemical vapor transportation deposition (CVTD) is a possible approach to achieve large-sized W single crystals for high-temperature application such as the cathode of a thermionic energy converter. In this work, CVTD W coatings were deposited on the monocrystalline molybdenum substrate (a tube with < 111 > axial crystalline orientation) using WCl{sub 6} as a transport medium. The microstructures of the coatings were investigated by a scanning electron microscope (SEM) and electron backscatter diffraction (EBSD). The as-deposited coatings are hexagonal prisms—rough surfaces perpendicular to < 110 > with alternating hill-like bulges and pits at the side edges of the prisms, and flat surfaces perpendicular to < 112 > with arc-shaped terraces at the side faces. This can be explained by two-dimensional nucleation -mediated lateral growth model. Some parts of the coatings contain hillocks of an exotic morphology (noted as “abnormal growth”). The authors hypothesize that the abnormal growth is likely caused by the defects of the Mo substrate, which facilitate W nucleation sites, cause orientation difference, and may even form boundaries in the coatings. A dislocation density of 10{sup 6} to 10{sup 7} (counts/cm{sup 2}) was revealed by an etch-pit method and synchrotron X-ray diffraction. As the depositing temperature rises, the dislocation density decreases, and no sub-boundaries are found on samples deposited over 1300 °C, as a result of atom diffusion and dislocation climbing. - Highlights: •The varied growth rate causes the different morphologies of different planes. •The W coating is a single crystal when only single hillocks appear. •The (110) plane tends to have the lowest dislocation density. •The dislocation density tends to decrease as the temperature increases.

36 MATERIALS SCIENCE↗

Microstructure control to improve creep strength of alumina-forming austenitic heat-resistant steel by pre-strain

Highlights: • The effect of pre-strain on creep strength of AFA steel was studied. • The creep test was performed at 700°C and 200Mpa, and the aging test was carried out using box furnace at 700°C to simulate the microstructural evolution during creep. • Microstuctural evolution was observed by using SEM, EBSD, and TEM to investigate the relationship between creep strength and microstructure. - Abstract: At 700 °C and 200 MPa, the creep rupture time of W-containing alumina-forming austenitic heat-resistant (WAFA) steel increases from 1044 to 3119 h by pre-strain. Pre-strain introduces a lot of dislocation into the matrix and most of the dislocations remain stable to the end of creep without recovery and recrystallization. In addition, the dislocations have enabled secondary NbC and Laves phase to be uniformly distributed and refined. However, the dislocations lower grain boundary strength due to the coarsening of precipitates along grain boundaries Therefore, the increase in the creep rupture time in spite of deterioration of grain boundary strength is attributed to the dislocation strengthening and enhanced precipitation hardening within grains.

36 MATERIALS SCIENCE↗

The shape recovery conditions for Fe–Mn–Si alloys: An interplay between martensitic transformation and plasticity

Highlights: • Fe15Mn5Si9Cr5Ni samples were rolled at 800 °C and annealed at 650 (C1) and 1000 °C (C2). • TEM analysis was performed. • High density of stacking faults and appropriate density of dislocation appears in C1. • Complex dislocation arrays due to plastic deformation are observed in C2. • Shape memory properties depend on the thermomechanical treatment. - Abstract: This work analyses the improvement of the shape memory properties of Fe-Mn-Si based alloys, and expands upon and deepens recently published developments concerning this topic. We prepared TEM specimens from a Fe-15Mn-5Si-9Cr-5Ni sheet rolled at 800 °C and annealed at 650 °C–92% shape recovery – and from another sheet annealed at 1000 °C–45% shape recovery. Here, we analyse the development of microstructure during the γ ↔ ε martensitic transformation and correlate it with the shape memory behaviour. Among the observed microstructural features, the introduction of complex dislocation arrays due to plastic deformation appears to be critical for shape memory development, since they can arrest the backward movement of Shockley partial dislocations over the original path. Tailoring the microstructure in order to introduce a high stacking-fault density accompanied by an appropriate dislocation density remains a key issue in the design of these kinds of functional materials.

36 MATERIALS SCIENCE↗

Cyclic plastic deformation behaviour of a directionally solidified nickel base superalloy at 850 °C: Damage micromechanisms

Highlights: • Isothermal LCF life of CM 247 DS is reduced using R = 0 instead of R = −1. • Reduction in LCF life is significant at lower values of Δε/2. • Reduction in fatigue life is attributed to the development of sustained mean stress. • Sustained mean stress prevents the slip transfer from γ-channels to γ′-precipitates. • Sustained mean stress promotes dislocation network formation and looping. - Abstract: Dislocation based deformation micromechanisms during low cycle fatigue deformation of nickel base superalloy CM 247 DS LC at 850 °C was investigated by conducting fatigue tests employing constant strain amplitudes for strain ratio (R) values of 0, −1 and carrying out extensive SEM and TEM examinations. Cyclic life of the alloy reduces for all fatigue tests conducted employing R = 0 in comparison with R = −1 owing to sustained mean stress developed during fatigue at R = 0. TEM examinations confirmed that sustained mean stress developed during low strain amplitude fatigue test (Δε/2 = 0.5%) using R = 0 condition prevented slip transfer from γ-channels to γ′-precipitates and resulted in the formation of dislocation substructures such as networks, nodes etc. and also promoted dislocation looping around γ′-precipitates. Lower fatigue life at R = 0 is mainly attributed to the development of these types of substructures, which promotes strain localization in both intra as well intergranular regions. Whereas, in specimen fatigue tested (Δε/2 = 0.5%) using R = −1 condition, shearing of γ′-precipitates by APB coupled dislocation and formation of stacking faults were observed. The formation and nature of stacking faults were analysed using weak beam imaging technique. Stacking fault formed during fatigue tests using R = −1 condition matured to micro-twins when Δε/2 value was increased to 0.8%. The mechanism of formation of these microtwins is discussed in detail. SEM based microstructural and fractographic examinations revealed that mean stress induced creep effect resulted in intergranular crack initiation and grain boundary cavitation during fatigue tests under R = 0 condition and therefore verified the facts revealed in TEM studies.

36 MATERIALS SCIENCE↗

High-temperature damage evolution in 10 keV He+ irradiated W and W-5Re

Highlights: • High-temperature damage in pure W appeared strongly dependent upon foil thickness. • Visible bubbles occurred at above a threshold fluence of ~ 4.5×10{sup 19} He{sup +}/m{sup 2}. • Dislocations with b = ½ were identified and exhibited a wavy morphology. • The bypass of bubbles by dislocations operated through simple shear. • Rhenium gave rise to ~ 10-40% increase in bubble size and a pronounced change in bubble morphology. - Abstract: High-temperature damage evolution in pure W and W-5Re has been studied by combining transmission electron microscopy and in-situ irradiations with 10 keV He{sup +} ions. The irradiations covered a temperature range of T{sub irr} = 773–1473 K and a fluence range of (4.5–15) × 10{sup 19} He{sup +}/m{sup 2}. In pure W, detailed characterizations have shown that damage evolution is highly dependent upon the foil thickness. Regions of thickness irr from 773 K to 1473 K, a pronounced bubble growth and an increased degree of bubble ordering were observed. In thicker regions (≳100 nm), 1/2<111> dislocation loops and line entanglements were found up to 1473 K, and were often seen to be decorated with helium bubbles. In W-5Re, areas of different foil thickness exhibited only small differences in damage evolution. The densities of bubbles were comparable to those seen in pure W at all temperatures, while the average size of bubbles was found to be ~10–40% higher. The damage microstructure transformed from a mixture of dislocation loops and bubbles at 773 K to dislocation line entanglements decorated with bubbles at 1473 K.

36 MATERIALS SCIENCE↗

In-situ synchrotron X-ray study of microstructural evolution during creep deformation in Grade 91 steel

Here, creep deformation mechanism of Grade 91 steel at 650 °C was investigated in-situ via wide-angle X-ray scattering (WAXS). WAXS peak broadening and a modified Williamson-Hall analysis provided information on evolution of dislocation densities in the primary α–Fe phase, while WAXS peak shifts provided lattice strains in the α–Fe matrix, M 23 C 6 and MX precipitates. Load transfer was not evident during in-situ creep deformation, suggesting that precipitates did not significantly strengthen the matrix during creep deformation. Peak broadening results illustrated an increase in average dislocation density during primary stage creep. After onset of secondary creep, there was a decrease in dislocation density, attributed to annihilation and re-ordering of dislocations in the subgrain structure, followed by a relatively constant average dislocation density with increasing strain.

36 MATERIALS SCIENCE↗

Deformation of Diopside Single Crystal at Mantle Pressure, 1, Mechanical Data

Steady-state deformation experiments were carried out in a deformation-DIA (D-DIA) high-pressure apparatus on oriented diopside single crystals, at pressure (P) ranging from 3.8 to 8.8 GPa, temperature (T) from 1100 to 1400 C, and differential stress ({sigma}) between 0.2 and 1.7 GPa. Three compression directions were chosen in order to test the activity of diopside dislocation slip systems, i.e., 1/2<1 1 0>{l_brace}1 {bar 1} 0{r_brace} systems activated together, both [1 0 0](0 1 0) and [0 1 0](1 0 0) systems together, or [0 0 1] dislocation slip activated in (1 0 0), (0 1 0) and {l_brace}1 1 0{r_brace} planes. Constant applied stress and specimen strain rates ({var_epsilon}) were monitored in situ using time-resolved synchrotron X-ray diffraction and radiography, respectively. Transmission electron microscopy (TEM) investigation of the run products revealed that dislocation creep was responsible for sample deformation. Comparison of the present high-P data with those obtained at room-P by Raterron and Jaoul (1991) - on similar crystals deformed at comparable T-{sigma} conditions - allows quantifying the effect of P on 1/2<1 1 0>{l_brace} 1 {bar 1} 0{r_brace} activity. This translates into the activation volume V* = 17 {+-} 6 cm{sup 3}/mol in the corresponding creep power law. Our data also show that both 1/2<1 1 0> dislocation slips and [0 0 1] have comparable slip activities at mantle P and T, while [1 0 0](0 1 0) and [0 1 0](1 0 0) slip systems remain marginal. These results show that P has a significant effect on high-T dislocation creep in diopside, the higher the pressure the harder the crystal, and that this effect is stronger on 1/2<1 1 0> slip than on [0 0 1] slip.

58 GEOSCIENCES↗

Growth of highly strained CeO 2 ultrathin films

Large biaxial strain is a promising route to tune the functionalities of oxide thin films. However, large strain is often not fully realized due to the formation of misfit dislocations at the film/substrate interface. In this work, we examine the growth of strained ceria (CeO 2 ) thin films on (001)-oriented single crystal yttria-stabilized zirconia (YSZ) via pulsed-laser deposition. By varying the film thickness systematically between 1 and 430 nm, we demonstrate that ultrathin ceria films are coherently strained to the YSZ substrate for thicknesses up to 2.7 nm, despite the large lattice mismatch (~5%). The coherency is confirmed by both X-ray diffraction and high-resolution transmission electron microscopy. This thickness is several times greater than the predicted equilibrium critical thickness. Partial strain relaxation is achieved by forming semirelaxed surface islands rather than by directly nucleating dislocations. In situ reflective high-energy electron diffraction during growth confirms the transition from 2-D (layer-by-layer) to 3-D (island) at a film thickness of ~1 nm, which is further supported by atomic force microscopy. We propose that dislocations likely nucleate near the surface islands and glide to the film/substrate interface, as evidenced by the presence of 60° dislocations. Finally, an improved understanding of growing oxide thin films with a large misfit lays the foundation to systematically explore the impact of strain and dislocations on properties such as ionic transport and redox chemistry.

36 MATERIALS SCIENCE↗

Strain relaxation properties of InAs{sub y}P{sub 1-y} metamorphic materials grown on InP substrates

The strain relaxation mechanism and defect properties of compositionally step-graded InAs{sub y}P{sub 1-y} buffers grown by molecular beam epitaxy on InP have been investigated. InAsP layers having lattice misfits ranging from 1% to 1.4% with respect to InP, as well as subsequently grown lattice matched In{sub 0.69}Ga{sub 0.31}As overlayers on the metamorphic buffers were explored on both (100) and 2 deg. offcut (100) InP substrates. The metamorphic graded buffers revealed very efficient relaxation coupled with low threading dislocation densities on the order of (1-2)x10{sup 6} cm{sup -2} for the range of misfit values explored here. A detailed analysis via high resolution x-ray diffraction revealed that the strain relaxed symmetrically, with equivalent numbers of {alpha} and {beta} dislocations, and to greater than 90% for all cases, regardless of substrate offcut. Further analysis showed the relaxation to always be glide limited in these materials when grown on a graded buffer compared to a single step layer. The threading dislocation density was observed by plan-view transmission electron microscopy to be constant for the range of misfit values studied here in the top layer of the graded structures, which is attributed to the very efficient use of residual dislocations and the dominance of dislocation glide over nucleation in these graded anion metamorphic buffers, suggesting great promise for metamorphic devices with lattice constants greater than that of InP to be enabled by InAsP metamorphic structures on InP.

36 MATERIALS SCIENCE↗

In situ strain relaxation comparison between GaAsBi and GaInAs grown by molecular-beam epitaxy

The strain relaxation of GaAsBi is studied in order to determine both the maximum thickness before dislocations form for various misfits and the potential of GaAsBi for usage in the compositionally graded buffer of lattice-mismatched devices. Low-misfit GaAsBi epilayers are grown and compared with GaInAs, a well-studied material currently used in compositional grades. Relaxation behavior and dislocation energetics are compared using in situ wafer curvature. Samples are grown using molecular-beam epitaxy under similar conditions with misfit up to -0.81%. GaAsBi begins to relax at a lower thickness than GaInAs of the same mismatch. This leads to the majority of GaAsBi strain relaxation occurring with less material growth than comparable GaInAs. However, GaAsBi has greater residual strain than GaInAs after 2 {mu}m of growth. These results indicate that GaAsBi requires less elastic energy to form dislocations and more elastic energy to either encourage glide or multiply dislocations than GaInAs. GaAsBi shows less surface roughness than GaInAs for all samples, ruling out roughness as a source of dislocations and hindered glide in these alloys.

36 MATERIALS SCIENCE↗

A comparative study on shock compression of nanocrystalline Al and Cu: Shock profiles and microscopic views of plasticity

Shock compressions of nanocrystalline (nc) metals Al and Cu with the same grain size and texture are studied by using molecular dynamics simulations. Results have revealed that the shock front of both Al and Cu can be divided into three stages: elastic, grain-boundary-mediated, and dislocation-mediated plastic deformation. The transition planes among these three stages are proven to be non-planar by two-dimensional shock response analysis, including local stress, shear, temperature, and atom configuration. The difference between shocked Al and Cu is that the rise rate of the elastic stage of Cu is slightly higher than that of Al, and that the shock-front width of Al is wider than Cu at the same loading conditions. For the plastic stage, the dislocation density of shocked Al is lower than Cu, and the contribution of grain-boundary-mediated plasticity to shock front and strain for nc Al is more pronounced than for nc Cu. These results are explained through intrinsic material properties and atomistic analysis of the plastic process. In the case of the shocked Al sample, partial dislocations, perfect dislocations, and twins are observed, but few evidence of perfect dislocations and twins are observed in the shocked Cu.

36 MATERIALS SCIENCE↗

The behaviour of niobium and molybdenum during uni-axial strain loading

The mechanical response of niobium and molybdenum during one dimensional shock loading in the weak shock regime is investigated in terms of the Hugoniot elastic limit (dynamic yield) and spall (tensile) strengths. Results indicate that although both metals have high elastic limits of ca. 2 GPa, their responses are very different. Deformation in the weak shock regime in niobium is controlled by both the motion and generation of dislocations, resulting in high spall (dynamic tensile) strengths and ductility. In contrast, molybdenum has low spall strength and ductility, which suggests lower dislocation mobility in this metal. We have also shown that the strain-rate in the rising part of the shock front is related to the stress amplitude by the fourth power, as first shown by Swegle and Grady. Although we have not been able to elucidate further on the power relation, we believe that the scaling factor A is related to a materials ability to accommodate shock imposed plasticity via slip and dislocation generation. Overall, we have used arguments about the Peierls stress in body centred cubic metals to explain these results, with niobium (low Peierls stress) having a high dislocation mobility, resulting in behaviour showing some similarities to face centred cubic metals. Molybdenum, with its much higher Peierls stress has a much lower dislocation mobility, and hence lower spall strengths and ductility.

36 MATERIALS SCIENCE↗

Eshelby twist and correlation effects in diffraction from nanocrystals

Molecular dynamics simulations were used to model the Eshelby dislocation inside Pd and Ir nanowires and to predict the powder diffraction pattern using the Debye scattering equation. We find that the ideal dislocation solution by Eshelby is in good agreement with the observed twist angle and deviatoric strain, even though it ignores both the splitting of the Eshelby dislocation into two partials and surface stress. Surface stress plays a significant role only for nanorods with small aspect ratio (∼1:1). We also find that Wilson's prediction on the diffraction peak broadening for the Eshelby dislocation is overestimated because it ignores the fact that the Eshelby twist relaxes the deviatoric strain. Moreover, the twist loosens the correlation along the nanorod, causing additional line profile broadening, which is read by diffraction as a decrease of coherent domain size when the total twist angle is bigger than 1.5°. Overall, our findings suggest a novel way to predict and analyze the dislocations as well as the resulting strain fields in the twisted nanocrystalline rods.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Effects of aging time and temperature of Fe-1wt.%Cu on magnetic Barkhausen noise and FORC

Magnetic Barkhausen noise (MBN), hysteresis measurements, first order reversal curves (FORC), Vickers microhardness, and Transmission Electron Microscopy (TEM) analyses were performed on Fe-1wt.%Cu (Fe-Cu) samples isothermally aged at 700°C for 0.5 – 25 hours to obtain samples with different sized Cu precipitates and dislocation structures. Fe-Cu is used to simulate the thermal and irradiation-induced defects in copper-containing nuclear reactor materials such as cooling system pipes and pressure vessel materials. The sample series showed an initial increase followed by a decrease in hardness and coercivity with aging time, which is explained by Cu precipitates formation and growth as observed by TEM measurements. Further, the MBN envelope showed a continuous decrease in its magnitude and the appearance of a second peak with aging. Also, FORC diagrams showed multiple peaks whose intensity and location changed for different aging time. The changes in FORC diagrams are attributed to combined changes of the magnetic behavior due to Cu precipitate characteristics and dislocation structure. A second series of samples aged at 850°C, which is above the solid solution temperature of Fe-Cu, was studied to isolate the effects of dislocations. These samples showed a continuous decrease in MBN amplitude with aging time although the coercivity and hardness did not change significantly. The decrease of MBN amplitude and the appearance of the second MBN envelope peak are attributed to the changes in dislocation density and structure. This study shows that the effect of dislocations on MBN and FORC of Fe-Cu materials can vary significantly and should be considered in interpreting magnetic signatures.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Deformation mechanisms of bent Si nanowires governed by the sign and magnitude of strain

In this study, the deformation mechanisms of bent Si nanowires are investigated at the atomic scale with bending strain up to 12.8%. The sign and magnitude of the applied strain are found to govern their deformation mechanisms, in which the dislocation types (full or partial dislocations) can be affected by the sign (tensile or compressive) and magnitude of the applied strain. In the early stages of bending, plastic deformation is controlled by 60° full dislocations. As the bending increases, Lomer dislocations can be frequently observed. When the strain increases to a significant level, 90° partial dislocations induced from the tensile surfaces of the bent nanowires are observed. This study provides a deeper understanding of the effect of the sign and magnitude of the bending strain on the deformation mechanisms in bent Si nanowires.

36 MATERIALS SCIENCE↗

Size-Dependent Elasticity of Nanocrystalline Titania

Synchrotron-based high-pressure x-ray diffraction measurements indicate that compressibility, a fundamental materials property, can have a size-specific minimum value. The bulk modulus of nanocrystalline titania has a maximum at particle size of 15 nm. This can be explained by dislocation behavior because very high dislocation contents can be achieved when shear stress induced within nanoparticles counters the repulsion between dislocations. As particle size decreases, compression increasingly generates dislocation networks (hardened by overlap of strain fields) that shield intervening regions from external pressure. However, when particles become too small to sustain high dislocation concentrations, elastic stiffening declines. The compressibility has a minimum at intermediate sizes.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

On the polarization dynamics in the presence of flexoelectricity and morphotropic phase boundary in ferroelectrics

It is shown that anomalous piezoelectric properties of epitaxial nanostructures arise on the morphotropic phase boundary (MPB) due to the strong flexoelectric effect on dislocation walls. The MPB (typical of many materials) exhibits a coexistence of various phases and partition of these phases to minimum sizes. This minimum size l{sub c} (nanoscale) is found using the dislocation theory; it coincides with the distance between individual dislocations in dislocation walls, which is much larger than the Burgers vector b, regardless of the type of crystalline material. The flexoelectric coefficients f are estimated taking into account dimensional relations and experimental data on the rotations of ferroelectric nanodomains in multiferroics. These estimates coincide with classical values. The critical value l{sub c} ~ 10b specifies the measured dependence on the dielectric susceptibility χ{sub e}, f ~ χ{sub e}{sup 1/2}. The quantity χ{sub e} depends on the frequency of the ac electric field applied to a sample and on the dislocation density. The Ba{sub 0.6}Sr{sub 0.4}TiO{sub 3}/Ni{sub 0.8}Zn{sub 0.2}Fe{sub 2}O{sub 4} ceramic composite shows typical frequency dispersion of χ{sub e} in a wide frequency range. The frequency dependence of flexoelecric coefficients is shown to reproduce the frequency dependence of permittivity at high frequencies.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗