Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “refinement”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,495 records · Page 83

Microstructure and mechanical properties of duplex stainless steel subjected to hydrostatic extrusion

The nanostructure and mechanical properties of ferritic-austenitic duplex stainless steel subjected to hydrostatic extrusion were examined. The refinement of the structure in the initial state and in the two deformation states (ε = 1.4 and ε = 3.8) was observed in an optical microscope (OM) and a transmission electron microscope (TEM). The results indicate that the structure evolved from microcrystalline with a grain size of about 4 μm to nanocrystalline with a grain size of about 150 nm in ferrite and 70 nm in austenite. The material was characterized mechanically by tensile tests performed in the two deformation states. The ultimate strength appeared to increase significantly compared to that in the initial deformation stages, which can be attributed to the grain refinement and plastic deformation. The heterogeneity observed in microregions results from the dual-phase structure of the steel. The results indicate that hydrostatic extrusion is a highly potential technology suitable for improving the properties of duplex steels. - Highlights: • Duplex stainless steel was hydro extruded to a total strain of 3.8 • After the last stage of deformation heterogeneous structure was obtained in the material • As a result of stresses non-diffusive transformation γ→α’ occurred in the material • Nanometric (sub)grains were obtained in the austenite regions.

36 MATERIALS SCIENCE↗

The effect of boron addition on microstructure and mechanical properties of biomedical Ti35Nb6Ta alloy

The beta-titanium alloys are promising materials for bioapplications but their processing via melting is difficult. Coarse grains have been observed in as-cast specimens. Subsequent thermo-mechanical processing seems to be necessary in order to obtain fine-grained microstructure with better mechanical properties. The grain size can be decreased significantly by addition of small boron amount. In this work Ti–35Nb–6Ta alloy with various B additions (0, 0.05, 0.1, 0.3 and 0.5 wt.%) has been studied. Even the smallest amount of B leads to significant grain refinement in Ti–35Nb–6Ta alloy (from 1300 to about 350 μm). Slight grain refinement has been observed also after hot forging and solution treatment. TiB particles emerged in specimens due to B addition. These particles contribute to changes in mechanical properties not only in hot forged and solution treated specimens (hardness increase from 140 to 180 HV10), but also in cold swaged specimens (hardness from 230 to 250 HV10, tensile strength from 800 to 920 MPa). The hardness values can be increased up to 370 HV10 during aging at 400 °C (specimen with 0.5 wt.% B). It has been observed that specimens with low boron addition 0.05 wt.% possess no cytotoxicity. On the other hand in specimens with 0.1 wt.% B or more slight adverse effect on cytotoxicity has been observed. - Highlights: • The influence of boron on microstructure and mechanical properties has been studied. • Beta-transus temperature has been determined. • Cytotoxicity depending on boron content has been evaluated. • Possibility of final heat treatment has been determined.

36 MATERIALS SCIENCE↗

An EBSD investigation of cryogenically-rolled Cu–30%Zn brass

Electron backscatter diffraction was used to study grain structure development in heavily cryogenically-rolled Cu–30%Zn brass. The produced microstructure was found to be very inhomogeneous. At a relatively coarse scale, it consisted of texture bands having crystallographic orientations close to the α- and γ-fibers. The texture bands contained internal structure comprising shear bands, mechanical twins, and low-angle boundaries. Such features were more pronounced within the γ-fiber, and this resulted in a heterogeneous ultrafine grain structure. The cryogenic rolling was concluded to be not straightforward for production of nanocrystalline grain structure in Cu–30%Zn brass. - Highlights: • Cryogenic rolling produced an inhomogeneous ultrafine-grained microstructure. • Grain refinement was mainly related with twinning and shear banding. • Grain refinement preferentially occurred in (111) fiber texture.

36 MATERIALS SCIENCE↗

Friction stir processing of an aluminum-magnesium alloy with pre-placing elemental titanium powder: In-situ formation of an Al{sub 3}Ti-reinforced nanocomposite and materials characterization

A fine-grained Al–Mg/Al{sub 3}Ti nanocomposite was fabricated by friction stir processing (FSP) of an aluminum-magnesium (AA5052) alloy with pre-placed titanium powder in the stirred zone. Microstructural evolutions and formation of intermetallic phases were analyzed by optical and electron microscopic techniques across the thickness section of the processed sheets. The microstructure of the nanocomposite consisted of a fine-grained aluminum matrix (1.5 µm), un-reacted titanium particles (<40 µm) and reinforcement particles of Al{sub 3}Ti (<100 nm) and Mg{sub 2}Si (<100 nm). Detailed microstructural analysis indicated solid-state interfacial reactions between the aluminum matrix and micro-sized titanium particles to form Al{sub 3}Ti intermetallic phase. The hard inclusions were then fractured and re-distributed in the metal matrix by the severe thermo-mechanical conditions imposed by FSP. Evaluation of mechanical properties by hardness measurement and uniaxial tensile test determined significant enhancement in the mechanical strength (by 2.5 order of magnetite) with a high ductility (~22%). Based on a dislocation-based model analysis, it was suggested that the strength enhancement was governed by grain refinement and the presence of hard inclusions (4 vol%) in the metal matrix. Fractographic studies also showed a ductile-brittle fracture mode for the nanocomposite compared with fully ductile rupture of the annealed alloy as well as the FSPed specimen without pre-placing titanium particles. - Highlights: • FSP was employed to fabricate in situ nanocomposite. • The AA5052 Al alloy with pre-placed micro-sized Ti particles were utilized. • The structural analysis was revealed that the in situ formation of Al{sub 3}Ti nanophase. • The SZ grain structure was refined by PSN and ZHP mechanisms during DRX. • Hardness and tensile strength were improved up to ~2.5 times with a good ductility.

36 MATERIALS SCIENCE↗

Microstructure characterization of LAE442 magnesium alloy processed by extrusion and ECAP

The magnesium alloy LAE442 was processed by extrusion and equal channel angular pressing (ECAP) to achieve ultrafine grained microstructure. Detailed characterization of the microstructure was performed by scanning electron microscope, electron back scattered diffraction (EBSD) and transmission electron microscope. The initial, as-cast, microstructure consisted of large grains of ~ 1 mm. The grain refinement due to the processing by severe plastic deformation led to a decrease of the average grain size to ~ 1.7 μm after the final step of ECAP. A detailed characterization of secondary phases showed the precipitation of Al{sub 11}RE{sub 3}, Al{sub 2}Ca and Al{sub 10}RE{sub 2}Mn{sub 7} intermetallic phases. X-ray diffraction measurements proved that Li is dissolved within the magnesium matrix in the as-cast condition. Newly formed Al{sub 3}Li phase was observed after ECAP. The texture formation due to the extrusion and ECAP was different from that in the other magnesium alloys due to the activation of non-basal slip systems as a result of the decrease of the c/a ratio. - Highlights: • Combined extrusion and equal channel angular pressing results in significant grain refinement by factor 1000 approximately. • Al{sub 11}RE{sub 3}, Al{sub 2}Ca and Al{sub 10}RE{sub 2}Mn{sub 7} secondary phases are present in the as-cast material while Li was dissolved in the Mg matrix. • Extrusion and ECAP have no effect on the composition of the secondary phases but they influence strongly their distribution. • Texture evolution is affected by decrease of c/a ratio due to the presence of Li and resulting activation of non-basal slip.

36 MATERIALS SCIENCE↗

Experimental investigation of grain boundaries misorientations and nano twinning induced strengthening on addition of silicon carbide in pulse electrodeposited nickel tungsten composite coating

Nanoindentation was performed on silicon carbide (SiC) reinforced pulse electrodeposited nickel-tungsten (Ni-W) composite coating. Addition of 5 vol.% of SiC in Ni-W coating increased the hardness from 10.31 ± 0.65 GPa to 14.32 ± 0.63 GPa and elastic modulus from 119.74 ± 3.15 GPa to 139.26 ± 2.09 GPa. Increased hardness and elastic modulus directly translates to the improved strengthening in the coating. An experimental investigation of strengthening mechanism was carried out in Ni-W-5 vol.% SiC alloy. Two simultaneous phenomena viz. grain refinement and increased internal strain was observed, which increased the dislocation density from 5.51 × 10{sup 18} m{sup −2} to 1.346 × 10{sup 19} m{sup −2} on reinforcement of 5 vol.% of SiC in Ni-W coating. Increased dislocation density promoted the formation of grain boundary misorientations and nano twinning. Low angle grain boundary, high angle grain boundary and nano twinning were identified using high resolution transmission electron microscope (HR-TEM) image and their role in strengthening mechanism was discussed in details. - Highlights: • SiC reinforced pulse electrodeposition Ni-W coating was deposited on steel. • Nanoindentation showed the increased mechanical properties on addition of SiC. • Grain refinement and increased internal strain was observed in Ni-W-SiC coating. • Dislocation density increased on reinforcement of SiC in Ni-W coating. • Increased dislocation density triggered grain boundary misorientation and twinning.

36 MATERIALS SCIENCE↗

Correlative characterization of primary particles formed in as-cast Al-Mg alloy containing a high level of Sc

Primary particles formed in as-cast Al-5Mg-0.6Sc alloy and their role in microstructure and mechanical properties of the alloy were investigated using optical microscopy (OM), scanning electron microscopy (SEM), electron back-scatter diffraction (EBSD) and tensile testing. It was found that primary particles due to a close orientation to matrix could serve as the potent heterogeneous nucleation sites for α-Al during solidification and thus impose a remarkable grain refinement effect. Eutectic structure consisted of layer by layer of ‘Al{sub 3}Sc + α-Al + Al{sub 3}Sc + ⋯’ and cellular-dendritic substructure were simultaneously observed at the particles inside, indicating that these particles could be identified as the eutectics rather than individual Al{sub 3}Sc phase. A calculating method, based on EBSD results, was introduced for the spatial distribution of these particles in matrix. The results showed that these eutectic particles randomly distributed in matrix. In addition, the formation of primary eutectic particles significant improved the strength of the Al-Mg alloy in as-cast condition, which is ascribed to the structural evolution from coarse dendrites to prefect fine equiaxed grains. On the other hand, these large-sized particles due to the tendency to act as the microcrack sources could cause a harmful effect in the ductility of Al-Mg-Sc alloy. - Highlights: •Primary particles exhibit an ‘Al{sub 3}Sc + α-Al + Al{sub 3}Sc + ⋯’ multilayer feature with a cellular-dendritic mode of growth. •EBSD analyses the mechanism of grain refinement and the distribution of primary particles in α-Al matrix. •A computational method was presented to calculate the habit planes of primary particles.

36 MATERIALS SCIENCE↗

Nanostructure formation during accumulative roll bonding of commercial purity titanium

In this investigation, commercial purity titanium (CP–Ti) was subjected to accumulative roll bonding (ARB) process up to 8 cycles (equivalent strain of 6.4) at the ambient temperature. Transmission electron microscopy (TEM) and X–ray diffraction line profile analysis (XRDLPA) were utilized to investigate the microstructure and grain size evolution. Both characterization techniques could clarify the non–uniform microstructure in the early stages and the uniform microstructure in the final stages of the process. The effectiveness of ARB for the fabrication of the nano–grained structure in CP–Ti was revealed. It was found that the SFE is not the only factor affecting grain refinement, as compared with other studies on ARB of FCC materials. Influence of other factors such as the melting temperature and the crystalline structure of the material was determined on the grain refinement. - Highlights: •Nano–grained commercial purity titanium was produced by accumulative roll bonding. •TEM and XRDLPA were used for the characterization of the microstructure. •Important factors affecting the grain size of ARBed materials were discussed.

36 MATERIALS SCIENCE↗

Microstructure, microtexture and precipitation in the ultrafine-grained surface layer of an Al-Zn-Mg-Cu alloy processed by sliding friction treatment

Precipitate redistribution and texture evolution are usually two concurrent aspects accompanying grain refinement induced by various surface treatment. However, the detailed precipitate redistribution characteristics and process, as well as crystallographic texture in the surface refined grain layer, are still far from full understanding. In this study, we focused on the microstructural and crystallographic features of the sliding friction treatment (SFT) induced surface deformation layer in a 7050 aluminum alloy. With the combination of transmission electron microscopy (TEM) and high angle angular dark field scanning TEM (HAADF-STEM) observations, a surface ultrafine grain (UFG) layer composed of both equiaxed and lamellar ultrafine grains and decorated by high density of coarse grain boundary precipitates (GBPs) were revealed. Further precession electron diffraction (PED) assisted orientation mapping unraveled that high angle grain boundaries rather than low angle grain boundaries are the most favorable nucleation sites for GBPs. The prominent precipitate redistribution can be divided into three successive and interrelated stages, i.e. the mechanically induced precipitate dissolution, solute diffusion and reprecipitation. The quantitative prediction based on pipe diffusion along dislocations and grain boundary diffusion proved the distribution feasibility of GBPs around UFGs. Based on PED and electron backscatter diffraction (EBSD) analyses, the crystallographic texture of the surface UFG layer was identified as a shear texture composed of major rotated cube texture (001) 〈110〉 and minor (111) 〈112〉, while that of the adjoining lamellar coarse grained matrix was pure brass. The SFT induced surface severe shear deformation is responsible for texture evolution. - Highlights: •The surface ultrafine grain layer in a 7050 aluminum alloy was focused. •Precipitate redistribution and texture evolution were discussed. •The quantitative prediction proved the distribution feasibility of GBPs. •Precession electron diffraction orientation mapping showed a shear texture.

36 MATERIALS SCIENCE↗

Microstructure detection of Mg-Zi-Ti-Si amorphous composite coating prepared by SMAT

Highlights: • The Mg-Zn-Ti-Si amorphous composite coating was prepared on Mg alloy via SMAT. • Except for amorphous portion, the phases of coating include Zn, Mg{sub 7}Zn{sub 3}, and Si. • The coating was thick and rough but it was well combined with the matrix. • During SMAT, the matrix surface was also strengthened because of solid-solution and grain refinement. - Abstract: The Mg-Zn-Ti-Si coating was prepared on Mg alloy through surface mechanical attrition treatment (SMAT) which was simple and low-cost. The microstructure and phase composition of coating were detected through a scanning electron microscope (SEM), an X-ray diffractometer (XRD) and a high resolution transmission electron microscope (HRTEM). The results demonstrated that the layer thickness, which depended on the rotation speed, was 20–80 μm. Although the coating was rough, it was well combined with the matrix. The XRD pattern and HRTEM image analysis demonstrated that the coating contained both amorphous and crystalline phases (Zn, Mg{sub 7}Zn{sub 3} and Si). The process also led to matrix surface strengthening; the mechanisms are solid solution and grain refinement.

36 MATERIALS SCIENCE↗

The effect of Cerium addition on microstructure and mechanical properties of high pressure die cast Mg-5Sn alloy

Highlights: • The alloying additive has good grain refinement effect. • The addition of Ce to the Mg-5Sn alloy led to the formation of the new intermetallic phases CeMgSn and Ce{sub 5}Sn{sub 4}. • The hardness, yield and tensile strength of Mg-5Sn alloy were improved with addition of Ce. • The elongation of Mg-5Sn was increased up to 5wt.%Ce addition, and then decreased with addition of 7 wt.%Ce. • The yield and tensile strength of the Ce added alloy were higher than those of the base alloy at elevated temperatures. - Abstract: The effect of Cerium addition to Mg-5Sn alloy and its influence on the microstructure and mechanical properties of the alloy were investigated in this work. The microstructural investigations indicate that the alloying addition of Ce leads to effective grain refinement. Also, it was observed that adding Ce to the Mg-5Sn alloy results in the formation of new phases in the alloy such as Ce{sub 5}Sn{sub 4} and CeMgSn. These intermetallic phases were considered to be effective on the enhancement of the hardness of Mg-5Sn alloy. Furthermore, the tensile test results at room temperature and elevated temperatures revealed that the yield and tensile strength of the Ce added alloy were higher than those of the base alloy. The elongation was also improved up to 5 wt% Ce addition while higher amounts decreased the elongation both at room and elevated temperatures.

36 MATERIALS SCIENCE↗

Microstructure evolution in the conventional single side and bobbin tool friction stir welding of thick rolled 7085-T7452 aluminum alloy

Highlights: • Comparison of microstructure evolution via EBSD of SS-FSW and BB-FSW was investigated. • Friction heat, strain rate and degree of recrystallization affected grain size. • Discontinuously dynamic recrystallization occurred in the weld nugget zone. • The degree of recrystallization was mainly controlled by the strain rate. - Abstract: The microstructure evolution during the conventional single side friction stir welding (SS-FSW) and the bobbin tool FSW (BB-FSW) of 7085-T7452 alloy thick plate was extensively studied by using the state-of-the-art materials characterization techniques. The Electron backscattering diffraction results reveal that a significant grain refinement and a larger percentage of high angle grain boundaries (HAGBs) exist in the weld nugget zone (WNZ) and the thermal-mechanical affected zone (TMAZ) compared with the base material. Meanwhile, more obviously inhomogeneous refined grains and HAGBs in WNZ along the thickness direction and a larger percentage of low angle grain boundaries (LAGBs) were observed in SS-FSW joint than that in BB-FSW joint. The change of the average grain size is the result of friction heat and strain rate of plastic deformation combined with a certain degree of recrystallization. Moreover, the recrystallization is mainly controlled by the strain rate during the FSW process. The presence of Cube and Cube ND after welding shows that the discontinuously dynamic recrystallization (DDRX) is a major factor in the final microstructural response. The research and findings help the understanding of the mechanism of microstructure homogenization and further optimizing the welding process for application.

36 MATERIALS SCIENCE↗

Microstructure and mechanical performance of welded joint between a novel heat-resistant steel and Inconel 617 weld metal

Highlights: • MGBs were suspected as the DDC crack source during high-temperature tensile test. • Microhardness variations in different passes of joint denote grain refinement effect induced by the multi-pass welds. • After tensile test, changes in microhardness can be attributed to the extent of deformation and amount of precipitation. - Abstract: In the present study, the microstructure and mechanical performance of a tungsten inert gas welded joint between a novel heat-resistant austenitic steel and Inconel 617 weld metal were examined. Migrated grain boundaries were discovered more frequently in the lower portion of the weld metal that solidifies in austenite type. Ti-rich precipitates were observed in weld metal and Cr-rich and Nb-rich precipitates were observed in base metal. The fusion boundary area had the lowest impact toughness due to the large non-homogeneity of the microstructure. Microhardness profiles of the joint were obtained and the backing passes were found to produce the highest microhardness values, which was caused by the grain refinement effect. Ductile failure with slipping separation occurred in those joints ruptured after tensile tests at both room temperature and 923 K. In addition, multiscale precipitates in the joint after high-temperature tensile tests were inspected, where it was found that nanoscale particles contributed to the high-temperature resistance of the joint. Furthermore, microhardness changes in the joint after tensile tests were analysed according to the precipitation and strain-hardening mechanism.

36 MATERIALS SCIENCE↗

Twining and dynamic recrystallization in austenitic Alloy 718 during friction welding

Highlights: • DDRX was the primary grain refinement mechanism in friction welding of Alloy 718. • Two models were developed to explain the twin formation mechanism. • Intragranular twins were caused by grain boundary growth incidents. • Intergranular twin boundaries were ascribed to boundary growth stagnation. - Abstract: Quantitative boundary misorientation analysis verified that discontinuous dynamic recrystallization (DDRX) was the primary grain refinement mechanism in friction welding of Alloy 718. Two models were developed to explain the formation mechanism of intragranular twins and intergranular twins, respectively. Intragranular twins were caused by grain boundary growth incidents. After twin initiation, the twin boundary migrated toward the plastic-deformed grain interior to reduce the stored energy. Additionally, intergranular twin boundaries were ascribed to boundary growth stagnation. When boundary growth stagnation occurred, twin boundaries could form and altered the orientation of the boundary migration front, so that boundary migration could progress, leaving a single twin boundary behind.

36 MATERIALS SCIENCE↗

Influence of velocity of pressing in RCS processed AA8090 Al-Li alloy

Highlights: • For the first time the Influence of RCS on the properties of AA 8090 has been studied by processing velocity. • It is found that the properties vary according to pressing velocity and number of passes. • Reported significant property improvement achieved through the pressing velocity of 1.5mm/s. - Abstract: The effect of the velocity of pressing on grain refinement in AA8090 Al-Li alloy sheets during repetitive corrugation and straightening (RCS) at 300 °C is studied. V-groove corrugation dies and flattening dies were used at three different pressing velocities of 1.5 mm/s, 2 mm/s and 2.5 mm/s. The specimen temperature was maintained at 300 °C. Grain refinement was significantly influenced by the pressing velocity. The samples processed for 8 passes at a pressing velocity of 1.5 mm/s had an improved microhardness value of 104 HV and an increased tensile strength of 405 MPa which is respectively 39% and 113% more than the corresponding values in the parent material. TEM analysis showed that samples processed at a pressing velocity of 1.5 mm/s had in places a grain size down to 50 nm and the EBSD results revealed that the average grain size was 2 μm, with 86% of the total number of grain boundaries of the high angle type.

36 MATERIALS SCIENCE↗

Effects of Sr, Ce and P on the microstructure and mechanical properties of rapidly solidified Al7Si alloys

Highlights: • Rapid solidification caused formation of nanoscaled Si particle chains. • Sr or Ce induced the columnar transition zone only at extremely high cooling rate. • Enhancement of hardness is attributed to fine dispersion of eutectic Si, grain refinement and the supersaturation of Si. • Sr or Ce caused further enhancement of hardness, attributing to Si modification. - Abstract: A series of Al7Si based alloys with trace addition of Sr, Ce or P were prepared using melt-spinning at two different high cooling rates, and the microstructure as well as the hardness of the ribbons was comprehensively studied. The results show that Sr or Ce induces the formation of columnar transition zone and modifies the morphology of eutectic Si phase from dispersed particle chains to fine fibers only at extremely high cooling rate. However, P has little effect on the microstructure of either α-Al or eutectic Si. Compared with conventional casting, the Al7Si ribbons exhibit extremely high hardness due to the fine dispersion of eutectic Si, the grain refinement and the supersaturation of Si. The hardness is further enhanced by Sr or Ce addition at extremely high cooling rate, especially for columnar and equiaxed zones, attributing to the modification effect on Si phase.

36 MATERIALS SCIENCE↗

Characteristics of kinetic sprayed Ta in terms of the deposition behavior, microstructural evolution and mechanical properties: Effect of strain-rate-dependent response of Ta at high temperature

Highlights: • The effect of high-temperature rate-dependent response of BCC Ta on the deposition state of kinetic sprayed Ta particles with synergistic effect of powder oxidation • Abnormal increase of dislocation density above certain powder preheating temperature under the lower condition (N{sub 2} carrier gas), whereas considerable occurrence of grain refinement under the higher condition (He carrier gas). • Most significant dislocation density with the smallest volume-averaged domain size under the condition of 600 {sup o}C powder pre-heating with N{sub 2} carrier gas due to characteristic response of Ta. - Abstract: Numerous efforts have been focused on the fundamental research regarding kinetic spraying processes, but previous studies were biased to only few kinds of metallic materials. In particular, for Ta with body-centered cubic crystal structure, systematic studies are currently lacking in the literature. In this study, the characteristic deposition behaviors, microstructures, and mechanical properties of kinetic sprayed Ta under various impact conditions were systematically investigated. Generally, unusual features were usually related to strain-rate-dependent response (i.e. Peierls-Nabarro short range barriers) of Ta at high-temperature. This made thermal softening effect to be saturated above a certain degree of temperature, contributing to inferior deposition efficiency for the pre-heating at 600 °C than those of 400 and 500 °C by creating synergy with powder oxidation. In terms of microstructural evolutions, the dislocation density was abnormally increased at a certain powder preheating temperature (i.e., 600 °C), owing to the strain-rate-dependent response of Ta at high-temperature. On the other hand, grain refinement generated by rotational dynamic recrystallization was mainly observed under the higher kinetic energy condition (He carrier gas) at RT. Especially, the dislocation density and volume-average domain size evaluated via high-resolution X-ray diffraction peak profile analysis were corresponding to the results of the microstructural observations. Additionally, the nanomechanical properties (i.e., nanohardness and elastic modulus) evaluated via nanoindentation tests were in good agreement with the results from transmission electron microscopy investigations.

36 MATERIALS SCIENCE↗

Microstructure of titanium on complex deformation paths: Comparison of ECAP, KOBO and HE techniques

Highlights: • Method for producing CP titanium rods for medical implants is searched. • Three processing methods producing ultra-fine grain titanium are compared. • Microstructure and textures are examined and analysed. • Mechanical characteristics are determined based on microhardness and tensile tests. • Hydrostatic extrusion (HE) leads to the best properties of titanium rods for medical implants. - Abstract: In this work samples of commercial purity grade 2 titanium were severely deformed by three different extrusion techniques: equal-channel angular pressing (ECAP), extrusion through oscillating die (KOBO), and hydrostatic extrusion (HE). Resulting microstructures and mechanical properties of processed titanium samples are studied and compared with regard to potential application as a material for dental implants. The obtained results demonstrate the effect of different strain paths, involved by three applied deformation methods, on microstructure refinement, mechanical properties and textures of the studied material. Heterogeneous microstructures with bimodal grain size distributions are observed for all deformation techniques in the examined material, however differences in their internal structures and grain boundary distributions point to different grain refinement mechanisms. The fraction of ultra-fine grains is the highest in titanium deformed by HE. Also the internal grain fragmentation is the most important after HE deformation. This leads to the best mechanical and microstructural properties obtained in this type of deformation. Consequently, the HE process seems to be very interesting for production of material for medical implants.

36 MATERIALS SCIENCE↗