Selected fretting-wear-resistant coatings for Ti-6 pct Al-4 pct V alloy
The ability of several wear-resistant coatings to reduce fretting in the Ti-6Al-4V alloy is investigated. The experimental apparatus and procedures for evaluating fretting in uncoated Ti-6Al-4V alloy and in the alloy with plasma-sprayed coatings, polymer-bonded coating, and surface treatments are described. The wear volume and wear rate for the alloys are measured and compared. It is concluded that Al2O3 with 13 percent TiO2, preoxidation and nitride surface treatments, and MoS2 sputtering result in wear-resistant surfaces; however, the polyimide coating is the most wear resistant coating in both dry and moist air, and it causes the least wear to the uncoated alloy surface.