Soot Oxidation in Laminar Hydrocarbon/Air Diffusion Flames at Atmospheric Pressure

Soot oxidation was studied experimentally in laminar hydrocarbon/air diffusion flames at atmospheric pressure. Measurements were carried out along the axes of round jets burning in coflowing air considering acetylene, ethylene, proplyene and propane as fuels. Measurements were limited to the initial stages of soot oxidation (carbon consumption less than 70%) where soot oxidation mainly occurs at the surface of primary soot particles. The following properties were measured as a function of distance above the burner exit: soot concentrations by deconvoluted laser extinction, soot temperatures by deconvoluted multiline emission, soot structure by thermophoretic sampling and analysis using Transmission Electron Microscopy (TEM), concentrations of stable major gas species (N2, H2O, H2, 02, CO, CO2, CH4, C2H2, C2H4, C2H6, C3H6, and C3H8) by sampling and gas chromatography, concentrations of some radical species (H, OH, O) by the deconvoluted Li/LiOH atomic absorption technique and flow velocities by laser velocimetry. It was found that soot surface oxidation rates are not particularly affected by fuel type for laminar diffusion flames and are described reasonably well by the OH surface oxidation mechanism with a collision efficiency of 0.10, (standard deviation of 0.07) with no significant effect of fuel type in this behavior; these findings are in good agreement with the classical laminar premixed flame measurements of Neoh et al. Finally, direct rates of surface oxidation by O2 were small compared to OH oxidation for present conditions, based on estimated O2 oxidation rates due to Nagle and Strickland-Constable, because soot oxidation was completed near the flame sheet where O2 concentrations were less than 1.2% by volume.

Xu, F.↗

Soot Oxidation in Hydrocarbon/Air Diffusion Flames at Atmospheric Pressure

Soot oxidation was studied experimentally in laminar hydrocarbon/air diffusion flames at atmospheric pressure. Measurements were carried out along the axes of round jets burning in coflowing air considering acetylene, ethylene, propylene and propane as fuels. Measurements were limited to the initial stages of soot oxidation (carbon consumption less than 70%) where soot oxidation mainly occurs at the surface of primary soot particles. The following properties were measured as a function of distance above the burner exit: soot concentrations by deconvoluted laser extinction, soot temperatures by deconvoluted multiline emission, soot structure by thermophoretic sampling and analysis using Transmission Electron Microscopy (TEM), concentrations of stable major gas species (N2, H2O, H2, O2, CO, CO2, CH4, C2H2,C2H4, C2H6, C3H6, and C3H8) by sampling and gas chromatography, concentrations of some radical species (H, OH, O) by the deconvoluted Li/LiOH atomic absorption technique and flow velocities by laser velocimetry. It was found that soot surface oxidation rates are not particularly affected by fuel type for laminar diffusion flames and are described reasonably well by the OH surface oxidation mechanism with a collision efficiency of 0.10, (standard deviation of 0.07) with no significant effect of fuel type in this behavior; these findings are in good agreement with the classical laminar premixed flame measurements of Neoh et al. Finally, direct rates of surface oxidation by O2 were small compared to OH oxidation for present conditions, based on estimated O2 oxidation rates due to Nagle and Strickland-Constable (1962), because soot oxidation was completed near the flame sheet where O2 concentrations were less than 1.2% by volume.

Xu, F.↗

Parallelized Carbon Oxidation and Surface Recession Model in Direct-Simulation Monte Carlo Code, SPARTA

Ablative thermal protection system (TPS) materials for spacecraft are composites that often consist of a carbon-based reinforcement and a polymeric matrix. During Earth re-entry, they endure high-temperature oxidation and surface recession. Oxidation is an important mechanism for ablation, sometimes leading to the weakening, spallation, or failure of the oxidized fibers at the surface and in the char layer. However, more details are required including accurate material properties of the fiber microstructure, whether the fibers recede homogenously or localized at pits, and the role of pyrolysis outgassing in order to evaluate the role oxidation plays in the degradation and failure mechanisms of these materials. In this work, we demonstrate a parallelizable oxidation-driven ablation model developed for detailed, large-scale simulations in the DSMC code SPARTA. We also develop robust algorithms which handle the conservation of the surface state after an ablation step. Finally, we verify our model for both simple and more complex chemistry as well as microstructures with reaction statistics, oxidation depth calculations, and detailed visualization of oxidation-induced material recession at the microscale.

V Arias↗

Studies of the kinetics and mechanisms of perfluoroether reactions on iron and oxidized iron surfaces

Polymeric perfluoroalkylethers are being considered for use as lubricants in high temperature applications, but have been observed to catalytically decompose in the presence of metals. X-ray photoelectron spectroscopy (XPS) and temperature programmed desorption (TPD) were used to explore the decomposition of three model fluorinated ethers on clean polycrystalline iron surfaces and iron surfaces chemically modified with oxygen. Low temperature adsorption of the model fluorinated ethers on the clean, oxygen modified and oxidized iron surfaces was molecular. Thermally activated defluorination of the three model compounds was observed on the clean iron surface at remarkably low temperatures, 155 K and below, with formation of iron fluoride. Preferential C-F bond scission occurred at the terminal fluoromethoxy, CF3O, of perfluoro-1-methoxy-2-ethoxy ethane and perfluoro-1-methoxy-2-ethoxy propane and at CF3/CF2O of perfluoro-1,3-diethoxy propane. The reactivity of the clean iron toward perfluoroalkylether decomposition when compared to other metals is due to the strength of the iron fluoride bond and the strong electron donating ability of the metallic iron. Chemisorption of an oxygen overlayer lowered the reactivity of the iron surface to the adsorption and decomposition of the three model fluorinated ethers by blocking active sites on the metal surface. Incomplete coverage of the iron surface with chemisorbed oxygen results in a reaction which resembles the defluorination reaction observed on the clean iron surface. Perfluoro-1-methoxy-2-ethoxy ethane reacts on the oxidized iron surface at 138 K, through a Lewis acid assisted cleavage of the carbon oxygen bond, with preferential attack at the terminal fluoromethoxy, CF3O. The oxidized iron surface did not passivate, but became more reactive with time. Perfluoro-1-methoxy-2-ethoxy propane and perfluoro-1,3-diethoxy propane desorbed prior to the observation of decomposition on the oxidized iron surface.

Napier, Mary E.↗

Active Phase on SrCo 1–x Fe x O -δ (0 ≤ x ≤ 0.5) Perovskite for Water Oxidation: Reconstructed Surface versus Remaining Bulk

Perovskite oxides based on earth-abundant transition metals have been extensively explored as promising oxygen evolution reaction (OER) catalysts in alkaline media. The (electro)chemically induced transformation of their initially crystalline surface into an amorphous state has been reported for a few highly active perovskite catalysts. However, little knowledge is available to distinguish the contribution of the amorphized surface from that of the remaining bulk toward the OER. In this work, we utilize the promoting effects of two types of Fe modification, i.e., bulk Fe dopant and Fe ions absorbed from the electrolyte, on the OER activity of SrCoO 3-δ model perovskite to identify the active phase. Transmission electron microscopy and X-ray photoelectron spectroscopy confirmed the surface amorphization of SrCoO 3-δ as well as SrCo 0.8 Fe 0.2 O 3-δ after potential cycling in Fe-free KOH solution. By further cycling in Fe-spiked electrolyte, Fe was incorporated into the amorphized surface of SrCoO 3-δ (SrCoO 3-δ + Fe 3+ ), yielding approximately sixfold increase in activity. Despite the difference in remaining perovskites, SrCoO 3-δ + Fe 3+ and SrCo 0.8 Fe 0.2 O 3-δ exhibited remarkably similar activity. These results reflect that the in situ developed surface species are directly responsible for the measured OER activity, whereas the remaining bulk phases have little impact.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

dynamics of organic-mineral interactions at the metal oxide-solution interface as studied via binding energetics (Final report)

This project focused on addressing longstanding fundamental and experimental uncertainties on how dissolved organic substances (DOS) interact with metal oxide surface under environmentally relevant conditions. By leveraging a custom-built real-time, in-tandem flow adsorption microcalorimetry-UV-Vis/fluorescence spectroscopy platform, we characterized the binding energetics, kinetics and mechanistic pathways driving DOS-metal oxide interactions at temporal resolution on the order of 1-5 seconds. We studied a diverse suite of model organic compounds/substances – including monocarboxylates (e.g. acetate and benzoate), di-carboxylates (oxalate and succinate), amino acids, amino-based nanparticles and natural organic matter – interacting at the mineral-water interface of structurally- and/or chemically distinct metal oxides (including SiO2, boehmite, ferrihydrite, and γ-Al2O3). Our results indicated that DOS-metal oxide interactions are governed by multi-step reaction pathways, often switching between distinct, resolvable enthalpy- and entropy-driven non-electrostatic or electrostatic configurations. To quantify these interactions, we developed and implemented an analytical workflow that integrates peak deconvolution and Monte-Carlo based error propagation to determine site-specific thermodynamic and kinetic parameters for individual binding/debinding events. In addition to resolving apparent first-order rate constants of each event, we were able to quantify associated apparent equilibrium constants as well as free energy, enthalpy and entropy contribution to the activation and subsequent progression of the binding/debinding process across compounds, compound class and metal oxide surfaces. The kinetic-thermodynamic data produced in this study captured how the interplay between oxide surface reactivity and DOS molecular structure jointly drives binding-debinding dynamics. Notably, that at pH below PZC of the oxide surface, neutral species were heavily involved in monocarboxylate binding, while anionic species drove dicarboxylate binding. Also, that among amino acids 1) positional isomers show distinctive binding characteristics to each other while enantiomers show no significant differences in binding characteristics, 2) molecules that bind via outer-sphere complexation show a larger entropic shift between binding and debinding with no impact on oxide surface while 3) inner-sphere interactions increased anion exchange capacity of the oxide surface. The new insights and data from this work has great potential for improving predictive modeling of carbon dynamics and specifically organic-mineral interactions in environmental and industrial systems.

54 ENVIRONMENTAL SCIENCES↗

Unraveling Electronic Trends in O* and OH* Surface Adsorption in the MO 2 Transition-Metal Oxide Series

Understanding the bond strength of O* and OH* intermediates to metal-oxide surfaces is key to predicting the catalytic activity in oxygen-based electrochemistry. Here, we uncover highly non-linear trends in O* and OH* adsorption energies across the 3d, 4d, and 5d series of MO 2 transition-metal (TM) oxide surfaces computed within Hubbard- U corrected density functional theory (DFT + U ). Investigating the electronic structure with crystal orbital Hamiltonian populations (COHP) of the relevant metal–oxygen bonds reveals that the spin-dependent coupling strength between metal-d and oxygen-2p atomic orbitals together with the extent of filling of bonding and anti-bonding orbitals are the primary contributors to the adsorption energy. Importantly, we show that the integrated COHP obtained purely from bulk calculations is a highly accurate descriptor for surface adsorption energetics that captures trends across the group 5–12 TM oxide series within 0.19–0.36 eV. Our results suggest a pathway to prediction of adsorption energies for an arbitrary metal–ligand catalyst system.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Tailoring the Physicochemical Properties of Nb Thin Films via Surface Engineering Methods

The modification of surface oxide layers formed on niobium (Nb) thin films via chemical mechanical planarization (CMP) and accelerated neutral atom beam (ANAB) processing provides a promising route toward tailoring their emergent properties and performance when used as superconducting qubits. Here, in this study, we show that CMP- and ANAB-formed Nb oxides are significantly thinner and smoother than the native oxide, as revealed by transmission electron microscopy (TEM) and atomic force microscopy. Scanning TEM and energy-dispersive X-ray spectroscopy along with X-ray photoelectron spectroscopy identified an oxidation gradient within the native and surface-engineered oxides. The topside layer is dominated by Nb 5+ (Nb 2 O 5 ), with various Nb suboxides present closer to the oxide/metal interface. Time-of-flight secondary ion mass spectrometry (ToF-SIMS) depth profiling confirmed the presence of an oxygen content gradient and demonstrated the enhanced resistance of the CMP- and ANAB-formed oxides to oxygen surface exchange and subsequent diffusion via 18 O 2 isotopic labeling experiments. ToF-SIMS also identified an interfacial layer containing trapped hydrogen (H)-containing species at the Nb oxide/metal interface. In situ ToF-SIMS and TEM revealed migration of the H/OH interfacial layer coinciding with decomposition of the surface oxide. Furthermore, our density functional theory calculations indicated that both H from moisture present in ambient air and bulk H in Nb films tend to segregate at the interface. These findings underscore the importance of understanding surface oxidation mechanisms, hydrogen incorporation, and their impact on the designed functionalities of Nb-based devices.

36 MATERIALS SCIENCE↗

Mineral surface-catalyzed oxidation of Mn(II) by bromate: Implications for the occurrence of Mn oxides on Mars

The occurrence of manganese (Mn) oxides on Mars is believed to be an indicator of an O 2 -rich paleoenvironment of Mars because Mn oxides often form through the oxidation of Mn(II) by O 2 on the surface of Earth. An alternative formation pathway was recently proposed, in which Mn(II) is oxidized by bromate (BrO 3 - ), a common oxidant in contemporary Martian regolith. However, the oxidation of Mn(II) by bromate in solution is kinetically controlled and slow unless using very high concentrations (100 mM) of reactants that may be irrelevant to the conditions of Mars. We conducted laboratory simulations to determine whether iron (Fe) oxides (hematite and goethite) and a phyllosilicate (montmorillonite), abundant minerals on the surface of Mars, could catalyze the oxidation of Mn(II) by bromate. Hematite and goethite, but not montmorillonite, dramatically accelerated the oxidation with a low concentration (1 mM) of Mn(II) and bromate under various solution conditions. Further, the reaction system was autocatalytic with Fe oxides initiating the oxidation of Mn(II) at the early stage and the subsequent catalysis mainly provided by the Mn oxide products. In contrast to producing Mn(IV)O 2 only during the homogeneous oxidation of Mn(II) by bromate in solutions, the heterogeneous mineral-surface catalyzed oxidation resulted in a mixture of Mn(III)OOH and Mn(IV)O 2 phases. Mn(III)OOH was an intermediate product and can be further oxidized by bromate to Mn(IV)O 2 . The occurrence and accumulation of the intermediate product MnOOH can be attributed to its rapid formation due to surface-enhanced nucleation and growth on Fe oxide surfaces and to its higher resistance to oxidation by bromate than Mn(III) ions or clusters. Overall, mineralsurface catalyzed oxidation of Mn(II) by bromate is favorable from both thermodynamic and kinetic perspectives, and can be a major pathway for the occurrence of Mn oxides on Mars where microorganisms are lacking to catalyze the reaction. Our study further improves our understanding of the thermodynamic and kinetic controls on Mn(II) oxidation.

54 ENVIRONMENTAL SCIENCES↗

Deformation band corrosion as a result of applied stress and cold-work in 304 stainless steel in simulated pressurized water reactor primary water conditions

Stainless steels like 304SS are commonly used in pressurized water reactor primary water environments due to their excellent resistance to stress corrosion cracking (SCC). However, SCC susceptibility has been observed in cold-worked 304SS. Cold-rolling introduces a high density of defects, such as deformation bands or dislocations, into the microstructure; applied stress, even if macroscopically below the yield stress, can result in regions with high localized stresses. Cold-worked and non-cold-worked samples were exposed to 360 °C simulated PWR primary water for 1500 h with and without active loading. Corrosion susceptibility of dislocations and deformation bands induced by cold-rolling and/or applied stress was studied using high-resolution (analytical) transmission electron microscopy. Deformation bands were generated in all specimens examined in the study. Penetrative oxidation was observed in some deformation bands in each specimen. The depth of penetrative deformation band oxidation frequently exceeded the depth of grain boundary oxidation in all specimens. However, deformation band oxides generally were narrowly confined to the deformation band plane. Highly Ni-rich regions were observed beyond all oxidation fronts. Surface oxides were thicker in the specimens exposed under active loading. In conclusion, the implications of these findings at surfaces for deformation bands intersecting stress corrosion crack paths are discussed.

EFTEM↗

Synthesis and Surface Attachment of Molecular Re(I) Hydride Species with Silatrane Functionalized Bipyridyl Ligands

Three molecular Re hydrides of the form ( R bpy)Re(CO) 3 H with 2,2′-bipyridine (bpy) ligands containing silatrane functional groups for surface attachment on metal oxide surfaces were synthesized. IR spectroscopy and cyclic voltammetry (CV) demonstrated that the complexes containing the silatrane functional groups have electronic properties similar to those of a control compound, which did not contain functional groups for attachment. Additionally, in a similar fashion to the control compound, the silatrane containing Re hydrides are electrocatalysts for the reduction of CO 2 to CO in solution. The silatrane containing complexes were immobilized on a thin layer of TiO 2 on Si, and the resulting composites were characterized using X-ray photoelectron and IR spectroscopy as well as cyclic voltammetry in the dark and under illumination. Control experiments indicated that the hydride complexes are not stable on the surface and degrade to species which contain a bpy ligand, three CO ligands, and an unknown ligand in the sixth site. Similarly, when one of the silatrane containing Re hydride complexes was immobilized on Si nanoparticles with a thin layer of SiO 2 or silica nanoparticles, the hydride ligand was lost. Density functional theory calculations were used to corroborate the observed behavior of hydride species on a surface. Altogether, this work demonstrates the difficulties associated with attaching well-defined molecular hydride complexes to metal oxide surfaces.

Anions↗

Silver Adsorption on Calcium Niobate(001) Nanosheets: Calorimetric Energies That Explain Sinter-Resistant Support

Metal nanoparticles deposited on oxide supports are essential to many technologies, including catalysts, fuel cells and electronics. Therefore, understanding the chemical bonding strength between metal nanoparticles and oxide surfaces is of great interest. The adsorption energetics, adhesion energy and adsorbate structure of Ag on dehydrated HCa 2 Nb 3 O 10 (001) nanosheets at 300 K have been studied using metal adsorption calorimetry and surface spectroscopies. These dehydrated (“dh”) calcium niobate nanosheets “(dh-HCa 2 Nb 3 O 10 (001))” have stoichiometry Ca 4 Nb 6 O 19 . They impart unusual stability to metal nanoparticles when used as catalyst supports and are easy-to-prepare by Langmuir-Blodgett (LB) techniques, highly ordered, and essentially single-crystal surfaces of mixed oxides with a huge ratio of terrace to edge sites. Below monolayer coverage, Ag grows on dh-HCa 2 Nb 3 O 10 (001) as 2D islands of thickness ~2 layers. The differential heat of Ag adsorption is initially ~303 kJ/mol, increasing slowly to ~338 kJ/mol by 0.8 ML. At higher coverages, Ag atoms mainly add on top of these 2D islands, growing 3D nanoparticles of increasing thickness, as the heat decreases asymptotically towards silver’s heat of sublimation (285 kJ/mol). The adhesion energy of Ag(s) to this Ca niobate surface is estimated to be 4.33 J/m 2 , larger than on any oxide surface previously measured. This explains the sinter resistance reported for metal nanoparticles on this support. Electron transfer from Ag into the calcium niobate is also measured. Furthermore, these results demonstrate an easy way to do singlecrystal-type surface science studies - and especially thermochemical measurements - on the complex surfaces of mixed oxides: using LB-deposited perovskite nanosheets and ultrahigh vacuum annealing in O 2 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Bidentate N‐based Ligands for Highly Reusable, Ligand‐coordinated, Supported Pt Hydrosilylation Catalysts

Abstract A significant challenge in designing supported metal‐ligand catalysts for solution‐phase reactions is the stabilization of the metal active sites against leaching into solution. Here, we examine alkene hydrosilylation reactions as model systems to improve the stability of highly dispersed Pt using a metal‐ligand coordination strategy on high surface area oxide supports. By evaluating a series of bidentate N‐based ligands, we demonstrate several design strategies to improve stability of the highly dispersed Pt 2+ centers against leaching, while maintaining a high level of catalytic activity, selectivity, and recyclability for alkene hydrosilylation batch reactions under mild conditions. These involve a bi‐functional approach to ligand design, which considers interaction to the support and a well‐defined coordination environment for the metal active site. Three strategies are reported: modifying ligands for stronger interaction with oxide surfaces, mixing ligands, and pre‐depositing an “anchoring ligand” to the support before loading the metal‐ligand catalyst. Each of these is successful in enhancing Pt recyclability. Particularly, two Pt‐phenanthroline catalysts exhibit excellent reusability for multiple batch reaction cycles, due to high stability of the active Pt species. Addressing the active site leaching problem significantly enhances the utility of ligand‐coordinated supported metal catalysts as highly stable and selective catalysts for solution‐phase reactions.

Chen, Linxiao↗

The Oxidation of the HiSiMo Cast Irons Alloyed with Cr/Al at 800 °C

To improve the oxidation resistance of cast iron containing Si and Mo (HiSiMo), 1wt.% Cr and 3wt.% Al were added into the base alloy to improve high temperature oxidation resistance for exhaust manifold applications. Oxidation tests were performed in both dry and wet air (air + 10% H 2 O) at 800 °C for 1, 10, 24, and 50 h. The mass change and oxide thickness were measured to evaluate the oxidation resistance. Scanning electron microscopy with energy dispersive X-ray spectroscopy (SEM/EDS) and transmission electron microscopy (TEM) were employed to characterize the oxidized samples. Here, the results showed that the additions of Al or Cr selectively oxidized to form a more oxidation resistant surface oxide layer, which reduced the mass gain during these experiments.

36 MATERIALS SCIENCE↗

A study to investigate the chemical stability of gallium phosphate oxide/gallium arsenide phosphide

The elemental composition with depth into the oxide films was examined using secondary ion mass spectrometry. Results indicate that the layers are arsenic-deficient through the bulk of the oxide and arsenic-rich near both the oxide surface and the oxide-semiconductor interface region. Phosphorus is incorporated into the oxide in an approximately uniform manner. The MIS capacitor structures exhibited deep-depletion characteristics and hysteresis indicative of electron trapping at the oxide-semiconductor interface. Post-oxidation annealing of the films in argon or nitrogen generally results in slightly increased dielectric leakage currents and decreased C-V hysteresis effects, and is associated with arsenic loss at the oxide surface. The results of bias-temperature stress experiments indicate that the major instability effects are due to changes in the electron trapping behavior. No changes were observed in the elemental profiles following electrical stressing, indicating that the grown films are chemically stable under device operating conditions.

Kuhlman, G. J.↗

Improved adherence of T1C coatings to steel

Modified process for RF sputtering of titanium carbide coatings onto 440-C steel has resulted in improved adherence. Small partial pressure of nitrogen, approximately 0.5 percent, during first minutes of deposition markedby improved adherence, friction, and wear properties when compared with coatings applied on sputter-etched surfaces, or oxidized surfaces or in presence of small oxygen partial pressure. X-ray photoelectron spectroscopy and X-ray diffraction were used to characterize resultant coatings.

Brainard, W. A.↗

Effect of Applied Stress on the Selective Oxidation of Alloy 600 Exposed to PWR Primary Water and Rhines Pack Environments

A mechanistic understanding of corrosion and oxidation processes is crucial to ensure long-term resistance to stress corrosion cracking of Ni-base structural alloys in pressurized water reactor (PWR) primary and secondary systems. Aqueous corrosion of Ni-base alloys under PWR primary water conditions was previously compared to gaseous oxidation with comparable oxygen potentials. However, those studies considered only stress-free conditions, which removes a critical parameter for understanding stress corrosion behaviors. A significant knowledge gap exists for the role of applied stresses on selective internal oxidation in gaseous environments. A micro-4-point-bend jig was designed to facilitate stress in a Rhines Pack set-up. Selective oxidation at different stress and strain conditions was investigated in a series of Rhines Pack experiments for Alloy 600. Focused ion beam milling enabled the extraction of site-specific specimens containing selected high-energy grain boundaries from tensile and compressive stress regions. Analytical transmission electron microscopy was employed to analyze the microstructure and chemical composition of the resulting oxides. Protective surface oxide films and selective intergranular oxides were observed at different conditions. The implications of these fundamental differences are discussed relative to intergranular attack and stress corrosion cracking mechanisms in PWR primary water.

stress, 4-point-bend, selective oxidation, Alloy 6↗

Grain boundary oxidation and an analysis of the effects of pre-oxidation on subsequent fatigue life

The effects of preoxidation on subsequent fatigue life were studied. Surface oxidation and grain boundary oxidation of a nickel-base superalloy (TAZ-8A) were studied at 600 to 1000 C for 10 to 1000 hours in air. Surface oxides were identified and the kinetics of surface oxidation was discussed. Grain boundary oxide penetration and morphology were studied. Pancake type grain boundary oxide penetrates deeper and its size is larger, therefore, it is more detrimental to fatigue life than cone-type grain boundary oxide. Oxide penetration depth, a (sub m), is related to oxidation temperature, T, and exposure time, t, by an empirical relation of the Arrhenius type. Effects of T and t on statistical variation of a (sub m) were analyzed according to the Weibull distribution function. Once the oxide is cracked, it serves as a fatigue crack nucleus. Statistical variation of the remaining fatigue life, after the formation of an oxide crack of a critical length, is related directly to the statistical variation of grain boundary oxide penetration depth.