Dissimilar joining of ZEK100 and AA6022 for automotive application

Mg and Al joining is problematic due to different high temperature flow characteristics that often results in weld defects and brittle intermetallic compounds (IMC). We present process development on lap joining of 1.27 mm 6022 (top sheet) and 1.5mm ZEK100 (bottom sheet) for an automotive door application. We conducted process development in linear welding using power control mode (modulating torque and spindle speed) with multiple tool designs, and welding parameters. Process variables were correlated to joint micro-structure and mechanical properties. A 2D computational model was created to understand the failure mechanism and contribution of mechanical interlocking towards joint strength. For a thin (< 2 mm) automotive sheet with softer material as a bottom sheet, adequate control of process variables is critical to maintain weld stability and avoid excessive IMC layer at the interface. A combination of mechanical anchoring and metallurgical reaction is likely responsible for bonding.

Das, Hrishikesh↗

Abnormal grain growth suppression in Al alloys

The present invention provides a process for suppressing abnormal grain growth in friction stir welded aluminum alloys by inserting an intermediate annealing treatment (“IAT”) after the welding step on the article. The IAT may be followed by a solution heat treatment (SHT) on the article under effectively high solution heat treatment conditions. In at least some embodiments, a deformation step is conducted on the article under effective spin-forming deformation conditions or under effective superplastic deformation conditions. The invention further provides a welded article having suppressed abnormal grain growth, prepared by the process above. Preferably the article is characterized with greater than about 90% reduction in area fraction abnormal grain growth in any friction-stir-welded nugget.

Hales, Stephen J.↗

ADDITIVE MANUFACTURING AND REGULATORY TESTING OF CANISTERS FOR SPENT NUCLEAR FUEL MANAGEMENT

The back end of the fuel cycle focuses on the interim storage, transportation, and final disposition of the spent nuclear fuel from nuclear reactors. Commercial light water nuclear power stations across the United States operate with fuel assemblies being irradiated for up to 6 years (planned) in the reactor pressure vessel. After their planned irradiation, the fuel assemblies are moved to a spent fuel pool within the facility complex. After the spent nuclear fuel is removed from the fuel pool, it is typically inserted into a welded metal canister that can be transferred between overpacks for storage, transportation and possibly disposal. Most dry storage systems being used by industry today use dual purpose canisters (DPCs), designed for use in storage and transportation overpacks, but not specifically designed for disposal. Triple purpose-canisters, designed for disposal in addition to storage and transportation, have also been researched. Traditional manufacturing methods for spent fuel canisters involve fusion welding along the length or circumference of the canister which results in high tensile residual stresses in the joint weld zone (WZ) and heat affected zone (HAZ). In this paper, spent fuel canister designs were printed by wire arc additive manufacturing (AM) using the 316L SS welding wire to demonstrate: 1. Feasibility of spent nuclear fuel canister fabrication using this advanced manufacturing method, 2. Dynamic response of the additive manufacture canister design when subjected to the federally mandated Normal Conditions of Transport (NCT) and Hypothetical Accident Conditions (HAC) physical tests for Type B packages. This paper will focus on the canister printing design and structural tests. The AM 3D printed design, regulatory testing, and post-test evaluation of the canister tested to the 10 CFR 71.71 and 10 CFR 71.73 requirements will be presented. One AM canister design was subjected to the penetration, free drop, and puncture test. Before and after the dynamic structural tests, the AM canister design was scanned with a handheld scanner to capture a 3D CAD geometry to compare to the 3D printed canister design in the deformed shape. The scanned geometry was sectioned in areas with deformation and the cross-section profile was measured to determine accurate and repeated results of the deformed shape of the AM canister design.

Martinez, Oscar↗

APR1400 In-Core Instrumentation Penetration Failure by Zirconia Melt

Light water reactors have many penetrations at the reactor vessel lower head which are called ICI (in-core instrumentation tubes), ICM-GT (in-core monitoring guide tubes), CRGT (control rod guide tubes) and drain tubes. For Korean PWRs (pressurized water reactors), there are dozens of bottom-up type ICI penetration tubes (45 for OPR1000 and 61 for APR1400). For the typical BWRs (boiling water reactors), hundreds of penetrations are positioned at the reactor vessel lower head due to the structural complexity at the reactor upper head. These penetrations are regarded as the most vulnerable structures during a severe accident as they could be failed by high temperature of melt (or debris) and its decay heat. That is, tube rupture and/or tube ejection could occur because there exist an empty hole inside the penetration tube which can be a melt flow path, and they are attached to the inside of the reactor vessel by a partial weld with a gap between the tubes and reactor vessel. Therefore, the research on the penetration failure is of importance, as it could lead to melt discharge into the containment and subsequent release of radioactive materials to the environment due to the containment failure. This paper focuses on the experimental investigation on the tube ejection failure for the APR1400 ICI penetration. The tube ejection experiments were performed as it was exposed to high temperature of zirconia melt and high pressure. The tube ejection failure experiments were performed for the APR1400 in-core instrumentation penetration nozzle. Zirconia melt was used as a simulant of molten corium and interacted with the penetration specimen. The specimen was pressurized up to 2.6 bar during the interaction with melt to induce the tube ejection. The penetration weld was heated up to its melting temperature, and the penetration tube and weld above the reactor vessel surface were eroded severely by the melt. However, even though it was estimated that the weld failure occurred and the reactor vessel with stainless steel cladding was ablated severely by the melt, the tube ejection did not take place, and consequently the integrity for the APR1400 ICI penetration was confirmed in the present experimental conditions. The goal of this research is to improve the penetrations failure models in MAAP5 codes based on the experimental data. To achieve this goal, it is necessary to increase the heat flux and pressure acting on the penetration tube to find the conditions for the tube ejection failure. Moreover, the penetration failure experiments will be performed by delivering melt into the penetration specimen to simulate the melt relocation process in a real severe accident situation. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Progress on Advancing Robotic Ultrasonic Volumetric Inspection Technology for Hanford Under-tank Inspection - 19474

The Hanford River Protection Project is reliant on safe interim storage of high-level waste at the Hanford site and will continue to depend on it until the waste has been treated and vitrified by the Hanford Waste Treatment and Immobilization Plant (WTP). The Hanford double-shell tanks (DSTs) have provided interim storage since the DSTs were put into service (1971 - 1986) and the RPP will continue to rely on their service until least 2050, at which time the 27 in-service DSTs will be 14-54 years beyond their original design lives. As the DSTs continue to age and be operated beyond design life, reliable leak integrity assessments of primary tanks and secondary liners will become increasingly important in order to provide situational awareness to tank operations personnel and to support risk-informed decisions on the selection of DSTs as waste feed staging tanks and the order and timing of future DST refurbishment or, alternatively, DST retrieval sequence. This paper summarizes progress made in fiscal year (FY) 2018 on the engineering of a robotic air-slot volumetric inspection system (RAVIS) that is designed to perform ultrasonic (volumetric) leak integrity inspections of physically inaccessible primary tank bottom plates and welds. Leak integrity inspections performed with the RAVIS will supplement today's primary tank leak integrity inspections, which are currently limited to physically accessible sidewall plates and welds. The RAVIS will be deployed into air slots of the insulating concrete (refractory) pad beneath the primary tanks and use its ultrasonic guided wave phased-array (GWPA) sensor to electronically steer an ultrasonic beam 360-degrees around the sensor to volumetrically examine adjacent carbon steel plates and welds covered by refractory pad material. Deployments of RAVIS down multiple air-slots will be performed to determine which regions of a tank bottom have sound leak integrity or which regions are in need of future wall thickness restoration or weld repair due to pitting corrosion, general corrosion, or heat/stress-induced cracks. The initial RAVIS design and the flaw detection test results for the first air-slot GWPA sensor that was designed to fit inside the air-slots will be presented in this paper. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Design, Fabrication and Testing of Surveillance Test Articles for MSR Materials Degradation Management

This report details the design, fabrication, and testing of surveillance test articles aimed at assessing material damage in reactor-relevant environments for effective degradation management. Two types of surveillance test articles with reduced sizes were developed based on design algorithms and finite element modeling: welded design and interlocking design. A furnace heating setup was adopted to apply multiple thermal cyclic loading profiles on the test articles with a temperature range of 500°C - 700°C, while the strain response was monitored using a digital image correlation technique. The testing results demonstrated the successful capturing of expected strain range for welded design while machining tolerance should be improved to engage strain coupling in the interlocking design. Mid-term (500 hours) and long-term (1500 hours) cyclic tests were conducted on welded test articles. A constant strain range of ~0.6% was observed at the specimen with testing under 500 hours, while a gradual decrease of strain at specimen was observed after 500 hours. Non-destructive evaluation through X-ray computed tomography confirmed the microcracks in the welds at specimen-driver joints after cyclic test that caused the strain change. Creep testing of the specimen after long-term cyclic test revealed a short creep life than expected. A multi-profile cyclic test was also conducted on a test article and demonstrated consistent strain response under different temperature ramp rates. The report also briefly discussed the challenges and future research efforts to advance test article development for material surveillance.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Titanium Wire Arc Additive Manufacturing Inert Enclosure and Material Handling Safety Considerations

Wire arc additive manufacturing (WAAM) via metal inert gas (MIG)/gas metal arc welding (GMAW) is a viable option for fabrication of large-scale titanium parts; however, it introduces new safety hazards associated with both the material and the additional system hardware required for the process. Localized gas shielding of the weld arc via standard GMAW torch is inadequate for titanium due to its affinity for oxygen; thereby requiring the use of an inert enclosure to protect the weld from entraining oxygen. The use of the inert enclosure presents potential safety hazards such as operator asphyxiation and brings up discussion of confined space considerations. In addition, the titanium welding process creates pyrophoric titanium soot residue around the deposit, which can undergo deflagration during part cleaning and part removal. This paper provides an overview of the titanium WAAM process along with safety considerations for the design and operation of the inert enclosure as well as functional solutions for the safe handling of the titanium soot by-product.

Walters, Alex↗

Structure and crystallography of martensite–austenite constituent in the intercritically reheated coarse-grained heat affected zone of a high strength pipeline steel

Highlights: • Structure and crystallography of M-A constituent in ICCGHAZ of X100 weld joint was studied via multi-scale characterization. • Majority of M-A constituent preferred to form lamellar lath structure, which primarily consisted of lath martensite (87%). • The retained austenite had K-S orientation relationship with its neighboring martensite. • Adjacent martensite laths within M-A had large misorientation but no fixed crystallographic orientation relationship. • Martensite laths within the M-A constituent did not inherit the crystallographic orientation of the parent matrix. - Abstract: The structure and crystallography of martensite-austenite (M-A) constituent in the intercritically reheated coarse-grained heat affected zone (ICCGHAZ) of X100 (690 MPa) pipeline steel weld joint was studied via multi-scale characterization. The results suggested that majority of the necklace-type M-A constituent in the ICCGHAZ preferred to form lamellar lath structure, which primarily consisted of lath martensite (87%). Only small fraction of retained austenite (9%) was found between martensite laths. The retained austenite had K-S orientation relationship with its neighboring martensite: (10-1){sub M} // (11-1){sub γ} and [111]{sub M} // [011]{sub γ}. Adjacent martensite laths within M-A constituent had large misorientation but no fixed crystallographic orientation relationship which implied that martensite laths may nucleate independently and encounter with each other during growth. M-A constituent and matrix microstructure belonged to different prior austenite grains. The martensite laths within the M-A constituent did not inherit the crystallographic orientation of the parent matrix during the intercritical reheating and subsequent cooling process of the second pass welding.

36 MATERIALS SCIENCE↗

Characterization of different forms of Zr-2.5Nb samples before and after neutron irradiation

Deleterious effects of hydride precipitation on the mechanical properties of Zr-based alloy systems have been studied for many years. Most of these studies have been conducted at high-temperature irradiation conditions that are compatible with those in commercial reactor systems, such as light water and pressurized water reactors. Evaluations of hydride effects on the mechanical properties of welded Zr-2.5Nb are sparse among these reported studies. Research on the mechanical properties of Zr-based alloys neutron irradiated at low temperatures (<100 °C) is also very rare in the literature. Since some companies are interested in using Zr-based alloys as structural materials and in other parts such as pressure tubes in small reactor systems, low-temperature irradiation studies of these materials are important. The current work presents an evaluation of the tensile properties of Zr-2.5Nb welded using tungsten inert gas and electron beam welding as a function of hydrogen charging and neutron irradiation at low temperatures (60–100 °C).

36 MATERIALS SCIENCE↗

Design and Manufacturing Criteria for Beam Position Monitor (BPM) of Taiwan Photon Source (TPS)

There are quite some considerations when the button feedthrough is designed and manufactured in a new 3rd generation synchrotron light source like the to-be-constructed TPS. It is the responsibility of the button feedthrough designer to design a feedthrough with the lowest probable HOM problem. It is also required for the designer to analyze the consequences for each possible mechanical error during manufacturing and therefore set standards of tolerance. We have been using MAFIA to optimize the design of feedthrough including flange type on bending chamber section and primary BPM on insertion device section. We also have set some criteria for feedthrough manufacturing, inspection, and welding based on hands-on experience on feedthrough electrical properties measuring, sorting, inspection, and laser welding. Here we will present the MAFIA results, electrical measurement results, and laser welding results and analysis. Criteria based on these results will also be presented.

43 PARTICLE ACCELERATORS↗

Structure and constitution of glass and steel compound in glass-metal composite

The research using methods of optical and scanning electronic microscopy was conducted and it discovered common factors on structures and diffusing zone forming after welding glass C49-1 and steel Ct3sp in technological process of creating new glass-metal composite. Different technological modes of steel surface preliminary oxidation welded with and without glass were investigated. The time of welding was varied from minimum encountering time to the time of stabilizing width of diffusion zone.

36 MATERIALS SCIENCE↗

Preliminary Analysis of the General Performance and Mechanical Behavior of Irradiated FeCrAl Base Alloys and Weldments

The iron-based, iron-chromium-aluminum (FeCrAl) alloys are promising, robust materials for deployment in current and future nuclear power plants. This class of alloys demonstrates excellent performance in a range of environments and conditions, including high-temperature steam (>1000°C). Furthermore, these alloys have the potential to have prolonged survival under loss-of-coolant accident (LOCA) conditions compared to the more traditional cladding materials that are either Zr-based alloys or austenitic steels. However, one of the issues associated with FeCrAl alloys is cracking during welding. The present project investigates the possibility of mitigating welding-induced cracking via alloying and precise structure control of the weldments; in the frame work of the project, several advanced alloys were developed and are being investigated prior to and after neutron irradiation to provide insight into the radiation tolerance and mechanical performance of the weldments. The present report provides preliminary results on the post-irradiation characterization and mechanical tests performed during United States Fiscal Year (FY) 2016. Chapter 1 provides a general introduction, and Chapter 2 describes the alloy compositions, welding procedure, specimen geometry and manufacturing parameters. Also, a brief discussion of the irradiation at the High Flux Isotope Reactor (HFIR) is provided. Chapter 3 is devoted to the analysis of mechanical tests performed at the hot cell facility; tensile curves and mechanical properties are discussed in detail focusing on the irradiation temperature. Limited fractography results are also presented and analyzed. The discussion highlights the limitations of the testing within a hot cell. Chapter 4 underlines the advantages of in-situ testing and discusses the preliminary results obtained with newly developed miniature specimens. Specimens were moved to the Low Activation Materials Development and Analysis (LAMDA) laboratory and prepared for mechanical tests. Tensile tests were conducted at LAMDA using a modern digital image correlation approach allowing for strain distribution analysis. Plastic strain initiation and necking are discussed in detail; a concept of strain rate maps is also introduced and discussed. Follow-on SEM-EBSD and FIBTEM analysis is planned.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Optical Evidence of Compositional Fractioning between Plasma‐Condensed and Melt Pool Matter

Control of multicomponent alloys during welding is challenging because it lacks a real‐time understanding of composition. The optical emissions of plasma formed during laser‐induced metal welding correlate with the composition of particles ejected from the melt pool. Plasma emissions observed in this study contain large iron, manganese, chrome, and copper signatures, which match the composition of emitted particles. Particles recovered closest to the melt pool exhibit a core–shell morphology that is composed of iron‐manganese‐chrome intermetallic cores within copper shells. Particles collected farther from the melt pool, do not share this core–shell morphology, though similar elemental compositions are observed. The correlation between plasma optical emissions and particle composition can be used to predict the composition of the melt pool, allowing for real‐time welding and sintering control.

36 MATERIALS SCIENCE↗

Design, Development and Testing of Inconel Alloy IN718 Spherical Gas Bottle for Oxygen Storage

This paper describes the details of design, manufacture and testing of 200 mm diameter spherical gas bottle of Inconel 718 (IN718) with nominal wall thickness of 2.3 mm. Gas bottle was designed for the specified internal pressure loading with a thickness of 2.9 mm at the circumferential weld which was brought down to 2.3 mm at the membrane locations. Hemispherical forgings produced through closed-die hammer forging were machined and electron beam welded to produce a spherical gas bottle. Duly welded gas bottle was subjected to standard aging treatment to achieve the required tensile strength. Aged gas bottle was inspected for dimensions and other stringent quality requirements using various nondestructive testing techniques. After inspection, gas bottle was subjected to pressure test for maximum expected operating pressure and proof pressure of 25 and 37.5 MPa, respectively. Strain gauges were bonded at different locations on the gas bottle to monitor the strains during the pressure test and correlated with the predicted values. The predicted strain matched well with the experimental strain confirming the design and structural integrity.

36 MATERIALS SCIENCE↗

Influence of Rotation Rate on Microstructure and Comprehensive Performance of FSWed Mg Alloy

Die-casting AZ31 Mg alloys were successfully friction stir welded at a constant welding speed and different rotation rates. More uniform and fine grains were obtained at the rotation rate of 1400 rpm due to more suitable temperature for dynamic recrystallization in this welding condition. In addition, the intensity of (0001) texture in stir zone increased with the increasing rotation rate. The results of mechanical property test indicated joint with rotation rate of 1400 rpm had better tensile property, which was associated with fine grains, uniform transition in the interface between thermo-mechanically affected zone and stir zone as well as more favorable Schmidt factor for basal slip and twinning. The corrosion resistance of joints increased with the increasing rotation rate, which is significantly related to the (0001) texture with basal plane parallel to the corroded surfaces.

36 MATERIALS SCIENCE↗

Impact of neutron irradiation on mechanical performance of FeCrAl alloy laser-beam weldments

Oxidation-resistant iron-chromium-aluminum (FeCrAl) alloys demonstrate better performance in Loss-of-Coolant Accidents, compared with austenitic- and zirconium-based alloys. However, further deployment of FeCrAl-based materials requires detailed characterization of their performance under irradiation; moreover, since welding is one of the key operations in fabrication of light water reactor fuel cladding, FeCrAl alloy weldment performance and properties also should be determined prior to and after irradiation. In this paper, advanced C35M alloy (Fe-13%Cr-5%Al) and variants with aluminum (+2%) or titanium carbide (+1%) additions were characterized after neutron irradiation in Oak Ridge National Laboratory's High Flux Isotope Reactor at 1.8–1.9 dpa in a temperature range of 195–559 °C. Specimen sets included as-received (AR) materials and specimens after controlled laser-beam welding. Tensile tests with digital image correlation (DIC), scanning electron microscopy-electron back scatter diffraction analysis, fractography, and x-ray tomography analysis were performed. DIC allowed for investigating local yield stress in the weldments, deformation hardening behavior, and plastic anisotropy. Finally, both AR and welded material revealed a high degree of radiation-induced hardening for low-temperature irradiation; however, irradiation at high-temperatures (i.e., 559 °C) had little overall effect on the mechanical performance.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of thermal and thermo-mechanical cycling on the boron segregation behavior in the coarse-grained heat-affected zone of low-alloy steel

The boron segregation behavior in the coarse-grained heat-affected zone (CGHAZ) of 10 ppm boron-added low-alloy steel during the welding cycle was investigated by taking the changes in the microstructure and hardness into account. Various CGHAZs were simulated with a Gleeble system as a function of the heat input and external stress, and the boron segregation behavior was analyzed by secondary ion mass spectrometry (SIMS) and particle tracking autoradiography (PTA). The segregation of boron was found to initially increase, and then decrease with an increase in the heat input. This is believed to be due to the back-diffusion of boron with an increase in the exposure time at high temperature after non-equilibrium grain boundary segregation. The grain boundary segregation of boron could be decreased by an external stress applied during the welding cycle. Such behavior may be due to an increase in the grain boundary area as a result of the grain size reduction induced by the external stress. - Highlights: • Boron segregation behavior in the CGHAZ of low-alloy steel during a welding cycle was investigated. • Various CGHAZs were simulated with a Gleeble system as a function of the heat input and external stress. • Boron segregation behavior was analyzed using SIMS and PTA techniques.

36 MATERIALS SCIENCE↗

Validation of Manufacturing Process Designs for Stamped Microchannel Recuperators

Microchannel recuperators can achieve high-efficiency power cycles and chemical reactions by recovering waste heat from hot turbine exhaust and chemical reaction streams. However, the industrial application of microchannel recuperators are restricted by the high cost of patterning and bonding. The objective of this study was thus to investigate new methods for producing microchannel recuperators for emerging markets. Based on greenfield cost estimates, process designs based on stamping, laser welding and vacuum brazing of 316L stainless steel laminae were found to be more economical than conventional photochemical machining and diffusion bonding. Subsequently, validation experiments were conducted to produce stamped microchannel components using cost model parameters. At a mass flow rate of 0.99 g/s, the test article made with laser welding was found to provide higher effectiveness than the test article produced using vacuum brazing. Preliminary investigations showed that residual stresses during laser welding of the laminae led to significant warpage, collapsing channels and making lamina-to-lamina fit up challenging. In contrast, the test article produced by vacuum brazing of stamped laminae showed no clogging and 4.6% and 10.5% channel height standard deviation for the cold and hot channels, respectively. Channel variation in the vacuum brazing sample was determined to be caused by misregistration of laminae during brazing. In future work, efforts are needed to choose cheaper, more ductile brazing foils as well as design a brazing fixture to improve lamina-to-lamina registration.

42 ENGINEERING↗