Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “etching”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Defect formation during chlorine-based dry etching and their effects on the electronic and structural properties of InP/InAsP quantum wells

The general objective is the investigation of the defects formed by dry etching tools such as those involved in the fabrication of photonic devices with III–V semiconductors. Emphasis is put on plasma exposures with chlorine-based chemistries. In addition to identifying these defects and describing their effects on the electro-optic and structural properties, the long-term target would be to predict the impact on the parameters of importance for photonic devices, and possibly include these predictions in their design. The work is first centered on explaining the experimental methodology. This methodology starts with the design and growth of a quantum well structure on indium phosphide, including ternary indium arsenide/phosphide quantum wells with graded arsenic/phosphor composition. These samples have then been characterized by luminescence methods (photo- and cathodoluminescence), high-resolution transmission electron microscopy, and secondary ion mass spectrometry. As one of the parameters of importance in this study, the authors have also included the doping level. The samples have been exposed to the etching plasmas for “short” durations that do not remove completely the quantum wells, but change their optical signature. No masking layer with lithographic features was involved as this work is purely oriented to study the interaction between the plasma and the samples. A significant difference in the luminescence spectra of the as-grown undoped and doped samples is observed. A mechanism describing the effect of the built-in electric field appearing as a consequence of the doping profile is proposed. This mechanism involves quantum confined Stark effect and electric-field induced carrier escape from the quantum wells. In the following part, the effects of exposure to various chlorine-based plasmas were explored. Differences are again observed between the undoped and doped samples, especially for chemistries containing silicon tetrachloride. Secondary ion mass spectrometry indicates penetration of chlorine in the structures. Transmission electron microscopy is used to characterize the quantum well structure before and after plasma bombardment. By examining carefully the luminescence spectral properties, the authors could demonstrate the influence of the etching plasmas on the built-in electric field (in the case of doped samples), and relate it to some ionic species penetrating the structures. Etching plasmas involving both chlorine and nitrogen have also been studied. The etching rate for these chemistries is much slower than for some of the silicon tetrachloride based chemistries. Their effects on the samples are also very different, showing much reduced effect on the built-in electric field (for the doped samples), but significant blue-shifts of the luminescence peaks that the authors attributed to the penetration of nitrogen in the structures. Nitrogen, in interstitial locations, induces mechanical compressive stress that accounts for the blue-shifts. Finally, from the comparison between secondary ion mass spectrometry and luminescence spectra, the authors suggest some elements for a general mechanism involved in the etching by chloride-chemistries, in which a competition takes place between the species at the surface, active for the etching mechanism, and the species that penetrate the structure, lost for the etching process, but relevant in terms of impact on the electro-optic and structural features of the exposed materials.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

High temperature isotropic and anisotropic etching of silicon carbide using forming gas

Plasma-etched micropillars in 4H-SiC were etched in forming gas (4% H2, 96% N2) at 1500, 1550, and 1600 °C at 2.4 and 9.4 standard liters per min (slm). At 2.4 slm, oxygen from the aluminum oxide components of the tube furnace oxidized the SiC surface, and the pillars etched isotropically. Additionally, at 9.4 slm, the pillars etched crystallographically at 1500 and 1550 °C, and sharp 4H-SiC needless with tips as narrow as 15 nm were produced. The lateral etch rates of both 4H- and 6H-SiC were measured with the a-plane etching faster than the m-plane at 1500 and 1550 °C. At 1600 °C, the m-plane and a-plane etch at comparable rates. Due to the difference in etch rates between the m-plane and a-plane, convex surfaces tend to produce facets parallel to the a-plane, while concave surfaces produce facets parallel to the m-plane.

42 ENGINEERING↗

HF-based etching processes for improving laser damage resistance of fused silica optical surfaces

The effect of various HF-based etching processes on the laser damage resistance of scratched fused silica surfaces has been investigated. Conventionally polished and subsequently scratched fused silica plates were treated by submerging in various HF-based etchants (HF or NH{sub 4}F:HF at various ratios and concentrations) under different process conditions (e.g., agitation frequencies, etch times, rinse conditions, and environmental cleanliness). Subsequently, the laser damage resistance (at 351 or 355 nm) of the treated surface was measured. The laser damage resistance was found to be strongly process dependent and scaled inversely with scratch width. The etching process was optimized to remove or prevent the presence of identified precursors (chemical impurities, fracture surfaces, and silica-based redeposit) known to lead to laser damage initiation. The redeposit precursor was reduced (and hence the damage threshold was increased) by: (1) increasing the SiF{sub 6}{sup 2-} solubility through reduction in the NH4F concentration and impurity cation impurities, and (2) improving the mass transport of reaction product (SiF{sub 6}{sup 2-}) (using high frequency ultrasonic agitation and excessive spray rinsing) away from the etched surface. A 2D finite element crack-etching and rinsing mass transport model (incorporating diffusion and advection) was used to predict reaction product concentration. The predictions are consistent with the experimentally observed process trends. The laser damage thresholds also increased with etched amount (up to {approx}30 {micro}m), which has been attributed to: (1) etching through lateral cracks where there is poor acid penetration, and (2) increasing the crack opening resulting in increased mass transport rates. With the optimized etch process, laser damage resistance increased dramatically; the average threshold fluence for damage initiation for 30 {micro}m wide scratches increased from 7 to 41 J/cm{sup 2}, and the statistical probability of damage initiation at 12 J/cm{sup 2} of an ensemble of scratches decreased from {approx}100 mm{sup -1} of scratch length to {approx}0.001 mm{sup -1}.

42 ENGINEERING↗

Comparison of the structural and optical properties of porous In{sub 0.08}Ga{sub 0.92}N thin films synthesized by electrochemical etching

This paper presents the structural and optical study of porous (1 µm) In{sub 0.08}Ga{sub 0.92}N synthesized by photoelectrochemical etching under various conditions. Field emission scanning electron microscope and atomic force microscope images showed that the pre-etched thin films have a sufficiently smooth surface over a large region with wurtzite structure. The roughness increased with an increase in etching duration. The blue shift phenomenon was measured for photoluminescence emission peaks at 300 K. The energy band gap increased to be 3.18 and 3.16 eV for post-etched films at ratios of 1:4 and 1:5, respectively. At the same time, the photoluminescence intensities of the post-etched thin films indicated that the optical properties have been enhanced. - Graphical abstract: PL spectra of the as-grown and porous In{sub 0.08}Ga{sub 0.92}N under various etching duration. - Highlights: • Nanoporous structures of In{sub 0.08}Ga{sub 0.92}N. • The roughness of the porous thin films increased with an increase in etching durations. • No phase segregation in XRD pattern. • Blue shifts were observed in the PL spectra of the post-etched films.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Edge-Controlled Growth and Etching of Two-Dimensional GaSe Monolayers

Understanding the atomistic mechanisms governing the growth of two-dimensional (2D) materials is of great importance in guiding the synthesis of wafer-sized, single-crystalline, high-quality 2D crystals and heterostructures. Etching, in many cases regarded as the reverse process of material growth, has been used to study the growth kinetics of graphene. In this paper, we explore a growth–etching–regrowth process of monolayer GaSe crystals, including single-crystalline triangles and irregularly shaped domains formed by merged triangles. We show that the etching begins at a slow rate, creating triangular, truncated triangular, or hexagonally shaped holes that eventually evolve to exclusively triangles that are rotated 60° with respect to the crystalline orientation of the monolayer triangular crystals. The regrowth occurs much faster than etching, reversibly filling the etched holes and then enlarging the size of the monolayer crystals. A theoretical model developed based on kinetic Wulff construction (KWC) theory and density functional theory (DFT) calculations accurately describe the observed morphology evolution of the monolayer GaSe crystals and etched holes during the growth and etching processes, showing that they are governed by the probability of atom attachment/detachment to/from different types of edges with different formation energies of nucleus/dents mediated by chemical potential difference Δμ between Ga and Se. Finally, our growth–etching–regrowth study provides not only guidance to understand the growth mechanisms of 2D binary crystals but also a potential method for the synthesis of large, shape-controllable, high-quality single-crystalline 2D crystals and their lateral heterostructures.

36 MATERIALS SCIENCE↗

In situ and selective area etching of GaN by tertiarybutylchloride (TBCl)

In situ etching (ISE) of gallium nitride (GaN) can enable lateral and vertical junctions through selective area etching (SAE) and regrowth. We report the study of ISE and SAE of GaN using an organometallic precursor, tertiarybutylchloride (TBCl), in a metal-organic chemical vapor deposition reactor. Compared to the conventional etching in hydrogen, the use of TBCl allows in situ etching at a much lower temperature (<850 °C), likely due to a more reactive etchant and a more efficient desorption rate of the etching products. The TBCl etching is near equilibrium and can be significantly changed with the change of the NH3 flow rate. We also report initial results of SAE on SiO 2 patterned GaN samples. An important finding is the need to control the desorption of the reaction products in order to achieve smooth surfaces. TBCl etching is crystallographically anisotropic with low etch rates on N-terminated facets. The use of TBCl and possibly other organometallic halogen precursors is expected to enable the design and implementation of III-nitride lateral junction devices that have not been possible.

42 ENGINEERING↗

Optimization of a chlorine-based deep vertical etch of GaN demonstrating low damage and low roughness

The dry etching of GaN to form deep vertical structures is a critical step in many power device processes. To accomplish this, a chlorine and argon etch is investigated in detail to satisfy several criteria simultaneously such as surface roughness, crystal damage, and etch angle. Etch depths from 2 to 3.4 μm are shown in this paper. The authors investigate the formation of etch pits and its contributing factors. In addition, a nickel hard mask process is presented, with an investigation into the causes of micromasking and a pre-etch to prevent it. The authors show the results of optimized etch conditions resulting in a 2 μm deep, 0.831 nm rms roughness etch, with a 7.6° angle from vertical and low surface damage as measured by photoluminescence.

Tahhan, Maher↗

Highly selective Si 3 N 4 /SiO 2 etching using an NF 3 /N 2 /O 2 /H 2 remote plasma. II. Surface reaction mechanism

Developing processes for highly selective etching of silicon nitride (Si 3 N 4 ) with respect to silicon dioxide (SiO 2 ) is a major priority for semiconductor fabrication processing. In this paper and in Paper I [Volynets et al., J. Vac. Sci. Technol. A 38, 023007 (2020)], mechanisms are discussed for highly selective Si3N4 etching in a remote plasma based on experimental and theoretical investigations. The Si 3 N 4 /SiO 2 etch selectivity of up to 380 was experimentally produced using a remote plasma sustained in NF 3 /N 2 /O 2 /H 2 mixtures. A selectivity strongly depends on the flow rate of H 2 , an effect attributed to the formation of HF molecules in vibrationally excited states that accelerate etching reactions. Based on experimental measurements and zero-dimensional plasma simulations, an analytical etching model was developed for etch rates as a function of process parameters. Reaction rates and sticking coefficients were provided by quantum chemistry models and also fitted to the experimental results. Etch rates from the analytical model show good agreement with the experimental results and demonstrate why certain etchants accelerate or inhibit the etch process. In particular, the modeling shows the important role of HF molecules in the first vibrationally excited state [HF( v = 1)] in achieving high Si 3 N 4 /SiO 2 selectivity.

42 ENGINEERING↗

Plasma enhanced atomic layer deposition and atomic layer etching of gallium oxide using trimethylgallium

Atomic layer etching driven by self-limiting thermal reactions has recently been developed as a highly conformal and isotropic technique for low damage atomic scale material removal by sequential exposures of vapor phase reactants. Gallium oxide (Ga2O3) is currently among the materials of interest due to a large variety of applications including power electronics, solar cells, gas sensors, and photon detectors. In this study, Ga2O3 was deposited by plasma enhanced atomic layer deposition using trimethylgallium [TMG, Ga(CH3)3] and O2 plasma at a substrate temperature of 200 °C. We report a newly developed method for Ga2O3 thermal atomic layer etching, in which surface modification is achieved through HF exposure resulting in a gallium fluoride surface layer, and then removed through volatile product formation via ligand exchange with TMG. Saturation of the precursor exposure at a substrate temperature of 300 °C resulted in an etch rate of 1.0 ± 0.1 Å/cycle for amorphous Ga2O3. Uniformity and conformality of the atomic layer etching process were confirmed via atomic force microscopy with a measured surface roughness of 0.55 ± 0.05 nm that remains unchanged after etching. The use of TMG for etching may expand available precursors for atomic layer etching processes, while allowing for both etching and deposition of Ga2O3 using the same metalorganic precursor.

Hatch, Kevin A. (ORCID:0000000283118623)↗

Future of plasma etching for microelectronics: Challenges and opportunities

Plasma etching is an essential semiconductor manufacturing technology required to enable the current microelectronics industry. Along with lithographic patterning, thin-film formation methods, and others, plasma etching has dynamically evolved to meet the exponentially growing demands of the microelectronics industry that enables modern society. At this time, plasma etching faces a period of unprecedented changes owing to numerous factors, including aggressive transition to three-dimensional (3D) device architectures, process precision approaching atomic-scale critical dimensions, introduction of new materials, fundamental silicon device limits, and parallel evolution of post-CMOS approaches. The vast growth of the microelectronics industry has emphasized its role in addressing major societal challenges, including questions on the sustainability of the associated energy use, semiconductor manufacturing related emissions of greenhouse gases, and others. The goal of this article is to help both define the challenges for plasma etching and point out effective plasma etching technology options that may play essential roles in defining microelectronics manufacturing in the future. The challenges are accompanied by significant new opportunities, including integrating experiments with various computational approaches such as machine learning/artificial intelligence and progress in computational approaches, including the realization of digital twins of physical etch chambers through hybrid/coupled models. These prospects can enable innovative solutions to problems that were not available during the past 50 years of plasma etch development in the microelectronics industry. To elaborate on these perspectives, the present article brings together the views of various experts on the different topics that will shape plasma etching for microelectronics manufacturing of the future.

Engineering↗

DEFECT SELECTIVE ETCHING OF THICK ALN LAYERS GROWN ON 6H-SIC SEEDS - A TRANSMISSION ELECTRON MICROSCOPY STUDY

In the present study, the type and densities of defects in AlN crystals grown on 6H-SiC seeds by the sublimation-recombination method were assessed. The positions of the defects in AlN were first identified by defect selective etching (DSE) in molten NaOH-KOH at 400 C for 2 minutes. Etching produced pits of three different sizes: 1.77 m, 2.35 m , and 2.86 m. The etch pits were either aligned together forming a sub-grain boundary or randomly distributed. The smaller etch pits were either isolated or associated with larger etch pits. After preparing crosssections of the pits by the focused ion beam (FIB) technique, transmission electron microscopy (TEM) was performed to determine which dislocation type (edge, mixed or screw) produced a specific etch pit sizes. Preliminary TEM bright field and dark field study using different zone axes and diffraction vectors indicates an edge dislocation with a Burgers vector 1/3[1120] is associated with the smallest etch pit size.

36 MATERIALS SCIENCE↗

Selected Area Manipulation of MoS 2 via Focused Electron Beam-Induced Etching for Nanoscale Device Editing

Here we demonstrate direct-write patterning of single and multilayer MoS 2 via a focused electron beam-induced etching (FEBIE) process mediated with the XeF 2 precursor. MoS 2 etching is performed at various currents, areal doses, on different substrates, and characterized using scanning electron and atomic force microscopies as well as Raman and photoluminescence spectroscopies. Scanning transmission electron microscopy reveals a sub-40 nm etching resolution and the progression of point defects and lateral etching of the consequent unsaturated bonds. The results confirm that the electron beam-induced etching process is minimally invasive to the underlying material in comparison to ion beam techniques, which damage the subsurface material. Single-layer MoS 2 field-effect transistors are fabricated, and device characteristics are compared for channels that are edited via the selected area etching process. The source–drain current at constant gate and source–drain voltage scale linearly with the edited channel width. Moreover, the mobility of the narrowest channel width decreases, suggesting that backscattered and secondary electrons collaterally affect the periphery of the removed area. Focused electron beam doses on single-layer transistors below the etching threshold were also explored as a means to modify/thin the channel layer. The FEBIE exposures showed demonstrative effects via the transistor transfer characteristics, photoluminescence spectroscopy, and Raman spectroscopy. While strategies to minimize backscattered and secondary electron interactions outside of the scanned regions require further investigation, here, we show that FEBIE is a viable approach for selective nanoscale editing of MoS 2 devices.

36 MATERIALS SCIENCE↗

The Underlying Chemical Mechanism of Selective Chemical Etching in CsPbBr 3 Nanocrystals for Reliably Accessing Near-Unity Emitters

Reliably accessing nanocrystal luminophores with near-unity efficiencies aids in the ability to understand the upper performance limits in optoelectronic applications that require minimal nonradiative losses. Constructing structure-function relationships at the atomic level, while accounting for inevitable defects, allows for the development of robust strategies to achieve near-unity quantum yield luminophores. For CsPbBr 3 perovskite nanocrystals, bromine vacancies leave behind undercoordinated lead atoms that act as traps, limiting the achievable optical performance of the material. Here, we show that selective etching represents a promising path for mitigating the consequences of optical defects in CsPbBr 3 nanocrystals. A mechanistic understanding of the etching reaction is essential for developing strategies to finely control the reaction. We report a study of the selective etching mechanism of CsPbBr3 nanocrystal cubes by controlling the etchant chemical potential. We observe optical absorption and luminescence trajectories while varying the extent and rate of lead removal, removing in some cases up to 75% of the lead from the original nanocrystal ensemble. At modest etchant chemical potentials, the size and shape uniformity of the nanocrystal ensemble improves in addition to the quantum yield, proceeding through a layer-by-layer etching mechanism. Operating with excessively high etchant chemical potentials is detrimental to the overall optical performance as the etching transitions to nonselective, while too low of a chemical potential results in incomplete etching. Through this general approach, we show how to finely control selective etching to consistently access a steady state or chemical stability zone of near-unity quantum yield CsPbBr 3 nanocrystals postsynthetically, suggesting a practical framework to extend this treatment to other perovskite compositions and sizes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization of plasma etching damage on p-type GaN using Schottky diodes

The plasma etching damage in p-type GaN has been characterized. From current-voltage and capacitance-voltage characteristics of Schottky diodes, it was revealed that inductively coupled plasma (ICP) etching causes an increase in series resistance of the Schottky diodes and compensation of acceptors in p-type GaN. We investigated deep levels near the valence band of p-type GaN using current deep level transient spectroscopy (DLTS), and no deep level originating from the ICP etching damage was observed. On the other hand, by capacitance DLTS measurements for n-type GaN, we observed an increase in concentration of a donor-type defect with an activation energy of 0.25 eV after the ICP etching. The origin of this defect would be due to nitrogen vacancies. We also observed this defect by photocapacitance measurements for ICP-etched p-type GaN. For both n- and p-type GaN, we found that the low bias power ICP etching is effective to reduce the concentration of this defect introduced by the high bias power ICP etching.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Dry etching characteristics of amorphous As{sub 2}S{sub 3} film in CHF{sub 3} plasma

The authors describe the dry etching characteristics of amorphous As{sub 2}S{sub 3} films in CHF{sub 3} plasma and the development of an optimized fabrication process for compact waveguides. The observed etching behavior is due to the relative densities of fluorine atoms, polymer precursors, and ions in the plasma which are controlled by the process parameters. In particular, the flow rate of the CHF{sub 3} gas has a significant influence on the etched profile and surface roughness as well as the etch rate of the As{sub 2}S{sub 3}. The profile evolves from isotropic to vertical with the flow rate due to passivation by increasing polymer deposition on the sidewalls. Such passivation also helps achieve smooth sidewalls because it inhibits differential etching between the phases in the inherently phase-separated As{sub 2}S{sub 3} film, which otherwise results in a grainy and rough etched surface. At the highest flow rate, however, excessive polymer deposition occurs and this results in positive-sloped sidewall and grassy etched surface due to micromasking.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

High Speed Si Etching with ClF{sub 3} Cluster Injection

The reactive gas cluster injection process is an etching method that uses a neutral cluster beam without plasma. ClF{sub 3}-Ar neutral cluster was generated and the Si etching characteristics with this beam were investigated. ClF{sub 3} is very high reactive gas. Adiabatic expansion of a high-pressure gas through a conical nozzle is utilized for the formation of cluster beams. The source gas was a mixture of ClF{sub 3}(6%) with Ar (94%). The etching rate increased with source gas pressure nonlinearly, and the etching rate achieved more than 30 {mu}m/min at 0.85 MPa. Although the irradiation energy was very low (<1 eV/atom or molecule), the chemical etching was enhanced with cluster impacts and the cluster bombarded area on the surface was etched selectively. These results indicated that high speed anisotropic etching with low damage can be realized with the ClF{sub 3} cluster injection process.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Charging effect simulation model used in simulations of plasma etching of silicon

Understanding the consequences of local surface charging on the evolving etching profile is a critical challenge in high density plasma etching. Deflection of the positively charged ions in locally varying electric fields can cause profile defects such as notching, bowing, and microtrenching. We have developed a numerical simulation model capturing the influence of the charging effect over the entire course of the etching process. The model is fully integrated into ViPER (Virtual Plasma Etch Reactor)-a full featured plasma processing simulation software developed at Ilmenau University of Technology. As a consequence, we show that local surface charge concurrently evolves with the feature profile to affect the final shape of the etched feature. Using gas chopping (sometimes called time-multiplexed) etch process for experimental validation of the simulation, we show that the model provides excellent fits to the experimental data and both, bowing and notching effects are captured-as long as the evolving profile and surface charge are simultaneously simulated. In addition, this new model explains that surface scallops, characteristic of gas chopping technique, are eroded and often absent in the final feature profile due to surface charging. The model is general and can be applied across many etching chemistries.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Porous silicon formation during Au-catalyzed etching

The formation of “black” nano-textured Si during the Au-catalyzed wet-chemical etch process was investigated with respect to photovoltaic applications. Cross-sectional scanning electron microscopy (SEM) images recorded at different stages of the etch process exhibit an evolution of a two-layer structure, consisting of cone-like Si hillocks covered with a nano-porous Si (np-Si) layer. Optical measurements confirm the presence of a np-Si phase which appears after the first ∼10 s of the etch process and continuously increases with the etch time. Furthermore, the etch process was investigated on Si substrates with different doping levels (∼0.01–100 Ω cm). SEM images show a transition from the two-layer morphology to a structure consisting entirely of np-Si for higher doping levels (<0.1 Ω cm). The experimental results are discussed on the basis of the model of a local electrochemical etch process. A better understanding of the metal-catalyzed etch process facilitates the fabrication of “black” Si on various Si substrates, which is of significant interest for photovoltaic applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗