At least 145 records · Page 8

Space Plasma Testing of High-Voltage Thin-Film Solar Arrays with Protective Coatings

This paper gives an overview of the space plasma test program for thin-film photovoltaics (TFPV) technologies developed at the Air Force Research Laboratory (AFRL). The main objective of this program is to simulate the effects of space plasma characteristic of LEO and MEO environments on TFPV. Two types of TFPV, amorphous silicon (a-Si) and copper-indium-gallium-diselenide (CIGS), coated with two types of thin-film, multifunctional coatings were used for these studies. This paper reports the results of the first phase of this program, namely the results of preliminary electrostatic charging, arcing, dielectric breakdown, and collection current measurements carried out with a series of TFPV exposed to simulated space plasma at the NASA Glenn Plasma Interaction Facility. The experimental data demonstrate that multifunctional coatings developed for this program provide effective protection against the plasma environment while minimizing impact on power generation performance. This effort is part of an ongoing program led by the Space Vehicles Directorate at the AFRL devoted to the development and space qualification of TFPV and their protective coatings.

Tlomak, Pawel↗

Assessment and Control of Spacecraft Charging Risks on the International Space Station

Electrical interactions between the F2 region ionospheric plasma and the 160V photovoltaic (PV) electrical power system on the International Space Station (ISS) can produce floating potentials (FP) on the ISS conducting structure of greater magnitude than are usually observed on spacecraft in low-Earth orbit. Flight through the geomagnetic field also causes magnetic induction charging of ISS conducting structure. Charging processes resulting from interaction of ISS with auroral electrons may also contribute to charging albeit rarely. The magnitude and frequency of occurrence of possibly hazardous charging events depends on the ISS assembly stage (six more 160V PV arrays will be added to ISS), ISS flight configuration, ISS position (latitude and longitude), and the natural variability in the ionospheric flight environment. At present, ISS is equipped with two plasma contactors designed to control ISS FP to within 40 volts of the ambient F2 plasma. The negative-polarity grounding scheme utilized in the ISS 160V power system leads, naturally, to negative values of ISS FP. A negative ISS structural FP leads to application of electrostatic fields across the dielectrics that separate conducting structure from the ambient F2 plasma, thereby enabling dielectric breakdown and arcing. Degradation of some thermal control coatings and noise in electrical systems can result. Continued review and evaluation of the putative charging hazards, as required by the ISS Program Office, revealed that ISS charging could produce a risk of electric shock to the ISS crew during extra vehicular activity. ISS charging risks are being evaluated in ongoing ISS charging measurements and analysis campaigns. The results of ISS charging measurements are combined with a recently developed detailed model of the ISS charging process and an extensive analysis of historical ionospheric variability data, to assess ISS charging risks using Probabilistic Risk Assessment (PRA) methods. The PRA analysis (estimated frequency of occurrence and severity of the charging hazards) are then used to select the hazard control strategy that provides the best overall safety and mission success environment for ISS and the ISS crew. This paper presents: 1) a summary of ISS spacecraft charging analysis, measurements, observations made to date, 2) plans for future ISS spacecraft charging measurement campaigns, and 3) a detailed discussion of the PRA strategy used to assess ISS spacecraft charging risks and select charging hazard control strategies

Koontz, Steve↗

High-Temperature, High-Load-Capacity Radial Magnetic Bearing

A radial heteropolar magnetic bearing capable of operating at a temperature as high as 1,000 F (=540 C) has been developed. This is a prototype of bearings for use in gas turbine engines operating at temperatures and speeds much higher than can be withstood by lubricated rolling-element bearings. It is possible to increase the maximum allowable operating temperatures and speeds of rolling-element bearings by use of cooling-air systems, sophisticated lubrication systems, and rotor-vibration- damping systems that are subsystems of the lubrication systems, but such systems and subsystems are troublesome. In contrast, a properly designed radial magnetic bearing can suspend a rotor without contact, and, hence, without need for lubrication or for cooling. Moreover, a magnetic bearing eliminates the need for a separate damping system, inasmuch as a damping function is typically an integral part of the design of the control system of a magnetic bearing. The present high-temperature radial heteropolar magnetic bearing has a unique combination of four features that contribute to its suitability for the intended application: 1. The wires in its electromagnet coils are covered with an insulating material that does not undergo dielectric breakdown at high temperature and is pliable enough to enable the winding of the wires to small radii. 2. The processes used in winding and potting of the coils yields a packing factor close to 0.7 . a relatively high value that helps in maximizing the magnetic fields generated by the coils for a given supplied current. These processes also make the coils structurally robust. 3. The electromagnets are of a modular C-core design that enables replacement of components and semiautomated winding of coils. 4. The stator is mounted in such a manner as to provide stable support under radial and axial thermal expansion and under a load as large as 1,000 lb (.4.4 kN).

Provenza, Andrew↗

Reliability of High-Voltage Tantalum Capacitors. Parts 3 and 4)

Weibull grading test is a powerful technique that allows selection and reliability rating of solid tantalum capacitors for military and space applications. However, inaccuracies in the existing method and non-adequate acceleration factors can result in significant, up to three orders of magnitude, errors in the calculated failure rate of capacitors. This paper analyzes deficiencies of the existing technique and recommends more accurate method of calculations. A physical model presenting failures of tantalum capacitors as time-dependent-dielectric-breakdown is used to determine voltage and temperature acceleration factors and select adequate Weibull grading test conditions. This model is verified by highly accelerated life testing (HALT) at different temperature and voltage conditions for three types of solid chip tantalum capacitors. It is shown that parameters of the model and acceleration factors can be calculated using a general log-linear relationship for the characteristic life with two stress levels.

Teverovsky, Alexander↗

High-Temperature Switched-Reluctance Electric Motor

An eight-pole radial magnetic bearing has been modified into a switched-reluctance electric motor capable of operating at a speed as high as 8,000 rpm at a temperature as high as 1,000 F (=540 C). The motor (see figure) is an experimental prototype of starter-motor/generator units that have been proposed to be incorporated into advanced gas turbine engines and that could operate without need for lubrication or active cooling. The unique features of this motor are its electromagnet coils and, to some extent, its control software. Heretofore, there has been no commercial-off-the-shelf wire capable of satisfying all of the requirements for fabrication of electromagnet coils capable of operation at temperatures up to 1,000 F (=540 C). The issues addressed in the development of these electromagnet coils included thermal expansion, oxidation, pliability to small bend radii, micro-fretting, dielectric breakdown, tensile strength, potting compound, thermal conduction, and packing factor. For a test, the motor was supported, along with a rotor of 18 lb (.8-kg) mass, 3-in. (.7.6-cm) diameter, 21-in. (.53-cm) length, on bearings packed with high-temperature grease. The motor was located at the mid span of the rotor and wrapped with heaters. The motor stator was instrumented with thermocouples. At the time of reporting the information for this article, the motor had undergone 14 thermal cycles between room temperature and 1,000 F (.540 C) and had accumulated operating time >27.5 hours at 1,000 F (=540 C). The motor-controller hardware includes a personal computer equipped with analog-to-digital input and digital-to-analog output cards. The controller software is a C-language code that implements a switched-reluctance motor-control principle: that is, it causes the coils to be energized in a sequence timed to generate a rotating magnetic flux that creates a torque on a scalloped rotor. The controller can operate in an open- or closed-loop mode. In addition, the software has been modified to enable the simultaneous operation of the prototype motor or another, similar apparatus as both a motor and a magnetic bearing. Combined bearing/motor operation has been demonstrated at room temperature but had not yet been demonstrated at high temperature at the time of reporting the information for this article.

Montague, Gerald↗

Electrostatic Evaluation of the ARES I FTS Antenna Materials

Surface resistivity and volume resistivity data show all the tested non-metallic materials of the Ares I FTS antenna assembly to be insulative. The external materials (White foam, phenolic) should be able to develop a large surface charge density upon tribocharging with ice crystal impingement. Dielectric breakdown tests on the FTS antenna housing materials show that each of the insulative materials are very resistive to electrical breakdown. The thicknesses of these materials in a nominal housing should protect the antenna from direct breakdown from external triboelectric charging potentials. Per data from the Air Force study, a maximum external electric potential in the range of 100kV can be developed on surfaces tribocharged by ice crystal impingement. Testing showed that under operational pressure ranges, this level of exterior voltage can result in a potential of about 6 kV induced on the electrically floating interior antenna vanes. Testing the vanes up to this voltage level showed that electrostatic discharges can occur between the electrically floating vanes and the center, grounded screw heads. Repeated tests with multiple invisible and visible discharges caused only superficial physical damage to the vanes. Fourier analysis of the discharge signals showed that the frequency range of credible discharges would not interfere with the nominal operation of the FTS antenna. However, due to the limited scope, short timetable, and limited funding of this study, a direct measurement of the triboelectric charge that could be generated on the Ares I antenna housing when the rocket traverses an ice cloud at supersonic speeds was not performed. Instead, data for the limited Air Force study [3] was used as input for our experiments. The Air Force data used was not collected with a sensor located to provide us with the best approximation at the geometry of the Ares I rocket, namely that of the windshield electrometer, because brush discharges to the metal frame of the windshield periodically depleted any charge accumulated. The configuration of the Ares I antenna assembly does not include any exposed metals in the vicinity and the windshield data could not be used. Since the windshield sensor data was unusable, we decided that the Patch 2 location would provide us with a rough approximation to the Ares I antenna configuration and would give us an indication of the possible charging levels that would develop. This was the data that we used in this study. Whether these charging levels would be of the same order of magnitude as the actual charges developed by the Ares I traversing a cloud with ice particles is at this point unknown. An actual experimental test, requiring the acquisition of additional instrumentation, is strongly advised before a final recommendation can be formulated regarding the safe levels of electrostatic charging on the antenna housing. Thus the results of this study should be considered to be preliminary.

Hogue, Michael D.↗

Characterization of Tantalum Polymer Capacitors

Overview Reviewed data Caution must be taken when accelerating test conditions Data not useful to establish an acceleration model Introduction of new failure mechanism skewing results Evidence of Anti-Wear-Out De-doping of polymer Decreased capacitance Increased ESR Not dielectric breakdown Needs further investigation Further investigation into tantalum polymer capacitor technology Promising acceleration model for Manufacturer A Possibility for use in high-reliability space applications with suitable voltage derating.

Voltage Acceleration↗

Analysis of Weibull Grading Test for Solid Tantalum Capacitors

Weibull grading test is a powerful technique that allows selection and reliability rating of solid tantalum capacitors for military and space applications. However, inaccuracies in the existing method and non-adequate acceleration factors can result in significant, up to three orders of magnitude, errors in the calculated failure rate of capacitors. This paper analyzes deficiencies of the existing technique and recommends more accurate method of calculations. A physical model presenting failures of tantalum capacitors as time-dependent-dielectric-breakdown is used to determine voltage and temperature acceleration factors and select adequate Weibull grading test conditions. This, model is verified by highly accelerated life testing (HALT) at different temperature and voltage conditions for three types of solid chip tantalum capacitors. It is shown that parameters of the model and acceleration factors can be calculated using a general log-linear relationship for the characteristic life with two stress levels.

Teverovsky, Alexander↗

Acceleration Factors for Reliability Assessment of Polymer Tantalum Capacitors

Using polymer tantalum capacitors in Hi-Rel systems requires an assessment of the reliability characteristics of the parts. For this assessment, tantalum capacitors are typically subjected to reliability testing at temperatures and voltages exceeding their specified values, and the failure rate (FR) — or the probability of failure during use conditions — is calculated based on voltage and temperature acceleration factors. In this work, various types and lots of polymer tantalum capacitors have been tested at highly accelerated life test (HALT) conditions and the acceleration factors have been determined using different techniques. It has been shown that the behavior of capacitors under HALT conditions can be described based on the time-dependent dielectric breakdown (TDDB) model, which explains the presence of infant mortality (IM) and wear-out failures using the same failure mechanisms and allows for an assessment of the acceleration factors. The difference in acceleration factors obtained using exponential and power models is discussed. Analysis shows that with proper derating, screening, and qualification testing, the reliability of frameless Hi-Rel COTS polymer tantalum capacitors is adequate for space missions.

Alex Eidelman↗

Acceleration Factors for Reliability Assessment of Polymer Tantalum Capacitors

Using polymer tantalum capacitors in Hi-Rel systems requires an assessment of the reliability characteristics of the parts. For this assessment, tantalum capacitors are typically subjected to reliability testing at temperatures and voltages exceeding their specified values, and the failure rate (FR) — or the probability of failure during use conditions — is calculated based on voltage and temperature acceleration factors. In this work, various types and lots of polymer tantalum capacitors have been tested at highly accelerated life test (HALT) conditions and the acceleration factors have been determined using different techniques. It has been shown that the behavior of capacitors under HALT conditions can be described based on the time-dependent dielectric breakdown (TDDB) model, which explains the presence of infant mortality (IM) and wear-out failures using the same failure mechanisms and allows for an assessment of the acceleration factors. The difference in acceleration factors obtained using exponential and power models is discussed. Analysis shows that with proper derating, screening, and qualification testing, the reliability of frameless Hi-Rel COTS polymer tantalum capacitors is adequate for space missions.

Alex Eidelman↗

Infant Mortality and Wear-Out Failures in Polymer and MnO2 Tantalum Capacitors

Reliability testing of modern tantalum capacitors shows the presence of both types, infant mortality (IM) and wearout (WO) failures. To assure reliable operation, the probability of IM failures should be reduced to below the specified level, and the time of WO inception should be greater than the required useful life of the parts at operation conditions. In this work, several types of MnO2 and polymer cathode tantalum capacitors have been tested at highly accelerated conditions to assess voltage acceleration factors, determine adequate burn-in conditions, and assess the useful life. A modified time dependent dielectric breakdown (TDDB) model has been suggested to explain both types of failure, and a physical mechanism of degradation that is based on migration and reactions of oxygen vacancies explains increase of the defect related, IM failures with the level of stress.

tantalum capacitors↗

Useful Life of Tantalum Capacitors

Currently, the major reliability characteristic of tantalum capacitors is the failure rate, which is a constant used to characterize random failures of electronic components. However, contemporary MnO2 and polymer tantalum capacitors have both infant mortality (IM) and wear-out (WO) failures. This requires assessments of the useful life of the parts that is limited by the time of inception of WO failures that can be determined using an adequate reliability model and results of highly accelerated life testing (HALT). In this presentation, a modified time dependent dielectric breakdown (TDDB) model is used to describe both IM and WO failures during HALT. Specifics of physical processes resulting in degradation and failures in polymer and MnO2 tantalum capacitors are discussed, and the increase of IM failures with the level of stress is explained. The model justifies exponential dependence of the acceleration factors on voltage and predicts higher values of the voltage acceleration constant for IM compared to WO failures.

tantalum capacitors↗

Feasibility of Micro-Multilayer Multifunctional Electrical Insulation (MMEI) System for High Voltage Applications

The newly patented micro-multilayer multifunctional electrical insulation (MMEI) system was developed for future electric aircraft applications which critically require lightweight but high voltage (HV), high temperature, and corona or partial discharge (PD) resistant insulation. During the initial development stages, the concept and practicability of the MMEI system were successfully validated with its exceptionally high dielectric breakdown voltages. The multilayer structures were optimized in terms of material type, individual layer thickness, and overall layer configuration along with potential mechanisms identified for its superior performance. Subsequently, scalability, manufacturability, and commercial applicability of the MMEI system were demonstrated with the 1 meter long, 3-phase HV, high power (HP) bus bar prototypes. Two prototypes, one with the conventional SOA insulation system including Mica sheet and the other with an optimized MMEI, were designed, fabricated, and tested successfully. Both prototypes passed both HiPot and PD tests up to the highest test voltage available, 15 kVAC, although the latter showed a slight increase in PD activities at 12.5 kV. However, the prototype with MMEI was 15% lighter or 12% thinner than the other one. Current efforts to significantly enhance the PD resistance of the MMEI system by employing semiconductive shielding layers, which can be also multifunctional, e.g., electromagnetic interference shielding, moisture blocking, heat dissipation, for various HV applications are also discussed in this paper.

Novel Electrical Insulation↗

Feasibility of Micro-Multilayer Multifunctional Electrical Insulation (MMEI) System for High Voltage Applications

The newly patented micro-multilayer multifunctional electrical insulation (MMEI) system was developed for future electric aircraft applications which critically require lightweight but high voltage (HV), high temperature, and corona or partial discharge (PD) resistant insulation. During the initial development stages, the concept and practicability of the MMEI system were successfully validated with its exceptionally high dielectric breakdown voltages. The multilayer structures were optimized in terms of material type, individual layer thickness, and overall layer configuration along with potential mechanisms identified for its superior performance. Subsequently, scalability, manufacturability, and commercial applicability of the MMEI system were demonstrated with the 1 meter long, 3-phase HV, high power (HP) bus bar prototypes. Two prototypes, one with the conventional SOA insulation system including Mica sheet and the other with an optimized MMEI, were designed, fabricated, and tested successfully. Both prototypes passed both HiPot and PD tests up to the highest test voltage available, 15 kVAC, although the latter showed a slight increase in PD activities at 12.5 kV. However, the prototype with MMEI was 15% lighter or 12% thinner than the other one. Current efforts to significantly enhance the PD resistance of the MMEI system by employing semiconductive shielding layers, which can be also multifunctional, e.g., electromagnetic interference shielding, moisture blocking, heat dissipation, for various HV applications are also discussed in this paper.

Novel Electrical Insulation↗

BACKFLIP: A Comparison of Emerging Non-Fluoropolymer-Based, Co-Extruded PV Backsheets to Industry-Benchmark Technologies

As the photovoltaic (PV) industry is rapidly expanding around the world, there has been an increasing interest in extending the lifespan of PV modules. Concern has also emerged regarding the recyclability of modules and their component materials, including fluoropolymer-based backsheets. Laminated polyethylene-terephthalate (PET) core backsheets have traditionally been used in the PV industry, but new, co-extruded polyolefin (PO) backsheets show promise as an improved alternative. Mini-module and coupon samples of seven different backsheets (made of layers including contemporary PET and fluoropolymers, novel PO, and polyamide (PA) materials) were run through hygrometric- or UV photolytic-accelerated aging to identify and better understand each material’s degradation modes and the backsheets’ field reliability. In addition to the artificial aging, the natural weathering methods used in this study are described. The comprehensive set of chemical, mechanical, and structural characterizations at intermittent read points in this study is presented, including: visual appearance and color; gloss; mechanical tensile testing; I-V performance; electroluminescence (EL) imaging; dielectric breakdown; FTIR-chemical structure; X-ray-polymer structure (WAXS); and DSC-crystalline content. After 4000 h of aging, a strong correlation occurs between initial physical characteristics (mechanical tensile test) and operating performance (EL and I-V characteristics).

41 EE - Solar Energy Technologies Office (EE-4S)↗

BACKFLIP: A Comparison of Emerging Non-Fluoropolymer-Based, Co-Extruded PV Backsheets to Industry-Benchmark Technologies

As the photovoltaic (PV) industry is rapidly expanding around the world, there has been an increasing interest in extending the lifespan of PV modules. Concern has also emerged regarding the recyclability of modules and their component materials, including fluoropolymer-based backsheets. Laminated polyethylene-terephthalate (PET) core backsheets have traditionally been used in the PV industry, but new, co-extruded polyolefin (PO) backsheets show promise as an improved alternative. Mini-module and coupon samples of seven different backsheets (made of layers including contemporary PET and fluoropolymers, novel PO, and polyamide (PA) materials) were run through hygrometric- or UV photolytic-accelerated aging to identify and better understand each material's degradation modes and the backsheets' field reliability. In addition to the artificial aging, the natural weathering methods used in this study are described. The comprehensive set of chemical, mechanical, and structural characterizations at intermittent read points in this study is presented, including: visual appearance and color; gloss; mechanical tensile testing; I-V performance; electroluminescence (EL) imaging; dielectric breakdown; FTIR-chemical structure; X-ray-polymer structure (WAXS); and DSC-crystalline content. After 4000 h of aging, a strong correlation occurs between initial physical characteristics (mechanical tensile test) and operating performance (EL and I-V characteristics). This presentation focuses on gloss, FTIR, and breakdown voltage measurements. Results for MiMo power, grayness from EL imaging, optical micrscopy, and specimen morphology (on extraction when cut from MiMos) is also presented.

backsheet↗

Higher Harmonics in Multipactor Induced Plasma Ionization Breakdown near a Dielectric Surface

In this Letter, the novel physics of higher harmonic (HH) generation of the normal electric field near a dielectric surface is reported in multipactor induced plasma ionization breakdown, as determined by kinetic particle-in-cell simulations. The observed HH frequency is around ten times the fundamental rf driving frequency, but lower than the electron plasma frequency. A theory is constructed which indicates that stream plasma interaction-induced instability is the mechanism of HH generation in the collisional regime. The HH frequency and its corresponding growth rate of the HH oscillation amplitude from the theory are in good agreement with kinetic particle-in-cell simulations.