Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “TENSILE STRESS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,441 records · Page 80

Creep Strain and Strain Rate Response of 2219 Al Alloy at High Stress Levels

As a result of high localized plastic deformation experienced during proof testing in an International Space Station connecting module, a study was undertaken to determine the deformation response of a 2219-T851 roll forging. After prestraining 2219-T851 Al specimens to simulate strains observed during the proof testing, creep tests were conducted in the temperature range from ambient temperature to 107 C (225 F) at stress levels approaching the ultimate tensile strength of 2219-T851 Al. Strain-time histories and strain rate responses were examined. The strain rate response was extremely high initially, but decayed rapidly, spanning as much as five orders of magnitude during primary creep. Select specimens were subjected to incremental step loading and exhibited initial creep rates of similar magnitude for each load step. Although the creep rates decreased quickly at all loads, the creep rates dropped faster and reached lower strain rate levels for lower applied loads. The initial creep rate and creep rate decay associated with primary creep were similar for specimens with and without prestrain; however, prestraining (strain hardening) the specimens, as in the aforementioned proof test, resulted in significantly longer creep life.

Taminger, Karen M. B.↗

Design and Manufacturing Considerations for Shockproof and Corrosion-Immune Superelastic Nickel-Titanium Bearings for a Space Station Application

An intermetallic nickel-titanium alloy, 60NiTi (60wt%Ni, 40wt%Ti), is a promising tribological material for space mechanisms. 60NiTi offers a broad combination of physical properties that make it unique among bearing materials. 60NiTi is hard, electrically conductive, highly corrosion resistant, readily machined prior to final heat treatment, easily lubricated and is non-magnetic. It also falls within the class of superelastic alloys and can elastically endure large strains (beyond 5 percent) making it highly resistant to excessive and unexpected (shock) loads. Key material properties and characteristics such as elastic modulus, tensile fracture sensitivity and residual stress behavior, however, differ from conventional alloys such as steel and this significantly affects bearing design and manufacturing. In this paper, the preliminary design and manufacture of ball bearings made from 60NiTi are considered for a highly corrosive, lightly loaded, low speed bearing application found inside the International Space Station s water recycling system. The information presented is expected to help guide more widespread commercialization of this new technology into space mechanism and other applications.

DellaCorte, Christopher↗

The direct-stress fatigue strength of 17S-T aluminum alloy throughout the range from 1/2 to 500,000,000 cycles of stress

Fatigue-test were conducted on six specimens made from 3/4-inch-diameter 17S-T rolled-and-drawn rod for the purpose of obtaining additional data on the fatigue life of the material at stresses up to the static strength. The specimens were tested in direct tension using a stress range from zero to a maximum in tension. A static testing machine was used to apply repeated loads in the case of the first three specimens; the other three specimens were tested in a direct tension-compression fatigue machine. The direct-stress fatigue curve obtained for the material indicates that, in the range of stresses above about two-thirds the tensile strength, the fatigue strength is higher than might be expected by simply extrapolating the ordinary curve of stress plotted against the number of cycles determined at lower stresses.

Hartmann, E C↗

A plane strain analysis of the blunted crack tip using small strain deformation plasticity theory

A deformation plasticity analysis of the tip region of a blunted crack in plane strain is presented. The power hardening material is incompressible both elastically and plastically, in order to simulate behavior of a stress freezing material above critical temperature. Stress and displacement fields surrounding the crack tip are presented. The results indicate that the maximum stress seen at the crack tip is indeed limited and is determined by the tensile properties; however, the scale over which the stresses act is dependent on the loading. Comparisons are good between the forward crack tip displacement and micro-fractographic measurments of stretch zones observed in plane strain fracture toughness tests.

Mcgowan, J. J.↗

Tensile Creep of Polycrystalline Near-Stoichiometric NiAl

Long term tensile creep studies were conducted on binary NiAl in the temperature range 700-1200 K with the objectives of characterizing and understanding the creep mechanisms. Inverse and normal primary creep curves were observed depending on stress and temperature. It was concluded that the creep of NiAl is limited by dislocation mobility. The stress exponent for creep, n, increased from 5.5 at 1200 K to 13.9 at 700 K. The true activation energy for creep, Qc, was constant and equal to about 400 kJ per mole between 20 and 50 MPa but decreased to a constant value of 250 kJ per mole between 50 and 110 MPa. The activation energy was observed to be stress dependent above 110 MPa. The tensile creep results reported in this investigation were compared with compression creep data reported in the literature. A detailed discussion of the probable dislocation creep mechanisms governing compressive and tensile creep of NiAl is presented. It is concluded that the non-conservative motion of jogs on screw dislocations influenced the nature of the primary creep curves, where the climb of these jogs involves either the next nearest neighbor or the six-jump cycle vacancy diffusion mechanism. The probable nature of the atom vacancy exchange that occur within the core of an edge dislocation undergoing climb in NiAl are schematically examined.

Raj, Sai V.↗

Internal Stresses in Laminated Construction

This report reviews the procedure employed in an investigation of the sources and influence of internal stresses in laminated construction, and discusses the influence of shrinkage and swelling stresses caused by atmospheric conditions upon the tensile strength across grain in laminated construction with special reference to airplane propellers. The investigation covered three sources of internal stress, namely, the combination of plain-sawed and quarter-sawed material in the same construction, the gluing together of laminations of different moisture contents, and the gluing together of laminations of different densities. Glued specimens and free specimens, made up under various manufacturing conditions, were subjected to various climatic changes inducing internal stresses and then were tested.

Heim, A L↗

Characterization of SiC/SiC Composites Subjected to Sequential Tensile Creep and Dwell Fatigue in Air under Thermal Gradient Conditions

Uncoated SiC/SiC composites, with 2D and 3D fiber architectures, were investigated under steady state thermal gradient conditions with sequential tensile creep and dwell fatigue. Melt infiltration (MI), chemical vapor infiltration (CVI), polymer impregnation and pyrolysis (PIP), and hybrid (CVI and PIP) techniques were used to fabricate ceramic matrix composites (CMCs) with a 2D balanced fiber architecture. CMCs with 3D fiber weaves were also fabricated using MI and hybrid methods. Steady state through the thickness thermal gradients were generated for the tensile specimens using laser heating on the front (hot side) and forced air cooling on the back (cold side). Hot side and cold side temperatures of 2400 and 2200 °F, respectively, were used for testing CMCs fabricated with the MI process, whereas hot side and cold side temperatures of 2700 and 2400 °F, respectively, were used for CMCs fabricated with CVI, PIP, and hybrid processes. Each CMC specimen was initially tested under tensile creep at 69 MPa (10 ksi) for 80 hours, which was then followed by tensile dwell fatigue testing at a maximum stress of 69 MPa (10 ksi) for another 80 hours for a total of 160 hours. This type of sequential tensile creep followed by tensile dwell fatigue testing was performed to ascertain the integrity of uncoated CMCs under steady state thermal gradient conditions. Tensile creep and dwell fatigue test results, generated under steady state thermal gradient conditions on different types of SiC/SiC composites, are compared with corresponding creep behaviors observed under isothermal conditions to determine the influence of both monotonic creep (static fatigue) and dwell fatigue on accumulated strains and deformation behaviors of the CMCs.

Kalluri, Sreeramesh↗

Wrought FeCrAl alloy (C26M) cladding behavior and burst under simulated loss-of-coolant accident conditions

Cladding burst experiments for FeCrAl cladding were performed in the Severe Accident Test Station facility at Oak Ridge National Laboratory. These experiments were simulated using the BISON fuel performance code to better understand the cladding plastic behavior and failure under simulated loss-of-coolant accident conditions. 3D cladding surface boundary conditions were generated using composite axial and azimuthal profiles from experiment thermocouple data. To improve the simulation analysis capabilities in BISON for cladding burst behavior, new thermal creep, plasticity, and failure stress models specific to C26M, a wrought FeCrAl alloy, were developed and implemented. Initial cladding burst results indicated a general underprediction in the failure temperature of the six cladding burst simulations versus the observed failure temperatures. Close investigation of the experiment timing versus the underlying tensile test data revealed that, compared with the tensile specimens, the cladding tubes did not experience the same long holding time at high temperatures. New tensile tests were performed at high temperatures using a temperature ramp similar to the simulated loss-of-coolant accident experiments. These new tensile curves showed an approximately 80% increase in the ultimate tensile strength of the C26M alloy, indicating that a holding time of 10 min at 700 °C and 800 °C allows annealing to change the material microstructure. Using the updated tensile properties, the burst temperatures and stresses from the simulations showed remarkable agreement with the experimental results. This study was then extended by varying the initial pressure to highlight the burst temperature difference between standard Zircaloy-4 and C26M cladding under equivalent conditions. The results show that C26M has a burst temperature that is approximately 70–130 K greater than that of Zircaloy-4. In conclusion, these modeling predictions can be further improved by collecting high-temperature tensile data for C26M beyond the temperature ranges used in this work.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Room temperature mechanical properties of shuttle thermal protection system materials

Tests were conducted at room temperature to determine the mechanical properties and behavior of materials used for the thermal protection system of the space shuttle. The materials investigated include the LI-900 RSI tiles, the RTV-560 adhesive and the .41 cm (.16 thick) strain isolator pad (SIP). Tensile and compression cyclic loading tests were conducted on the SIP material and stress-strain curves obtained for various proof loads and load cyclic conditioning. Ultimate tensile and shear tests were conducted on the RSI, RTV, and SIP materials. The SIP material exhibits highly nonlinear stress-strain behavior, increased tangent modulus and ultimate tensile strength with increased loading rate, and large short time load relaxation and moderate creep behavior. Proof and cyclic load conditioning of the SIP results in permanent deformation of the material, hysteresis effects, and much higher tensile tangent modulus values at large strains.

Sawyer, J. W.↗

Engineering Prediction of Axial Wellbore Shear Failure Caused by Reservoir Uplift and Subsidence

Injection and production can cause significant regional uplift or settlement. We analytically evaluate the potential for cement-annulus failure in response to injection-induced deformation in a coupled casing/cement/rock poromechanical vertical-well system. Deformation is calculated with respect to the initial near-wellbore stress state, occurring immediately after cement curing. Tensile-failure and shear-failure lengths along this well are predicted using a stress-development-length method. The analytical model is verified by Abaqus modeling. Lastly, a sensitivity analysis identifies critical engineering-well-design parameters for ensuring wellbore-annulus integrity.

58 GEOSCIENCES↗

Measurement of the forming limit stress curve using a multi-axial tube expansion test with a digital image correlation system

A servo-controlled tension-internal pressure testing machine with an optical 3D deformation analysis system (ARAMIS) was used to measure the multi-axial plastic deformation behavior of a high-strength steel sheet for a range of strain from initial yield to fracture. The testing machine is capable of applying arbitrary principal stress or strain paths to a tubular specimen using an electrical, closed-loop servo-control system for axial force and internal pressure. Tubular specimens with an inner diameter of 44.6 mm were fabricated from a high-strength steel sheet with a tensile strength of 590 MPa and a thickness of 1.2 mm by roller bending and laser welding. Several linear and non-linear stress paths in the first quadrant of the stress space were applied to the tubular specimens in order to measure the forming limit curve (FLC) and forming limit stress curve (FLSC) of the as-received test material, in addition to the contours of plastic work and the directions of plastic strain rates. The contours of plastic work and the directions of plastic strain rates measured for the linear stress path experiments were compared with those calculated using selected yield functions in order to identify the most appropriate yield function for the test material. Moreover, a Marciniak-Kuczyński type (M-K) forming limit analysis was performed using the most appropriate yield function. The calculated and measured FLC and FLSC were compared in order to validate the M-K approach. The path-dependence of the FLC and FLSC was also investigated.

97 MATHEMATICS AND COMPUTING↗

Modeling growth of fatigue cracks which originate at rivet holes

When a structural component is subjected to repeated stress cycles, it can fail at stresses which are well below the tensile strength of the material. The processes leading to this failure are termed fatigue. Instances of fatigue failure in aircraft have become an increasing concern. The crack leading to failure often originate at rivet holes and then grow in response to stress cycles which occur during the operation of the aircraft. A necessary step to preventing failures in todays fleet of aging aircraft is to increase the frequency and quality of inspections; steps were already taken in this direction. There is also a need for modeling of fatigue crack growth in the aircraft structures so that improvements in design can be established and predictions of the life of the components can be made. The purpose is to provide a method to accurately predict the growth of fatigue cracks and to use this method to make predictions about the life of aircraft structural components. The method relies on the formulation and numerical solution of a singular integral equation(s) for an arbitrarily shaped crack(s) which propagate in response to the applied loading. Of special interest to the aging aircraft studies are cracks which originate at circular holes (i.e., rivet holes), but other crack geometries can be treated equally as well.

Mear, Mark E.↗

Creep and failure at metal-oxide interfaces

Small-scale bicrystal creep experiments were performed on contacts formed via in situ high-temperature diffusion bonding of metal-oxide interfaces including Ag-ZrO 2 , Pd-ZrO 2 , Pt-ZrO 2 , and Ag-high entropy oxide. This work characterizes deformation and failure at metal-oxide interfaces during mechanical loading. Interfacial sliding can be activated easily, while tensile interfacial creep was not observed at any condition of stress or temperature measured. Plastic strain, instead, localizes within the metal under tensile loading. A variety of mechanisms for plastic strain occur in the metal including lattice dislocation-mediated plasticity, twinning, low-angle grain boundary formation, and low-angle grain boundary creep. Surface and low-angle grain boundary diffusion occur under conditions where no metal-oxide tensile creep is observed, highlighting the significant differences in their interfacial mechanical response. High-temperature interfacial failure occurs when the mean curvature at the contact neck is approximately zero and the applied stresses comparable to brittle fracture stresses. The brittle fracture stresses were measured to be σ ƒ = 180 ± 90 MPa at the Ag-ZrO 2 interface at 225 °C, σ ƒ = 460 ± 160 MPa at the Pd-ZrO 2 interface at 680 °C, and σ ƒ = 640 ± 440 MPa at the Pt-ZrO 2 interface at 1010 °C.

Creep↗

Structure and tensile strength of LaS(1.4)

The tensile strength of LaS(1.4) has been estimated by diametral stress testing at room temperature, 800 and 1300 K. Brittle, tensile-type failures were obtained at all temperatures when the crosshead speed was 0.0021 mm/s; however, a 1300 K test at 0.00085 mm/s produced plastic flow. The microstructure of LaS(1.4) consisted of two phases with beta-La2S3 comprising about 15 vol percent of the structure and gamma-La2S3 the remainder. Because of the limited amount of material available for testing, no correlation between microstructure and mechanical strength could be drawn.

Whittenberger, J. Daniel↗

Microstructures and mechanical properties of Ti-Mo alloys cold-rolled and heat treated

In this study, the microstructures and mechanical properties of Ti-10Mo and Ti-20Mo alloys (mass%) are investigated to assess the potential use in biomedical applications. The microstructures are examined by X-ray diffraction analysis (XRD) and scanning electron microscopy (SEM). The mechanical properties are determined from uniaxial tensile tests. The experimental results indicate that the microstructures and mechanical properties of Ti-Mo alloys are dependent upon the cold rolling, solution heat treatment, and Mo content. The Ti-10Mo alloy exhibits ({alpha}'' + {beta}) and ({beta} + {omega}) phases under the cold rolling (CR) and solution treatment (ST), respectively. By contrast, the Ti-20Mo alloy comprises only {beta} phase under such conditions. The quenched Ti-20Mo alloy has the lowest elastic modulus and CR Ti-20Mo alloy has the highest tensile strength. The quenched Ti-10Mo alloy exhibits the excellent ductility and two-stage yielding from stress-strain curves due to the stress-induced martensite transformation from {beta} to {alpha}'' during tensile deformation. These Ti-Mo alloys exhibit low yield strength and good ductility, and they are more suitable for biomedical applications than the conventional metallic biomaterials from the viewpoint of better mechanical compatibility. The quenched Ti-10Mo alloy has some advantages over the other {beta} binary Ti-Mo alloys for biomedical applications. {beta} type Ti-Mo-Sn alloys are expected to be promising candidates for novel metallic biomaterials. - Highlights: {yields} The microstructures and mechanical properties of Ti-Mo alloys are dependent upon the cold rolling, solution heat treatment, and Mo content. {yields} The quenched Ti-10Mo alloy exhibits the excellent ductility and two-stage yielding due to stress-induced martensite transformation from beta to alpha double prime during tensile deformation. {yields} The Ti-Mo alloys are more suitable for biomedical applications than the conventional metallic biomaterials from the viewpoint of better mechanical compatibility. {yields} The quenched Ti-10Mo alloy has more advantages over the other beta binary Ti-Mo alloys for biomedical applications.

36 MATERIALS SCIENCE↗

Microstructure and residual stress of magnetron sputtered nanocrystalline palladium and palladium gold films on polymer substrates

The authors report the structural properties and residual stresses of 500-nm-thick nanocrystalline Pd and PdAu films on compliant substrates prepared by magnetron sputtering as a function of the pressure of the Ar-sputtering gas. Films were analyzed by x-ray diffraction, cross-sectional transmission electron microscopy, and x-ray photoelectron spectroscopy. At low pressures the metal films exhibit strong compressive stresses, which rapidly change to highly tensile with increasing pressure, and then gradually decrease. Along with this effect a change in microstructure is observed from a dense equiaxed structure at low pressures to distinctive columns with reduced atomic density at the column walls at higher pressures. The preparation of nearly stress-free dense nanocrystalline films is demonstrated.

36 MATERIALS SCIENCE↗

Environmental protection to 922K (1200 F) for titanium alloys

Evaluations are presented of potential coating systems for protection of titanium alloys from hot-salt stress-corrosion up to temperatures of 755 K (900 F) and from oxidation embrittlement up to temperature of 922 K (1200 F). Diffusion type coatings containing Si, Al, Cr, Ni or Fe as single coating elements or in various combinations were evaluated for oxidation protection, hot-salt stress-corrosion (HSSC) resistance, effects on tensile properties, fatigue properties, erosion resistance and ballistic impact resistance on an alpha and beta phase titanium alloy (Ti-6Al-2Sn-4Zr-2Mo). All of the coatings investigated demonstrated excellent oxidation protectiveness, but none of the coatings provided protection from hot-salt stress-corrosion. Experimental results indicated that both the aluminide and silicide types of coatings actually decreased the HSSC resistance of the substrate alloy. The types of coatings which have typically been used for oxidation protection of refractory metals and nickel base superalloys are not suitable for titanium alloys because they increase the susceptibility to hot-salt stress-corrosion, and that entirely new coating concepts must be developed for titanium alloy protection in advanced turbine engines.

Groves, M. T.↗