Plastic deformation behaviors of Ni- and Zr-based bulk metallic glasses subjected to nanoindentation

Plastic deformation behaviors of Ni{sub 42}Ti{sub 20}Zr{sub 21.5}Al{sub 8}Cu{sub 5}Si{sub 3.5} and Zr{sub 51}Ti{sub 5}Ni{sub 10}Cu{sub 25}Al{sub 9} bulk metallic glasses at room temperature were studied by nanoindentation testing and atomic force microscopy under equivalent indentation experimental conditions. The different chemical composition of these two bulk metallic glasses produced variant tendencies for displacement serrated flow to occur during the loading process. The nanoindentation strain rate was calculated as a function of indentation displacement in order to verify the occurrence of displacement serrated flow at different loading rates. Atomic force microscopy revealed decreasing numbers of discrete shear bands around the indentation sites as loading rates increased from 0.025 to 2.5 mNs{sup −1}. Variations in plastic deformation behaviors between Ni and Zr-based glasses materials can be explained by the different metastable microstructures and thermal stabilities of the two materials. The mechanism governing plastic deformation of these metallic glasses was analyzed in terms of an established model of the shear transformation zone. - Highlights: • Plastic deformation of Ni- and Zr-based BMG is studied under identical conditions • Zr-based BMG undergoes a greater extent of plastic deformation than Ni-based BMG • Nanoindentation strain rate is studied to clarify variation in plastic deformation • Metastable microstructure, thermal stability affect BMG plastic deformation.

36 MATERIALS SCIENCE↗

Dynamic recrystallization behavior of an as-cast TiAl alloy during hot compression

High temperature compressive deformation behaviors of as-cast Ti–43Al–4Nb–1.4W–0.6B alloy were investigated at temperatures ranging from 1050 °C to 1200 °C, and strain rates from 0.001 s{sup −1} to 1 s{sup −1}. Electron back scattered diffraction technique, scanning electron microscopy and transmission electron microscopy were employed to investigate the microstructural evolutions and nucleation mechanisms of the dynamic recrystallization. The results indicated that the true stress–true strain curves show a dynamic flow softening behavior. The dependence of the peak stress on the deformation temperature and the strain rate can well be expressed by a hyperbolic-sine type equation. The activation energy decreases with increasing the strain. The size of the dynamically recrystallized β grains decreases with increasing the value of the Zener–Hollomon parameter (Z). When the flow stress reaches a steady state, the size of β grains almost remains constant with increasing the deformation strain. The continuous dynamic recrystallization plays a dominant role in the deformation. In order to characterize the evolution of dynamic recrystallization volume fraction, the dynamic recrystallization kinetics was studied by Avrami-type equation. Besides, the role of β phase and the softening mechanism during the hot deformation was also discussed in details. - Highlights: • The size of DRXed β grains decreases with increasing the value of the Z. • The CDRX plays a dominant role in the deformation. • The broken TiB{sub 2} particles can promote the nucleation of DRX.

36 MATERIALS SCIENCE↗

High-temperature low cycle fatigue behavior of a gray cast iron

The strain controlled low cycle fatigue properties of the studied gray cast iron for engine cylinder blocks were investigated. At the same total strain amplitude, the low cycle fatigue life of the studied material at 523 K was higher than that at 423 K. The fatigue behavior of the studied material was characterized as cyclic softening at any given total strain amplitude (0.12%–0.24%), which was attributed to fatigue crack initiation and propagation. Moreover, this material exhibited asymmetric hysteresis loops due to the presence of the graphite lamellas. Transmission electron microscopy analysis suggested that cyclic softening was also caused by the interactions of dislocations at 423 K, such as cell structure in ferrite, whereas cyclic softening was related to subgrain boundaries and dislocation climbing at 523 K. Micro-analysis of specimen fracture appearance was conducted in order to obtain the fracture characteristics and crack paths for different strain amplitudes. It showed that the higher the temperature, the rougher the crack face of the examined gray cast iron at the same total strain amplitude. Additionally, the microcracks were readily blunted during growth inside the pearlite matrix at 423 K, whereas the microcracks could easily pass through pearlite matrix along with deflection at 523 K. The results of fatigue experiments consistently showed that fatigue damage for the studied material at 423 K was lower than that at 523 K under any given total strain amplitude. - Highlights: • The low cycle fatigue behavior of the HT250 for engine cylinder blocks was investigated. • TEM investigations were conducted to explain the cyclic deformation response. • The low cycle fatigue cracks of HT250 GCI were studied by SEM. • The fatigue life of the examined material at 523 K is higher than that at 423 K.

36 MATERIALS SCIENCE↗

Microstructural evolution and the variation of tensile behavior after aging heat treatment of precipitation hardened martensitic steel

The effects of aging temperature on the microstructural evolution and the tensile behavior of precipitation hardened martensitic steel were investigated. Microscopic analysis using transmission electron microscope (TEM) was combined with the microstructural analysis using the synchrotron X-ray diffraction (XRD) to characterize the microstructural evolution with aging temperature. Peak hardness was obtained by precipitation of the Ni{sub 3}Al ordered phase. After aging at temperature range from 420 to 590 °C, spherical Ni{sub 3}Al precipitates and ellipsoidal M{sub 23}C{sub 6} carbides were observed within laths and at lath boundaries, respectively. Strain hardening behavior was analyzed with Ludwik equation. It is observed that the plastic strain regimes can be divided into two different stages by a rapid increase in strain hardening followed by a comparatively lower increase. At the first strain hardening stage, the aged specimen exhibited higher strain hardening exponent than the as-quenched specimen, and the exponent in the aged specimen was not changed considerably with increasing aging temperature. It is revealed that the strain hardening exponents at the first and the second stages were associated with the Ni{sub 3}Al precipitates and the domain size representing the coherent scattering area, respectively. - Highlights: • All of aged specimen exhibited higher strain hardening exponent than the as-quenched specimen at the first stage. • The value of strain hardening exponent in the aged specimen was nearly constant with aging temperature. • Ni{sub 3}Al precipitation dominantly influenced to the increase of strain hardening exponent at the first strain hardening stage. • Domain size was associated with strain hardening exponent at the second strain hardening stage.

36 MATERIALS SCIENCE↗

Comparative study of structure formation and mechanical behavior of age-hardened Ti–Nb–Zr and Ti–Nb–Ta shape memory alloys

This work sets out to study the peculiar effects of aging treatment on the structure and mechanical behavior of cold-rolled and annealed biomedical Ti–21.8Nb–6.0Zr (TNZ) and Ti–19.7Nb–5.8Ta (TNT) (at.%) shape memory alloys by means of transmission electron microscopy, X-ray diffractometry, functional fatigue and thermomechanical testing techniques. Dissimilar effects of aging treatment on the mechanical behavior of Zr- and Ta-doped alloys are explained by the differences in the ω-phase formation rate, precipitate size, fraction and distribution, and by their effect on the alloys' critical stresses and transformation temperatures. Even short-time aging of the TNZ alloy leads to its drastic embrittlement caused by “overaging”. On the contrary, during aging of the TNT alloy, formation of finely dispersed ω-phase precipitates is gradual and controllable, which makes it possible to finely adjust the TNT alloy functional properties using precipitation hardening mechanisms. To create in this alloy nanosubgrained dislocation substructure containing highly-dispersed coherent nanosized ω-phase precipitates, the following optimum thermomechanical treatment is recommended: cold rolling (true strain 0.37), followed by post-deformation annealing (600 °C, 15–30 min) and age-hardening (300 °C, 30 min) thermal treatments. It is shown that in TNT alloy, pre-transition diffraction effects (diffuse reflections) can “mask” the β-phase substructure and morphology of secondary phases. - Highlights: • TNZ alloy is characterized by much higher ω-phase precipitation rate than TNT alloy. • Difference in precipitation rates is linked to the difference in Zr and Ta diffusion mobility. • Aging of nanosubgrained TNZ alloy worsens its properties irrespective of the aging time. • Aging time of nanosubgrained TNT alloy can be optimized to improve its properties.

36 MATERIALS SCIENCE↗

Influence of grain orientation on the incipient oxidation behavior of Haynes 230 at 900 °C

Ni-based superalloy Haynes 230 is used in many applications such as very high temperature reactor (VHTR) or solid oxide fuel cells (SOFCs) where it is exposed to high temperature service environment. In order to improve the resistance for high temperature oxidation, the effect of crystallographic orientation on the early stage oxidation was investigated. It was demonstrated that different oxide thicknesses are formed on grains having different orientations. Comparison of electron backscatter diffraction (EBSD) orientation maps before and after oxidation at 900 °C indicates that grains near (111) orientation, especially with the deviation angle from <111> that is smaller than 20°, are more oxidation resistant than grains of other orientations. Correlation between the results of electron backscatter diffraction (EBSD) and atomic force microscopy (AFM) was used to compare the oxidation rate of grains having different crystallographic orientation. The oxidation rate was found to change with the crystallographic orientation as follows (111) < (110) < (100), also it was demonstrated that the oxidation rate changes are a nearly linear function of the angle of deviation from <111> direction. The morphology of surface oxide also depends on the orientation of grains. - Highlights: • Comparison of EBSD maps before and after oxidation allows to investigate the effect of orientation on oxidation in a more direct way; • Effect of crystallographic orientation on oxidation behavior of alloy 230 is studied by combination of EBSD and AFM; • Different thickness of oxide is formed on grain with different orientation and dependence of anisotropic oxidation behavior is discussed; • The morphology of grains is also orientation dependence.

36 MATERIALS SCIENCE↗

Microstructural characterization, formation mechanism and fracture behavior of the needle δ phase in Fe–Ni–Cr type superalloys with high Nb content

Microstructural characterization, formation mechanism and fracture behavior of the needle δ phase in Fe–Ni–Cr type superalloys with high Nb content (GH4169, equivalent to Inconel 718) have been quantitatively investigated in this research. The typical microstructures of δ phases with the stick, mixed and needle shapes obviously present in Inconel 718 after the isothermal upsetting at the temperature of 980–1060 °C with the initial strain rate of 10{sup −3}–10{sup −1} s{sup −1}. It is found that the shape of the δ phase has a great effect on the mechanical properties of the alloy, viz., the stick δ phase behaves good plasticity and the needle δ phase has good strength. In addition, the needle δ phase can be used to control the grain size as it can prevent grain growth. The combined effect of the localized necking and microvoid coalescence leads to the final ductile fracture of the GH4169 components with the needle δ phase. Both dislocation motion and atom diffusion are the root-cause for the needle δ phase to be firstly separated at grain boundary and then at sub-boundary. The formation mechanism of the needle δ phase is the new finding in this research. Furthermore, it is the primary mechanism for controlling the needle δ phase in Fe–Ni–Cr type superalloys with high Nb content. - Highlights: • Shape of the δ phase takes great effect on mechanical property. • Needle δ phase plays a great role to prevent grain growth. • Needle δ phase can enhance the fracture strength. • Microstructure mechanism of the needle δ phase has been investigated. • Fracture behavior of the needle δ phase has been studied.

36 MATERIALS SCIENCE↗

Mechanical behavior and microstructure of Ti{sub 20}Hf{sub 20}Zr{sub 20}Ta{sub 20}Nb{sub 20} high-entropy alloy loaded under quasi-static and dynamic compression conditions

The microstructure and the mechanical behavior of equimolar Ti{sub 20}Hf{sub 20}Zr{sub 20}Ta{sub 20}Nb{sub 20} high-entropy alloy in a wide range of initial strain rates between ~ 10{sup −3} s{sup −1} and ~ 3.4 × 10{sup 3} s{sup −1} were studied. A significant increment in the yield strength with increasing strain rate was observed. The yield strength at ~ 3.4 × 10{sup 3} s{sup −1} was about 40% higher than that measured at ~ 10{sup −3} s{sup −1}. Analysis by electron backscatter diffraction shows that in the low strain rate regime (up to ~ 10 s{sup −1}) the deformation occurs mainly in evenly distributed bands, while in the dynamic regime the deformation is strongly localized in macroscopic shear bands accompanied by softening even after the onset of yielding. The Kernel Average Misorientation technique reveals a high level of lattice rotation within these bands that also carries intense shear. In addition, X-ray diffraction line profile analysis indicates that the sharp increase in the flow stress is mostly related to an increase of the dislocation density. - Highlights: • Strain rate effect on the plastic behavior of Ti{sub 20}Hf{sub 20}Zr{sub 20}Ta{sub 20}Nb{sub 20} HEA was studied. • Low strain rate regime was characterized by a continuous hardening. • At high strain rates softening occurred shortly after the onset of yielding. • Intense strain localization in shear bands occurred in the high strain rate regime. • High dislocation density explained the upturn of flow stress at high strain rates.

36 MATERIALS SCIENCE↗

Room temperature creep behavior of Ti–Nb–Ta–Zr–O alloy

The room temperature creep behavior and deformation mechanisms of a Ti–Nb–Ta–Zr–O alloy, which is also called “gum metal”, were investigated with the nanoindentation creep and conventional creep tests. The microstructure was observed with electron backscattered diffraction analysis (EBSD) and transmission electron microscopy (TEM). The results show that the creep stress exponent of the alloy is sensitive to cold deformation history of the alloy. The alloy which was cold swaged by 85% shows high creep resistance and the stress exponent is approximately equal to 1. Microstructural observation shows that creep process of the alloy without cold deformation is controlled by dislocation mechanism. The stress-induced α' martensitic phase transformation also occurs. The EBSD results show that the grain orientation changes after the creep tests, and thus, the creep of the cold-worked alloy is dominated by the shear deformation of giant faults without direct assistance from dislocations. - Highlights: •Nanoindentation was used to investigate room temperature creep behavior of gum metal. •The creep stress exponent of gum metal is sensitive to the cold deformation history. •The creep stress exponent of cold worked gum metal is approximately equal to 1. •The creep of the cold-worked gum metal is governed by the shear deformation of giant faults.

36 MATERIALS SCIENCE↗

High temperature oxidation behavior of Ni-based superalloy GH202

The isothermal oxidation kinetic and oxidation behavior of Ni-based superalloy GH202 were investigated at temperatures from 800 °C to 1100 °C. The microstructure of GH202 was characterized by scanning electron microscope (SEM) and electron back-scattered diffraction (EBSD). The composition and morphologies of oxide scales of the surface and cross-section samples were examined by X-ray diffraction (XRD), electron probe microanalysis (EPMA), and SEM combined with energy-dispersive spectroscopy (EDS). The results show that the growth of the oxide scales on GH202 obeyed a parabolic law with an activation energy of 247.8 KJ·mol{sup −1} from 800 °C to 1100 °C. The continuous and dense oxide scales that formed at 800 °C and 900 °C were composed of Cr{sub 2}O{sub 3}, NiCr{sub 2}O{sub 4} and a small amount of TiO{sub 2}. Beneath the oxide scales, aluminum-rich oxides formed along the grain boundaries due to internal oxidation. After treatment at 1000 °C for 150 h, the oxide scale was separated into two layers, the outer layer with sparse holes that was mainly composed of Cr{sub 2}O{sub 3} and TiO{sub 2} and an inner layer of dense Cr{sub 2}O{sub 3}. At 1100 °C for 100 h the outer layer was spalled, due to the looser oxide scale with large blocks of TiO{sub 2} and NiCr{sub 2}O{sub 4} which provided channels for oxygen diffusion. - Highlights: •Isothermal oxidation kinetic of GH202 obeys a parabolic law from 800 °C to 1100 °C. •The activation energy of GH202 is closed to the diffusion activation of Cr{sup 3+}. •The evolution process of oxide scales from 800 °C to 1100 °C is displayed by EPMA. •The oxidation behavior of GH202 is mainly controlled by Cr{sup 3+} and Ti{sup 4+}.

36 MATERIALS SCIENCE↗

Improving precipitation hardening behavior of Mg−Zn based alloys with Ce−Ca microalloying additions

The precipitation hardening behavior of newly developed Mg−Zn−Ca−Ce alloys, with modified texture and improved ductility, is studied to delineate the microstructural characteristics that lead to effective hardening upon ageing treatments. Advanced electron microscopy and atom probe techniques are used to analyze the structural characteristics in relevance to the hardening potential. It has been found that the formation of a new basal precipitate phase, which evolves from a single atomic layer GP zone, and is finely distributed in both under-aged and peak-aged microstructures, has a significant impact in the improvement of the hardening response compared with the base Mg−Zn alloys. It has also been found that the β′{sub 1} rod precipitates, commonly formed during ageing treatments of Mg−Zn alloys, have their size and distribution significantly refined in the Ca−Ce containing alloys. The role of alloy chemistry in the formation of the fine basal plate GP zones and the refinement in β′{sub 1} precipitation and their relationships to the hardening behavior are discussed. It is proposed that Ca microalloying governs the formation of the GP zones and the enhancement of hardening, particularly in the under-aged conditions, but that this is aided by a beneficial effect from Ce. - Highlights: • Ce−Ca microalloying additions improve hardening in Mg−Zn, over Ce or Ca alone. • Improved hardening is due to refined β′{sub 1} rods, and fine basal plate precipitates. • Atom probe tomography identifies Ca in both β′{sub 1} and the fine basal plates. • The fine basal plates originate as ordered monolayer GP zones with 1:1 Zn:Ca (at.%). • With ageing GP zones become more Zn-rich and transform to the fine basal plates.

36 MATERIALS SCIENCE↗

Microstructure evolution and dynamic recrystallization behavior of a powder metallurgy Ti-22Al-25Nb alloy during hot compression

The flow behavior of a powder metallurgy (P/M) Ti-22Al-25Nb alloy during hot compression tests has been investigated at a strain rate of 0.01 s{sup −1} and a temperature range of 980–1100 °C up to various true strains from 0.1 to 0.9. The effects of deformation temperature and strain on microstructure characterization and nucleation mechanisms of dynamic recrystallization (DRX) were assessed by means of Optical microscope (OM), electron backscatter diffraction (EBSD) and transmission electron microscope (TEM) techniques, respectively. The results indicated that the process of DRX was promoted by increasing deformation temperature and strain. By regression analysis, a power exponent relationship between peak stresses and sizes of stable DRX grains was developed. In addition, it is suggested that the discontinuous dynamic recrystallization (DDRX) and continuous dynamic recrystallization (CDRX) controlled nucleation mechanisms for DRX grains operated simultaneously during the whole hot process, and which played the leading role varied with hot process parameters of temperature and strain. It was further demonstrated that the CDRX featured by progressive subgrain rotation was weakened by elevating deformation temperatures. - Highlights: •Flow behavior of a P/M Ti-22Al-25Nb is studied by hot compression tests. •Microstructure evolution of alloy is affected by deformation temperature and strain. •The relationship between peak stress and stable DRX grain size was developed. •The process of DRX was promoted by increasing deformation temperature and strain. •Nucleation mechanisms of DRX were identified by EBSD analysis and TEM observation.

36 MATERIALS SCIENCE↗

Aging behavior of an in-situ TiB{sub 2}/Al-Cu-Li-x matrix composite

Transmission electron microscopy, differential scanning calorimetry and hardness tests have been performed on an in-situ TiB{sub 2}/Al-3.3Cu-1.0Li-0.60Mg-0.40Ag-0.14Zr-0.13Si composite to study its aging behavior at 175 °C. A cubic phase suspected to be the σ (Al{sub 5}Cu{sub 6}Mg{sub 2}) phase or its variant is precipitated at all aging stages studied, and this phase is not typically observed in the Al-Cu-Li alloys. The primary hardening (aging for 3 h) phases consist of δ′ (Al{sub 3}Li), β′ (Al{sub 3}Zr) and the cubic phase. After aging for 18 h, all precipitates including T{sub 1} (Al{sub 2}CuLi), S (Al{sub 2}CuMg), θ′ (Al{sub 2}Cu), δ′, β′ and the cubic phase have appeared, and the formation of T{sub 1} and S results in a rapid increase in hardness. With prolonging of aging time, the apparent coarsening of T{sub 1} and S results in a decline in hardness. - Highlights: •The aging behavior of an in-situ TiB{sub 2}/Al-Cu-Li-x composite was studied. •A cubic phase suspected to be σ (Al{sub 5}Cu{sub 6}Mg{sub 2}) or its variant was precipitated. •The hardness change was dominated by the evolution of T{sub 1} (Al{sub 2}CuLi) and S (Al{sub 2}CuMg).

36 MATERIALS SCIENCE↗

Hot deformation behaviors and processing maps of B{sub 4}C/Al6061 neutron absorber composites

In this study, the hot deformation behaviors of 30 wt.% B{sub 4}C/Al6061 neutron absorber composites (NACs) have been investigated by conducting isothermal compression tests at temperatures ranging from 653 K to 803 K and strain rates from 0.01 to 10 s{sup −1}. It was found that, during hot compression, the B{sub 4}C/Al6061 NACs exhibited a steady flow characteristic which can be expressed by the Zener-Hollomon parameter as a hyperbolic-sine function of flow stress. High average activation energy (185.62 kJ/mol) of B{sub 4}C/Al6061 NACs is noted in current study owing to the high content of B{sub 4}C particle. The optimum hot working conditions for B{sub 4}C/Al6061 NACs are found to be 760–803 K/0.01–0.05 s{sup −1} based on processing map and microstructure evolution. Typical material instabilities are thought to be attributed to void formation, adiabatic shear bands (ASB), particle debonding, and matrix cracking. Finally, the effect of the plastic deformation zones (PDZs) on the microstructure evolution in this 30 wt.% B{sub 4}C/Al6061 composite is found to be very important. - Highlights: •The hot deformation behavior of the 30 wt.% B{sub 4}C/Al6061 NACs was first analyzed. •The 3D efficiency map and the instability map are developed. •The optimum hot working conditions were identified and validated by SEM and TEM. •The hot deformation schematic diagram of 30 wt.% B{sub 4}C/Al6061 NACs is developed.

36 MATERIALS SCIENCE↗

Effect of cooling rates on the structure, density and micro-indentation behavior of the Fe, Co-based bulk metallic glass

The experiments demonstrate that ductility of the samples of bulk metallic glass (BMG) with the same chemical composition increased with decreasing sample size. It is shown that microhardness and density increases with decreasing the cooling rate. The fracture morphology of rods after compressive fracture were different on the cross section. Two characteristic features of the compressive fracture morphologies of metallic glasses (MGs) were observed in samples: smooth region and the vein pattern. Many parallel shear bands were observed on the deformed specimen with ϕ = 2 mm in diameter. The results provide more understanding on the relationship among the cooling rate, structure and micro-indentation behavior of the Fe-Co-based BMGs. - Highlights: •Fracture morphology and micro-indentation behavior is studied. •The smaller BMG sample exhibits the larger plasticity. •Microhardness and density increase with decreasing the cooling rate. •Formation of shear bands has been reported in deformed specimens. •Structure and mechanical properties of BMGs can be controlled by the cooling rate.

36 MATERIALS SCIENCE↗

Through-thickness microstructural evolution during grain boundary engineering type thermomechanical processing and its implication on sensitization behavior in austenitic stainless steel

Highlights: • GBE-treated 304L steel exhibits thickness-dependent microstructural evolution. • Degree of sensitization increases from surface to interior in GBE specimen. • Low fractal dimension and large TRD size lead to lesser sensitization at surface. • As-received specimen shows high albeit thickness-independent sensitization behavior. • Higher residual strain leads to higher sensitization at surface of deformed sample. - Abstract: Through-thickness microstructural variations and their synergistic influence on degree of sensitization in grain boundary engineering (GBE) treated 304L stainless steel was compared with solution-annealed and marginally cold-worked (~ 3% thickness reduction) specimens. The solution-annealed specimen has shown higher degree of sensitization due to the presence of lower fraction of Σ3 (as well as other low Σ CSL) boundaries and dominant random high-angle boundaries (RHAGBs) connectivity. However, it has shown thickness-independent sensitization behavior as grain boundary character distribution, residual strain and grain boundary network topology towards thickness direction are similar. Owing to higher residual strain, as revealed by local misorientation analysis, the cold-worked specimen showed maximum degree of sensitization (higher than solution-annealed condition) at surface. The GBE specimen has shown much lower degree of sensitization at surface due to higher-fraction of Σ3 boundaries and discontinuous RHAGBs connectivity. However, increasing fraction of RHAGBs and their connectivity, as confirmed by twinning-related domain and fractal analysis, cause more sensitization at interior of this specimen. In spite of this, the degree of sensitization at the interior of GBE specimen is lower than the solution-annealed or cold-worked specimen. Even though the residual strain in GBE specimen is higher than the solution-annealed condition, the lower degree of sensitization indicates that the grain boundary character distribution and grain boundary network topology have higher implication than residual strain in controlling sensitization.

36 MATERIALS SCIENCE↗

Mechanical behavior and texture development of over-aged and solution treated Al-Cu-Mg alloy during multi-directional forging

The effects of initial heat treatments, i.e. solution treating and over ageing, on deformation behavior of an age hardenable Al-Cu-Mg alloy, including mechanical properties and texture evolution, during multi-directional forging (MDF) are investigated. Hardness measurements, electron back scatter diffraction (EBSD) maps, and differential scanning calorimetry (DSC) are carried out. Mechanical behaviors of the alloy in terms of compressive stress and hardness test after MDF are investigated. In both solution treated and over-aged alloys, the compressive stress during MDF shows an increase up to the second pass, and by further straining the flow stress is decreased. However, shear and deformation bands are formed in both solution treated and over-aged alloys, the density of these instabilities in the solution treated alloy is higher than that in over-aged alloy. In the solution treated alloy, not only large particles induce deformation bands, but also the dynamically formed GPB zones/Cu-Mg co-clusters. Texture analysis shows that the shear component of C {001}<110> (Φ{sub 1} = 90°, Φ = 0°, Φ{sub 2} = 45°) is developed with 18 mrd during MDF of the over-aged alloy. In the solution treated alloy, due to the high density of deformation bands and different microchemistry of the matrix in comparison with that of the over-aged alloy, the Copper type texture component {112}<111> (Φ{sub 1} = 90°, Φ = 35°, Φ{sub 2} = 45°) is developed with 11 mrd.

36 MATERIALS SCIENCE↗

The effects of Cr particles addition on the aging behavior and mechanical properties of SiCp/7075Al composites

Highlights: • The novel investigated the effects of Cr particles on the aging behavior and mechanical properties of SiC{sub p}/7075Al composites. • The addition of Cr particles didn't change precipitation sequence, but significantly degraded precipitation kinetics of composites. • Cr particles had a significant effect on the tensile properties of the peak-aged composite because of Mg aggregation. - Abstract: The effects of Cr particles addition on the aging behavior and mechanical properties of SiC{sub p}/7075Al composites were systematically investigated. The results show that the precipitation sequence of (5 vol% Cr + 50 vol% SiC)/7075Al composites (C-7075Al) is still: GP zone → η′ → η (MgZn{sub 2}), but Cr particles degrade the precipitation kinetics of the C-7075Al composite in comparison to (5 vol% SiC{sub p} + 50 vol% SiC{sub p})/7075Al (B-7075Al) because of reduced dislocation density present in the matrix and higher thermal activation energy of the η′ phase. Besides, the addition of Cr particles has a significant effect on the mechanical properties of the C-7075Al composite during the aging process. In contrast to the as-cast state, the ultimate tensile strength of the C-7075Al composite obtains an increase of 120 MPa at the peak-aged period, significantly lower than those of 7075Al alloy (207 MPa) and the B-7075Al composite (151 MPa), which is attributable to the severe aggregation of elemental Mg at the interface between Cr particles and the Al matrix.

36 MATERIALS SCIENCE↗