Aurivillius phases of PbBi{sub 4}Ti{sub 4}O{sub 15} doped with Mn{sup 3+} synthesized by molten salt technique: Structure, dielectric, and magnetic properties
Doping of manganese (Mn{sup 3+}/Mn{sup 4+}) into the Aurivillius phase Pb{sub 1-x}Bi{sub 4+x}Ti{sub 4-x}Mn{sub x}O{sub 15} was carried out using the molten salt technique for various Mn concentrations (x=0, 0.2, 0.4, 0.6, 0.8, and 1). Single phase samples could be obtained in the composition range with x up to 0.6 as confirmed by X-ray and neutron diffraction analysis. Dielectric measurements show a peak at 801, 803, 813 and 850 K for samples with x=0, 0.2, 0.4, and 0.6, respectively, related to the ferroelectric transition temperature (T{sub c}). The main contribution of the in-plane polarization for x{<=}0.2 which was calculated from the atomic positions obtained by the structure analysis is the dipole moment in the Ti(1)O{sub 6} layer; however, for x{>=}0.4 the polarization originates from the dipole moment in the Ti(2)O{sub 6} layer. Mn doping in the Pb{sub 1-x}Bi{sub 4+x}Ti{sub 4-x}Mn{sub x}O{sub 15} does not show any long range magnetic ordering. -- Graphical abstract: The dipole moment of TiO{sub 6} dependence of x in Pb{sub 1-x}Bi{sub 4+x}Ti{sub 4-x}Mn{sub x}O{sub 15} (0{<=}x{<=}0.6): (a) along a-axis and (b) on the ab plane. This figure indicated that polarization in the ab-plane contribute to the total polarization. Display Omitted Highlights: {yields} We have prepared Pb{sub 1-x}Bi{sub 4+x}Ti{sub 4-x}Mn{sub x}O{sub 15}, 0{<=}x{<=}1 by the molten-salt method. {yields} The oxides adopted A2{sub 1}am space group. {yields} Dipole moments of the inner Ti(1)O{sub 6} are the main polarization contributor for x{<=}0.2. {yields} Dipole moments of the outer Ti(2)O{sub 6} are the main polarization contributor for x>0.2. {yields} Ferromagnetic interactions show the contribution of mixed valence of Mn{sup 3+}/Mn{sup 4+}.