Oil-Well Cement and C[subscript 3]S Hydration Under High Pressure as Seen by In Situ X-Ray Diffraction, Temperatures 80[degrees]C with No Additives

The hydration kinetics of a white cement and batches of both Class G and H oil-well cements were examined between 0 and 60 MPa, at {le}80 C, using in situ synchrotron X-ray diffraction. This gives a continuous measure of the C{sub 3}S (Ca{sub 3}SiO{sub 5}), CH (Ca(OH){sub 2}), C{sub 4}AF (Ca{sub 2}FeAlO{sub 5}), ettringite, and other phases in the hydrating slurries. Slurries prepared from single-phase C{sub 3}S; synthetic C{sub 4}AF, and gypsum; and white cement, synthetic C{sub 4}AF and gypsum were also examined. An increasing pressure enhanced the rate of hydration for all slurries. Analysis of the data, using a kinetic model, provided rate constants that were used to obtain activation volumes for C{sub 3}S hydration. For all the cement and C{sub 3}S slurries studied, similar activation volumes were obtained (average {Delta}{double_dagger}{approx}-35 cm{sup 3}/mol), indicating that the presence of cement phases other than C{sub 3}S has a modest influence on the pressure dependence of C{sub 3}S hydration. An alternative analysis, using the time at which 90% of the initial C{sub 3}S remained, gave similar activation volumes. Pressure accelerated the formation of ettringite from synthetic C{sub 4}AF in the presence of gypsum. However, in slurries containing cement, the pressure dependence of C{sub 3}S hydration plays a major role in determining the pressure dependence of ettringite formation.

36 MATERIALS SCIENCE↗

Grain size variation in nanocrystalline silicon carbide irradiated at elevated temperatures

This study reports on ion irradiation-induced grain growth in nanocrystalline SiC films on Si substrates. The SiC grains with average size ranging from ~2 to 20 nm were embedded in amorphous SiC matrices. Irradiation was performed using 5 MeV Xe23+ ions to 115 ions/nm2 at 700 K. The irradiated films were characterized using x-ray diffraction, transmission electron microscopy and Raman spectroscopy. Significant grain growth is observed for smaller grains that tend to saturate at ~8 nm. In contrast, irradiation of larger grains (~20 nm in size) leads to a decrease in the grain size, which could be associated with the production of lattice disorder within the grains. Homonuclear C-C bonds in the irradiated amorphous SiC matrix are found to be graphitized. This bonding transformation could limit or inhibit grain growth and contribute to the size saturation. The results from this study may suggest nanocrystalline SiC as a promising candidate structural or cladding material for applications in advanced nuclear reactors.

Grain growth, ion irradiation, SiC↗

Low temperature oxidation of plutonium

The initial oxidation of gallium stabilized {delta}-plutonium metal at 193 K has been followed using x-ray photoelectron spectroscopy. On exposure to Langmuir quantities of oxygen, plutonium rapidly forms a trivalent oxide followed by a tetravalent plutonium oxide. The growth modes of both oxides have been determined. Warming the sample in vacuum, the tetravalent oxide reduces to the trivalent oxide. The kinetics of this reduction reaction have followed and the activation energy has been determined to be 38.8 kJ mol{sup -1}.

36 MATERIALS SCIENCE↗

Emergence of room-temperature ferroelectricity at reduced dimensions

Thinning films induces ferroelectricity Thin ferroelectric films are needed in computers and medical devices. However, traditional ferroelectric films typically become less and less polarized the thinner the films become. Instead of using a good ferroelectric and making it thinner, Lee et al. started with SrTiO 3 , which in its bulk form is not ferroelectric. This material does have naturally occurring nanosized polarized regions. and when the thickness of the SrTiO 3 films reaches the typical size of these regions, the whole film aligns and becomes ferroelectric. Science , this issue p. 1314