Influence of Melt-Pouring Temperature and Composition of Primary Coating of Shell Mold on Tensile Strength and Creep Resistance of Ni-Based Superalloy

Eight investment castings of Inconel 713C superalloy were fabricated, varying in the melt-pouring temperature, from 1400 to 1520 °C, and CoAl{sub 2}O{sub 4} inoculant content, 0 or 5 wt.%, in the primary coat. Their influence on grain size on tensile and creep properties was investigated. The best combination of yield stress (815 MPa) and elongation (A{sub 4} = 7.65%) at ambient temperature was obtained in surface-modified castings poured from 1520 °C. The longest time to rupture was for the unmodified castings (76.8 h) poured from 1520 °C, while for the modified variant, the time to rupture was lower around, 7.4 h, which was still a satisfactory value. During tensile testing, microcracks were formed in large eutectic γ′, carbides and borides, due to the accumulation of stress at interfaces with the matrix. During creep, N-type rafting of γ′ precipitates and phase transformation MC + γ → γ′ + M{sub 23}C{sub 6} took place.

36 MATERIALS SCIENCE↗

Influence of Rolling Temperature on the Mechanical Properties and Microstructure of Variable-Plane-Rolled Mg-3Al-1Zn Alloy

AZ31 magnesium alloy was produced via variable-plane rolling (VPR) under different temperatures. The effects of rolling temperature on the microstructure, texture and mechanical properties were investigated. A double-peak basal texture was formed during VPR treatment. Dynamic recrystallization (DRX) was observed during the VPR treatment, and it can reduce the texture intensity owing to the coalescence of sub-grains. Four types of twins were observed in the VPR treatment: {10-12} extension twins, {10-13}, {10-11} contraction twins and {10-11}-{10-12} double twins. The suitable temperature of AZ31 magnesium alloy for VPR treatment is determined as 623 K through experiments with tensile yield strength of 240 MPa, compressive yield strength of 162 MPa and elongation of 13%. Owing to the important impact of temperature on mechanical properties, the alloy was further VPRed with a decrease in temperature pass-by-pass. The high temperature of 623 K at the initial passes randomized the texture, which led to notably high ductility.

36 MATERIALS SCIENCE↗

Effects of Nb on Superelasticity and Low Modulus Properties of Metastable β-Type Ti-Nb-Ta-Zr Biomedical Alloys

In this work, a series of Ti-xNb-2Ta-3Zr (x = 25, 30, 35, 40 wt.%) alloys are designed, and the transformation of β-phase to α″ martensitic, β-phase stability, microstructure, mechanical properties and corrosion performance of these alloys are investigated. The phase analysis shows as the Nb content increases, the α″ phase in these alloys decreases, while the intensity of the two main peaks β(110) and β(211) of Ti-40Nb-2Ta-3Zr alloy is reduced. These results can be attributed to the variation of β-phase stability caused by Nb element of alloy and cold rolling process. The mechanical properties test shows that the elastic modulus (52 GPa) of the Ti-35Nb-2Ta-3Zr alloy is the lowest and the elongation (18.8%) is the maximum. In addition, the alloy is susceptible to β-phase elastic deformation and stress-induced martensitic transformation resulting in the highest recovery strain of the alloy (66.87%). The polarization curves show that the Ti-35Nb-2Ta-3Zr alloy has the highest corrosion potential (− 0.34 V) and the lowest corrosion current density (0.21 μA cm{sup −2}) exhibiting the best corrosion resistance.

36 MATERIALS SCIENCE↗

In Vitro Degradation, Antibacterial Activity and Cytotoxicity of Mg-3Zn-xAg Nanocomposites Synthesized by Mechanical Alloying for Implant Applications

A class of biodegradable Mg-3Zn-xAg nanocomposites was presented in the present study with the assessments for implant application. The evaluations included the effects of increasing the Ag content from 0.5 to 3 wt.% on the corrosion behavior, mechanical properties, antibacterial activity and cytotoxicity of Mg-3Zn-xAg nanocomposite. Microstructural analysis revealed the secondary phase intermetallic Mg{sub 54}Ag{sub 17} along the grain boundaries, with grain refinement as a result of increasing the Ag concentration. 0.5 wt.% Ag results in increasing the compressive strength and elongation; however, further addition decreases the compressive strength. The nanocomposite samples were verified for the improved antimicrobial activity by utilizing both E. coli and S. aureus bacteria, the growth of which was suppressed around all Ag-containing nanocomposites, whereas bacterial proliferations were detected around the Mg-3Zn nanocomposite. The escalating levels of Ag in the nanocomposite resulted in the elevated antimicrobial effect. Cell adhesion and proliferation were not significantly influenced by the inclusion of 0.5-1 wt% Ag into Mg-3Zn nanocomposite; however, cell adhesion and proliferation were lower on the surfaces of the nanocomposite containing 2-3 wt.% Ag counterparts. According to the mechanical, corrosion and biological assessments in the current research, it can be concluded that the nanocomposite containing 0.5 wt.% Ag can be properly applied as an orthopedic implant biomaterial.

36 MATERIALS SCIENCE↗

Effects of the Addition of Micro-amounts of Calcium on the Corrosion Resistance of Mg-0.1Mn-1.0Zn-xCa Biomaterials

Magnesium alloys have good biocompatibility and degradability, which are considered ideal characteristics of biomedical implants. However, there are few studies on the influence of the addition of micro-amounts of Ca on magnesium alloys. In this work, the effects of adding micro-amounts of Ca on the microstructure, mechanical properties, and corrosion properties of Mg-0.1Mn-1.0Zn-xCa (x = 0.1, 0.2, and 0.3 wt.%) alloys were investigated. The results reveal that the grain size of the alloy decreased and the yield strength and elongation both increased with increasing Ca concentrations. Corrosion tests in Kokubo simulated body fluid showed that the in vitro immersion rate first slowed down and then increased (6.395 → 6.283 → 6.395 mm/year) with increasing Ca concentrations. This phenomenon was due to the addition of Ca causing grain refinement, which slowed the corrosion rate and generated an Mg{sub 2}Ca phase to accelerate corrosion. The second-phase Mg{sub 2}Ca precipitated at the grain boundary and acted as a cathode, and the metal magnesium phase acted as an anode to form a primary battery, which caused corrosion of the magnesium phase and accelerated the corrosion rate.

36 MATERIALS SCIENCE↗

Development of a High-Strength Low-Carbon Steel with Reasonable Ductility through Thermal Cycling

In this research work, cost-effective structural material synthesis routes have been adopted in the form of thermal cycling designed and applied on a low-cost material (AISI 1010 steel). The main synthesis route consists of two-step thermal cycling (designed with respect to iron–carbon phase diagram) combining short-duration holding in upper critical and intercritical temperature regimes and different cooling conditions (forced air cooling and ice-brine quenching). Accordingly, the adopted hierarchical design approach (from nanoscale onwards) with a combination of hard and soft phases (to attain an adequate balance between mutually exclusive strength and ductility properties) results in origin of a novel microstructure. The microstructure consists of dislocation-enriched martensite regions (possessing plate and lath morphologies in 1:4 ratio) containing nanosized cementite particles and α-ferrite regions containing submicroscopic cementite particles. As a consequence, an excellent combination of strength (UTS = 905 MPa) and ductility (%Elongation = 17) is achieved in the synthesized material.

36 MATERIALS SCIENCE↗

The Hot Bending and Diffusion Bonding of TiAl-Based Alloy for Corrugated-Core Sandwich Structure

The multi-layer structure of TiAl-based alloys can meet the demand of having lightweight and high-strength properties at elevated temperature. In this paper, the corrugated-core sandwich structure of a TiAl-based alloy was fabricated by the hot bending/diffusion bonding process. In order to fabricate this structure, the high-temperature tensile property, hot bending behavior, and vacuum diffusion bonding of a Ti-47.5Al-Cr-V alloy were investigated. The flow behavior was evaluated by uniaxial tensile experiment, and the results showed that the alloy exhibited good plasticity at the given conditions, and the maximum elongation reached 200% at 1000 °C at strain rate of 3 × 10{sup −4} s{sup −1}. The bending experiments were also performed at temperatures of 950, 1000, and 1050 °C with fillet radii of R = 0, 0.5, and 1 mm, respectively. No micro-/macro-defects developed. The vacuum diffusion bonding of this alloy was also carried out, and the shear bonding strength of bonding joints was measured at room temperature. The maximum shear strength was 398 MPa, and the joint was obtained at 1000 °C/30 MPa/3 h. Combining the bonding interface with the shear strength of different joints, the appropriate bonding pressure and bonding time for diffusion bonding of the TiAl alloy at 1000 °C were 20 MPa and 2 h, respectively. Then, the forming process of the corrugated-core sheet was conducted at 1000 °C with a fillet radius of 1 mm. Finally, the corrugated-core sandwich structure was manufactured under vacuum atmosphere, and the mechanical properties and the interface microstructure were investigated.

36 MATERIALS SCIENCE↗

The Microstructure, and Mechanical and Corrosion Properties of As-Cast and As-Extruded Mg-2%Zn-x%Cu Alloys After Solution and Aging Heat Treatments

The effects of different Cu concentrations and heat treatment on the microstructure, mechanical and corrosion properties of the as-cast and hot-extruded Mg-2%Zn alloys were studied. The results showed that T6 heat treatment led to the dissolution of intermetallics and breaking the continuous networks of intermetallics. Also, the grain size of the base alloy decreased with further Cu additions after solution and aging heat treatments. Microstructural characterization indicated that Mg(Zn,Cu) and Mg(Zn,Cu){sub 2} intermetallics were formed which their volume fractions increased with exceeding Cu additions. Moreover, the addition of 3 wt.% Cu and T6 heat treatment increased the Brinell hardness of both as-cast and hot-extruded specimens reached to 94 HBN and 116 HBN, respectively. The optimum amounts of the ultimate tensile strength and elongation values obtained from 0.1 wt.% Cu addition for both conditions after T6 treatment which were 253 MPa, 11.5% and 263 MPa, 14.7%, respectively. However, more Cu addition (> 0.5 wt.%) deteriorated the tensile properties of the alloy due to the high volume fraction of intermetallics. The yield tensile strength increased continuously with different Cu additions for the cast and extruded alloys after solution and aging heat treatments. After T6 heat treatment, extruded alloys showed better anti-corrosion properties than those of the cast alloys, while the extruded Mg-2%Zn-0.1%Cu alloy exhibited the best anti-corrosion property. Further Cu addition increased the volume fraction of intermetallics and enhanced the corrosion rate which was due to the galvanic couple effect.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of a Multiphase FeCrCuMnNi High-Entropy Alloy

A FeCrCuMnNi high-entropy alloy was produced using vacuum induction melting, starting from high-purity raw materials. The microstructure and mechanical properties of the as-cast FeCrCuMnNi alloy were studied, considering x-ray diffraction (XRD), scanning electron microscopy, and hardness and tensile tests. XRD results revealed the existence of two FCC phases and one BCC phase. Microstructural evaluation illustrated that the as-cast alloy has a typical cast dendritic structure, where dendrite regions (BCC) were enriched in Cr and Fe. Interdendritic regions were saturated with Cu and Ni and revealed G/B(T) {110} 〈111〉 and Brass {110} 〈112〉 as the major texture components. The produced alloy revealed an excellent compromise in mechanical properties due to the mixture of solid solution phases with different structures: 300 HV hardness, 950 MPa ultimate tensile strength and 14% elongation. Microhardness test results also revealed that the BCC phase was the hardest phase. The fracture surface evidenced a typical ductile failure. Furthermore, heat treatment results revealed that phase composition remained stable after annealing up to 650 °C. Phase transformation occurred at higher temperatures in order to form more stable phases; therefore, FCC2 phase grew at the expense of the BCC phase.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Behavior of MnO{sub 2}/Pb Nanocomposite

MnO{sub 2}/Pb nanocomposite was produced by solid-state accumulative roll-bonding (ARB) technique. Composites with different amounts of MnO{sub 2} were synthesized with the highest probable ARB cycles. The mechanical properties of composites were studied by tensile, microhardness and shear punch tests. It was observed that yield stress, tensile stress and elongation were improved by increasing the ARB cycles. On the other hand, increasing the amount of MnO{sub 2} up to 0.5 wt.% improved the mechanical properties of the composites. Tensile tests results revealed that the maximum tensile strength could be achieved in the composite containing 0.5 wt.% MnO{sub 2} after 10 passes (up to 4.35 times higher than control sample, Pb-10 pass). In comparison with Pb-10 pass, the hardness of 0.5 wt.% MnO{sub 2}/Pb nanocomposite was enhanced up to 7.5 times after 10 ARB passes. ARB process led to a proper distribution of MnO{sub 2} particles in Pb matrix with the mean size of less than 30 nm.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Extruded Mg-7Sn-5Zn-xAl (x = 0, 1, 2 and 3 wt.%) Alloy

Microstructure and mechanical properties of extruded Mg-7Sn-5Zn-xAl (x = 0, 1, 2 and 3 wt.%) alloy were investigated. The as-cast Mg-7Sn-5Zn alloy mainly comprised α-Mg dendrites, Mg{sub 2}Sn and nanosized Mg-Zn phases in a Mg matrix, whereas the quasicrystal (icosahedral (I)) phase precipitated with the addition of Al. After extrusion, the grain size decreased due to dynamic recrystallization and the resulting particles were crushed and distributed along the extrusion direction. The highest tensile strength was exhibited by the extruded Mg-7Sn-5Zn-2Al alloy, which had a yield strength, ultimate tensile strength and elongation to failure of 198, 343 MPa and 18.7%, respectively. The high tensile strength was mainly attributed to grain refinement and precipitation strengthening of the Mg{sub 2}Sn and icosahedral phases.

36 MATERIALS SCIENCE↗

Effect of Through-Thickness Friction Stir Processing Parameters on Weld Repair and Modification of Fusion-Welded AA6061 Aluminum Alloy

Through-thickness friction stir processing was successfully carried out for microstructure modification and elimination of fusion defects of the gas metal arc welds by applying the process on as-welded joints. Variation in rotational speed from 750 to 1050 rpm and traveling speed from 50 to 200 mm/min resulted in minor changes (approximately 1 µm) in the grain size of nugget zone, while this variation in elongation result was up to 40%. The hardness profile, the width of softening zone, minimum hardness and fracture location also changed for different processing conditions. Furthermore, the defects were vanished efficiently across the welds profile by this method. The results also verified the geometric dynamic recrystallization phenomena as a dominant mechanism of microstructural modification.

36 MATERIALS SCIENCE↗

Microstructure Evolution and Mechanical Properties of Large-Scale AZ80 Magnesium Alloy Billets Produced by Multitemperature Multidirectional Forging

Grain refinement is an effective method to improve the mechanical properties of magnesium (Mg) alloys. In the present research, the combination of multidirectional forging (MDF) and forward extrusion for sizing with decreasing temperature pass by pass was employed to deform as-cast AZ80 magnesium alloy billet with large size to obtain fine grains and homogeneous microstructure. It was found that with the increasing number of MDF passes, the average grain size decreases; the homogeneity of microstructures and the percentages of dynamic recrystallised grains increase simultaneously. After six-pass MDF, fine and homogeneous microstructure with an average grain size of 15 μm was achieved; however, grain refinement became very difficult with a further increase in the MDF pass number. After eight-pass MDF plus forward extrusion for sizing, excellent mechanical properties of large-scale AZ80 magnesium alloy billet were obtained. The tensile strength, the yield strength and the elongation of billet are 410 MPa, 292 MPa and 14%, respectively. Furthermore, during multitemperature MDF, the inverse of the square root of grain size and tensile yield strength fit well with the Hall–Petch relationship.

36 MATERIALS SCIENCE↗

Mechanical and Electrochemical Behavior of Dual-Phase Steels Having Varying Ferrite–Martensite Volume Fractions

Dual-phase (DP) steels behave differently under corrosive environment depending upon the volume fractions of phases, mainly martensite, ferrite and bainite. The mechanical behavior and corrosion resistance of DP steels with varying martensite (from 32 to 100%) are investigated. The increase in martensite volume fraction of DP steel results in significant improvement in tensile strength and hardness with a subsequent reduction in elongation. Unlike the mechanical behavior, the increase in martensite volume fraction in steel does not exhibit a direct relationship with their corrosion resistance behavior. The corrosion mechanism in DP steels having different martensite and ferrite volume fractions depends on the self-corrosion resistance behavior of both the phases as well as the occurrence of galvanic corrosion between them.

36 MATERIALS SCIENCE↗

The Effect of Multistage Aging on Mechanical Properties and Microstructure of Forged 7050 Aluminum Alloys

A new four-stage aging treatment, which is composed of pre-aging, retrogression, natural aging (NA) and re-aging, is designed to increase the tensile properties and the fatigue life of forged 7050 aluminum alloy in this work. As compared to traditional T74 and RRA treatments, the four-stage aging-treated sample exhibits the highest tensile properties and ductility. The tensile strength and yield strength are 627 and 608 MPa, respectively, and the elongation is 11.3%. The results of TEM and DSC show that an increased G.P zones and fine η′ phase distributed in the matrix of the alloy are subjected by this new aging processing as compared with T74 and RRA treatments. The natural aging in four-stage aging treatment accelerates the diffusion of Mg vacancies, and promotes the precipitation of G.P zones in grain interior during re-aging stage. On the basis of dislocation shearing mechanism, more dense and fine G.P zones of four-stage aging temper result in the superior tensile strength as compared to T74 and RRA temper. In addition, a combination of shearable precipitates, fine GBPs and narrow PFZs is beneficial to the slip reversibility in the plastic zone at the crack tip, thereby reducing fatigue damage accumulation and increasing the fatigue life.

36 MATERIALS SCIENCE↗

Effect of Anisotropy on Microstructures and Mechanical Properties of Rolled Ti/Al/Mg/Al/Ti Laminates

TA2/5052Al/AZ31/5052Al/TA2 five-ply laminates were fabricated by hot rolling, and the effect of anisotropy on their microstructures and mechanical properties was studied. After rolling, the Mg/Al and Al/Ti interfaces were both closely connected, but the interfacial shapes were totally different. For the Mg layer microstructures in the middle area, regardless of the direction, dynamic recrystallized (DRXed) grains appeared around the deformation bands. However, twins and a shear zone appeared in the RD sample; the twins decreased in the sample along the 45° angle, and no twins appeared in the TD sample. The Ti layer showed equiaxed grains in different directions, which were attributed to the ability of Ti alloy to anti-deform. The tensile testing results showed that the fracture of the Ti/Al/Mg/Al/Ti laminates can be divided into four stages. The laminate had an ultimate tensile strength of 434 MPa and excellent elongation along the rolling direction (RD), which were attributed to its DRXed grains and twins. In conclusion, the laminates had significant anisotropy due to the presence of Mg alloys.

36 MATERIALS SCIENCE↗

Microstructural Characteristics and Mechanical Properties of Friction-Stir-Welded CuSn6 Tin Bronze

Tin bronze is widely applied in various industries for its excellent wear and corrosion resistance. Friction stir welding is a solid-state welding process, which generates less heat and avoids the melting-related defects. CuSn6 tin bronze plates of 4 mm in thickness were friction-stir-welded at welding speeds ranging from 50 to 150 mm/min under a constant rotation speed. The microstructural and mechanical properties of joints were investigated. The microstructure of the stir zone consists of refined equiaxed grains. The grain size decreased from top to bottom of the welds. The mean grain size is increased with increasing welding speed. The largest strength and elongation of welded joints were both obtained at the welding speed of 100 mm/min. During tensile test, all of the joints were fractured at the heat affected zone of retreating side with typical plastic fracture feature, since the grains were coarsened by welding heat.

36 MATERIALS SCIENCE↗

Forced Cooling Friction Stir Welding of 2060-T8 Al-Li Alloy

Friction stir welding of 2060-T8 Al-Li alloy was experimentally investigated. Forced cooling process was realized by placing two copper pressure plates with a waterway on both sides of weld top surface. The relations between joint formation, microstructures and mechanical properties were mainly discussed. Compared with conventional joint by natural cooling, the welding joint with smaller flashes by forced cooling has the smaller well-distributed grains and higher microhardness in the stir zone (SZ). The tensile strength and elongation of forced cooling joint, respectively, reach 445.7 MPa and 6.7%, which are obviously higher than those of the conventional joint. The fracture locations of the conventional and forced cooling joints are located in the SZ, and the fracture surface morphologies show a typical ductile fracture mode.

36 MATERIALS SCIENCE↗