Development of Digital Twin Predictive Model for PWR Components: Updates on Multi Times Series Temperature Prediction Using Recurrent Neural Network, DMW Fatigue Tests, System Level Thermal-Mechanical-Stress Analysis

The long-term operation (LTO) of nuclear power plant (NPP) beyond their original design life of 40 years, can lead to more material damage associated with cyclic fatigue under thermal-mechanical loading cycles and associated long-term exposure of reactor material to the deleterious reactor-coolant environments. However, under this LTO condition the reactor components can still safely operate but may require more frequent Nondestructive Evaluation (NDE) of reactor components. Frequent NDE requirement may lead to frequent shutdown of the NPP. This in turn can lead to power outage and additional NDE-inspection-cost related economic loss. The economic loss can be minimized by reducing uncertainty in life estimation of safety-critical pressure boundary components and by implementing more digital approach such as by using upcoming digital-twin (DT) technology for predicting the structural states (e.g., time and location dependent inside/outside thickness temperature, stress, strain, plastic deformation, etc.) and associated fatigue life of a component in real time. Towards this goal Argonne National Laboratory (ANL) with the sponsorship of DOE Light Water Reactor Sustainability (LWRS) program is working on the development of a DT framework that can be used for real time environmental fatigue prediction of reactor components. The DT framework is based on limited experiment-data, Artificial-intelligence (AI) – Machine-Learning (ML) - Deep-Learning (DL) based techniques and Multiphysics-computational-mechanics such as finite element (FE) based modeling tools. Towards this overall goal, following are some of the major contributions made during the FY21: 1) Multiple 82/182 dissimilar metal weld (DMW) specimens (both solid-weld and joint-weld representing the actual reactor multi-metal nozzles) were fatigue tested. The resulting fatigue lives were compared to the NUREG-6909 based best-fit and design fatigue curves. Additionally, the results of 52/152 DMW fatigue specimens (which were recently tested at Republic of Korea under the sponsorship of International Nuclear Energy Research Initiative - INERI program) were compared to the NUREG-6909 based best-fit and design fatigue curves. From the comparison of 82/182 and 52/152 DMW test data with NUREG-6909 best-fit curve, most of the reported test data fall way away from the NUREG-6909 suggested best-fit or mean curve. The NUREG-6909 suggested best-fit curve is the best-fit curve of austenitic stainless steel and due to lack of enough data on Nickel-based welds, this is currently being used for predicting the life of Nickel-alloy-based welded components. However, the above observation may require higher scaling factor (e.g., ASME suggested factor of 20 on cycles rather than the current NUREG-6909 suggested factor of 12 on cycles) for scaling the austenitic-stainless-steel best-fit-curve for estimating the design or safe-life of a welded component. Accordingly, for example, if a DMW component experience a strain amplitude of 0.6% the PWR-water life of the component would be 52 cycles instead of 85 cycles. However, more DMW tests are required to further ascertain the above-mentioned observations. 2) A system level CAD and finite element model were developed which consists of reactor pressure vessel (RPV), part of steam generator (SG), part of pressurizer (PRZ), hot leg (HL), and surge line (SL). This is with detailed nozzle geometry and thermal-mechanical material properties of different metals to simulate realistic thermal-mechanical stress under connected system global thermal-mechanical boundary conditions. 3) Different system level heat transfer analyses were performed with estimation of relevant heat transfer coefficients. The resulting data were used in subsequent system level thermal-mechanical stress analysis and for generating spatial-temporal training and validation data for a system level digital-twin based temperature predictor. Transient heat transfer analyses were performed considering thermal boundary condition under design-basis (DB) loading and EDF (Électricité de France) data-based grid-load-following (EDF-GLF) loading cycles. 4) System level thermal-mechanical stress analysis was performed for identifying damage-prone hotspots and for future extension of the model for cyclic state prediction. From the system-level model simulation under DB loading cycle it is found that HL and the SL nozzle that connect to the HL can experience significant stress and strain and could be one of the weakest links in the overall reactor coolant system (RCS). 5) An AI/ML based DT model was developed for multi-time-series temperature prediction at any inside/outside thickness locations of PWR pressure boundary components. This is by using Recurrent-neural-network (RNN) and keras machine learning libraries. The RNN model was validated against two laboratory test-based data sets with one obtained through ANL’s in-air fatigue test system and other through PWR-water test loop. The experimentally validated DT model further validated against FE model results to predict thermal scarification related spatialtemporal temperatures at random locations of a component. The well validated DT model was then used for demonstrating spatial-temporal temperature prediction under 100+ years of reactor operation subjected to combined DB, EDF-GLF and randomized grid-load-following (RANDOMGLF) loading Cycles. The expert-elicitation DT model framework was developed assuming field/input/process measurements can be available from a few existing plant sensors and can readily be used by the NPP operators. The above temperature prediction model will feed to the next-step stress analysis model based on which the life of a component can be predicted in realtime, which is one of our future works.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Collaborative Study on Weldability of Irradiated Stainless Steel 304 Materials Removed from The NRU Reactor

A collaborative research on developing advanced welding technologies for irradiated stainless steel 304 materials between CNL and ORNL has been established to support both U.S. and Canadian interests in evaluation of weld repair techniques on irradiated materials to support continuous operation of commercial nuclear power. The work utilizes unique material from the National Research Universal (NRU) reactor and the specialized welding hot cell facility at ORNL. The objective is to explore suitable welding technique and parameters and to determine the helium concentration limitation in terms of irradiated stainless-steel weldability. An additional objective is to develop the knowledge and understanding of cracking mechanisms induced by high concentration of helium in the process of weld repair of the irradiated structural alloys. This report summarizes the experimental welding evaluation on irradiated material from the NRU reactor containing helium concentrations ranging from 12 to 45 atomic parts per million (appm).

36 MATERIALS SCIENCE↗

Effect of thermal aging on microstructure and stress corrosion cracking behavior of Alloy 152 weldment

Nickel-based Alloy 690 and the associated weld Alloys 52 and 152 are typically used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels, because of their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate for 40-80 years. Likewise, water-cooled small modular reactors (SMRs) will use Ni-Cr alloys and are expected to receive initial operating licenses for 60 years. Hence, the thermal stability of Ni-Cr alloys is a potential concern for the long-term performance of both existing and advanced nuclear power plants, and possibly spent fuel storage containers. The objective of this research is to understand the microstructural changes occurring in high-Cr, Ni-based Alloy 152 weldments during long time exposure to the reactor operating temperatures, and the effect of these changes on the service performance. One area of particular concern is the potential for long range ordering (LRO), i.e. formation of the intermetallic Ni2Cr phase under prolonged exposure to reactor temperatures and/or irradiation, which can increase strength, decrease ductility, and cause dimensional changes or lead to in-service embrittlement of components made with these alloys. Hence, this research focused on the microstructural evolution and the SCC response of Alloy 152 under accelerated thermal aging. The materials studied involved three heats of Alloy 152 used to produce a dissimilar metal weld (DMW) joining an Alloy 690 plate to an Alloy 533 low alloy steel (LAS) plate, thermally aged at three different temperatures (370°C, 400°C and 450°C) for up to 75,000h (equivalent to 60 years of service). The microstructural characterization by means of synchrotron X-ray conducted in small, 0.2 mm - step line scans in the high-deformation regions of the weld root – covering areas spanning from the weld heat affected zone (HAZ) in Alloy 690 to the weld and weld butter on LAS - did not show evidence of LRO in any of the three Alloy 152 heats aged to an equivalent of 60 years of service. Testing in a primary water environment of two heats of Alloy 152 aged at 370°C to a 60-year service equivalent revealed a fatigue and corrosion fatigue crack growth responses similar to those measured on the un-aged alloys. However, the SCC CGR response of the aged samples appears to show a deterioration in performance, confirming our previous observation.

36 MATERIALS SCIENCE↗

Evaluation of the Mechanical Properties of Cast and Wrought CF8C-Plus Relevant to ASME Code Case Qualification

The mechanical behavior of a cast form of an advanced austenitic stainless steel, CF8C-Plus, is compared with that of its wrought equivalent in terms of both tensile and creep-rupture properties and estimated allowable stress values for pressurized service at temperatures up to about 850°C. A traditional Larson-Miller parametric model is used to analyze the creep-rupture data and to predict long-term lifetimes for comparison of the two alloy types. The cast CF8C-Plus exhibited lower yield and tensile strengths, but higher creep strength compared to its wrought counterpart. Two welding methods, shielded-metal-arc welding (SMAW) and gas-metal-arc welding, met the weld qualification acceptance criteria in ASME BPVC Section IX for the cast CF8C-Plus. However, for the wrought CF8C-Plus, while SMAW and gas-tungsten-arc welding passed the tensile acceptance criteria, they failed the side bend tests due to lack of fusion or weld metal discontinuities.

Chen, Xiang↗

Metal Big Area Additive Manufacturing: Process Modeling and Validation

Metal Big Area Additive Manufacturing (mBAAM) is a new additive manufacturing (AM) technology for printing large-scale 3D objects. mBAAM is based on the gas metal arc welding process and uses a continuous feed of welding wire to manufacture an object. An electric arc forms between the wire and the substrate, which melts the wire and deposits a bead of molten metal along the predetermined path. In general, the welding process parameters and local conditions determine the shape of the deposited bead. The sequence of the bead deposition and the corresponding thermal history of the manufactured object determine the long range effects, such as thermal-induced distortions and residual stresses. Therefore, the resulting performance or final properties of the manufactured object are dependent on its geometry and the deposition path, in addition to depending on the basic welding process parameters. Physical testing is critical for gaining the necessary knowledge for quality prints, but traversing the process parameter space in order to develop an optimized build strategy for each new design is impractical by pure experimental means. Computational modeling and optimization may accelerate development of a build process strategy and saves time and resources. Because computational modeling provides these opportunities, we have developed a physics-based Finite Element Method (FEM) simulation framework and numerical models to support the mBAAM process s development and design. In this paper, we performed a sequentially coupled heat transfer and stress analysis for predicting the final deformation of a small rectangular structure printed using the mild steel welding wire. Using the new simulation technologies, material was progressively added into the FEM simulation as the arc weld traversed the build path. In the sequentially coupled heat transfer and stress analysis, the heat transfer was performed to calculate the temperature evolution, which was used in a stress analysis to evaluate the residual stresses and distortions. In this formulation, we assume that physics is directionally coupled, i.e. the effect of stress of the component on the temperatures is negligible. The experiment instrumentation (measurement types, sensor types, sensor locations, sensor placements, measurement intervals) and the measurements are presented. The temperatures and distortions from the simulations show good correlation with experimental measurements. Ongoing modeling work is also briefly discussed.

Additive Manufacturing↗

Microstructural response to heat affected zone cracking of prewelding heat-treated Inconel 939 superalloy

The microstructural response to cracking in the heat-affected zone (HAZ) of a nickel-based IN 939 superalloy after prewelding heat treatments (PWHT) was investigated. The PWHT specimens showed two different microstructures: 1) spherical ordered {gamma} Prime precipitates (357-442 nm), with blocky MC and discreet M{sub 23}C{sub 6} carbides dispersed within the coarse dendrites and in the interdendritic regions; and 2) ordered {gamma} Prime precipitates in 'ogdoadically' diced cube shapes and coarse MC carbides within the dendrites and in the interdendritic regions. After being tungsten inert gas welded (TIG) applying low heat input, welding speed and using a more ductile filler alloy, specimens with microstructures consisting of spherical {gamma} Prime precipitate particles and dispersed discreet MC carbides along the grain boundaries, displayed a considerably improved weldability due to a strong reduction of the intergranular HAZ cracking associated with the liquation microfissuring phenomena. - Highlights: Black-Right-Pointing-Pointer Homogeneous microstructures of {gamma} Prime spheroids and discreet MC carbides of Ni base superalloys through preweld heat treatments. Black-Right-Pointing-Pointer {gamma} Prime spheroids and discreet MC carbides reduce the intergranular HAZ liquation and microfissuring of Nickel base superalloys. Black-Right-Pointing-Pointer Microstructure {gamma} Prime spheroids and discreet blocky type MC carbides, capable to relax the stress generated during weld cooling. Black-Right-Pointing-Pointer Low welding heat input welding speeds and ductile filler alloys reduce the HAZ cracking susceptibility.

36 MATERIALS SCIENCE↗

Archaeometallurgical investigation of the iron anchor from the Tantura F shipwreck

The Tantura F shipwreck was a coaster or a fishing vessel about 15.7 m long, discovered in the Dor/Tantura lagoon, Israel in 1995. It was dated to between the mid-7th and the end of the 8th centuries CE. Among the finds excavated were two T-shaped type iron anchors. Of the two anchors, one (anchor A) was thoroughly studied by archaeometallurgical methods in order to identify forge-welding lines, to determine the welding quality and to understand the manufacturing technology. The examinations included X-ray radiography, XRF analysis, optical microscopy, SEM/EDS observation and analysis, OES analysis and microhardness tests. The investigation included characterization of the composition, microstructure, thermal treatments, forge-welding junctions and slag analysis. The results revealed a heterogeneous microstructure, rich in glassy, fayalite and wüstite slag. Iron based phases included ferrite, pearlite, cementite and Widmanstätten plates, all typical to wrought iron. The forge-welds of Anchor A were located. Each arm was made of one piece, weighing about 2.5–3 kg and the shank was made of a few 1.5–2 kg pieces. The second anchor (anchor B) was only briefly examined visually and with a few radiographs, which support the results from anchor A. The research results revealed significant information about T-shaped anchors and their manufacturing process, including hot-working processes without any additional heat treatments, and folding techniques. The microstructure was similar to other ancient simple tools such as saws, sickles, axes and mortise chisels, and though the technology to make complicated structures and objects, such as swords, existed at that time, the anchors did not require this sophistication; thus simpler techniques were used, presumably because they were more cost-effective. - Highlights: ► Tantura F was a coaster dated to mid-7th–end-8th centuries. ► Two iron anchors were discovered at the Tantura F shipwreck-site. ► Anchor A was manufactured from heterogeneous wrought iron blooms. ► Forge-welding lines were detected using archaeometallurgical methods.

36 MATERIALS SCIENCE↗

Improvement of circumferential ductility by reducing discontinuities in a high-Mn TWIP steel weldment

Highlights: • This study focused on two key ways to improve expandability of TWIP steel pipe. • The amount of penetrator is remarkably reduced at low PO{sub 2} welding atmosphere. • The effect of PWHT on the morphological change in the bond line was characterized. - Abstract: Recently, high-frequency electrical resistance welded (HF-ERW) pipes have been introduced as an application of high-Mn twinning induced plasticity (TWIP) steels. However, the excellent ductility of the TWIP steels has been underutilized in expandable pipe applications due to discontinuities in the weldment. This work presents two key ways to improve the pipe expandability or circumferential ductility. In-depth microstructural analysis and flaring tests were conducted to identify bond line discontinuities and to evaluate the circumferential ductility. These results indicate that ductility formed to be strongly related to the welding atmosphere and post-weld heat treatment (PWHT) conditions. The welding atmosphere was related to oxide defects, while the PWHT conditions were related to intrinsic discontinuities. The distribution and amount of penetrator defects along the bond line are the main factors related to the deterioration of the circumferential ductility, which is affected by the sheet metal compositions and decreased remarkably at low PO{sub 2} content. We also suggest that PWHT is necessary for improving the ductility by inducing changes in the bond line texture and hardness distribution. The results were verified based on changes in the crack path propagation.

36 MATERIALS SCIENCE↗

Joining techniques for a reduced activation 12Cr steel for inertial fusion energy

At Lawrence Livermore National Laboratory, we are developing a reduced activation ferritic martensitic steel that is based on the ferritic martensitic steel HT-9. As a part of the development of this steel, we tested a series of welding processes for characterization, including conventional welds (electron beam, tungsten inert gas, and laser) as well as solid-state welds (hot isostatic pressing). We also heat treated the joints at various temperatures between 750 °C and 1050 °C to find a suitable normalization scheme. The modified HT-9 reduced activation ferritic martensitic steel appears highly suitable to welding and diffusion bonding. All welds showed good quality fusion zones with insignificant cracking or porosity. Additionally, a heat treatment schedule of 950 °C for one hour caused minimal grain growth while still converging the hardness of the base metal with that of the fusion and heat-affected zones. Also, modified HT-9 diffusion bonds that were created at temperatures of at least 950 °C for two hours at 103 MPa had interface tensile strengths of greater than 600 MPa. The diffusion bonds showed no evidence of increased hardness nor void formation at the diffusion bonded interface.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Building metallic glass structures on crystalline metal substrates by laser-foil-printing additive manufacturing

In laser-foil-printing additive manufacturing, 3D metallic glass structures can be built by laser welding of amorphous foils, layer by layer, upon a crystalline metal substrate. Here, in this paper, weldability studies for laser welding of Zr 52.5 Ti 5 Al 10 Ni 14.6 Cu 17.9 amorphous foils onto a Ti-6Al-4V (Ti 6-4) or Zr 702 substrate are conducted. After laser welding, the weldments are analyzed using X-ray diffractometer, optical microscope, scanning electron microscope equipped with energy dispersive spectroscopy and micro-hardness tester. The results show that Zr 702 is a suitable substrate for Zr-based metallic glass structure since crack-free weld joints can be obtained owing to the formation of ductile α-Zr, while Ti 6-4 is not an appropriate substrate since it has high cracking susceptibility due to the formation of a large amount of hard and brittle intermetallics near the foil-substrate interface. It was found that the mixing between melted substrate and foil is not uniform but exhibits a distinct “swirl” pattern. The swirl structure is more pronounced in Ti 6-4 than in Zr 702 substrate which may contribute to its high cracking susceptibility. The aforementioned mixing leads to partial crystallization of the first amorphous layer; however, fully amorphous is achieved in the additional welding layers.

36 MATERIALS SCIENCE↗

Characterization of Alloy 600 joints exposed to a high-temperature supercritical-carbon dioxide environment

Highlights: • Diffusion-bond showed similar corrosion and carburization behavior as parent matrix. • Diffusion-bond line migrated due to the Cr-depletion induced recrystallization. • Alloy 182 fusion-weld showed larger weight gains with outer Mn-rich oxides. • The presence of SiO{sub 2} in chromia suppressed carburization at the oxide/matrix interface. • Despite larger weight gains, Alloy 182 fusion-weld showed negligible tensile property changes. - Abstract: Two types of Alloy 600 joints, such as diffusion-bonded joint and Alloy 182 fusion-weld, were exposed to supercritical-CO{sub 2} environment at 550 and 650 °C (20 MPa) for 1000 h. The diffusion-bond region showed similar oxidation characteristics as parent Alloy 600, but the migration of diffusion bond line below oxide layer was observed due to the Cr-depletion induced recrystallization. For Alloy 182 fusion-weld, outer Mn-rich oxides (Mn{sub 3}O{sub 4} and MnCr{sub 2}O{sub 4}) and a small amount of inner SiO{sub 2} mixed with chromia were formed due to high Mn and Si contents. The presence of SiO{sub 2} in chromia suppressed carburization at the oxide/matrix interface, which resulted in the formation of an amorphous C layer between the outer Mn-rich oxide and inner Cr-rich oxide. For Alloy 182 fusion-weld, tensile property changes after exposure to supercritical-CO{sub 2} environment were negligible.

36 MATERIALS SCIENCE↗

ASSESSMENT OF RESIDUAL STRESSES IN SRS AND HANFORD 3013 INNER AND CONVENIENCE CANS

Chloride stress corrosion cracking (SCC) is a plausible corrosion mechanism for the stainless steel 3013 containers during their lifetime for plutonium material storage if sufficient electrolyte is present within the container. Contributing factors for SCC, such as fabrication and welding residual stresses, are present in the 3013 cans. Convenience and inner cans from both Hanford and SRS are made by a flow form process, which cold works the stainless steel during fabrication. Additionally, the inner cans also are sealed at the can top with a closure weld to the sealing plug. Only SRS and Hanford were tested since moisture levels were significant for SCC. As part of the 3013 corrosion plan for FY09, testing in a boiling magnesium chloride solution was performed on actual 3013 convenience and inner cans to determine if the residual stresses were sufficient for the initiation and propagation of SCC. Additional testing in a 40% calcium chloride solution was also performed on 304L stainless steel SCC coupons, i.e. stressed teardrop-shaped samples (teardrops), and an inner can welded top to provide comparative results and to assess the effect of residual stresses in a less aggressive environment. The testing performed under this task consisted of 3013 inner and convenience cans and 304L teardrops exposed to a boiling magnesium chloride solutions per ASTM G36 and a 40% calcium chloride solution at 100 C following the guidance of ASTM G123. Cracking occurred in all can types including the inner can bottom and welded top and the bottoms of the SRS and Hanford convenience cans when exposed to the boiling magnesium chloride solution at 155 C. Cracking occurred at different times indicative of the residual stress levels in the cans. 304L teardrops cracked in the shortest time interval and therefore provide a conservative estimate for can performance. Testing in a 40% calcium chloride solution at 100 C demonstrated that cracking occurs in a less aggressive environment but at significantly longer times than in the boiling magnesium chloride. Vapor space cracking was also found to occur in the inner can welded top exposed over the boiling magnesium chloride solution and on 304L teardrops exposed over a hot calcium chloride solution.

36 MATERIALS SCIENCE↗

Prediction and Monitoring Systems of Creep-Fracture Behavior of 9Cr-1Mo Steels for Teactor Pressure Vessels

A recent workshop on next-generation nuclear plant (NGNP) topics underscored the need for research studies on the creep fracture behavior of two materials under consideration for reactor pressure vessel (RPV) applications: 9Cr-1Mo and SA-5XX steels. This research project will provide a fundamental understanding of creep fracture behavior of modified 9Cr-1Mo steel welds for through modeling and experimentation and will recommend a design for an RPV structural health monitoring system. Following are the specific objectives of this research project: Characterize metallurgical degradation in welded modified 9Cr-1Mo steel resulting from aging processes and creep service conditions; Perform creep tests and characterize the mechanisms of creep fracture process; Quantify how the microstructure degradation controls the creep strength of welded steel specimens; Perform finite element (FE) simulations using polycrystal plasticity to understand how grain texture affects the creep fracture properties of welds; Develop a microstructure-based creep fracture model to estimate RPVs service life; Manufacture small, prototypic, cylindrical pressure vessels, subject them to degradation by aging, and measure their leak rates; Simulate damage evolution in creep specimens by FE analyses; Develop a model that correlates gas leak rates from welded pressure vessels with the amount of microstructural damage; Perform large-scale FE simulations with a realistic microstructure to evaluate RPV performance at elevated temperatures and creep strength; Develop a fracture model for the structural integrity of RPVs subjected to creep loads; and Develop a plan for a non-destructive structural health monitoring technique and damage detection device for RPVs.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Phase Field Modeling of Corrosion for Design of Next-Generation Magnesium-Aluminum Vehicle Joints

In this study, WPI and its partners sought to understand galvanic corrosion in Mg-Al friction stir weld (FSW) joints. Unlike fusion welds, FSW is done in the solid state. This limits (but does not eliminate) the formation of brittle Al-Mg intermetallics, resulting in better joint strength and corrosion resistance. This study aimed to understand corrosion behavior of Mg-Al FSW joints by using a Cahn-Hilliard phase field electrochemistry model based on the work of Pongsaksawad et al. Its context challenge problem was an ultra-light door designed by Magna with 6061-Al sheet outer and ZEK100-Mg sheet inner panels, joined by an adhesive and FSW. Unlike most FSW joints, which weld through the softer material into the harder one, the Al sheet’s hem joint around Mg required the FSW tool to through the harder Al into the softer Mg, which was itself a challenge. Despite this challenge, PNNL succeeded in consistently making very strong FSW lap joints, by using a triflute tool and power control. Characterization showed mostly separate Al and Mg regions in the weld, usually with a hook protruding from Al into Mg, which likely contributed to high joint strength. Nanohardness mapping showed higher hardness in thin Mg swirls into the Al nugget, likely due to the intermetallics. The study used the industry standard SAE J2334 Cyclic Corrosion Test (CCT) to simulate corrosion conditions over the life of a vehicle, as well as linear polarization testing and ASTM G71 pitting corrosion testing. Corrosion reactions were: H 2 O + ½O 2 + 2e - → 2OH - at the Al cathode, and either Mg → Mg 2+ + 2e - or Mg + 2OH - → Mg(OH) 2 + 2e - at the Mg anode, with electron transfer through the joint. Mass loss increased with Al section length, supporting the hypothesis that galvanic corrosion in Al-Mg joints is limited by the cathodic reaction. Both pitting corrosion (first anode reaction) and hydroxide film formation (second reaction) were observed. The J2334 CCT test method was slightly modified, adding a chromium solution cleaning step after each week of corrosion testing, in order to remove Mg oxides and hydroxides and accurately measure mass loss over time. That said, FSW joints treated in this way did not did not exhibit significant reduction in lap shear strength of the joints vs. newly welded samples which had not undergone corrosion. Corrosion appeared to consist mainly of pitting in Mg in a way which did not directly affect the bond between the materials where the joints failed. A Cahn-Hilliard phase field model coupled with electrical potential described the electronically mediated galvanic corrosion electrochemical reactions described above in the four-component Al-Mg-H 2 O-(H 2 O+½O 2 ) system. This 2-D model successfully predicted Mg(OH)₂ formation at the anode in some circumstances, and Mg pitting corrosion in others, and showed the correct electric field directions in both cases. The model predicted Mg pit corrosion depth within a factor of two of measured pits.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Wire-Based Additive Manufacturing of Stainless Steel Components

In this work three different wire-fed additive manufacturing (AM) processes were employed to evaluate differences between laser, arc, and electron beam heat sources used for high-deposition-rate AM on the order of 1 kg/h. Optimum weld and build parameters were developed independently to match the characteristics of each heat source using 308L stainless steel welding wire as the feedstock. Laser-wire AM was made with the lowest energy per unit length of weld and had the best control of the melt pool and surface finish. Wire arc-based AM had an intermediate energy per unit length of weld of approximately 5× that of the laser process, while electron beam wire AM had the highest energy per unit length of weld at approximately 10× that of the laser process. Analysis of the parts that were built included evaluation of mechanical properties and microstructures, and these properties are discussed with respect to the difference in input energy and cooling rates. Results show that all three processes build parts with properties that exceed those of annealed 304L wrought stainless steel. However, significant differences exist between the processes, and the results presented here can be used to help select the best wire-fed process for a given high-deposition-rate application.

36 MATERIALS SCIENCE↗

Factors Affecting the Service-life of HDPE Geomembranes in an LLW Disposal Facility - 19320

The assessment of a suitable maximum allowable strain (MAS) for high density polyethylene (HDPE) geomembranes (GMBs) considered suitable for a proposed low level radioactive waste engineered containment mound with a 550-year design-life is described in the context of the available literature and data in 2018. Consideration is given to both the material properties and the factors contributing to the development of sustained tensile strain in the GMB. The assessment is based on the service-life of the GMB eventually being reached due to stress cracking after depletion of the protective antioxidants to a residual value. With respect to the selection of a GMB with a suitable stress crack resistance (SCR), it is noted that morphological changes can result in a substantial reduction in SCR with time, from the initial just manufactured value (SCRo) to a more representative value (SCRm), as the material tends to a thermodynamically more stable post-manufactured state. Thus, SCRm should be considered more representative of the true SCR of the material than the value obtained from the off-roll material just after manufacture. SCRm of can be estimated by aging the candidate GMBs in liquid at 55 deg. C for 270 days. Considering the potential implications of failure of the textured GMB to be used at this facility, and the potential for repair and replacement if it does fail, it is recommended that a maximum allowable strain (MAS), from all sources, of 3%, 4% and 5% be adopted on the base, side slopes, and cover GMBs, respectively. These maximum allowable strain values were selected considering the nature of the waste to be contained and the design-life that is required; they may be too conservative for some other applications with a much shorter design-life or lower consequence of premature failure. It is also indicated that the most critical locations on the GMB are often the welded seams where GMB panels are joined or repaired. Welds act a stress-raisers (increasing the stress and strain the GMB compared to that on either side of the weld). To minimize the need for patching areas damaged by the removal of samples for destructive tests, it is recommended that destructive tests on welds should generally be restricted to the minimum possible. It is also recommended that the German limits on welded GMB thickness be adopted in construction. Since strains can be significantly increased by failure to construct in accordance with the design drawings and specifications, it is recommended that there be Construction Quality Assurance (CQA) by very experienced personnel with a good knowledge of compacted clay liners, Geosynthetic Clay Liners (GCLs), and GMBs and the facility design, and that there be an experienced individual watching the construction work at all times prior to completion of the liner system. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Mechanical Behavior of Commercially Pure Titanium Weldments at Lower Temperatures

Commercially pure titanium is used for low-temperature applications due to good toughness attributed to single-phase microstructure (α). Electron beam welding (EBW) and gas tungsten arc welding (GTAW) processes have been used for welding two grades of commercially pure titanium (Grade 2 and Grade 4). Martensitic microstructure is found to be finer in the case of EBW joint as compared to GTAW joint due to faster rate of cooling in the former process. Weldments have been characterized to study the mechanical behavior at ambient (298 K) and cryogenic temperatures (20 and 77 K). Strength of weldments increases with the decrease in temperature, which is found to be more prominent in case of Grade 4 titanium as compared to Grade 2. Weld efficiency of Grade 4 is found to be higher at all the temperatures (ambient, 77 and 20 K). However, ultimate tensile strength/yield strength ratio is higher for Grade 2 as compared to Grade 4. % Elongation is found to increase/retained at cryogenic temperatures for Grade 2, and it is found to decrease for Grade 4. Electron backscattered diffraction analysis and transmission electron microscopy of deformed samples confirmed the presence of extensive twinning in Grade 2 and the presence of finer martensitic structure in Grade 4. Fractography analysis of tested specimens revealed the presence of cleavage facets in Grade 4 and dimples in specimens of Grade 2. Higher strength in Grade 4 is attributed to higher oxygen restricting the twin-assisted slip, which is otherwise prominent in Grade 2 titanium.

36 MATERIALS SCIENCE↗

Influence of Austempering Temperature and Time on the Microstructure and Mechanical Properties of Ductile Iron Weldment Using Developed Coated Electrode

Sound welded joints of ductile iron were first made by developing coated electrodes as well as weld procedure. The weldments were then austenitized at 900 °C for 2-h holding time followed by austempering at 300 and 350 °C for three different holding times (1.5, 2 and 2.5 h) at each austempering temperature. The influence of austempering temperature and time on the microstructural and mechanical properties was studied. Microstructural characterization, phase analysis, microhardness and mechanical properties were performed to understand the effect of austempering heat treatment on microstructure, austempering kinetics and mechanical properties of welded joints. In spite of significant variation in microstructures among all the three zones of DI weldment before austempering, the response of both weld metal and HAZ to austempering heat treatment similar to a base metal was noted. However, a significant variation in matrix structures (bainitic ferrite, retained austenite) as well as graphite nodules among the three zones was observed with changing the austempering temperature and holding time. Also, 100% joint efficiency of the welded joints was achieved at both 300 and 350 °C for 2-h holding time. Hardness and charpy impact toughness mostly depended on the volume fraction of retained austenite and carbon content. Based on the results of tensile and charpy impact testing, 350 °C and 2-h holding time could be considered as an optimum austempering condition for ADI weldment.

36 MATERIALS SCIENCE↗