At least 1,459 records · Page 81

Capture of liquid hydrogen boiloff with metal hydride absorbers

A procedure which uses metal hydrides to capture some of this low pressure (,1 psig) hydrogen for subsequent reliquefaction is described. Of the five normally occurring sources of boil-off vapor the stream associated with the off-loading of liquid tankers during dewar refill was identified as the most cost effective and readily recoverable. The design, fabrication and testing of a proof-of-concept capture device, operating at a rate that is commensurate with the evolution of vapor by the target stream, is described. Liberation of the captured hydrogen gas at pressure .15 psig at normal temperatures (typical liquefier compressor suction pressure) are also demonstrated. A payback time of less than three years is projected.

Rosso, M. J.↗

Advanced rocket engine cryogenic turbopump bearing thermal model

A lumped node thermal model was developed representing the Space Shuttle Main Engine (SSME) liquid oxygen (LOX) turbopump turbine end bearings operating in a cryogenically cooled bearing tester. Bearing elements, shaft, carrier, housing, cryogen flow characteristics, friction heat, and fluid viscous energy are included in the model. Heat transfer characteristics for the regimes of forced convection boiling are modeled for liquid oxygen (LOX) and liquid nitrogen (LN2). Large temperature differences between the cryogenic fluid and baring contact surfaces require detailed nodal representation in these areas. Internal loads and friction heat are affected by temperature dependent operating clearances requiring iterations between bearing thermal and mechanical models. Analyses indicate a thermal-mechanical coupling resulting in reduced operating clearances, increased loading and heating which can contribute to premature bearing failure. Contact surfaces operate at temperatures above local saturation resulting in vapor rather than liquid in the contacts, precluding possible liquid film lubrication. Elevated temperatures can reduce lubrication, increase friction, and reduce surface hardness supporting a surface failure mode rather than subsurface fatigue.

Cody, J. C.↗

Condensation of anhydrides or dicarboxylic acids with compounds containing active methylene groups. Part 1: Condensation of phthalic anhydride with acetoacetic and malonic ester

Phthalic anhydride was condensed with acetoacetic ester in acetic anhydride and triethylamine solution, and when phthalyl chloride was reacted with sodium acetoacetic ester compounds were formed of the phthalide and indandione series: phthalylacetoacetic ester and a derivative of indan-1,3-dione which after boiling with hydrochloric acid yielded indan-1,3-dione. Phthalylmalonic ester was obtained from phthalic anhydride and malonic ester in the presence of triethylamine.

Oshkaya, V. P.↗

Adhesive evaluation of LARC-TPI and a water-soluble version of LARC-TPI

The results of a study to evaluate two Langley Research Center thermoplastic polimide (TPI) materials, identified as TPI/MTC for the material from Mitsui Toatsu Chemicals Inc. and TPI/H2O for the material from United Technologies Research Center, as high temperature thermoplastic adhesives and primers for bonding titanium (6AL-4V) adherends are discussed. A limited characterization of the materials was performed using a Diffuse Reflectance-Fourier Transform Infrared Spectroscopy (DR-FTIR) technique. Thermomechanical Analysis (TMA) and torsional braid techniques were used to determine glass transition temperature. The adhesive's strength, as determined by simple lap shear tests, as used to evaluate the effects of long term thermal exposure (up to 1000 hrs) at 204 deg C and a 72-hour water-boil.

Progar, D. J.↗

STPI/LARC: A 200 deg C polyimide adhesive

A copolyimide, STPI/LARC, was prepared from the reaction of 3,3'4'benzophenonetetracarboxylic dianhydride (BTDA), equimolar quantities of m-phenylenediamine and 4,4'-oxydianiline, and a small amount of phthalic anhydride to control the molecular weight. The processability and adhesive properties of STPI/LARC were compared to those of a commercially available form of LARC-TPI. LARC-TPI, a thermoplastic polyimide, from the reaction of BTDA and 3,3'-diaminobenzophenone, had previously shown promise as a high temperature structural adhesive. Lap shear specimens were fabricated using adhesive tape prepared from each of the two polymers. Lap shear tests were performed at room temperature, 177 C, and 204 C before and after exposure to a 72-hour water-boil and to aging at 204 C.

Progar, D. J.↗

Remarks on preparation of indandione detection reagents

A modified Claisen condensation with sliced sodium at a higher temperature was recommended for the production of ungranulated charcoal. A new ninhydrin production method by oxidation of benzaldiketohydrinden using available reagents was tried and was unsuccessful. Triketohydrinden was obtained by boiling ninhydrin in acetic acid anhydrides.

Stepan, J.↗

Sound speed measurements in liquid oxygen-liquid nitrogen mixtures

The sound speed in liquid oxygen (LOX), liquid nitrogen (LN2), and five LOX-LN2 mixtures was measured by an ultrasonic pulse-echo technique at temperatures in the vicinity of -195.8C, the boiling point of N2 at a pressure of I atm. Under these conditions, the measurements yield the following relationship between sound speed in meters per second and LN2 content M in mole percent: c = 1009.05-1.8275M+0.0026507 M squared. The second speeds of 1009.05 m/sec plus or minus 0.25 percent for pure LOX and 852.8 m/sec plus or minus 0.32 percent for pure LN2 are compared with those reported by past investigators. Measurement of sound speed should prove an effective means for monitoring the contamination of LOX by Ln2.

Zuckerwar, A. J.↗

Preparation and properties of silane-endcapped polyimide adhesives

Silane-endcapped polyimide high temperature adhesive formulations were prepared by reacting anhydride-terminated poly(amic acid), obtained from benzophenonetetracarboxylic dianhydride and a diamine (3,3'-, 3,4'- or 4,4'-diaminodiphenylmethane and 3,3', 3,4'- or 4,4'-diaminobenzophenone) with varying amounts of gama-aminopropyltriethoxysilane in dimethylacetamide. Resin properties were evaluated by torsional braid analysis and thermogravimetric analysis. Lap shear strengths of some of the adhesive bonds were determined at room temperature and at 177 C before and after ageing at 200 C for 2500 h and after boiling in water for 72 h.

Maudgal, S.↗

Electron acceleration in solar flares and the transition from nonthermal to thermal hard X-ray phases

Observations are reviewed which indicate that hard X-rays during the impulsive phase of a flare typically start with a primarily nonthermal phase which undergoes a transition to a primarily thermal phase as the flare progresses. Recent theoretical work on the modified two-stream instability as an efficient electron accelerator and modeling of thermal hard X-ray sources is considered. A scenario which is termed the dissipative thermal model is proposed to explain the observations. Fast tearing modes occurring in a loop give rise to cross-field ion motion. This in turn excites the modified two-stream instability which converts about 50 percent of the ion energy into accelerated electrons along the loop as long as the plasma beta is less than 0.3. These electrons impact the chromosphere and boil off a part of it which rises up the loop. This density increase coupled with the temperature increase due to tearing causes the beta to increase beyond 0.3 and efficient electron acceleration ceases. This leads to the primarily thermal phase.

Smith, D. F.↗

A new ozone standard - The vapor pressure of ozone at liquid argon temperatures

The vapor pressure of ozone has been measured at liquid argon temperatures. At the normal boiling point of argon (-185.9 C) an ozone pressure of 0.0405 torr was obtained with an accuracy of + or - 1.5 percent. Increases and decreases in liquid argon temperatures raised and lowered the ozone vapor pressure, respectively. During the vapor pressure measurements the purity of ozone was monitored with a mass spectrometer. The proposed ozone standard will considerably improve the calibration of experiments for atmospheric research, the determination of absorption cross sections and other laboratory ozone studies.

Mauersberger, K.↗

Impact properties of rubber-modified epoxy resin-graphite-fiber composites

To improve the impact resistance of graphite-fiber composites, a commercial and an experimental epoxy resin were modified with liquid reactive rubber and a brominated epoxy resin. The commercial epoxy was a tetrafunctional resin, and the experimental epoxy was a trifunctional resin. The reactive rubber was a carboxyl-terminated butadiene-acrylonitrile copolymer. The rubber content was varied from 0 to 25 percent (wt). The brominated epoxy resin was used at Br levels of 4, 19, and 35 percent of the resin. Composites were prepared with woven graphite cloth reinforcement. The composites were evaluated by using flexural strength in the dry state and an elevated temperature after saturation with water. The impact properties were determined by measuring shear strength after falling-ball impact and instrumented impact. The rubber-modified, trifunctional resin exhibited better properties, when tested in hot-wet conditions in a heated oven at 366 K (after boiling the material for 2 h in demineralized water), than the tetrafunctional resin. Improved impact resistance was observed with the addition of the reactive rubber to the epoxy resin. Further improvement was observed with the addition of the brominated epoxy resin.

Gilwee, W. J.↗

Precision ozone vapor pressure measurements

The vapor pressure above liquid ozone has been measured with a high accuracy over a temperature range of 85 to 95 K. At the boiling point of liquid argon (87.3 K) an ozone vapor pressure of 0.0403 Torr was obtained with an accuracy of + or - 0.7 percent. A least square fit of the data provided the Clausius-Clapeyron equation for liquid ozone; a latent heat of 82.7 cal/g was calculated. High-precision vapor pressure data are expected to aid research in atmospheric ozone measurements and in many laboratory ozone studies such as measurements of cross sections and reaction rates.

Hanson, D.↗

Pump for Saturated Liquids

Boiling liquids pumped by device based on proven components. Expanding saturated liquid in nozzle and diverting its phases along separate paths in liquid/vapor separator raises pressure of liquid. Liquid cooled in process. Pump makes it unnecessary to pressurize cryogenic liquids in order to pump them. Problems of introducing noncondensable pressurizing gas avoided.

Elliott, D. G.↗

An improved processible acetylene-terminated polyimide for composites

The newest member of a family of thermosetting acetylene-substituted polyimide oligomers is HR600P. This oligomer is the isoimide version of the oligomer known as HR600P and Thermid 600. Although both types of material yield the same heat resistant end products after cure, HR600P has much superior processing characteristics. This attributed to its lower melting temperature (160 + or - 10 C, 320 + or - 20 F) in contrast to 202 C (396 F) for Thermid MC-600, its longer gel time at its processing temperature (16 to 30 minutes bvs 3 minutes), and its excellent solubility in low boiling solvents such as tetrahydrofuran, glymes, or 4:1 methyl ethyl ketone/toluene mixtures. These advantages provide more acceptable coating and impregnation procedures, allow for more complete removal at lower temperatures, provide a longer pot life or working time, and allow composite structure fabrication in conventional autoclaves used for epoxy composite curing. The excellent processing characteristics of HR600P allow its use in large area laminated structures, structural composites, and molding compositions.

Landis, A. L.↗

Adhesive evaluation of thin films of LARC-TPI and LARC-TPI with 5 mol % ODA

A commercially available LARC-TPI film and an experimentally prepared film of LARC-TPI with 5 mol % of 4,4'-oxydianiline (ODA), designated as LARC-TPI/ODA in the report, supplied by Mitsui Toatsu Chemicals, Incorporated (MTCI), Japan, were evaluated as thermoplastic adhesive films for bonding Ti-6Al-4V. The LARC-TPI/ODA had been shown by MTCI to possess more flow than thermoplastic LARC-TPI and was, therefore, evaluated and compared to the LARC-TPI. Lap shear strength was used to evaluate the materials as adhesives. They were characterized after fracture by determining the glass transition temperature, Tg. The mode of failure was also reported. Thermal exposure at 204C for 500 and 1000 hrs and a 72-hour water-boil were conducted on lap shear specimens prepared with the two adhesive films. Lap shear tests were conducted at RT, 177C, 204C, and 232C before and after exposures.

Progar, D. J.↗

Dynamics insulation systems

Advanced dynamic insulation systems were analyzed from a thermodynamic point of view. A particular performance measure is proposed in order to characterize various insulations in a unique manner. This measure is related to a base quantity, the refrigeration power ratio. The latter is the minimum refrigeration power, for a particular dynamic insulation limit, to the actual reliquefaction power associated with cryoliquid boiloff. This ratio serves as reference quantity which is approximately constant for a specific ductless insulation at a chosen normal boiling point. Each real container with support structure, vent tube, and other transverse components requires a larger refrigeration power. The ratio of the actual experimental power to the theoretical value of the support-less system is a suitable measure of the entire insulation performance as far as parasitic heat leakage is concerned. The present characterization is illustrated using simple thermodynamic system examples including experiments with liquid nitrogen. Numerical values are presented and a comparison with liquid helium is given.

Chen, W. E. W.↗

Space Station momentum control and reboost requirements for two power generation concepts

Results are presented of dynamic structural analyses of 75 and 300 kW versions of a solar dynamic (SD) power supply for the Space Station (MSS). The SD is being seriously considered as an alternative to solar panels due to lower areal and mass requirements and higher efficiencies. The functioning principle is to use parabolic concentrators to focus sunlight on a heat engine to boil liquids to drive a turbine. Potential problems are foreseen in terms of the torques which would be experienced by the MSS and the subsequent orbital stability effects. The stability would be altered by changing aerodynmaic drag, altered moment of inertia and angular momentum and the altered center of mass location. The problem is exacerbated by the need to first equip the MSS with solar panels while the SD technology is developed. The analysis shows that the attitude control system will need to be redesigned and resized to accommodate MSS growth with either power system. The effects of the rotating parts of the SD system can be minimized, but further studies are required to determine the effects on the pointing accuracy of the SD, which must be 10 times as precise as that needed by a photovoltaic array.

Farmer, J. T.↗

Adhesive evaluation of LARC-TPI and a water-soluble version of LARC-TPI

The results of a study to evaluate two Langley Research Center thermoplastic polimide (TPI) materials, identified as TPI/MTC for the material from Mitsui Toatsu Chemicals Inc. and TPI/H2O for the material from United Technologies Research Center, as high temperature thermoplastic adhesives and primers for bonding titanium (6AL-4V) adherends are discussed. A limited characterization of the materials was performed using a Diffuse Reflectance-Fourier Transform Infrared Spectroscopy (DR-FTIR) technique. Thermomechanical Analysis (TMA) and torsional braid techniques were used to determine glass transition temperature. The adhesive's strength, as determined by simple lap shear tests, was used to evaluate the effects of long term thermal exposure (up to 1000 hrs) at 204 deg C and a 72-hour water-boil.

Progar, D. J.↗