A study on the assessment criteria of DHC in PWR spent fuel

One of the major degradation mechanisms of PWR spent fuel cladding is delayed hydride cracking (DHC), which can activate within a relatively low temperature range. Its maximum crack growth rate is estimated to be within the range of 10{sup -7} m/s, at which the cladding can rupture in 1 to 2 years during dry storage. For this reason, it is essential to prevent DHC crack growth itself, but most of the existing DHC studies have been focused on the crack growth rate. In this regard, the values and characteristics of the threshold stress intensity factor (K{sub IH}) for PWR Zircaloy-4 cladding were described. Based on the limited existing test results and analysis, the experimentally measured K{sub IH} were compared with the predicted K{sub IH}. The comparison shows that the predicted values are much lower than the measured ones and both theoretical estimation and measured values of K{sub IH} increase as the temperature increases. The possibilities of degradation by DHC were also discussed during long-term dry storage. For a more reliable analysis, additional information on a pre-existing crack of spent fuel is needed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Advances in Westinghouse fuel rod design technology (PAD5)

The Westinghouse Performance Analysis and Design (PAD) code for light-water reactors has been recently updated to version PAD5 and submitted to NRC for review. PAD5 incorporates extensive updates in fuel performance and material property models, including fuel thermal conductivity, pellet fragment relocation, fission gas release, fission gas swelling, and cladding creep and growth. Advances in thermal models are mainly in pellet fragment relocation, radial power distribution within the pellet, and the changes in fuel thermal conductivity due to changes in temperature, burnup and fuel porosity. The PAD5 thermal fission gas release model is a phenomenological model based on the irradiation dependence of the gas release from mechanistic processes for the diffusion of the fission gas generated in the fuel grains to the grain boundaries, formation of fission gas bubbles on the grain boundaries and release of the fission gas when these grain boundary bubbles inter-link. The PAD5 cladding creep model is predominantly a combination of the following mechanisms: thermal creep, irradiation induced creep, and irradiation enhanced creep. The fuel performance database used for the development, calibration and testing of the PAD5 code covers a broad range of both commercial irradiation data and test rod data and requires continuously additional data focusing on the latest development of the PAD5 code. Test programs are also included in the database. These data are checked and stored in a hierarchical database structure that supports the automation of model development and calibration. New data, once incorporated into the database, can be quickly evaluated with respect to key fuel and cladding performance models to confirm expected trends or to evaluate potential model improvements. This automated calibration system has been integrated with state-of-the-art optimization packages in DAKOTA Analysis Kit to provide for advanced statistical assessments and model coefficient optimization. Calibration results are automatically tabulated and plotted to provide easy assessment of trends or new behaviors.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Oxidation behavior of Zry-4 in steam-air mixtures at high temperature

This study dealt with the oxidation behavior of Zry-4 nuclear fuel cladding under a severe nuclear reactor accident scenario occurring in a light-water reactor. Influence of the reaction extent on cladding mechanical properties was also treated. Zry-4 fuel cladding segments were exposed to steam atmosphere containing different amount of air in composition ranging from 0 to 100 vol. %. Exposure times covered both pre- and post-breakaway regimes. Metallographic observations along with microhardness testing were carried out to study the effect of air fraction on the material microstructure. Hydrogen pick-up was measured and residual mechanical properties were assessed employing Ring Compression Tests. The results show that the addition of air in steam can lead to more than 300 % increase of weight gain in case of ∼50 % or higher air fraction after the exposure of 60 min., namely, 'late post-breakaway regime'. Approximately three times thicker oxide scales were observed in such cases, indicating that most of the weight gain was due to the oxide layer increase. Nitride phase was preferentially observed close to the interface between oxide and metal layers. The α-Zr(O) sublayer thickness decreases with the increasing fraction of air in steam. Microhardness, measured within the prior β-phase region, slightly depends on the air fraction. Hydrogen uptake, on the other hand, depends strongly on the air fraction in steam. In the case of shorter exposure times, the effect of air addition in steam was suppressed. Eventually, specimen plastic strains drastically reduced in the late post-breakaway regime. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High burn-up spent nuclear fuel vibration integrity study - 15134

The Oak Ridge National Laboratory (ORNL) has developed the cyclic integrated reversible-bending fatigue tester (CIRFT) approach to successfully demonstrate the controllable fatigue fracture of high burnup (HBU) spent nuclear fuel (SNF) in a normal vibration mode. CIRFT enables examination of the underlying mechanisms of SNF system dynamic performance. Due to the inhomogeneous composite structure of the SNF system, the detailed mechanisms of pellet-pellet and pellet-clad interactions and the stress concentration effects at the pellet-pellet interface cannot be readily obtained from a CIRFT system measurement. Therefore, finite element analyses (FEAs) are being used to complement the experimental work by estimating values of local stresses and strains from the measured global moment-curvature. These results and their implications will be used for further investigation. Major findings of CIRFT on the HBU SNF are as follows: - The degree of bonding between pellets, as well as the bonding between pellets and clad in the SNF system plays an important role in the vibration performance of SNF. - Fuel structure contributes to SNF system stiffness. - There are significant variations in stress and curvature of SNF systems during vibration cycles resulting from segment pellet and clad interactions. - SNF failure initiates at the pellet-pellet interface region and appears to be spontaneous. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Description of a Dry Cask Simulator for Measuring Internal and External Thermal-Hydraulic Performance

The thermal performance of a commercial nuclear spent fuel dry storage cask is evaluated through detailed analytical modeling. These modeling efforts are performed by the vendor to demonstrate the performance as well as regulatory compliance and are independently verified by the Nuclear Regulatory Commission (NRC). The majority of commercial dry storage casks in use today are aboveground. Cooling of the assemblies located inside the sealed canister is achieved by air flowing in the bottom of the cask and exiting out the top. Carefully measured data sets generated from testing of full sized casks or smaller cask analogs are widely recognized as vital for validating design and performance models. Numerous studies have been previously conducted. Recent advances in dry storage cask designs have significantly increased the maximum thermal load allowed in a cask in part by increasing the efficiency of internal conduction pathways and by increasing the internal convection through greater canister helium pressure. These vertical, canistered cask systems rely on ventilation between the canister and the overpack to convect heat away from the canister to the environment for both above and belowground configurations. While several testing programs have been previously conducted, these earlier validation attempts did not capture the effects of elevated helium pressures or accurately portray the external convection of aboveground and belowground canistered dry cask systems. Thus the enhanced performance of modern dry storage casks cannot be fully validated using previous studies. The purpose of the investigation described in this report is to produce data sets for the validation of assumptions associated with the thermal-hydraulic simulation of modern dry cask storage systems. Of particular interest are the steady-state cladding temperatures and the effect of elevated helium pressures in sealed canisters in both above and belowground designs. An existing electrically heated but otherwise prototypic BWR Incoloy-clad test assembly will be deployed inside of a representative storage basket and cylindrical pressure vessel that will represent the canister. The arrangement of a single assembly with well-controlled boundary conditions should simplify interpretation of results. Various arrangements of outer concentric ducting will be used to mimic conditions for above and belowground storage configurations of vertical, dry cask systems with canisters. Radial and axial temperature profiles will be measured for a wide range of decay power and helium cask pressures. As of this writing, the apparatus is currently under construction at Sandia National Laboratories in Albuquerque, NM and is expected to be operational starting in April 2016. Pre-test CFD calculations have been performed using best available information. These calculations are being used to assist in test design but will need to be validated and potentially reevaluated. The planned testing will be adjusted to reflect as-built conditions and measured system limitations. Dimensional analyses indicate that the anticipated ranges of relevant dimensionless groups (Reynolds, Modified Rayleigh, and Nusselt numbers) bracket or closely approach prototypic values for both the aboveground and belowground configurations. While designed to match prototypic values, the expected test matrix will include values that exceed currently acceptable values for decay heat, internal helium pressure, and peak cladding temperatures in order to gain more insight into the underlying behavior of the system. (authors)

42 ENGINEERING↗

Corrosion Behavior of Pressurized Austenitic Tubes in Oxygen Containing PbBi at 550 deg. C

Pb-alloys as coolant media are foreseen in the lead fast reactor (LFR) and the MYRRHA reactor in Belgium. For both 15-15 Ti-stabilized steel (1.4970) should be used as fuel cladding material due to its low swelling at high doses. Its compatibility with lead (Pb) and lead-bismuth eutectic (LBE) has been studied in the past focusing on its behaviour at different temperature, oxygen concentrations and different flow velocities of the liquid metal. During operation swelling of the fuel by irradiation or fuel cracking will lead increase the stresses on the cladding wall, which can influence the corrosion behaviour. To perform tests in Pb/PbBi on cladding tubes under stress a new test device was constructed in which an internal pressure can be applied to tubes. First tests with pressurized 1.4970 tubes at 550 deg. C in PbBi with an oxygen concentration of 10{sup -6} wt% were conducted. (authors)

36 MATERIALS SCIENCE↗

Recovery and Recrystallization Behavior of Nb-Containing Fe-Cr-Al Alloys

Nuclear-grade wrought Fe-Cr-Al alloys are currently under development as promising accident-tolerant fuel cladding materials for light water reactors (LWRs) due to their superior oxidation and corrosion resistance in high temperature steam environments when compared with current commercial Zr-based alloys. Sufficient amounts of Cr and Al additions in Fe-Cr-Al alloys provide the improved surface protection effects at both the service temperature and elevated temperatures in the accident case scenario. Minor alloying additions (such as Nb in the current study) also promote the second-phase precipitates to strengthen the alloys; e.g. sub-micron size Fe{sub 2}Nb-type Laves phase precipitates are likely to disperse at both inter- and trans-granular in BCC-Fe matrix after applying proper heat treatments. In LWRs, a seamless tube product is required for the fuel cladding which typically has ∼ 4 m length with an outside diameter of ∼ 10 mm and a wall thickness of less than 0.5 mm, and it imposes considerable challenges for tube fabrication process (e.g. tube drawing) of Fe-Cr-Al alloys. Research has been performed to achieve a balance between high-temperature performance and tube fabricability in newly developed Fe-Cr-Al alloys. BCC-Fe materials with Cr and Al additions typically suffer from poor ductility because of relatively high ductile-brittle transition temperature. In this sense, the microstructural stability of refined grain or subgrain structure, even at high temperature, is critical to maintain the deformability of the alloys during tube fabrication process, as well as sufficient mechanical properties at service condition. In this study, the recovery and recrystallization behaviors of Nb-containing Fe-Cr-Al alloys are studied. A specific focus was to evaluate the stability of the subgrain structure of the deformed Fe-Cr-Al alloys, and seek optimized processing parameters for seamless tube fabrication. The present results clearly demonstrated that the Nb addition stabilizes the refined subgrain microstructures of Fe-Cr-Al alloys below 700 deg. C due to Laves phase precipitations along sub-boundaries when compared with the Nb-free alloys, while maintaining sufficient strengths needed for fuel cladding in LWRs. At the same time, the results also showed that Nb-containing alloys can be softened through suitable annealing to improve the processability of tube drawing process. Detailed characterization efforts of subgrains and Laves phase precipitates are currently in progress. Completion of this work will deepen the understanding of the recovery and recrystallized behavior of Nb-containing Fe-Cr-Al alloys and provide guidelines to tube drawing process in the alloys. (authors)

36 MATERIALS SCIENCE↗

Study on Modeling of Nuclear Fuel End Drop during a Hypothetical Accident

It is well known that shell elements have been used to model the cladding of single nuclear fuel pins. These have been used, for example, to analyze the response of a fuel assembly by assuming that all fuel pins in a fuel assembly deform in the same pattern. It is increasingly significant to model the entire fuel assembly in order to capture more realistically the behavior of each individual nuclear fuel during a hypothetical accident in a manner that can account for interactions among single pins. However, modeling each individual fuel pin in an entire fuel assembly using shell elements will result in models with large amount of elements and degrees of freedom that take correspondingly larger amount of computational times to execute. Therefore, modeling the nuclear fuel assembly with beam elements may become an option. This paper presents the results of a set of analysis with the LS-DYNA finite element software that investigated the differences and similarities of modeling nuclear fuel assemblies using either shell elements or beam elements. This study provides additional insights on the appropriateness of using beam element models of the fuel pins in the simulation of a hypothetical accident. In this study, two single pin models, a single pin model using shell elements and a single beam model using beam elements, are constructed to analyze end drop scenarios with the LS-DYNA code. Each model is then analyzed for a 19 ft end drop scenario (linear behavior) and 30 ft end drop scenario (non-linear behavior). Comparisons are made between the results obtained with the single pin shell model and with the single pin beam model to study the differences and similarities resulting from the two modeling approaches. In this study, a B and W 15x15 PWR fuel is analyzed for both 30 ft and 19 ft end hypothetical accident drops using both single pin finite element model with shell elements and beam elements for the fuel cladding. It is found that for the 19 ft end drop, the difference in the Max/Min total axial strains is about 12% between the two models. For the 30 ft end drop, the maximum total axial strains calculated with both models is similar, and a difference of about 12% is observed for the minimum total axial strains calculated by the two models. Advantages of the single pin shell model are that it permits consideration of internal pressures and may capture local buckling. Therefore, use of beam elements to model the fuel cladding needs to take into account the possible significance of local buckling and internal pressurization for the problem being analyzed. (authors)

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Enhanced Thermal Conductivity UO{sub 2}-BeO and UO{sub 2}-SiC Fuels Behavior

Commercial light-water reactors currently use UO{sub 2} as a nuclear fuel, which has demonstrated several desirable characteristics. However, UO{sub 2} has a low thermal conductivity that leads to the development of a large temperature gradient across the fuel pellet. This temperature gradient contributes to limits in the operational performance of the reactor due to effects that include thermal stresses causing pellet cladding interaction and the release of fission product gases as demonstrated. These high fuel temperatures can be decreased and reactor performance improved by developing an enhanced thermal conductivity nuclear fuel. A high thermal conductivity nuclear fuel would decrease fuel temperatures and facilitate a reduction in pellet cladding interaction through lessening thermal stresses that result in fuel cracking, relocation, and swelling as described. Additionally, fission gas release would be decreased allowing for higher fuel burn-up, and the safety of the reactor would be improved with a faster thermal response and less stored energy in the fuel pins. A ceramic-ceramic composite nuclear fuel has an increased effective thermal conductivity due to adding a second compatible and high thermal conductivity ceramic to UO{sub 2}. SiC and BeO are two materials that demonstrate compatibility with UO{sub 2} and have a high thermal conductivity. In summary, the enhanced thermal conductivity UO{sub 2}-BeO and UO{sub 2}-SiC fuel performance has been modelled in a light water reactor, and a more complete and detailed understanding was achieved for enhanced thermal conductivity UO{sub 2}-BeO and UO{sub 2}-SiC fuels. BeO and SiC have high melting point, low neutron absorption, low thermal expansion coefficient and chemical compatibility with current UO{sub 2} fuels which makes them a suitable material for thermal conductivity enhancement. In our modeling and simulation work, the enhanced thermal conductivity nuclear fuel showed the capability of decreasing the fuel temperatures, increasing the gap total conductance, reducing the fission gas release, decreasing the gap/plenum pressure, lessening oxygen redistribution, and facilitating a reduction in pellet cladding interaction through lessening thermal stresses that result in fuel cracking, relocation, and swelling. The safety of the reactor operation would be then improved. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of PyC interlayer amorphization on the thermal conductivity of SiC/SiC composites - 18682

During the last two decades, silicon carbide based ceramic composites (SiC/SiC) have become a candidate material for nuclear fuel cladding, first for advanced nuclear systems, such as the GFR, and recently also as potential replacement material for nuclear fuel cladding in light water reactors. This work is contributing to the General Atomics/Westinghouse led CARAT project. This paper focuses on the consequences of the microstructural changes occurring at the pyrolytic (PyC) carbon interphases linking silicon carbide matrix and fibres in the composite. The experimental approach is two-fold: measurements of the thermal conductivity of short sections of prototype SiC/SiC cladding tubes deal with the macro-scale of the question, whereas the effects of radiation damage on the PyC interlayer are studied by energy filtered transmission electron microscopy (EFTEM) as well as spectrum imaging in STEM (ESI). The results from both parts of the experimental work are brought together in an effective medium model based on the work of Markworth and Youngblood et al. A detailed outlining of the radial heat flow experimental apparatus developed to this end has been presented at the 2016 ANS meeting in New Orleans. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

In-pile measurements of fuel rod dimensional changes utilizing the test reactor loop pressure for motion - 359

Different types of materials are being considered for fuel, cladding, and structures in existing and advanced nuclear reactors. These materials can undergo significant dimensional changes during irradiation. Currently in the US, such changes are measured with the 'cook and look' method (i.e. repeatedly irradiating a specimen for a specified period of time, and then removing it from the reactor for evaluation) - which leads to costly and time consuming experiments. In addition, such techniques provide limited data, and handling may disturb the phenomena of interest. Therefore, in-pile detection of geometric changes is needed to understand real-time behavior during irradiation testing of fuels and materials in high flux US Material and Test Reactors (MTRs). The developmental results of an advanced Linear Variable Differential Transformer (LVDT)-based test rig capable of detecting real-time changes in diameter or length of fuel rods or other material samples during irradiation in US MTRs are presented. The LVDT is being developed at the Idaho National Laboratory (INL), and will provide experimenters with the capability to measure dimensional changes associated with fuel and clad swelling, pellet-clad interaction, and crud buildup. The LVDT design utilizes the MTR's loop pressure to drive the test specimen at a constant rate. This leads to a simplified construction which only requires three pressure boundary penetrations. Further, the LVDT pressure boundary is a leak tight hydraulic ram capable of actuating under low differential pressure (e.g. 1 psid), and is able to survive the high irradiation tests at Pressurized Water Reactor (PWR) conditions. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Simulation of Proposed Heat Treatment Methods for the Sister Rods

The High Burnup Spent Fuel Data Project (the 'project'), sponsored by the U.S. Department of Energy (DOE) Office of Nuclear Energy (NE), is focused on experimentally evaluating the effects of long-term dry storage and transportation on high burnup (HBU) pressurized water reactor (PWR) fuel (>45 gigawatt days per metric ton uranium). The goals of the project are to provide confirmatory data for analytical model validation and potential improvement; to provide input to future dry storage cask design; to support license renewals and new licenses for Independent Spent Fuel Storage Installation facilities; and to support transportation licensing for high burnup used fuel. In support of these project goals, an instrumented TN-32B bolted-lid cask (the Research Project Cask or RPC) at the North Anna reactor site will be loaded with intact, HBU PWR fuel assemblies (Project Assemblies) having four different kinds of cladding: standard Zircaloy-4, low-tin Zircaloy-4, ZIRLO{sup R}, and M5{sup R}. In approximately ten years, the instrumented cask will be opened for inspection and several fuel rods from the Project Assemblies will be characterized. The project has also removed 25 'sister rods' from assemblies at North Anna: 9 directly from the project assemblies and 16 from similarly constructed and operated HBU assemblies. The 25 sister rods are all high burnup and cover the range of domestically-used cladding alloys. The 25 sister rods were shipped to Oak Ridge National Laboratory (ORNL) in early 2016 for detailed non-destructive examinations (NDE) followed by destructive examination (DE). Examination of the sister rods will provide a baseline for comparison with the cask rods and will allow for separate effects testing. Dry storage canister loading is completed under water in a designated area of the plant's spent fuel pool. In preparation for dry storage, the fuel assemblies and canister cavity must be drained and dried. Typically, the highest temperatures experienced by the fuel during dry storage are encountered either during drying or transfer of the canister to the storage pad; therefore, as a part of the sister rod testing these temperatures will be simulated in the lab to produce samples that are representative of the peak cladding temperature the fuel experiences either during drying, transfer, or storage. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A Degradation Model and Testing Protocol for Metallic Waste Forms

Metallic waste forms developed to immobilize high-level radioactive wastes generated in advanced (closed) fuel cycles are being evaluated as part of the US DOE Fuel Cycle Research and Development program. The electrometallurgical reprocessing of used metallic fuels to recover U and Pu generates two waste streams: salt waste comprised of electro-refiner salt contaminated with oxidized fission products and metallic waste comprised of activated cladding and metallic fission products that were not oxidized under the processing conditions. Metallic waste forms can be made by directly melting the cladding and fuel wastes with small amounts of trim metals to form a multiphase alloy material in which radionuclides and other waste constituents are immobilized within chemically durable intermetallic and iron-based solid solution phases. Some components of the waste streams serve as important constituents of phases comprising the waste form, such as Mo and Zr, which form Fe{sub 2}Mo and Fe{sub 2}Zr intermetallic phases. Other waste constituents are accommodated as substitutional contaminants, such as Tc within the Fe{sub 2}Mo intermetallic and U/TRU within the Fe{sub 2}Zr intermetallic. Sufficient amounts of these host phases must be available to accommodate all radionuclides in the waste stream. The compositional flexibility of the host phases to incorporate waste components is being utilized to formulate metal waste forms that will accommodate variations in waste streams compositions that will occur over long-term fuel reprocessing operations. Small amounts of trim metals can be added to tailor the phase assembly to match the waste stream composition and facilitate waste form processing. For example, additional Zr may be added during waste form production to ensure all U/TRU is sequestered in a durable Fe{sub 2}Zr host phase and trim Cr, Mo, and Ni can be added to supplement the amounts provided by the steel cladding to improve the durability of a metallic waste form. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Accelerated Corrosion Tests to Evaluate Long-Term Performance of BORAL{sup R} in Spent Fuel Pools

Neutron absorber materials are used to increase storage capacity in spent fuel pools (SFPs) while maintaining criticality safety margins. BORAL{sup R} - a neutron absorber material commonly used in SFPs - is a metal matrix composite containing boron carbide (B{sub 4}C) and Al-1100 mixture. The aluminum (Al) cladding, which is on both sides of the core, serves as a protective barrier. Al cladding is susceptible to corrosion, which can lead to blisters between the core material and the cladding over time. Based on operational experience to date, pits also have been observed via visual examination and microscopy. EPRI has maintained a database containing coupon data spanning more than 25 years, and to date no loss of BORAL{sup R} efficacy has been observed. In the United States, about 50% of the plants use BORAL{sup R} as neutron absorber material in SFPs. BORAL{sup R} is also used in nuclear plants in Mexico, Korea, Taiwan, and other countries. Given that the plant lifetime is increasing-and, hence, the SFP lifetime-EPRI initiated a five-year accelerated corrosion test in 2013 to evaluate and determine the long-term performance of BORAL{sup R} in SFPs. This paper presents an overview of the accelerated corrosion test project. Results from the Year 1 and Year 2 test results are also presented. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

SE2-ANL Subchannel Analysis with New Heating Calculation Based on VARIANT Transport Code

The multi-assembly, steady-state sub-channel analysis code SE2-ANL has been widely used in thermal-hydraulic analysis of sodium cooled fast reactors (SFR). It is used to compute the core-wide temperature profiles for a given flow distribution and to determine the assembly flow rates yielding a desired (assembly-wise) peak temperature distribution. It is a modified version of SUPERENERGY-2 coupled with the DIF3D/GAMSOR/DIF3D procedure for coupled neutron and gamma heating calculations, developed at Argonne National Laboratory (ANL). In the current version of SE2-ANL, the neutron and gamma fluxes are calculated using the finite-difference diffusion theory option of the DIF3D code with six triangular meshes per hexagonal assembly. In addition, the pin power distributions are estimated by assuming that the power distribution within an assembly is separable in the radial and axial directions. Furthermore, the total heat generation rate in an assembly duct wall is simply determined by a user-specified fraction of the total gamma heating within that assembly. In order to determine the pin power distributions more accurately by eliminating these limitations, a new coupled heating calculation procedure has recently developed based on the neutron and gamma transport calculations with the VARIANT code. For this, the GAMSOR code has been extended to generate the intra-nodal gamma source distribution to be consistent with the trial functions of VARIANT. Using the computed neutron and gamma flux distributions, the power distribution in each fuel pin and duct wall is determined using a new utility code CURVE, which has been developed to evaluate the VARIANT flux solution at the center of each fuel pin and along the duct mid-wall. For each pin segment contained in a VARIANT node, the axial power shape is represented as a quadratic profile. The SE2-ANL code has been modified to interface with the new, coupled neutron and gamma heating calculation scheme. In addition, several improvements have been made on the computational methods and models of SE2-ANL. To eliminate the limit on the axial mesh size due to the numerical instability problem of the current explicit scheme, the numerical scheme for discretizing the energy equation in the axial direction has been changed to the {theta}-method of the SLTHEN code. An automated flow allocation scheme has also been implemented in SE2-ANL to determine assembly flow rates such that the peak cladding mid-wall temperatures of individual orifice zones are equalized over the burn cycle. The impacts of the new heating calculation scheme based on VARIANT transport solutions on the cladding and fuel temperatures have been tested against the existing method of SE2-ANL. Using the existing and new heating calculation schemes, full-core subchannel analyses were performed for the metal core design of the 1000 MWt Advanced Burner Reactor (ABR-1000), and the resulting coolant, cladding and fuel temperatures were compared. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Effects of Coolant Void Condition on Melt Fragmentation using Simulants in Initial Phase of Metal-fueled SFR Severe Accident

Metal fuel has inherent safety characteristics, especially in severe accident conditions. However, the metal-fueled SFR severe accident scenarios need to be categorized since overall severe accident mitigation strategies have not been prepared. In addition, these mitigation strategies should be classified in specific phases. In an initial phase of metal-fueled SFR severe accident scenarios, fuel melting, and cladding failures would occur. After the occurrence of the cladding breach, the molten metal fuel would be ejected into a coolant channel due to fission gas in fuel cavity or rapid evaporation of sodium bond. This is called Ex-pin phenomena. There are few studies considering the Ex-pin phenomena of metal fuel. Related representative studies are transient reactor test facility (TREAT) M series tests. The TREAT M series tests provided fundamental metal fuel performance in transient condition. They informed partial experimental data such as the amount of melt ejected into coolant channel after the cladding failure. However, these experimental data did not examine the melt behavior during the Ex-pin phenomena. In metal-fueled SFR, it is a known fact that the negative reactivity feedback occurs in the initial phase of severe accident. In an unprotected loss-of-flow (ULOF) accident, the void-reactivity feedback may be positive depending on where in the reactor core the sodium voiding occurs. However, molten metal fuel would be better dispersed upward compared to those of an oxide fuel and significant negative reactivity feedback could be induced through such behaviors. Thus, a key safety strategy to mitigate the accident progression at the initial phase of severe accident is to discharge melt upwards out of the core. In this paper, the upward discharge of melt is defined as melt levitation. Such melt levitation could ensure early termination of severe accident. There could be different melting behaviors inside the pin depending on reactor types or the type of fuel. In case of pressurized water reactor (PWR) oxide fuel-water system, the rapid power excursion would initiate melting of fuel at the surface of the pellets. In this paper, the ULOF accident for the metal-fueled SFR is considered as an accident scenario. To induce the melt levitation, the driving force should be clarified. Heo et al. observed a built-up vapor pressure was suggested as one of the driving forces for the upward dispersion of the molten materials. The following factors also have the potential to induce the melt levitation; the pressure induced by fission gas in the cavity or rapid boiling of sodium bond, natural circulation flow of the sodium, the sodium vapor flow generated by the difference between inlet and outlet plenum in the reactor core, the built-up vapor pressure due to the fuel-coolant interaction etc. These factors are balanced each other. They should be examined through the Ex-pin experiments. Before conducting a parametric study for each factor, the general behavior of the molten metal fuel should be investigated in the coolant channel. Since rapid sodium coolant boiling could occur in the initial phase of severe accident scenarios, the molten fuel would be ejected and fragmented in voided channel. Unlike previous studies concerning an un-voided channel, differences in melt behavior in the voided channel are expected. In present study, molten material behavior was evaluated to reveal their characteristics in voided channel. The Ex-pin experiments were performed in both un-voided and voided channel, thus such behavior differences were explicitly observed. In the lab-scale experiments, the un-voided and voided channel were reflected by coolant-filled and air-filled channel, respectively. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Correlation between Grain Size Distribution and Grain Boundary Character in Polycrystalline Uranium Dioxide

Thermo-mechanical behavior of oxide nuclear fuels is extremely important to overall fuel element performance. Critical to the understanding of Pellet-Cladding Mechanical Interactions (PCMI) are elasticity, plasticity and creep, as this interaction with the cladding can lead to fuel rod fracture and in turn affect its thermal performance significantly. In addition, sub-grain scale mechanical behavior, e.g. elastic anisotropy, as well as dislocation-driven plasticity and creep, can also play a significant role on microstructure evolution of the fuel elements and their cladding, failure of which would severely reduce the useful service life of the elements and allow the release of fission products out into the working fluid of the reactor. Therefore, careful measurements of mechanical properties are key to validate robust fuel performance codes able to predict this PCMI behavior from inputs at the micro-scale, e.g., MARMOT, and to quantify its effects on other aspects of fuel behavior. In uranium dioxide (UO{sub 2}), the thermomechanical response at the meso-scale depends strongly on crystallography of individual grains, and available datasets are far from complete in terms of temperature, stress, and stoichiometry in parameter space. Therefore, details of the fuel microstructure, such as porosity distribution and location, as well as grain boundary (GB) character, distribution, and location are needed to create accurate multiscale models to predict the fuel's evolution in-pile, and in turn aid in the design and development of more efficient fuels that can last longer cycles.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Sensitivities and correlations of critical experiments due to uncertainties of system parameters and nuclear data - 14416

With increasing demand on accuracy of criticality calculations, correlations between benchmark experiments due to system parameter uncertainties become of interest in bias determination. The impact of different interpretations of system parameter uncertainties on the calculation of covariances and correlations of k{sub eff} is discussed in this article. Following the suggestion of the OECD/NEA EGUACSA Benchmark phase IV [1], 21 experiments from the ICSBEP international Handbook of Evaluated Criticality Safety Benchmarks [2] are used for this analysis (LEU-COMP-THERM series 07, exp. 01-04 and 39, exp. 01-17). The experiments share certain assembly and fuel features and were carried out in the same lab. Therefore, correlations in the calculation of k{sub eff} appear. Correlation coefficients between experiments due to nuclear data uncertainties are calculated with TSUNAMI [3] and show high values for most experiments. For the correlation analysis due to system parameter uncertainties mainly two scenarios are considered: In scenario A all uncertain parameters are varied mutually for all fuel rods, representing a systematic deviation of the actual experimental setup from the design value. This analysis is performed for all experiments listed above. In scenario E certain parameters like the outer cladding diameter are varied for each fuel rod individually, representing a random scattering of the varied parameter. Scenarios B, C and D represent intermediate scenarios between A and E, which are discussed shortly. Uncertainty and sensitivity calculations of k{sub eff} on the uncertain experimental parameters based on Monte Carlo sampling are presented and discussed. The calculations were performed with SUnCISTT (Sensitivities and Uncertainties in Criticality Inventory and Source Term Tool [4]) and SCALE 6.1.2 [3]. For the 21 EGUACSA proposed experiments the outer cladding diameter is the leading effect for the uncertainty of k{sub eff} for scenario A. In contrast, for scenario E the impact of the cladding diameter on k{sub eff} cancels out due to rod wise variations leaving the fuel diameter as the leading effect. The correlation analysis based on system parameter uncertainties indicates a significant dependence of the correlation coefficients on the interpretation of the uncertainties. It shows high values for scenario A, if the neutronic features are similar (EALF, H/U). For scenario E the overall correlations are significantly smaller and variations between experiments decrease. The impact of the determined correlations on bias calculations of application cases will be discussed by the authors in the accompanying paper 'Impact of correlated data in validation procedures'. (authors)