Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SiC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,495 records · Page 83

Mechanism of strength degradation for hot corrosion of alpha-SiC

Sintered alpha SiC was corroded by thin films of Na2SO4 and Na2CO3 molten salts at 1000%. This hot corrosion attack reduced room temperature strengths by as much as 50%. Strength degradation was porportional to the degree and uniformity of corrosion pitting attack as controlled by the chemistry of the molten salt. Extensive fractography identified corrosion pits as the most prevalent source of failure. A fracture mechanics treatment of the strength/pit depth relationship produced an average K sub IC equal to 2.6 MPa sub m 1/2, which is consistent with published values.

Smialek, J. L.↗

Feasibility study of the welding of SiC

In a brief study of the feasibility of welding sintered alpha-SiC, solid-state welding and brazing were investigated. Joint quality was determined solely by microstructural examination. Hot-pressure welding was shown to be feasible at 1950 C. Diffusion welding and brazing were also successful under hot isostatic pressure at 1950 C when boride, carbide, and silicide interlayers were used. Furnace brazing was accomplished at 1750 C when a TiSi2 interlayer was introduced.

Moore, T. J.↗

AES and LEED study of the zinc blende SiC(100) surface

Auger and LEED measurements have been carried out on the (100) surface of zinc blende SiC. Two different phases of the clean surface, in addition to two kinds of oxygen-covered surfaces, have been obtained, identified, and discussed. In the oxygen-covered surface, the oxygen is bonded to the Si. The carbon-rich phase is reconstructed (2 x 1), similar to the (100) clean surfaces of Si, Ge, and diamond. The Si-topped surface is reconstructed. A model of alternating Si dimers is suggested for this surface.

Dayan, M.↗

Evaluation of alpha-SiC sintering using statistical methods

The effect of time and temperature on the density and strength of alpha-SiC was studied and mathematically modeled using a central composite experimental design. A sintering temperature of 2150 C for 1.7 h maximized the flexural strength and densification values. However, temperatures above 2200 C promoted abnormal grain growth, with resulting appreciable decreases in strength. Flexural strength increased exponentially with increasing density for specimens with densities less than or equal to 92 percent of theoretical.

Hurst, J. B.↗

Kinetics and mechanism of corrosion of SiC by molten salts

Corrosion of sintered alpha-SiC under thin films of Na2CO3/CO2, Na2SO4/O2, and Na2SO4/SO3 was investigated at 1000 C. Chemical analysis was used to follow silicate and silica evolution as a function of time. This information coupled with morphology observations leads to a detailed corrosion mechanism. In all cases the corrosion reactions occur primarily in the first few hours. In the Na2CO3/CO2 case, rapid oxidation and dissolution lead to a thick layer of silicate melt in about 0.25 h. After this, silica forms a protective layer on the carbide. In the Na2SO4/O2 case, a similar mechanism occurs. In the Na2SO4/SO3 case, a porous nonprotective layer of SiO2 grows directly on the carbide, and a silicate melt forms above this. In addition, SiO2 and regenerated Na2SO4 form at the melt/gas interface due to reaction of silicate with SO3 and SO2 + O2. The reaction slows when the lower silica layer becomes nonporous.

Jacobson, N. S.↗

Burner rig corrosion of SiC at 1000 C

Sintered alpha-SiC was examined in both oxidation and hot corrosion with a burner rig at 400 kPa (4 atm) and 1000 C with a flow velocity of 94 m/s. Oxidation tests for times to 46 h produced virtually no attack, whereas tests with 4 ppm Na produced extensive corrosion in 13.5 h. Thick glassy layers composed primarily of sodium silicate formed in the salt corrosion tests. This corrosion attack caused severe pitting on the silicon carbide substrate and led to a 32 percent decrease in strength, compared to the as-received material. Parallel furnace tests of Na2SO4/air-induced attack yielded basically similar results, with slight product composition differences. The differences are explained in terms of the continuous sulfate deposition which occurs in a burner rig.

Jacobson, N. S.↗

Surface modification strategies for (100)3C-SiC

Several surface modificaation techniques were performed in situ in an ultrahigh vacuum as part of a program to develop electrical contacts on the (100) face of cubic SiC. The Auger electron spectroscopy line shapes and peak-to-peak heights of the Si LVV and CKLL transitions indicated changes in surface stoichiometry, bonding, and short range order. Changes in the low-energy electron diffraction pattern identified changes in the symmetry of long range ordering on the surface. Heating above 1050 C depleted the surface of Si with an activation energy of 120 kcal/mol, resulting eventually in a disordered graphitic layer which was several atomic layers thick. Bombardment by Ar ions of energies greater than 1000 eV enhanced the Si to C ratio on the surface and destroyed the LEED pattern. Long range order was recovered by simultaneous heating and ion bombardment. Finally, adsorption of Cr on the Ar ion damaged surface and subsequent desorption left a reconstructed, p(2 x 1)Si enriched surface. Similar treatments with Al did not produce a surface reconstruction.

Bellina, J. J., Jr.↗

The beta-SiC(100) surface studied by low energy electron diffraction, Auger electron spectroscopy, and electron energy loss spectra

The beta-SiC(100) surface has been studied by low energy electron diffraction, Auger electron spectroscopy, high resolution electron energy loss spectra (HREELS), and core level excitation EELS. Two new Si-terminated phases have been discovered, one with (3 x 2) symmetry, and the other with (2 x 1) symmetry. Models are presented to describe these phases. New results, for the C-rich surface, are presented and discussed. In addition, core level excitation EELS results are given and compared with theory.

Dayan, M.↗

Corrosion of SiC by Molten Salt

Advanced ceramic materials considered for wide range of applications as in gas turbine engines and heat exchangers. In such applications, materials may be in corrosive environments that include molten salts. Very corrosive to alloys. In order to determine extent of problem for ceramic materials, corrosion of SiC by molten salts studied in both jet fuel burners and laboratory furnaces. Surface of silicon carbide corroded by exposure to flame seeded with 4 parts per million of sodium. Strength of silicon carbide decreased by corrosion in flame and tube-furnace tests.

Jacobson, Nathan S.↗

Hot corrosion attack and strength degradation of SiC and Si(sub)3N(sub)4

Thin films of Na2SO4 and Na2CO3 molten salt deposits were used to corrode sintered SiC and Si3N4 at 1000 C. The resulting attack produced pitting and grain boundary etching resulting in strength decreases ranging from 15 to 50 percent. Corrosion pits were the predominant sources of fracture. The degree of strength decrease was found to be roughly correlated with the depth of the pit, as predicted from fracture toughness considerations. Gas evolution and bubble formation were key aspects of pit formation. Many of the observations of furnace exposures held true in a more realistic burner rig test.

Smialek, James L.↗

Friction and wear of sintered Alpha SiC sliding against IN-718 alloy at 25 to 800 C in atmospheric air at ambient pressure

The sliding friction and wear of the SiC-nickel based alloy IN-718 couple under line contact test conditions in atmospheric air at a linear velocity of 0.18 m/sec and a load of 6.8 kg (67N) was investigated at temperatures of 25 to 800 C. It was found that the coefficient of friction was 0.6 up to 350 C then decreased to 0.3 at 500 and 800 C. It is suggested that the sharp decrease in the friction in the range of 350 to 550 C is due to the lubrication value of oxidation products. The wear rate reaches a minimum of 1 x 10 to the -10 to 2 x 10 to the -10 cu cm/cm/kg at 400 to 600 C.

Deadmore, Daniel L.↗

Mechanism of strength degradation for hot corrosion of alpha-SiC

Sintered alpha SiC was corroded by thin films of Na2SO4 and Na2CO3 molten salts at 1000 percent. This hot corrosion attack reduced room temperature strengths by as much as 50 percent. Strength degradation was proportional to the degree and uniformity of corrosion pitting attack as controlled by the chemistry of the molten salt. Extensive fractography identified corrosion pits as the most prevalent source of failure. A fracture mechanics treatment of the strength/pit depth relationship produced an average K sub IC equal to 2.6 MPa sub m 1/2, which is cnsistent ith published values.

Smialek, James L.↗

Thermal expansion of the cubic (3C) polytype of SiC

Thermal expansion of the cubic beta or (3C) polytype of SiC was measured from 20 to 1000 C by the X-ray-diffraction technique. Over that temperature range, the coefficient of thermal expansion can be expressed by a second-order polynomial. It increases continuously from about 3.2 x 10 to the -6th/C at room temperature to 5.1 x 10 to the -6th/C at 1000 C, with an average value of 4.45 x 10 to the -6th/C between room temperature and 1000 C. This trend is compared with other published results and is discussed in terms of structural contributions to the thermal expansion.

Li, Z.↗

Antiphase boundaries in epitaxially grown beta-SiC

When the surface of beta-SiC, grown epitaxially on (001) silicon by chemical vapor deposition, is chemically etched, boundaries appear which may be observed by optical or scanning electron microscopy. Examination by plan-view and cross-sectional transmission electron microscopy shows boundaries in the film which exhibit line or fringe contrast. Convergent beam electron diffraction has been used to show that these boundaries separate domains that are in an antiphase relationship to each other. A model is presented which discusses the formation of these domains from independent nucleation on a stepped substrate surface.

Pirouz, P.↗

Pressure effects on the thermal stability of SiC fibers

Commercially available polymer derived SiC fibers were treated at temperatures from 1000 to 2200 C in vacuum and argon gas pressure of 1 and 1360 atm. Effects of gas pressure on the thermal stability of the fibers were determined through property comparison between the pressure treated fibers and vacuum treated fibers. Investigation of the thermal stability included studies of the fiber microstructure, weight loss, grain growth, and tensile strength. The 1360 atm argon gas treatment was found to shift the onset of fiber weight loss from 1200 to above 1500 C. Grain growth and tensile strength degradation were correlated with weight loss and were thus also inhibited by high pressure treatments. Additional heat treatment in 1 atm argon of the fibers initially treated at 1360 atm argon caused further weight loss and tensile strength degradation, thus indicating that high pressure inert gas conditions would be effective only in delaying fiber strength degradation. However, if the high gas pressure could be maintained throughout composite fabrication, then the composites could be processed at higher temperatures.

Jaskowiak, Martha H.↗

SiC fiber analysis

Polymer derived Nicalon SiC fibers are known to be thermally unstable at temperatures beyond 1200 C. In an effort to further understand the mechanisms of fiber degradation, Nicalon fibers were heat treated at temperatures up to 2200 C and argon gas pressures varying from 0 to 1360 atm. The effects of gas pressure on the thermal stability of the fibers were determined through property comparisons between the pressure-treated fibers and vacuum-treated fibers. Investigation of the thermal stability included studies of the fiber microstructure and mechanical and physical properties before and after treatments.

Jaskowiak, Martha H.↗

An initio calculations on C2, Si2, and SiC

Full-configuration-interaction (FCI) calculations have been performed for the Z 1Sigma(g)(+), a 3Pi(u), and b 3Sigma(g)(-) states of C2 and the X 3Sigma(g)(-) and A 3Pi(u) states of Si2 in valence double-zeta plus polarization one-particle basis sets. By carrying out the CASSCF multireference singles plus doubles CI (MRCI) procedure in a very large Gaussian basis set and correcting for errors with the FCI, the triplet-triplet separation in C2 is reproduced to within 47/cm. Analogous calculations on Si2 definitively determine the ground state to be 3Sigma(g)(-); the 3Pi(u) state is only 440 + or - 100/cm higher in energy. For the SiC molecule, which has never been observed spectroscopically but is believed to be an important component in carbon stars and to be present in interstellar space, the A 3Sigma(-) state is nearly 4000/cm above the X 3Pi ground state.

Bauschlicher, Charles W., Jr.↗

Behavior of ion-implanted junction diodes in 3C SiC

p-n junction diodes have been formed by ion implantation of B or Al in 3C SiC and annealing at 1365 C. The current-voltage characteristics of the Al-implanted structures show little rectification. The B-implanted diodes show rectification, with ideality factors of 2.2 and higher, breakdown voltages between 5 and 10 V, and a series resistance of the order of 20 kohm. The current-voltage characteristics were measured between room temperature and 270 C. The extracted ideality factors increase with temperature.

Avila, R. E.↗