Investigating Deep Material Networks as Representative Microstructures for the Mechanical Behavior of Composites
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Presentation for American Welding Society Professional Program 2025.
Explore the source record for details and available documents.
This is my paper for the 2025 AIAA SciTech conference. The submission is due 12/09.
Additively printed Ni-based superalloy with a compositionally graded transition from IN718 to René41 was fabricated by laser blown-powder directed energy deposition (DED/LB-M), with the goals of meeting location-specific temperature capability and reducing component cost for hot gas path turbine components. Residual stress distribution in thin wall specimens with three sets of DED build parameters in the as-built and stress-relieved states was measured by neutron diffraction. For calculating residual stress, the calculated d0 method was found to be more appropriate as stress-free reference than using the lattice spacing measured from the stress-relief heat treated specimens. Longer dwell time (lower interpass temperature), higher energy input, smaller layer thickness resulted in a higher magnitude of tensile residual stresses at edges and compressive residual stresses at center of the specimens. The residual stress results did not show a strong dependence on graded compositions, indicating that the residual stress build-up was more geometry and process dependent. Non-destructive neutron imaging based on the attenuation coefficient qualitatively visualized the compositional variation in the bulk and showed good agreement with quantitative Electron Probe Micro-Analysis (EPMA) measurement. Grain structure, texture, and residual plastic strain along the build direction were characterized by Electron Backscatter Diffraction (EBSD). Long columnar grains with (001) preferred grain orientation were dominant along the build direction. Compositional change did not show an obvious effect on the epitaxial growth of dendrites and the continuation of the columnar grains. Residual plastic strain was relatively low in the as-built specimens.
Due to the growing number of people infected with the new coronavirus globally, which weakens immunity, there has been an increase in bacterial infections. Hence, knowledge about simple and low-cost synthesis methods of materials with good structural and antimicrobial properties is of great importance. A material obtained through the combination of a nanoscale hydroxyapatite material (with good biocompatibility) and titanium dioxide (with good degradation properties of organic molecules) can absorb and decompose bacteria. In this investigation, three different synthesis routes used to prepare hydroxyapatite/titanium dioxide nanomaterials are examined. The morphology and semiquantitative chemical composition are characterized by scanning electron microscopy with energy dispersive X-ray analysis (SEM-EDX). The obtained materials’ phase and structural characterization are determined using the X-ray powder diffraction method (XRD). The crystallite sizes of the obtained materials are in the range of 8 nm to 15 nm. Based on XRD peak positions, the hexagonal hydroxyapatite phases are formed in all samples along with TiO 2 anatase and rutile phases. According to SEM and TEM analyses, the morphology of the prepared samples differs depending on the synthesis route. The EDX analysis confirmed the presence of Ti, Ca, P, and O in the obtained materials. The IR spectroscopy verified the vibration bands characteristic for HAp and titanium. The investigated materials show excellent antimicrobial and photocatalytic properties.
Friction stir welded (FSW) aluminum–magnesium lightweight vehicle joints have gained significant interest due to their high strength-to-weight ratio. In this work, the corrosion resistance of this material is analyzed through electrochemical tests, which include open circuit potential (OCP) inspection and potentiodynamic polarization (PD) scanning. Weight loss measurements tested the corrosion rate of the FSW weld through cyclic corrosion testing (CCT) according to the standard SAEJ 2334. Mechanical properties were also investigated, including lap-shear strength, micro- and nano-hardness mapping, and true stress–strain curves as a function of local processing history. The electrochemical results indicate that the center weld zone’s corrosion property stays between the two base alloys. Indentation-based testing demonstrated that the weld zone behaves differently from base alloys. Lap shear strength surprisingly did not drop much even after eight weeks of cyclic corrosion tests, indicating that the joint did not allow any ingress of the electrolyte.
Dry storage canisters of used nuclear fuels are fabricated using SUS 304L stainless steel. Chloride-induced stress corrosion cracking (CISCC) is one of the major failure modes of dry storage canisters. The cracked canisters can be repaired by friction stir welding (FSW), a low-heat input ‘solid-phase’ welding process. It is important to evaluate the ClSCC resistance of the friction stir welded material. Stress corrosion cracking (SCC) studies were carried out on mill-annealed base materials and friction stir welded 304L stainless U-bend specimens in 3.5% NaCl + 5 N H2SO4 solution at room temperature and boiling MgCl2 solution at 155 °C. The engineering stress on the outer fiber of the FSW U-bend specimen was ~60% higher than that of the base metal (BM). In spite of the higher stress level of the FSW, both materials (FSW and BM) showed almost similar SCC failure times in the two different test solutions. The SCC occurred in the thermo-mechanically affected zone (TMAZ) of the FSW specimens in the 3.5% NaCl + 5 N H2SO4 solution at room temperature, while the stirred zone (SZ) was relatively crack-free. The failure occurred at the stirred zone when tested in the boiling MgCl2 solution. Hydrogen reduction was the cathodic reaction in the boiling MgCl2 solution, which promoted hydrogen-assisted cracking of the heavily deformed stirred zone. The emergence of the slip step followed by passive film rupture and dissolution of the slip step could be the SCC events in the 3.5% NaCl + 5 N H2SO4 solution at room temperature. However, the slip step height was not sufficient to cause passivity breakdown in the fine-grained SZ. Therefore, the SCC occurred in the partially recrystallized softer TMAZ. Overall, the friction-stirred 304L showed higher tolerance to ClSCC than the 304L base metal.
Helium bubbles are known to form in nuclear reactor structural components when displacement damage occurs in conjunction with helium exposure and/or transmutation. If left unchecked, bubble production can cause swelling, blistering, and embrittlement, all of which substantially degrade materials and—moreover—diminish mechanical properties. On the mission to produce more robust materials, nanocrystalline (NC) metals show great potential and are postulated to exhibit superior radiation resistance due to their high defect and particle sink densities; however, much is still unknown about the mechanisms of defect evolution in these systems under extreme conditions. Here, the performances of NC nickel (Ni) and iron (Fe) are investigated under helium bombardment via transmission electron microscopy (TEM). Bubble density statistics are measured as a function of grain size in specimens implanted under similar conditions. While the overall trends revealed an increase in bubble density up to saturation in both samples, bubble density in Fe was over 300% greater than in Ni. To interrogate the kinetics of helium diffusion and trapping, a rate theory model is developed that substantiates that helium is more readily captured within grains in helium-vacancy complexes in NC Fe, whereas helium is more prone to traversing the grain matrices and migrating to GBs in NC Ni. Our results suggest that (1) grain boundaries can affect bubble swelling in grain matrices significantly and can have a dominant effect over crystal structure, and (2) an NC-Ni-based material can yield superior resistance to irradiation-induced bubble growth compared to an NC-Fe-based material and exhibits high potential for use in extreme environments where swelling due to He bubble formation is of significant concern.
Understanding mineral–fluid interactions in shale under supercritical CO 2 (scCO 2 ) conditions is relevant for assessing long-term geochemical containment. This study characterizes mineralogical transformations and elemental redistribution in five Caney Shale samples serving as proxies for reservoir (R1, R2, R3) and caprock (D1, D2) facies, subjected to 30-day static exposure to pure scCO 2 at 60 °C and 17.23 MPa (2500 psi), with no brine or impurities introduced. SEM-EDS analyses were conducted before and after exposure, with mineral phases classified into silicates, carbonates, sulfides, and organic matter. Initial compositions were dominated by quartz (38–47 wt.%), illite (16–23 wt.%), carbonates (12–18 wt.%), and organic matter (8–11 wt.%). Post-exposure, carbonate loss ranged from 15 to 40% in reservoir samples and up to 20% in caprock samples. Illite and K-feldspar showed depletion of Fe 2+ , Mg 2+ , and K + at grain edges and cleavages, while pyrite underwent oxidation with Fe redistribution. Organic matter exhibited scCO 2 -induced surface alteration and apparent sorption effects, most pronounced in R2 and R3. Elemental mapping revealed Ca 2+ , Mg 2+ , Fe 2+ , and Si 4+ mobilization near reactive interfaces, though no secondary mineral precipitates formed. Reservoir samples developed localized porosity, whereas caprock samples retained more structural clay integrity. The results advance understanding of mineral reactivity and elemental fluxes in shale-based CO 2 sequestration.
U3Si2 is a long term, accident-tolerant nuclear fuel candidate for light-water reactors because of its superior thermal conductivity and increased uranium density when compared to traditional uranium dioxide (UO2). While reducing internal thermal stresses and increasing efficiency, U3Si2 exhibits energetic oxidation during certain off-normal and accident scenarios, which include coolant or steam exposure. To mitigate this, Nb is investigated as an alloy constituent to enhance corrosion resistance and increase mechanical strength. The work presented investigates the response of Nb-alloyed U3Si2 to steam atmospheres. A thermogravimetric analysis is conducted in flowing steam to T > 1000 °C to assess oxidation resistance. The phase characterization of as-melted, thermally annealed and post-oxidation compositions with up to 12 vol% Nb by powder X-ray diffraction, scanning electron microscopy, and energy dispersive spectroscopy is reported.
Two-dimensional (2D) materials are uniquely suited for highly anisotropic thermal transport, which is important in thermoelectrics, thermal barrier coatings, and heat spreaders. Solution-processed 2D materials are attractive for simple, low-cost, and large-scale fabrication of devices on, virtually, any substrate. However, to date, there are only few reports with contrasting results on the thermal conductivity of graphene films, while thermal transport has been hardly measured for other types of solution-processed 2D material films. In this work, inkjet-printed graphene, h-BN and MoS2 films are demonstrated with thermal conductivities of ∼10 Wm−1K−1 and ∼0.3 Wm−1K−1 along and across the basal plane, respectively, giving rise to an anisotropy of ∼30, hardly dependent on the material type and annealing treatment. First-principles calculations indicate that portion of the phonon spectrum is cut-off by the quality of the thermal contact for transport along the plane, yet the ultra-low conductivity across the plane is associated with high-transmissivity interfaces. These findings can drive the design of highly anisotropic 2D material films for heat management applications.
Austenitic stainless steels are commonly used for hydrogen storage and transportation. These alloys have a high nickel (Ni) content, which increases alloy cost. In this study, high manganese (Mn) austenitic alloys were evaluated as potential lower cost alternatives. Two heats of high Mn alloys with different stacking fault energies (SFE) of ~29 mJ·m -2 and 49 mJ·m -2 were acquired. Additionally, a new vanadium (V)-microalloyed high Mn alloy was designed to achieve a SFE of 47 mJ·m -2 to minimize planar slip deformation mechanisms. Post-processing via cold working in conjunction with aging was also performed on the V-microalloyed high Mn steel. Hydrogen embrittlement sensitivity was investigated using circumferential notch tensile specimens cathodically charged with hydrogen in a 0.05M NaOH electrolytic solution. The alloys were compared to a cold-worked 316L stainless steel, which exhibited no strength loss due to hydrogen. The high Mn alloys with SFE of ~29 mJ·m 2 and 49 mJ·m -2 had notch strength losses of 11 and 6 pct, respectively. The V-microalloyed high Mn steel in the as-hot-rolled condition had a notch strength loss of 17 pct. Furthermore, the V-microalloyed high Mn steel in the cold worked and aged condition indicated no notch strength loss in hydrogen, which was comparable to the performance of the 316L stainless steel.
Explore the source record for details and available documents.
Explore the source record for details and available documents.