Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “PIN”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,531 records · Page 85

Analysis of the magnetic corrosion product deposits on a boiling water reactor cladding

The buildup of corrosion product deposits (CRUD) on the fuel cladding of the boiling water reactor (BWR) before and after zinc injection has been investigated by applying local experimental analytical techniques. Under the BWR water chemistry conditions, Zn addition together with the presence of Ni and Mn induce the formation of (Zn,Ni,Mn)[Fe{sub 2}O{sub 4}] spinel solid solutions. X-ray absorption spectroscopy (XAS) revealed inversion ratios of cation distribution in spinels deposited from the solid solution. Based on this information, a two-site ferrite spinel solid solution model is proposed. Electron probe microanalysis (EPMA) and extended X-ray absorption fine structure (EXAFS) findings suggest the zinc-rich ferrite spinels formation on BWR fuel cladding mainly at lower pin. - Graphical Abstract: Analysis of spinels in corrosion product deposits on boiling water reactor fuel rod. Combining EPMA and XAFS results: schematic representation of the ferrite spinels in terms of the end members and their extent of inversion. Note that the ferrites are represented as a surface between the normal (upper plane, M[Fe{sub 2}]O{sub 4}) and the inverse (lower plane, Fe[MFe]O{sub 4}). Actual compositions red Black-Small-Square for the specimen at low elevation (810 mm), blue Black-Small-Square for the specimen at mid elevation (1800 mm). The results have an impact on the properties of the CRUD material. Highlights: Black-Right-Pointing-Pointer Buildup of corrosion product deposits on fuel claddings of a boiling water reactor (BWR) are investigated. Black-Right-Pointing-Pointer Under BWR water conditions, Zn addition with Ni and Mn induced formation of (Zn,Ni,Mn)[Fe{sub 2}O{sub 4}]. Black-Right-Pointing-Pointer X-Ray Adsorption Spectroscopy (XAS) revealed inversion of cations in spinel solid solutions. Black-Right-Pointing-Pointer Zinc-rich ferrite spinels are formed on BWR fuel cladding mainly at lower pin elevations.

36 MATERIALS SCIENCE↗

Microstructural evolution of nanocrystalline Fe–Zr alloys upon annealing treatment

Nanocrystalline Fe–Zr alloys exhibit an extraordinary thermal stability at elevated temperatures, which enables their potential applications in various fields. However, there remain concerns regarding the controlling stabilization mechanisms responsible for their thermal stability. In this work, two nanocrystalline Fe–Zr alloys containing 1 at.% Zr and 5 at.% Zr were annealed at various temperatures (T{sub ann}) up to 900 °C. Microstructural evolution of the alloys upon annealing was investigated by means of an X-ray diffractometer equipped with a 2-dimensional detector and transmission electron microscopy. Below 600 °C, microstructures of the two alloys consist of single nanocrystalline ferrite whose grain size is rather stable upon annealing treatments. Above 600 °C, accompanying the precipitation of Fe{sub 3}Zr phase, an apparent grain coarsening of ferrite is observed, whereas the thermal stability of the alloys is still considerably higher than that of nanocrystalline pure Fe. Based on the experimental results, it was claimed that stabilization of the nanocrystalline Fe–Zr alloys should not be totally ascribed to the thermodynamic stabilization mechanism due to the reduction in grain boundary energy as suggested in earlier investigations [K.A. Darling et al., Scr. Mater. 59 (2008) 530 and K.A. Darling et al., Mater. Sci. Eng. A527 (2010) 3572]; when T{sub ann} is higher than 600 °C, along with the precipitation of Fe{sub 3}Zr, the effect of thermodynamic stabilization is weakened, the kinetic effect arising from Zener pinning of Fe{sub 3}Zr precipitates turns to be an important mechanism contributing to the stabilization of the nanoscale grain size. - Highlights: • We show clear evidence of precipitation of Fe{sub 3}Zr phase above 600 °C. • Stabilization of nanostructure is not solely controlled by thermodynamic mechanism. • Above 600 °C, Zener pinning plays an important role in stabilizing nanostructure.

36 MATERIALS SCIENCE↗

Feasibility of formation of nanocrystalline Fe-Cr-Y alloys: Mechanical properties and thermal stability

Aim of the present study is to investigate the feasibility of formation of Fe-Cr-Y disordered solid solutions by mechanical alloying and effect of Y on the thermal stability and mechanical properties of such nanocrystalline alloys. Thermodynamic analysis by Miedema's and Toop's models confirms that the energy barrier required to form the disordered solid solutions has been overcome by the stored energy due to strain dislocations and grain boundary defects. Although limited grain growth was observed during annealing of metastable Fe-15Cr-1Y alloy, the grains size found to stabilize at ~ 53 nm after annealing at 1000 °C; and the corresponding hardness value measured to be also quite high (8 GPa). The grain size analysis by TEM and AFM is well-corroborated with the XRD crystallite size. The high thermal stability and large strengthening effect have been discussed in the light of grain boundary pinning by solute segregation, solute drag effect and Zener pinning due to intermetallic phase(s). - Highlights: • Metastable Fe-Cr-Y alloys were developed by mechanical alloying for nuclear applications. • Formation of Fe-Cr-Y solid solutions was explained from the Gibbs free energy change using Toop's model. • 1 at.% Y found to be very effective in the stabilization of Fe-Cr alloys at high temperatures. • Solute drag effect and/or segregation of Y atoms played a pivotal role in the stabilization.

36 MATERIALS SCIENCE↗

Effect of vanadium carbide on dry sliding wear behavior of powder metallurgy AISI M2 high speed steel processed by concentrated solar energy

Mixtures of AISI M2 high speed steel and vanadium carbide (3, 6 or 10 wt.%) were prepared by powder metallurgy and sintered by concentrated solar energy (CSE). Two different powerful solar furnaces were employed to sinter the parts and the results were compared with those obtained by conventional powder metallurgy using a tubular electric furnace. CSE allowed significant reduction of processing times and high heating rates. The wear resistance of compacts was studied by using rotating pin-on-disk and linearly reciprocating ball-on-flat methods. Wear mechanisms were investigated by means of scanning electron microscopy (SEM) observations and chemical inspections of the microstructures of the samples. Better wear properties than those obtained by conventional powder metallurgy were achieved. The refinement of the microstructure and the formation of carbonitrides were the reasons for this. - Highlights: •Powder metallurgy of mixtures of M2 high speed steel and VC are studied. •Some sintering is done by concentrated solar energy. •Rotating pin-on-disk and linearly reciprocating ball-on-flat methods are used. •The tribological properties and wear mechanisms, under dry sliding, are studied.

36 MATERIALS SCIENCE↗

Development of nano-Y2O3 dispersed Zr alloys synthesized by mechanical alloying and consolidated by pulse plasma sintering

Highlights: • Zr-Fe-Cr-Cu-Ti-1.0wt% nano-Y{sub 2}O{sub 3} dispersed alloys are fabricated by mechanical alloying and pulse plasma sintering. • These alloys record extremely high compressive strength, Young’s modulus, and hardness. • These mechanical properties are superior as compared to other commercially available Zr based alloys. • Dispersion of nanometric FeZr{sub 2}, Y{sub 2}Ti{sub 2}O{sub 7}, Fe{sub 2}Ti, ZrCu, Cr{sub 2}Zr, Y{sub 2}O{sub 3} leads to grain boundary pinning at elevated temperature. - Abstract: In this paper, Zr alloys are synthesized with nominal compositions: 50Zr-30Fe-10Cr-5Cu-5Ti (alloy A), and 49Zr-30Fe-10Cr-5Cu-5Ti-1Y{sub 2}O{sub 3} (alloy B), 45Zr-30Fe-10Cr-10Cu-5Ti (alloy C), 44Zr-30Fe-10Cr-10Cu-5Ti-1Y{sub 2}O{sub 3} (alloy D) (all in wt%) by mechanical alloying and consolidated by pulse plasma sintering at 1173 K (900 °C), 1223 K (950 °C) and 1273 K (1000 °C) using 75 MPa uniaxial pressure applied for 5 min and 70 kA pulsed current at 3 Hz pulse frequency. The microstructure and phase evolution during mechanical alloying and sintering has been characterized by X-ray diffraction (XRD), scanning and transmission electron microscopy (SEM & TEM) and energy dispersive spectroscopy (EDS). Mechanical properties i.e. hardness and compressive strength were determined by using nano-indentation unit and universal testing machine. The produced alloys recorded very high levels of compressive strength (1359–2456 MPa), and hardness (7.05–10.05 GPa) which measures 1.5–2.0 times more than that of other Zr alloys (2 O{sub 3}) particles which can contribute to grain boundary pinning, and improved creep and oxidation resistance at elevated temperature.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Evaluation of microstructure stability at the interfaces of Al-6061 welds fabricated using ultrasonic additive manufacturing

Ultrasonic additive manufacturing (UAM) is a solid-state additive manufacturing process that uses fundamental principles of ultrasonic welding and sequential layering of tapes to fabricate complex three-dimensional (3-D) components. One of the factors limiting the use of this technology is the poor tensile strength along the z-axis. Recent work has demonstrated the improvement of the z-axis properties after post-processing treatments. The abnormally high stability of the grains at the interface during post-weld heat treatments is, however, not yet well understood. In this work we use multiscale characterization to understand the stability of the grains during post-weld heat treatments. Aluminum alloy (6061) builds, fabricated using ultrasonic additive manufacturing, were post-weld heat treated at 180, 330 and 580 °C. The grains close to the tape interfaces are stable during post-weld heat treatments at high temperatures (i.e., 580 °C). This is in contrast to rapid grain growth that takes place in the bulk. Transmission electron microscopy and atom-probe tomography display a significant enrichment of oxygen and magnesium near the stable interfaces. Based on the detailed characterization, two mechanisms are proposed and evaluated: nonequilibrium nano-dispersed oxides impeding the grain growth due to grain boundary pinning, or grain boundary segregation of magnesium and oxygen reducing the grain boundary energy.

36 MATERIALS SCIENCE↗

Temperature-dependent cyclic response and microstructure of AlSi10Mg(Cu) alloy

Highlights: • The cyclic behavior of AlSi10Mg(Cu) alloy in LCF regime is temperature-dependent. • The transition temperature of the cyclic behavior is about 180 °C. • Microstructure transitions were observed with increasing temperature. - Abstract: In the present work, the cyclic stress response and microstructure evolution of AlSi10Mg(Cu) alloy at high temperature were investigated. Samples were tested at high temperature, under total strain control and tensile-compression loading (R = −1) until failure. The cyclic stress response was analyzed, as well as the microstructures were examined by TEM. The results demonstrated that the cycle stress response of the studied alloy is experimental temperature dependence. Microstructure analysis indicated the precipitated phase was disruptive changed by high temperature compared to the as-received alloy. A lot of coherent β″-Mg{sub 2}Si precipitates and GP zones were observed in the as-received alloy, resulting in sustaining cyclic hardening by pinning effect. At high temperature, the vast majority of the tiny coherency precipitates and clusters transformed to the large semi-coherency Q′ and β′-Mg{sub 2}Si precipitates, leading to the sharp decrease of pinning number and the change of dislocation interaction mechanism, which is believed to be one of the reasons for softening. Another reason is that high temperatures can promote dislocations movement.

36 MATERIALS SCIENCE↗

Isothermal annealing behaviour of nuclear grade 20Cr-25Ni austenitic stainless steel

Highlights: • At 930 °C recrystallisation of deformed 20/25 Nb steel is completed after 120 s. • Recrystallisation proceeds by strain induced boundary migration. • An increase of cube oriented grains at the expense of S oriented is observed. • The boundary migration induced the precipitation of niobium carbides. • The grain size is limited by the particle dispersion according to Zener pinning. - Abstract: We have performed an in-depth characterisation of the microstructure evolution of 20Cr-25Ni Nb-stabilised austenitic stainless steel during isothermal annealing at 930 °C using scanning and transmission electron microscopy. This steel grade is used as cladding material in advanced gas-cooled fission reactors, due to its resistance to thermal creep and water corrosion. The initial deformed microstructure undergoes recrystallisation via a strain-induced boundary migration mechanism, attaining a fully recrystallised microstructure after 120 s of annealing. The transition from low-to-high grain boundaries has already occurred after 15 s, together with an increase in the cube grain orientation at the expense of the S texture component. After 120 s, the grain boundary migration induces the formation of new fine Nb(C,N) particles, whereas the pre-existing particles become enriched in Ni and Si. The resulting particle population limits the grain growth in the austenitic matrix, based on the Zener pinning model, resulting in relatively small recrystallised austenite grains and a high density of high-angle and special coincidence-lattice-site grain boundaries, together with a large number of particle/matrix interfaces.

36 MATERIALS SCIENCE↗

Low cycle fatigue behavior of AlSi10Mg(Cu) alloy at high temperature

Highlights: • The cyclic stress response of AlSi10Mg(Cu) alloy in LCF regime is temperature-dependent. • Precipitates transitions were observed after high temperature cycle loading. • Changes in the interaction mechanism between dislocations and nanoparticles lead to different cyclic stress responses. - Abstract: Low cycle fatigue (LCF) behavior of AlSi10Mg(Cu) alloy was investigated at 100 °C and 250 °C over a range of strain amplitude from 0.25% to 0.40%. Cycle stress response, hysteresis loops, fatigue life, as well as post-fatigue microstructure were studied in detail. Except 0.25%, the alloy performed cycle hardening behavior at 100 °C and softening behavior at 250 °C at any given strain amplitude, which corresponded well with the observed phenomena in hysteresis loops. At any given temperature, cyclic stress increases while fatigue life decreases with the increasing strain amplitude. The fatigue life of the studied alloy at 100 °C was higher than that at 250 °C under the same strain amplitude. Fractography indicated that most fatigue crack initiated from casting defects. The fatigue crack propagation was mainly characterized by fatigue striations and tear ridges in any conditions. Section inspection shows that the number of cracked eutectic Si increases with decreasing the temperature or increasing strain amplitude. Post-mortem transmission electron microscopy (TEM) investigations indicated that cyclic hardening behavior at 100 °C was due to the pinning effect of coherent precipitates (β″-Mg{sub 2}Si and GP zones). Most of tiny coherency precipitates and clusters transformed to large semi-coherency Q′ and β′-Mg{sub 2}Si precipitates after cyclic loading at 250 °C, leading to the sharp decrease of pinning number and dislocation density, which is a key reason for the cyclic softening. Another factor is that more dislocations can be activated and dislocation climb is easier at higher temperature.

36 MATERIALS SCIENCE↗

A Pb(In{sub 1/2}Nb{sub 1/2})O{sub 3}–Pb(Zn{sub 1/3}Nb{sub 2/3})O{sub 3}–PbTiO{sub 3} ternary ferroelectric system with high T{sub C} and high piezoelectric properties

Graphical abstract: Display Omitted Highlights: ► (0.79 − x)Pb(In{sub 1/2}Nb{sub 1/2})O{sub 3}–0.21Pb(Zn{sub 1/3}Nb{sub 2/3})O{sub 3}–xPbTiO{sub 3} ceramics were prepared by two-step method. ► A morphotropic phase boundary region has been determined in the composition range of 0.28 < x < 0.32. ► The compositions within MPB region exhibit excellent piezoelectric properties. -- Abstract: (0.79 − x)Pb(In{sub 1/2}Nb{sub 1/2})O{sub 3}–0.21Pb(Zn{sub 1/3}Nb{sub 2/3})O{sub 3}–xPbTiO{sub 3} (x = 0.23–0.35) ternary ferroelectric system in the form of ceramics have been synthesized. Its structure and properties have been studied by X-ray powder diffraction and electric measurements. A morphotropic phase boundary region has been determined in the composition range of 0.28 < x < 0.32, where the Curie temperature T{sub C} and the rhombohedral–tetragonal phase transition temperature T{sub RT} were found to vary from 243 °C to 295 °C and 145 °C to 191 °C, respectively, much higher than PMNT and PZNT systems. The compositions within MPB region exhibit excellent piezoelectric properties such as piezoelectric coefficient d{sub 33} > 646 pC/N, T{sub RT} > 145 °C, T{sub C} > 273 °C and E{sub C} > 13 kV/cm for 0.5PIN–0.21PZN–0.29PT and 0.49PIN–0.21PZN–0.30PT, making the ceramics of this system a promising material for high power and high temperature application.

36 MATERIALS SCIENCE↗

High-speed friction stir butt welding of 25.4 mm thick 7175-T79 aluminum alloy

This presents the first experimental demonstration of friction stir butt welding of 25.4 mm thick high-strength, precipitate-strengthened 7XXX aluminum alloy at a welding speed above 500 mm/min and penetration depth greater than 10 mm. Tool pin threads that terminate away from the shoulder region, helped mitigate nearby stress concentration during tool traversing, enabling a higher welding speed while avoiding pin fracture near shoulder. Two kinds of welds—one-sided with full penetration of the plate thickness and double-sided with partial penetration of the plate thickness—were conducted. Significant grain refinement (grain size 1.3 ± 0.8 µm) was evident at the junction of double-sided friction stir welding (FSW) compared to other regions of weld-nugget or base material. Cross-weld tensile testing with digital image correlation revealed high local strains at the junction of double-sided FSW before macro-yield. This strain concentration impeded the typical early necking on advancing/retreating sides of FSW joints, improving the yield strength of as-welded double-sided FSW by 20–24% over slow- to medium-speed one-sided FSW. In conclusion, the joint efficiency of as-welded, double-sided high-speed FSW was about 76% with respect to the base material’s ultimate tensile strength.

36 MATERIALS SCIENCE↗

Mechanism of the Bauschinger effect in Al-Ge-Si alloys

Here, wrought Al-Ge-Si alloys were designed and produced to ensure dislocation bypass strengthening ("hard pin" precipitates) without significant precipitate cutting/shearing ("soft pin" precipitates). They were processed from the melt, solution heat treated and aged.

36 MATERIALS SCIENCE↗

A review of inherent safety characteristics of metal alloy sodium-cooled fast reactor fuel against postulated accidents

The thermal, mechanical, and neutronic performance of the metal alloy fast reactor fuel design complements the safety advantages of the liquid metal cooling and the pool-type primary system. Together, these features provide large safety margins in both normal operating modes and for a wide range of postulated accidents. In particular, they maximize the measures of safety associated with inherent reactor response to unprotected, double-fault accidents, and to minimize risk to the public and plant investment. High thermal conductivity and high gap conductance play the most significant role in safety advantages of the metallic fuel, resulting in a flatter radial temperature profile within the pin and much lower normal operation and transient temperatures in comparison to oxide fuel. Despite the big difference in melting point, both oxide and metal fuels have a relatively similar margin to melting during postulated accidents. When the metal fuel cladding fails, it typically occurs below the coolant boiling point and the damaged fuel pins remain cool-able. Metal fuel is compatible with sodium coolant, eliminating the potential of energetic fuel coolant reactions and flow blockages. All these, and the low retained heat leading to a longer grace period for operator action, are significant contributing factors to the inherently benign response of metallic fuel to postulated accidents. This paper summarizes the past analytical and experimental results obtained in past sodium-cooled fast reactor safety programs in the United States, and presents an overview of fuel safety performance as observed in laboratory and in-pile tests.

inherent safety↗

An Internal ALD-Based High Voltage Divider and Signal Circuit for MCP-based Photodetectors

We describe a pin-less design for the high voltage (HV) resistive divider of the all-glass LAPPD (TM) 8 in,square thin photodetector module. The divider, which distributes high voltage applied to the photocathode to the two micro-channel plates (MCPs) that constitute the amplification stage, is comprised of the two MCPs and three glass mechanical spacers, each of which is coated with a resistive layer using atomic layer deposition (ALD). The three glass grid spacers and the two MCPs form a continuous resistive path between cathode and anode, with the voltages across the MCPs and the spacers determined by the resistance of each. High voltage is applied on an external tab on the top glass window that connects to the photocathode through the metal seal. The DC ground is supplied by microstrips on the bottom glass plate that form the high-bandwidth anode. The microstrips exit the package through the glass-frit seal of the anode base-plate and the package sidewall. The divider is thus completely internal, with no HV pins penetrating the low-profile flat glass package. Measurements of the performance of the divider are presented for the 8 in.-square MCP and spacer package in a custom test fixture and for an assembled externally pumped LAPPD (TM) prototype with an aluminum photocathode. (C) 2015 Elsevier B.V. All rights reserved.

Adams, Bernhard W.↗

Development and evaluation of a list mode neutron coincidence collar for spatial response measurements of fresh fuel assemblies

A traditional safeguards neutron coincidence counting system, the Neutron Coincidence Collar, has been modified to incorporate individual preamplifiers on each of its 18 3He tubes in active interrogation mode. When used with list mode data acquisition (LMDA) and analysis, a signal from each 3He tube can be recorded and analyzed to allow a spatial response measurement to be performed on an item based on count rate and 3He tube location within the system. The ultimate goal of this project is to demonstrate the capabilities of a list mode response matrix for the nondestructive assay of fresh nuclear fuel assemblies. To enable partial defect detection of fuel pin locations and absences within an assembly, the project aims to extend well-established correlated neutron analysis techniques on a preexisting Neutron Coincidence Collar by extracting a greater number of useful signatures from the system than are currently generated. LMDA, combined with the addition of multiple preamplifiers, facilitates this capability by increasing the number of simultaneous signals that can be measured; this allows an in-depth analysis of neutron coincidence events to determine a fissioning item’s location based on the measured doubles count rate in various channel logic coincidence combinations. All of this can be done from a single measurement pulse train in offline analysis, which is the major benefit provided by LMDA. Through various stages of development and testing, a Mirion Technologies model JCC-71 Neutron Coincidence Collar has been successfully retrofit with modern electronics designed in-house at Oak Ridge National Laboratory, matching preexisting JAB-01 electronics performance, while maintaining the original system footprint. This paper presents these various stages of development and experimental evaluation of the proof of concept system.

Moore, Angela S.↗

Modernizing the active neutron collar poison rod correction using simulations to enhance PWR fresh fuel verification

The declared inventory of 235 U in fresh, low enriched uranium, nuclear fuel assemblies is routinely verified by nuclear safeguards inspectorates using the UNCL (Uranium Neutron Collar – Light Water Reactor Fuel) nondestructive assay instrument. The trend in modern fuels is towards higher initial enrichment, which in turn requires a larger number of burnable poison pins with higher Gadolinia concentration to hold down the initial reactivity. UNCL assay error for modern fuel assemblies typically exceeds 10%. The traditional algorithm used to correct the response for burnable poison content needs revision to achieve accuracy comparable to the $\sigma_\text{R}$ of 4.5% expected for poison-free assemblies. Here we review the problem and use a large set of 287 Monte Carlo simulations based on an experimentally benchmarked model corresponding to the 16×16 PWR array used in Brazilian Angra type II and III fuel. Simulated relative responses are used to evaluate the functional form of the poison correction and determine parameters optimal for 16×16 PWR assemblies. This update is conducted using between 4–24 Gadolinia pins ranging 2–11 wt% Gd 2 O 3 with assemblies having mean enrichments ranging 2.5%–5%. Experimental validation of the updated coefficients using seven measurements shows bias is reduced by an order of magnitude and $\sigma_\text{R}$R reduced from 10% to less than 2%. Two updated sets of coefficients are provided, the most accurate of which is directly useable in the existing analysis code (INCC) in use by inspectorate at fuel fabrication facilities.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Interpretation of energy deposition data from historical operation of the transient test facility (TREAT)

The Transient Test Reactor (TREAT) at Idaho National Laboratory will resume operations in late 2017 after a 23 year hiatus while maintained in a cold standby state. Over that time period, computational power and simulation capabilities have increased substantially and now allow for new multiphysics modeling possibilities that were not practical or feasible for most of TREAT's operational history. Hence the return of TREAT to operational service provides a unique opportunity to apply state-of-the-art software and associated methods in the modeling and simulation of general three-dimensional steady state and kinetic behavior for reactor operation, and for coupling of the core power transient model to experiment simulations. However, measurements taken in previous operations were intended to predict power deposition in experimental samples, with little consideration of three-dimensional core power distributions. Hence, interpretation of data for the purpose of validation of modern methods can be challenging. For the research discussed herein, efforts are described for the process of proper interpretation of data from the most recent calibration experiments performed in the core, the M8 calibration series (M8-CAL). These measurements were taken between 1990 and 1993 using a set of fission wires and test fuel pins to estimate the power deposition that would be produced in fast reactor test fuel pins during the M8 experiment series. Because of the decision to place TREAT into a standby state in 1994, the M8 series of transients were never performed. However, potentially valuable information relevant for validation is available in the M8-CAL measurement data, if properly interpreted. This article describes the current state of the process of recovery of useful data from M8-CAL measurements and quantification of biases and uncertainties to potentially apply to the validation of multiphysics methods.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Weighted delta-tracking in scattering media

In this work, we expand the weighted delta-tracking routine to include a treatment for scattering. The weighted delta-tracking routine adds survival biasing to normal delta-tracking, improving problem figure of merit. In the original formulation of this method, only absorption events were considered. We have expanded the method to include scattering and investigated the method’s effectiveness with two test cases: a pressurized water reactor pin cell and a fast reactor pin cell. We compare the figure of merit for calculating infinite flux and total cross-section while incrementally changing the amount of weighted delta-tracking used. Thus, we find that this new weighted delta-tracking (WDT) routine has strong potential to improve the efficiency of fast reactor calculations, and may be useful for light water reactor calculations.

97 MATHEMATICS AND COMPUTING↗