Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “lithium”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,567 records · Page 87

Edge Turbulence Velocity Changes with Lithium Coating on NSTX

Lithium coating improves energy confinement and eliminates edge localized modes in NSTX, but the mechanism of this improvement is not yet well understood. We used the gas-puff-imaging (GPI) diagnostic on NSTX to measure the changes in edge turbulence which occurred during a scan with variable lithium wall coating, in order to help understand the reason for the confinement improvement with lithium. There was a small increase in the edge turbulence poloidal velocity and a decrease in the poloidal velocity fluctuation level with increased lithium. The possible effect of varying edge neutral density on turbulence damping was evaluated for these cases in NSTX.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Electronic Structure of Lithium Battery Materials

Lithium batteries are important as the power source for portable electronic devices and could also be used in hybrid vehicles with improvements in capacity. We have used first principles calculations of electronic structure to determine how charge is redistributed as Li is added or removed. In the final of year of the project we have examined Lix(NiMn)0.5O2 and Lix(NiMnCo)0.333O2 cathode materials in more detail. As lithium is removed electrons are removed from the valence band which is mainly Oxygen 2p states at the top of the band. There is very little change in the charge state of the transition element ions in either case. These results are confirmed by electron energy loss spectroscopy which shows a pre-peak on the oxygen K edge as lithium is removed, but no changes in the transition metal L edges. We have also investigated the LixFePO4 cathode material which is less costly than the LixCoO2 used at present and is also less damaging to the environment. In this case we find that as lithium is removed there is a change in charge state of iron while electrons are removed from oxygen 2p states at the top of the valence band. Again this is confirmed by the pre-peak on the oxygen K edge observed in electron energy loss spectroscopy and by the high resolution multiplet structure observed on the iron L edge which agrees with our calculations.

25 ENERGY STORAGE↗

Real Time Observation of Lithium Insertion into Pre-Cycled Conversion-Type Materials

Conversion-type electrode materials for lithium-ion batteries experience significant structural changes during the first discharge–charge cycle, where a single particle is taken apart into a number of nanoparticles. This structural evolution may affect the following lithium insertion reactions; however, how lithiation occurs in pre-cycled electrode materials is elusive. In this work, in situ transmission electron microscopy was employed to see the lithium-induced structural and chemical evolutions in pre-cycled nickel oxide as a model system. The introduction of lithium ions induced the evolution of metallic nickel, with volume expansion as a result of a conversion reaction. After pre-cycling, the phase evolutions occurred in two separate areas almost at the same time. This is different from the first lithiation, where the phase change takes place successively, with a boundary dividing the reacted and unreacted areas. Structural changes were restricted at the areas having large amount of fluorine, implying the residuals from the decomposition of electrolytes may have hindered the electrochemical reactions. This work provides insights into phase and chemical evolutions in pre-cycled conversion-type materials, which govern electrochemical properties during operation.

25 ENERGY STORAGE↗

Lithium-sulfur dioxide batteries on Mars rovers

NASA's 2003 Mars Exploration Rover (MER) missions, Spirit and Opportunity, have been performing exciting surface exploration studies for the past six months. These two robotic missions were aimed at examining the presence of water and, thus, any evidence of life, and at understanding the geological conditions of Mars, These rovers have been successfully assisted by primary lithium-sulfur dioxide batteries during the critical entry, descent, and landing (EDL) maneuvers. These batteries were located on the petals of the lander, which, unlike in the Mars Pathfinder mission, was designed only to carry the rover. The selection of the lithium-sulfur dioxide battery system for this application was based on its high specific energy and high rate discharge capability, combined with low heat evolution, as dictated by this application. Lithium-sulfur dioxide batteries exhibit voltage delay, which tends to increase at low discharge temperatures, especially after extended storage at warm temperatures, In the absence of a depassivation circuit, as provided on earlier missions, e.g., Galileo, we were required to depassivate the lander primary batteries in a unique manner. The batteries were brought onto a shunt-regulated bus set at pre-selected discharge voltages, thus affecting depassivation during constant discharge voltages. Several ground tests were preformed, on cells, cell strings and battery assembly with five parallel strings, to identify optimum shunt voltages and durations of depassivation. We also examined the repassivation of lithium anodes, subsequent to depassivation. In this paper, we will describe these studies, in detail, as well as the depassivation of the lander flight batteries on both Spirit and Opportunity rover prior to the EDL sequence and their performance during landing on Mars.

Lithium-SO2 batteries↗

Improvement in Plasma Performance with Lithium Coatings in NSTX

Lithium as a plasma-facing material has attractive features, including a reduction in the recycling of hydrogenic species and the potential for withstanding high heat and neutron fluxes in fusion reactors. Dramatic effects on plasma performance with lithium-coated plasma-facing components (PFC's) have been demonstrated on many fusion devices, including TFTR, T-11M, and FT-U. Using a liquid-lithium-filled tray as a limiter, the CDX-U device achieved very significant enhancement in the confinement time of ohmically heated plasmas. The recent NSTX experiments reported here have demonstrated, for the first time, significant and recurring benefits of lithium PFC coatings on divertor plasma performance in both L- and H- mode regimes heated by neutral beams.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

NSTX plasma response to lithium coated divertor

NSTX experiments have explored lithium evaporated on a graphite divertor and other plasma-facing components in both L- and H- mode confinement regimes heated by high-power neutral beams. Improvements in plasma performance have followed these lithium depositions, including a reduction and eventual elimination of the HeGDC time between discharges, reduced edge neutral density, reduced plasma density, particularly in the edge and the SOL, increased pedestal electron and ion temperature, improved energy confinement and the suppression of ELMs in the H-mode. However, with improvements in confinement and suppression of ELMs, there was a significant secular increase in the effective ion charge Z(eff) and the radiated power in H-mode plasmas as a result of increases in the carbon and medium-Z metallic impurities. Lithium itself remained at a very low level in the plasma core, < 0.1%. Initial results are reported from operation with a Liquid Lithium Divertor (LLD) recently installed. (C) 2010 Elsevier B.V. All rights reserved.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Quantification of Electrochemical Nanoscale Processes in Lithium Batteries By OperandoEC-(S)TEM

Lithium (Li)-ion batteries are currently used for a wide variety of portable electronic devices, electric vehicles and renewable energy applications. In addition, extensive worldwide research efforts are now being devoted to more advanced “beyond Li-ion” battery chemistries - such as lithium-sulfur (Li-S) and lithium-air (Li-O2) - in which the carbon anode is replaced with Li metal. However, the practical application of Li metal anode systems has been highly problematic. The main challenges involve controlling the formation of a solid-electrolyte interphase (SEI) layer and the suppression of Li dendrite growth during the charge/discharge process (achieving “dendrite-free” cycling). The SEI layer formation continuously consumes the electrolyte components creating highly resistive layer, which leads to the rapid decrease of cycling performance and degradation of the Li anode. The growth of Li metal dendrites at the anode contributes to rapid capacity fading (the presence of “dead Li” created during the discharge leads to an increased overpotential) and, in the case of continuous growth, leads to internal short circuits and extreme safety issues. Here we demonstrate the application of an operando electrochemical scanning transmission electron microscopy (ec-(S)TEM) cell to study the SEI layer formation and the initial stages of Li dendrite growth - the goal is to develop a mechanism for mitigating the degradation processes and increasing safety. Bright field (BF) STEM images in Figure 1 A-C show Li metal deposition and dissolution processes at the interface between the Pt working electrode and the lithium hexafluorophosphate (LiPF6) in propylene carbonate (PC) electrolyte during three charge/discharge cycles. A contrast reversal caused by Li metal being lighter/less dense than surrounding electrolyte (Li appears brighter than the background in BF STEM images) allows Li to be uniquely identified from the other components in the system - the only solid material that is less dense than the electrolyte is Li metal. Using these images, we can precisely quantify the total volume of Li deposition, the thickness of the SEI layer (observed as a ring of positive contrast around the electrode) and alloy formation due to Li+ ion insertion during each cycle. Furthermore, at the end of each discharge cycle we can quantify the presence of “dead Li” detached from the Pt electrode, thereby demonstrating the degree of irreversibility (and degradation of Pt electrode) associated with insertion/removal of Li+during this process with direct correlation to electrochemical performance. Such analyses provide significant insights into Li metal dendrite growth, which is critical to understand the complex interfacial reactions needed to be controlled for future Li-based and next generation energy storage systems.

batteries↗

Measurements of impurity concentrations and transport in the Lithium Tokamak Experiment

This thesis presents new measurements of core impurity concentrations and transport in plasmas with lithium coatings on all-metal plasma facing components (PFCs) in the Lithium Tokamak Experiment (LTX). LTX is a modest-sized spherical tokamak uniquely capable of operating with large area solid and/or liquid lithium coatings essentially surrounding the entire plasma (as opposed to just the divertor or limiter region in other devices). Lithium (Li) wall-coatings have improved plasma performance and confinement in several tokamaks with carbon (C) PFCs, including the National Spherical Torus Experiment (NSTX). In NSTX, contamination of the core plasma with Li impurities was very low (<0.1%) despite extensive divertor coatings. Low Li levels in NSTX were found to be largely due to neoclassical forces from the high level of C impurities. Studying impurity levels and transport with Li coatings on stainless steel surfaces in LTX is relevant to future devices (including future enhancements to NSTX-Upgrade) with all-metal PFCs. The new measurements in this thesis were enabled by a refurbished Thomson scattering system and improved impurity spectroscopy, primarily using a novel visible spectrometer monitoring several Li, C, and oxygen (O) emission lines. A simple model was used to account for impurities in unmeasured charge states, assuming constant density in the plasma core and constant concentration in the edge. In discharges with solid Li coatings, volume averaged impurity concentrations were low but non-negligible, with~2-4% Li, ~0.6-2% C, ~0.4-0.7% O, and Z_eff<1.2. Transport was assessed using the TRANSP, NCLASS, and MIST codes. Collisions with the main H ions dominated the neoclassical impurity transport, unlike in NSTX, where collisions with C dominated. Furthermore, neoclassical transport coefficients calculated with NCLASS were similar across all impurity species and differed no more than a factor of two, in contrast to NSTX where they differed by an order of magnitude. However, time-independent simulations with MIST indicated that unlike NSTX, neoclassical theory did not fully capture the impurity transport and anomalous transport likely played a significant role in determining impurity profiles.

Lithium plasma facing components↗

Electron Transport in Plasmas with Lithium-Coated Plasma-Facing Components

The Lithium Tokamak Experiment (LTX) is a spherical tokamak designed to study the low-recycling regime through the use of lithium-coated shells conformal to the last closed flux surface (LCFS). A lowered recycling rate is expected to flatten core $T_\mathrm{e}$ profiles, raise edge $T_\mathrm{e}$, strongly affect $n_\mathrm{e}$ profiles, and enhance confinement. To study these unique plasmas, a Thomson scattering diagnostic uses a $\le 20$~J, 30~ns FWHM pulsed ruby laser to measure $T_\mathrm{e}$ and $n_\mathrm{e}$ at 11 radial points on the horizontal midplane, spaced from the magnetic axis to the outer edge at a single temporal point for each discharge. Scattered light is imaged through a spectrometer onto an intensified CCD. The diagnostic is absolutely calibrated using a precision light source and Raman scattering. Measurements of $n_\mathrm{e}$ are compared with line integrated density measurements from a microwave interferometer. Adequate signal to noise is obtained with $n_\mathrm{e} \ge 2 \times 10^{18}\,\mathrm{m^{-3}}$. Thomson profiles of plasmas following evaporation of lithium onto room-temperature plasma-facing components (PFCs) are used in conjunction with magnetic equilibria as input for TRANSP modeling runs. Neoclassical calculations are used to determine $T_\mathrm{i}$ profiles, which have levels that agree with passive charge exchange recombination spectroscopy (CHERS) measurements. TRANSP results for confinement times and stored energies agree with diamagnetic loop measurements. Results of $\chi_\mathrm{e}$ result in values as low as 7 m$^2$/s near the core, which rise to around 100 m$^2$/s near the edge. These are the first measurements of $\chi_\mathrm{e}$ in LTX, or its predecessor, the Current Drive Experiment-Upgrade (CDX-U), with lithium PFCs.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Active lithium analysis for the elimination of battery thermal runaway

Active lithium that is still present in end-of-life batteries poses threats of flammability and reactivity, making disposal and transportation unsafe and costly. OnTo’s deactivation method uses supercritical CO2 to eliminate the hazards of active lithium. Until now, there has been no quantitative method to determine the active lithium content within a battery. The objective of this project is to demonstrate a simple, rapid measurement of active lithium to evaluate battery treatment processes and eliminate class 9 hazards.

battery safety↗

Experimental Activities with the IELLLO Lithium-Lead Facility

Fusion power offers the prospect of an almost inexhaustible source of energy for future generations. Although this may be true, it also presents so far serious scientific and engineering challenges. Breeding Blanket is one of key components of future fusion reactors, since it directly involves tritium breeding and energy extraction, both of them critical to development of fusion power. To deal with the development of Breeding Blankets, ENEA (Italian National Agency for New Technologies, Energy and Sustainable Economic Development) designed and built a lead lithium loop (IELLLO: Integrated European Lead Lithium Loop): the experiment aims to support R and D activities for the conceptual and preliminary design of the European test blanket systems. IELLLO was completed, installed and operated at ENEA Brasimone Research Centre. The purpose of this work is to describe the experimental activities that have been carried out concerning the qualification of the facility, and relative instrumentations, for lead lithium applications. A series of thermo-hydraulic investigations on IELLLO facility has been elaborated: lead lithium pressure transducers, heat exchanger, permanent magnet pumping system, mass flow meters and air cooler have been tested. The absolute pressure meter in contact with Pb-16Li was qualified in pressure range up to 10 bar and temperature up to 400 deg. C. The installation of new kinds of Pb-16Li differential pressure transducers will allow to check the pump characteristic curve and accurately calculate valves pressure drops. These factors could give a better information for the thermo-hydraulic qualification of the facility. Vortex Mass Flow Meter has shown good results in terms of accuracy. The performance has been validated by thermal balance with a dedicated heating system. Nevertheless, the installations of different types of mass flow meters will enable to test IELLLO at ITER relevant conditions, and at lower mass flow rates than those tested up to now. The new pumping system with a PM Pump, was qualified for the first time in Pb-16Li, and the procedure for the operation and maintenance of the pump was developed. The pump is able to supply a mass flow rate in the range from 1.2 to 2.4 kg/s with a temperature of Pb-16Li up to 550 deg. C in the test section. Significant results have been obtained also for the heat exchanger, which has shown high efficiencies, even more than expected. Likewise, the Air Cooler has been verified to be able to cool Pb-16Li in a relatively short time, even at the worst temperature and mass flow conditions. (authors)

42 ENGINEERING↗

Ion-Depleted Microenvironments During Lithium Deposition Revealed by Operando Freezing Cryogenic Electron Microscopy

Local structures and chemistry at active electrochemical interfaces are critical to determining safety, lifetime, and energy density in lithium metal batteries and other devices, but they are challenging to characterize at the nanoscale. We address this issue by developing operando freezing cryogenic electron microscopy (cryo-EM) to preserve battery interfaces in an active state for subsequent high-resolution characterization. We find that ion-depleted microenvironments form locally in the electrolyte adjacent to the lithium deposition interface in lithium metal batteries and are linked to heterogenous growth morphologies. These depleted environments arise locally even under conditions for which ion depletion is not predicted at steady state; this provides a mechanistic explanation for why dangerous lithium morphologies can still propagate in such systems and lead to thermal runaway. Operando freezing cryo-EM thus provides a method to directly visualize nanoscale heterogeneities that arise locally at electrochemical interfaces and play key roles in device failure.

CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSICS,E↗

Improvement in Plasma Performance with Lithium Coatings in NSTX

Lithium as a plasma-facing material has attractive features, including a reduction in the recycling of hydrogenic species and the potential for withstanding high heat and neutron fluxes in fusion reactors. Dramatic effects on plasma performance with lithium-coated plasma-facing components (PFCOs) have been demonstrated on many fusion devices, including TFTR, [1] T-11M, [2] and FT-U. [3] Using a liquid-lithium-filled tray as a limiter, the CDX-U device achieved very significant enhancement in the confinement time of ohmically heated plasmas. [4] The recent NSTX experiments reported here have demonstrated, for the first time, significant and recurring benefits of lithium PFC coatings on divertor plasma performance in both L- and H- mode regimes heated by neutral beams.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Liquid Metal Walls, Lithium, And Low Recycling Boundary Conditions In Tokamaks

At present, the only solid material believed to be a viable option for plasma-facing components (PFCs) in a fusion reactor is tungsten. Operated at the lower temperatures typical of present-day fusion experiments, tungsten is known to suffer from surface degradation during long-term exposure to helium-containing plasmas, leading to reduced thermal conduction to the bulk, and enhanced erosion. Existing alloys are also quite brittle at temperatures under 700oC. However, at a sufficiently high operating temperature (700 - 1000 oC), tungsten is selfannealing and it is expected that surface damage will be reduced to the point where tungsten PFCs will have an acceptable lifetime in a reactor environment. The existence of only one potentially viable option for solid PFCs, though, constitutes one of the most significant restrictions on design space for DEMO and follow-on fusion reactors. In contrast, there are several candidates for liquid metal-based PFCs, including gallium, tin, lithium, and tin-lithium eutectics. We will discuss options for liquid metal walls in tokamaks, looking at both high and low recycling materials. We will then focus in particular on one of the candidate liquids, lithium. Lithium is known to have a high chemical affinity for hydrogen, and has been shown in test stands1 and fusion experiments2,3 to produce a low recycling surface, especially when liquid. Because it is also low-Z and is usable in a tokamak over a reasonable temperature range (200 - 400 oC), it has been now been used as a PFC in several confinement experiments (TFTR, T11- M, CDX-U, NSTX, FTU, and TJ-II), with favorable results. The consequences of substituting low recycling walls for the traditional high recycling variety on tokamak equilibria are very extensive. We will discuss some of the expected modifications, briefly reviewing experimental results, and comparing the results to expectations.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

A Pentafluorophenylboron Oxalate Additive in Non-aqueous Electrolytes 3 for Lithium Batteries

A novel compound named pentafluorophenylboron oxalate (PFPBO) has been synthesized. PFPBO has a unique molecular structure containing a boron atom center with electron deficiency and an oxalate group. It is found that when PFPBO is used as additive, the solubility of lithium fluoride (LiF) or lithium oxide (Li{sub 2}O, Li{sub 2}O{sub 2}) in propylene carbonate (PC) and dimethyl carbonate (DMC) solvents can be increased dramatically. The new electrolytes show high ionic conductivity, high lithium ion transference number and good compatibility with LiMn{sub 2}O{sub 4} cathode and MCMB anode. PFPBO was synthesized with the designed structure to act as a bi-functional additive: boron-based anion receptor (BBAR) additive and stable solid electrolyte interphase (SEI) formation additive in PC-based electrolytes. The results show it does possess these two desired functionalities.

25 ENERGY STORAGE↗

Mesoporous TiO2-B Microspheres with Superior Rate Performance for Lithium Ion Batteries

Mesoporous TiO2-B microsperes with a favorable material architecture are designed and synthesized for high power lithium ion batteries. This material, combining the advantages of fast lithium transport with a pseudocapacitive mechanism, adequate electrode-electrolyte contact and compact particle packing in electrode layer, shows superior high-rate charge-discharge capability and long-time cyclability for lithium ion batteries.

25 ENERGY STORAGE↗

Functionalizing the Surface of Lithium-Metal Anodes

Metal-air batteries are an important aspect of many beyond lithium ion research efforts. However, as our understanding of how molecular oxygen can act as a rechargeable cathode has progressed; the problems associated with how these materials at various states of charge interact with the lithium metal anode are only beginning to come to the surface. In this study we have devised a method to coat the surface a lithium with a functional group to act as either an anchor for further derivation studies or be polymerized to create a nanometer thick polymer coating attached to the surface by silane groups. These stable films, formed by polymerization of vinyl substituents, lower cell impedance at the electrode and over the first 50 cycles, increase cycling efficiency and demonstrate lower capacity fade.

25 ENERGY STORAGE↗

Tackling issues of lithium metal anodes with a novel polymeric lithicone coating

Lithium metal (Li) has been hindered from as anodes in commercial batteries for over 50 years, due to two main issues: continuous formation of solid electrolyte interphase (SEI) and lithium dendritic growth. In this work, we report a new strategy to tackle these issues, i.e., using molecular layer deposition (MLD) to grow an ionically conducting but electrically insulating polymeric lithicone coating, an Li-containing triethanolamine (LiTEA). Our electrochemical tests revealed that this LiTEA coating could serve as an exceptional protection layer over Li anodes. Consequently, the LiTEA-coated Li electrodes could achieve a superior cyclability of > 10000 Li stripping/plating cycles at a current density of 5 mA cm -2 and a long cyclability of > 5500 cycles at 2 mA cm -2 in Li||Li symmetric cells without failures, under a fixed areal capacity of 1 mAh cm -2 . Characterizations using scanning electron microscopy and X-ray photoelectron microscopy verified that Li + ions could be easily extracted through and deposited under the LiTEA coating during the stripping/plating processes. Consequently, this LiTEA coating significantly inhibited the formation of SEI and Li dendrites. This underlies the long cycling lifetime of the LiTEA-coated Li||Li cells. Coupling with the nickel-rich LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes, more encouragingly, the LiTEA-coated Li anodes could remarkably extend the cyclability and sustainable capacity of the resultant Li||NMC full cells. Finally, we also demonstrated that the performance of Li||NMC cells could be further improved through combining an LiTEA-coated Li anode with an Li 2 S-modified NMC811 via atomic layer deposition (ALD). Thus, this study is inspiring for developing high-energy Li||NMC lithium metal batteries.

25 ENERGY STORAGE↗