Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “intercalation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,441 records · Page 80

Chemical preintercalation of magnesium ions into ⍺-MoO 3 structure for improved electrochemical stability in Li-ion cells

Chemical preintercalation of layered materials, used as electrodes in intercalation-based energy storage devices, represents a promising strategy to enhance electrochemical stability and extend cycle life. However, standardized synthesis approaches for the chemical preintercalation of diverse ions into various layered materials are lacking, necessitating the development of specific synthesis routes for each ion and layered phase combination. In this study, we present the first successful demonstration of Mg 2+ ion chemical preintercalation into the interlayer region of α-MoO 3 , revealing its stabilizing effect during cycling in non-aqueous Li-ion cells. Using ethanol during hydrothermal treatment facilitated molybdenum reduction, which was critical for Mg 2+ ion preintercalation. Interestingly, we found that Mg preintercalation was accompanied by the incorporation of water. Mg-preintercalated α-MoO 3 exhibited enhanced charge storage capacity, electrochemical stability, and power capability compared to pristine α-MoO 3 electrodes. This improved performance is attributed to the structural stabilization provided by Mg 2+ pillars, which prevent undesirable phase transformations during repeated Li intercalation/deintercalation, and increased Li + ion diffusion due to the shielding of electrostatic interactions between electrochemically cycled ions and the α-MoO 3 lattice, enabled by structural water. In conclusion, our study offers new insights into developing chemical preintercalation synthesis approaches that can be broadly applied to a wide range of pillaring ions and layered material hosts.

25 ENERGY STORAGE↗

Hybrid bilayered vanadium oxide electrodes with large and tunable interlayer distances in lithium-ion batteries

The interlayer distances in layered electrode materials, influenced by the chemical composition of the confined interlayer regions, have a significant impact on their electrochemical performance. Chemical preintercalation of inorganic metal ions affects the interlayer spacing, yet expansion is limited by the hydrated ion radii. Herein, we demonstrate that using varying concentrations of decyltrimethylammonium (DTA + ) and cetyltrimethylammonium (CTA + ) cations in chemical preintercalation synthesis followed by hydrothermal treatment, the interlayer distance of hybrid bilayered vanadium oxides (BVOs) can be tuned between 11.1 Å and 35.6 Å. Our analyses reveal that these variations in interlayer spacing are due to different amounts of structural water and alkylammonium cations confined within the interlayer regions. Increased concentrations of alkylammonium cations not only expand the interlayer spacing but also induce local bending and disordering of the V-O bilayers. Electrochemical cycling of hybrid BVO electrodes in non-aqueous lithium-ion cells show that specific capacities decrease as interlayer regions expand, suggesting that the densely packed alkylammonium cations obstruct intercalation sites and hinder Li + ion transport. Furthermore, we found that greater layer separation facilitates the dissolution of active material into the electrolyte, resulting in rapid capacity decay during extended cycling. In conclusion, this study emphasizes that layered electrode materials require both spacious interlayer regions as well as high structural and chemical stabilities, providing guidelines for structural engineering of organic–inorganic hybrids.

25 ENERGY STORAGE↗

Solid phase characterization and transformation of illite mineral with gas-phase ammonia treatment

In situ remediation applications of ammonia (NH 3 ) gas have potential for sequestration of subsurface contamination. Ammonia gas injections initially increase the pore water pH leading to mineral dissolution followed by formation of secondary precipitates as the pH is neutralized. However, there is a lack of understanding of fundamental alteration processes due to NH 3 treatment. In these batch studies, phyllosilicate minerals (illite and montmorillonite) were exposed to NH 3 gas with subsequent aeration to simulate in situ remediation. Following treatments, solids were characterized using a variety of techniques, including X-ray diffraction, N 2 adsorption-desorption analysis for surface area, Fourier transform infrared (FTIR) spectroscopy, nuclear magnetic resonance (NMR), and microscopy methods to investigate physicochemical transformations. The results of this study indicate that, at high pH, the clays are altered as observed by differences in morphology and particle size via microscopy. However, the two clays interact differently with NH 3 . While montmorillonite interlayers collapsed due to intercalation, illite layers were unaffected as confirmed by FTIR analysis. Further, structural changes in silicate ([SiO 4 ] n- ) and aluminol (Al-OH) groups were identified by NMR and FTIR. This research showed that mineral alteration processes occur during and after NH 3 gas treatment which may be used to remove radionuclides from the aqueous phase through sorption, co-precipitation, and coating with secondary phyllosilicate alteration products.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Large-scale paleo water-table rise in a deep desert aquifer recorded by dissolved noble gases

Illuminating past hydrological and climatological conditions in arid regions may provide insights into future trends in groundwater availability. The main objective of this study is to explore paleorecharge processes in the deep regional Nubian Sandstone Aquifer (NSA), which stretches below the hyperarid deserts of the Sinai Peninsula (Egypt) and the Negev (Israel), using dissolved noble gas data. Extremely high amounts of dissolved excess air (Ne concentrations up to 4 × solubility equilibrium) were observed in the ancient ( 81 Kr-depleted) groundwater that was recharged during past pluvial epochs in the basin. Here, the observed unique excess air signal and the clear spatiotemporal structure of the noble gas compositions in the aquifer are hypothesized to reflect two major characteristics of the groundwater system: (a) large-scale, long-term rises in the water table that facilitate the entrapment and dissolution of air bubbles under increased hydrostatic pressure, and (b) the geological settings in the southern recharge area in Sinai, including an almost horizontal position of the layers and intercalation of low-permeability rock formations within the aquifer, which inefficiently reject air bubbles from groundwater, thereby allowing for substantial entrapment of bubbles that dissolve as the water table rises. Enhanced dissolution of entrapped air was also observed in other paleo-groundwater-containing regional sandstone aquifers across North Africa, which, together with the recent findings from the NSA, suggest that largescale water table fluctuations have likely extensively occurred during past pluvial periods over these (and possibly other) arid regions. A preliminary assessment of noble gas recharge temperatures (NGTs) indicates an apparent decoupling of surface and water table temperatures in the case of deep aquifers with a thick (hundreds of m) unsaturated zone. This observed decoupling calls for a re-evaluation of previously obtained NGT records and a need for future work to consider the modification of NGTs due to soil air fractionation and geothermal heating of the underlying deep unsaturated zones.

54 ENVIRONMENTAL SCIENCES↗

Highly reversible Zn anode with a practical areal capacity enabled by a sustainable electrolyte and superacid interfacial chemistry

Aqueous zinc-metal batteries are plagued by poor Zn reversibility owing to zinc dendrite and layered double hydroxide (LDH) formation. Here, we introduce a novel additive—N,N-dimethylformamidium trifluoromethanesulfonate (DOTf)—in a low-cost aqueous electrolyte that can very effectively address these issues. The initial water-assisted dissociation of DOTf into triflic superacid creates a robust nanostructured solid-electrolyte interface (SEI)—revealed by operando spectroscopy and cryomicroscopy—which excludes water and enables dense Zn deposition. We demonstrate excellent Zn plating/stripping in a Zn||Cu asymmetric cell for more than 3,500 cycles. Furthermore, near 100% CE is realized at a combined high current density of 4 mA cm -2 and an areal capacity of 4 mAh cm -2 over long-term cycling. Zn||Zn 0.25 V 2 O 5 ·nH 2 O full cells retain ~83% of their capacity after 1,000 cycles with mass-limited Zn anodes. By restricting the depth of discharge, the cathodes exhibit less proton intercalation and LDH formation with an extended lifetime of 2,000 cycles.

25 ENERGY STORAGE↗

Lithium halide cathodes for Li metal batteries

Lithium halides cathodes potentially offer a high energy density at a low cost for rechargeable batteries. However, these cathodes suffer from quick capacity decay in organic electrolytes and the failiure mechanism remains elusive. Here, we report that liquefying the halogen or interhalogen compounds is a prerequisite for achieving high reversibility for the lithium halides cathodes. The gas or solid halogen can be liquefied by using interhalogen compounds with different electronegativity or changing the temperature. As a proof of concept, reversible LiCl conversion-intercalation chemistry in organic electrolyte is demonstrated by using either redox coupling with less electronegative I/Br to form liquid ICl/BrCl or reducing the temperature to -30oC. Further, the LiCl-LiBr-graphite cathodes in 1.6M lithium difluoro(oxalato)borate/1.6M lithium triflate in diglyme electrolytes achieve a high reversible specific capacity of 250 mAh/g at 3.7 V with an energy density being comparable to or higher than transition metal oxide cathodes at a much lower cost.

25 ENERGY STORAGE↗

Reinvestigation on the state-of-the-art nonaqueous carbonate electrolytes for 5 V Li-ion battery applications

The charging voltage limits of mixed carbonate solvents for Li-ion batteries have been systematically investigated from 4.9 to 5.3 V in half cells using Cr-doped spinel cathode material LiNi0.45Cr0.05Mn1.5O4. We found that the stability of conventional carbonate electrolytes is strongly related to the stability and properties of the cathode materials at both lithiated and de-lithiated states. It is the first time to report that the conventional electrolytes based on mixtures of ethylene carbonate (EC) and linear carbonate (dimethyl carbonate - DMC, ethyl methyl carbonate - EMC, and diethyl carbonate - DEC) have shown very similar long-term cycling performance when cycled up to 5.2 V on LiNi0.45Cr0.05Mn1.5O4. The discharge capacity increases with the charge cutoff voltage and reaches the highest discharge capacity at 5.2 V. The capacity retention is about 87% after 500 cycles at 1C rate for all three carbonate mixtures when cycled between 3.0 V and 5.2V. The first-cycle efficiency has a maximum value at 5.1 V, with an average from 83% to 85% at C/10 rate. When cycled to 5.3 V, EC-DMC still shows good cycling performance but EC-EMC and EC-DEC show faster capacity fading. EC-DMC and EC-EMC have much better rate capability than EC-DEC. In addition, the first-cycle irreversible capacity loss increases with the cutoff voltage and the 'inactive' conductive carbon has also been found to be partly associated with the low first-cycle Coulombic efficiency at high voltages due to electrolyte decomposition and probably the PF6- anion irreversible intercalation.

25 ENERGY STORAGE↗

Rate dependence of swelling in lithium-ion cells

Swelling of a commercial 5 Ah lithium-ion cell with a nickel/manganese/cobalt-oxide cathode is investigated as a function of the charge state and the charge/discharge rate. In combination with sensitive displacement measurements, knowledge of the electrode configuration within this prismatic cell's interior allows macroscopic deformations of the casing to be correlated to electrochemical and mechanical transformations in individual anode/separator/cathode layers. Thermal expansion and interior charge state are both found to cause significant swelling. At low rates, where thermal expansion is negligible, the electrode sandwich dilates by as much as 1.5% as the charge state swings from 0% to 100% because of lithium-ion intercalation. At high rates a comparably large residual swelling was observed at the end of discharge. Thermal expansion caused by joule heating at high discharge rate results in battery swelling. The changes in displacement with respect to capacity at low rate correlate well with the potential changes known to accompany phase transitions in the electrode materials. Although the potential response changes minimally with the C-rate, the extent of swelling varies significantly, suggesting that measurements of swelling may provide a sensitive gauge for characterizing dynamic operating states. (C) 2014 Elsevier B.V. All rights reserved.

Oh, KY↗

Hybrid phosphazene anodes for energy storage applications

The use of hybrid cyclic phosphazene polymer/graphite anodes, where the phosphazene serves as distributed loci for Li deposition, has been investigated. Capacity within the hybrid system was found to occur reversibly in distinct regions. At the most positive voltages, above 0.06 V vs Li/Li+, the capacity was associated mostly with Li+ intercalation into graphite. In the most negative region, deposition of Li within the polymer was the predominate mechanism. A transitional region is inferred by the data whereby bulk aggregation or clustering of Li atoms occurs in proximity to the phosphazene sites that then serve as a template for more widespread population of Li within the anode at higher voltages, akin to a nucleation process. In full cells with a mixed oxide cathode, controlling the extent of Li deposition by limiting the charging voltage to 4.45 V enabled repeated cycling with no loss in capacity. Capacities as high as 183 mAh g-1 have been achieved for systems containing as little as 10% graphite while retaining coulombic efficiencies of 98% over 50 cycles. This level of cycling equates to the deposition of 7.4 Li per cyclic phosphazene.

25 ENERGY STORAGE↗

Galvanostatic interruption of lithium insertion into magnetite: Evidence of surface layer formation

Magnetite is a known lithium intercalation material, and the loss of active, nanocrystalline magnetite can be inferred from the open-circuit potential relaxation. Specifically, for current interruption after relatively small amounts of lithium insertion, the potential first increases and then decreases, and the decrease is hypothesized to be due to a formation of a surface layer, which increases the solid-state lithium concentration in the remaining active material. Comparisons of simulation to experiment suggest that the reactions with the electrolyte result in the formation of a thin layer of electrochemically inactive material, which is best described by a nucleation and growth mechanism. Simulations are consistent with experimental results observed for 6, 8 and 32-nm crystals. As a result, simulations capture the experimental differences in lithiation behavior between the first and second cycles.

25 ENERGY STORAGE↗

In situ characterization of charge rate dependent stress and structure changes in V 2 O 5 cathode prepared by atomic layer deposition

Here, the insertion/extraction of lithium into/from various host materials is the basic process by which lithium-ion batteries reversible store charge. This process is generally accompanied by strain in the host material, inducing stress which can lead to capacity loss. Therefore, understanding of both the structural changes and the associated stress – investigated almost exclusively separate to date – is a critical factor for developing high-performance batteries. Here, we report an in situ method, which utilizes Raman spectroscopy in parallel with optical interferometry to study effects of varying charging rates (C-rates) on the structure and stress in a V 2 O 5 thin film cathode. Abrupt stress changes at specific crystal phase transitions in the Li—V—O system are observed and the magnitude of the stress changes with the amount of lithium inserted into the electrode are correlated. A linear increase in the stress as a function of x in Li x V 2 O 5 is observed, indicating that C-rate does not directly contribute to larger intercalation stress. However, a more rapid increase in disorder within the Li x V 2 O 5 layers is correlated with higher C-rate. Ultimately, these experiments demonstrate how the simultaneous stress/Raman in situ approach can be utilized as a characterization platform for investigating various critical factors affecting lithium-ion battery performance.

25 ENERGY STORAGE↗

Next generation molten NaI batteries for grid scale energy storage

Robust, safe, and reliable grid-scale energy storage continues to be a priority for improved energy surety, expanded integration of renewable energy, and greater system agility required to meet modern dynamic and evolving electrical energy demands. We describe here a new sodium-based battery based on a molten sodium anode, a sodium iodide/aluminum chloride (NaI/AlCl 3 ) cathode, and a high conductivity NaSICON (Na 1+x Zr 2 Si x P 3–x O 12 ) ceramic separator. This NaI battery operates at intermediate temperatures (120–180 °C) and boasts an energy density of >150 Wh kg –1 . The energy-dense NaI-AlCl 3 ionic liquid catholyte avoids lifetime-limiting plating and intercalation reactions, and the use of earth-abundant elements minimizes materials costs and eliminates economic uncertainties associated with lithium metal. Moreover, the inherent safety of this system under internal mechanical failure is characterized by negligible heat or gas production and benign reaction products (Al, NaCl). Scalability in design is exemplified through evolution from 0.85 to 10 Ah (28 Wh) form factors, displaying lifetime average Coulombic efficiencies of 99.45% and energy efficiencies of 81.96% over dynamic testing lasting >3000 h. Here, this demonstration promises a safe, cost-effective, and long-lifetime technology as an attractive candidate for grid scale storage.

25 ENERGY STORAGE↗

Balancing formation time and electrochemical performance of high energy lithium-ion batteries

Most lithium-ion batteries still rely on intercalation-type graphite materials for anodes, and the formation process for them typically takes several days or even more to provide a stable solid electrolyte interphase (SEI). The slow formation step results in lower LIB production rates, requires a large number of battery cyclers, and constitutes the second highest cost during battery manufacturing. In an effort to decrease the high manufacturing cost associated with long formation times, here we studied five different formation protocols in nickel-rich LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811)/graphite cells where the total formation time varied from 10 to 86 h. Electrochemical characterization and post mortem analysis show that very long formation time do not necessarily improve long-term performance while very short formation protocols result in lithium plating and poorer electrochemical performance. Finally, we find the optimum formation cycling protocol is intermediate in length to minimize impedance growth, improve capacity retention, and avoid lithium plating.

25 ENERGY STORAGE↗

Consequences of long-term water exposure for bulk crystal structure and surface composition/chemistry of nickel-rich layered oxide materials for Li-ion batteries

Water exposure of layered nickel-rich transition metal oxide electrodes, widely used in high-energy lithium-ion batteries, has detrimental effects on the electrochemical performance, which complicates electrode handling and prevents implementation of environmentally benign aqueous processing procedures. Elucidating the degradation mechanisms in play may help rationally mitigate/circumvent key challenges. Here, the bulk structural consequences of long-term (>2.5 years) deuterated water (D2O) exposure of intercalation materials with compositions Li x Ni 0.5 Co 0.2 Mn 0.3 O 2 (NCM523) and Li x Ni 0.8 Co 0.1 Mn 0.1 O 2 (NCM811) are studied by neutron powder diffraction (NPD). Detailed inspection of the NPD data reveals gradual formation of a secondary crystalline phase in all exposed samples, not previously reported for this system. This unknown phase forms faster in liquid- compared to vapor-exposed compounds. Structural modelling of the NPD data shows a stable level of Li/Ni anti-site defects and does not indicate any significant changes in lattice parameters or hydrogen-lithium (D + /Li + ) exchange in the structure. Consequently, the secondary phase formation must take place via transformation rather than modification of the parent material. X-ray photoelectron spectroscopy data indicate formation of LiHCO 3 /Li 2 CO 3 at the surface and a Li-deficient oxide in the sub-surface region of the pristine compounds, and the presence of adsorbed water and transition metal hydroxides at the exposed sample surfaces.

25 ENERGY STORAGE↗

Spatially-resolved lithiation dynamics from operando X-ray diffraction and electrochemical modeling of lithium-ion cells

In this study, energy dispersive X-ray diffraction is used to profile the time evolution of ordered Li x C 6 phases in solid electrodes of lithium-ion cells charged at rates between 0.2 and 4.7C (where 1C corresponds to full discharge in 1 h). The methods for quantifying lithium concentration in these phases from the acquired diffraction patterns are described. Compact expressions for time-dependent concentration gradients in the solid electrodes using orthogonal polynomial expansions are presented. Experimentally, these gradients persisted in lithiated graphite electrodes even after the cells rested at open-circuit for over 9 h. A multiphase electrochemical model of graphite intercalation captured many of the observed behaviors, including the progression of phase transitions and the persistent gradients at zero current. However, the magnitude of concentration gradients in both the oxide cathode and graphite anode is underestimated by the model, even at moderate currents.

25 ENERGY STORAGE↗

Operando detection of Li plating during fast charging of Li-ion batteries using incremental capacity analysis

A major challenge that limits fast charging of Li-ion batteries is lithium (Li) plating on the graphite electrode. Furthermore, it remains challenging to detect and diagnose Li plating in operando during charging. In this work, incremental capacity (IC) analysis is applied while charging graphite-NMC pouch cells over a range of rates from C/2 to 4C. Three-electrode pouch cell measurements and post-mortem SEM imaging was performed to demonstrate that the onset of Li plating is correlated with a specific IC peak. IC analysis was also applied to study the fast-charge performance of multi-layer pouch cells with 3-D anode architectures. The results demonstrate that: 1) IC curves have a characteristic peak that is an indicator of Li plating during fast charging, which grows in magnitude as charging rate increases; 2) the plating IC peak correlates with the voltage minimum of the graphite anode, indicating a transition from intercalation to plating; 3) the plating IC peak is sensitive to small amounts of Li plating; 4) IC analysis can be applied to study Li plating in novel cell architectures; 5) the plating IC peak evolves during extended fast-charge cycling, which is a result of reduced Li plating as the Li inventory decreases.

25 ENERGY STORAGE↗