Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “welding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,459 records · Page 81

Precipitate evolution in friction stir welding of 2219-T6 aluminum alloys

Precipitate evolution in friction stir welding of 2219-T6 aluminum alloys was characterized by transmission electron microscopy. In the weld nugget zone and the thermo-mechanically affected zone some metastable precipitates overaged to equilibrium phase while others solutionized into the aluminum solid solution. In the heat-affected zone the precipitates coarsened.

36 MATERIALS SCIENCE↗

Microstructures in a resistance spot welded high strength dual phase steel

The microstructure of a high strength dual phase steel resistance spot welded with tempering-pulse technology is characterized in this paper. In the fusion zone, there is a needle-like microstructure identified as acicular or side plate ferrite that has a cube-on-cube orientation relationship with respect to the surrounding martensite. In contrast to the microstructures produced by the lower cooling rate arc or laser welding techniques, the nucleation of this fine intragranular ferrite takes place independent of inclusions. Further, a leaf-like microstructure within the martensitic matrix is found to contain primitive orthorhombic Cr{sub 3}C{sub 2} and face-centered cubic CrC chromium carbides, rather than Cr{sub 23}C{sub 6} or Cr{sub 7}C{sub 3} as is commonly observed in steel alloys. The formation histories of both the ferrite phase and the chromium carbides are analyzed.

36 MATERIALS SCIENCE↗

Microstructural evolution of fusion zone in laser beam welds of pure titanium

Microstructural evolution of fusion zone in laser beam welds of pure titanium was studied by means of electron backscattering diffraction. The microstructural evolution is strongly affected by the {beta} {yields} {alpha} transformation mechanism dependent on the cooling rate during phase transformation. The long-range diffusional transformation mainly occurs in the fusion zone at the low cooling rate, and the massive transformation dominantly takes place at the high cooling rate. For this reason, the grain morphologies probably change from the granular-like to columnar-like grains with the cooling rate increasing. - Highlights: Black-Right-Pointing-Pointer Microstructures of fusion zone in laser beam welds of pure titanium are studied. Black-Right-Pointing-Pointer Increasing cooling rate changes grain morphology from granular to columnar one. Black-Right-Pointing-Pointer Final microstructures depend on the {beta}{yields}{alpha} transformation mechanisms.

36 MATERIALS SCIENCE↗

Microstructure evolution in the fusion zone of laser-welded Mg–Gd–Y–Zr alloy during solution and aging treatment

The microstructure evolution in the fusion zone of laser-welded Mg-Gd-Y-Zr alloy during solution and aging treatment is investigated. The morphology of the Mg{sub 24}(Gd,Y){sub 5} in the divorced eutectic at the grain boundary transforms from a continuous network to disconnected and fragmentized islands and then to spheroidal particles before complete dissolution during the solution treatment at 430 °C. During the subsequent aging treatment at 225 °C, the precipitation sequence in the fusion zone follows the order of supersaturated solid solution (SSSS) → βʺ(D0{sub 19}) → βʹ(cbco) → β{sub 1}(fcc) → β(fcc). High-density precipitates are present at the original grain boundaries of the fusion zone from the welded structure but there are less precipitates in the interior of the original grains. The grain growth during the solution treatment at 430 °C comprises the slowly increasing stage, rapidly increasing stage, and stable stage. The network-distributed Mg{sub 24}(Gd,Y){sub 5} impedes migration of the grain boundaries, restricts grain growth in the first slowly increasing stage, and segregation of zirconium near the grain boundaries also affects migration of the grain boundaries. - Highlights: •Different quantities of precipitates are present at different location of grain. •The network-distributed Mg{sub 24}(Gd,Y){sub 5} restricts grain growth. •Segregation of Zr affects migration of grain boundaries.

36 MATERIALS SCIENCE↗

Microstructure, texture, and mechanical properties of friction stir welded commercial brass alloy

Microstructural evolution during friction stir welding of single-phase brass and corresponding mechanical properties were investigated. For this purpose, 2 mm thick brass plate was friction stir welded at a rotational speed of 450 rpm and traverse speed of 100 mm/min. The microstructure of the joint was studied using optical microscopy, scanning electron microscopy equipped with electron back scattered diffraction system, and scanning transmission electron microscopy. The mechanical properties were measured using hardness and tensile tests. The formation of subgrains and their transformation into new grains in conjunction with existence of A{sub 1}{sup ⁎}, A{sub 2}{sup ⁎} and C texture components revealed that the continuous dynamic recrystallization plays a dominant role in the microstructural evolution. However, grain boundary bulging, along with the formation of twin boundaries, and presence of the G texture component showed that the discontinues dynamic recrystallization may participate in the new grain formation. Furthermore, the different strengthening mechanisms, which caused the higher strength of the joint, were discussed. - Highlights: •Microstructural evolution during FSW of a single phase brass was investigated. •CDRX and DDRX were the main mechanisms of the grain structure formation during FSW. •GDRX and SRX were not contributed in grain structure formation. •The lamellas TBs were formed in the SZ of the joints. •Grain boundary, dislocation, and texture effects resulted in higher strength.

36 MATERIALS SCIENCE↗

In situ investigation of the tensile deformation of laser welded Ti{sub 2}AlNb joints

The tensile deformation behavior of laser welded Ti{sub 2}AlNb joints was investigated using in situ analysis methods. The fracture mode of the single-B2-phase fusion zone was quasi-cleavage at room temperature and intergranular at 650 °C, while that of base metal was microvoid coalescence at both room temperature and 650 °C. Tensile deformation at room temperature was observed using in situ SEM tensile testing. In base metal, microcracks nucleated and propagated mainly within the O phase or along O/B2 phase boundaries. While both the cross- and multi-slips were found in the single-B2-phase fusion zone, a confocal laser scanning microscopy was used to observe the crack initiation and propagation process in situ at 650 °C. Cracks mainly formed along the B2/O phase boundaries in base metal, along the fragile grain boundaries of B2 phase in the fusion zone. The thermal simulation experiment and following TEM analysis indicated that the precipitation of continuous O-phase films along the B2 grain boundaries resulted in the high temperature brittleness of laser welded Ti{sub 2}AlNb joints. - Highlights: •Cracks formed within O phase or along B2/O boundaries in the base metal. •Cross- and multi-slips relieved stress in the fusion zone at room temperature. •Cracks mainly formed along the B2/O boundaries at 650 °C. •In the fusion zone, intergranular cracks were in situ observed at 650 °C. •O-phase films along B2 grain boundaries caused the high temperature brittleness.

36 MATERIALS SCIENCE↗

Microstructure of a safe-end dissimilar metal weld joint (SA508-52-316L) prepared by narrow-gap GTAW

The microstructure, residual strain and interfacial chemical composition distribution of a safe-end dissimilar metal weld joint (DMWJ, SA508-52-316L) prepared by narrow-gap gas-tungsten arc welding (NG-GTAW) were studied by optical microscope (OM) and scanning electron microscope equipped with an energy dispersive X-ray microanalysis (SEM/EDX) and an electron back scattering diffraction (EBSD) system. Complex microstructure and chemical composition distribution are found, especially at the SA508-52 interface and the 52-316L interface. In brief, a complicated microstructure transition exists within the SA508 heat affected zone (HAZ); the residual strain, the fraction of high angle random grain boundaries and low angle boundaries decrease with increasing the distance from the fusion boundary in 316L HAZ; neither typical type II boundary nor obvious carbon-depleted zone is found near the SA508-52 interface; dramatic and complicated changes of the contents of the main elements, Fe, Cr and Ni, are observed at the distinct interfaces, especially at the SA508-52 interface. No carbon concentration is found at the SA508-52 interface. - Highlights: •Residual strain and GBCD change as a function of the distance from FB in 316L HAZ. •Neither type II boundary nor obvious carbon-depleted zone is found in SA508 HAZ. •No carbon concentration is found at the SA508-52 interface. •The middle part of the DMWJ has the highest residual strain.

36 MATERIALS SCIENCE↗

Synchrotron experiment and simulation studies of magnesium-steel interface manufactured by impact welding

The effective weight reduction in the automotive industry by the wide adoption of lightweight magnesium (Mg) alloys demands high-quality joint between magnesium alloys and massively-used steels in order to wring the excess weight with strength and safety assurance. However, Mg-steel joint is difficult to achieve because there is no mutual solubility between magnesium and steel and huge disparity in physical properties. An impact-based welding method recently showed successful Mg-steel joining. In this work, the characteristics of Mg-steel interface joined by the impact welding method were investigated. Synchrotron high-energy X-ray computed tomography and diffraction were applied to characterize the microstructure across Mg-steel interface. Results revealed a deposit layer formed at the joint interface where Fe-rich particles spread deep into the Mg matrix. High-resolution 3D morphology of Mg-steel interface demonstrated the trapped pores and cracks inside the deposit layer. Finally, the formation of the deposit layer and the void/cracking evolution were analyzed by using finite element models. These findings provide insights into the immiscible Mg-steel joining process.

36 MATERIALS SCIENCE↗

Eutectic structures in friction spot welding joint of aluminum alloy to copper

A dissimilar joint of AA5083 Al alloy and copper was produced by friction spot welding. The Al-MgCuAl{sub 2} eutectic in both coupled and divorced manners were found in the weld. At a relatively high temperature, mass transport of Cu due to plastic deformation, material flow, and atomic diffusion, combined with the alloy system of AA5083 are responsible for the ternary eutectic melting.

36 MATERIALS SCIENCE↗

Features of the microstructure development under conditions, reproducing the process of friction stir welding. Molecular-dynamics study

Friction stir welding is a recently developed technology which is used in various branches of modern engineering. The basis of this technology is the friction of the rotating cylindrical or specially shaped tool between two metal plates brought together either to meet their ends of one above another with the overlap. When applying the FSW process in various economical sectors, the important task is to study the mechanisms and identify the physical laws and factors leading to formation of structural inhomogeneities and discontinuities in the weld seam. This paper analyzes the basic mechanisms behind the structural state generation in the material subjected to severe plastic deformation and heating. To investigate the atomic mechanisms of structural changes in FSW, the modeling at atomic scale has been carried out. Results of work can be a basis for new knowledge about the microstructure evolution in FSW.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure based modeling of friction stir welded joint of dissimilar metals using crystal plasticity

We report the friction stir welding (FSW) process shows promising results in joining dissimilar metals which are otherwise almost impossible to join using traditional welding techniques. Being a new technique, the deformation and the failure mechanism of the joints made by the FSW process needs to be investigated. In this work, a joint between AZ31 Mg alloy and DP590 steel is modeled using phenomenological crystal plasticity formulation on the mesoscale in the form of a representative volume element (RVE). The interface of the two materials is modeled using a cohesive zone model. A parametric study has been performed to understand the effect of grain size and interface fracture toughness as well as strength on the mechanical performance of the joint. It was found that the grain size of AZ31 Mg alloy, as well as DP590 steel, has little effect on the overall joint performance. On the other hand, interface fracture toughness and strength have a significant impact on the mechanical properties of the joint

36 MATERIALS SCIENCE↗

Ultrasonic Evaluation of Two Dissimilar Metal Weld Overlay Specimens

Two dissimilar metal weld (DMW) pipe-to-nozzle specimens were implanted with thermal fatigue cracks in the 13% to 90% through-wall depth range. The specimens were ultrasonically evaluated with phased-array probes having center frequencies of 0.8, 1.0, 1.5, and 2.0 megahertz (MHz). An Alloy 82/182 weld overlay (WOL) was applied and the specimens were ultrasonically re-evaluated for flaw detection and characterization. The Post-WOL flaw depths were approximately 10% to 56% through-wall. This study has shown the effectiveness of ultrasonic examinations of Alloy 82/182 overlaid DMW specimens. Phased-array probes with center frequency in the 0.8- to 1.0-MHz range provide a strong coherent signal but the greater ultrasonic wavelength and larger beam spot size prevent the reliable detection of small flaws. These small flaws had nominal through-wall depths of less than 15% and length in the 50-60 mm (2-2.4 in.) range. Flaws in the 19% and greater through-wall depth range were readily detected with all four probes. At the higher frequencies, the reflected signals are less coherent but still provide adequate signal for flaw detection and characterization. A single inspection at 2.0 MHz could provide adequate detection and sizing information but a supplemental inspection at 1.0 or 1.5 MHz is recommended.

36 MATERIALS SCIENCE↗

Exploration Extravehicular Mobility Unit (xEMU): Electron Beam Welding of the Portable Life Support System (PLSS) Ti-6Al-4V Backplate with Integrated Cooling Channels

The Exploration Extravehicular Mobility Unit (xEMU) is the first clean sheet redesign of the astronaut spacesuit in approximately 40 years. NASA Langley Research Center’s electron beam welding team, of which the author is a member, is leading the development of the weld technology required to manufacture the backplate component of the Portable Life Support System (PLSS). This backplate will provide both structural support and integral cooling for the life support systems, communications, and other electronics inside the spacesuit.

electron beam welding↗