At least 145 records · Page 8

Hot Hydrogen Exposure of U x Zr 1-x C y Nuclear Fuel: The Influence of Composition and Density

Refractory carbide nuclear fuel has been one of the most promising fuel candidates for space nuclear propulsion due to its high melting point, temperature stability, and compatibility in a hot hydrogen environment. In this study, U x Zr 1-x C y fuel was produced by means of a carbothermic reduction process in different UC compositions including 5,10, 20, and 30 at.% UC in the fuel compound. The powder feedstock was consolidated via direct current sintering with densities up to 97% of the theoretical density. The samples with different U x Zr 1-x C y compositions were exposed to hot hydrogen at 2600 K for a cumulative time of 300 min. The samples were characterized by SEM, XRD, density, and measured for mass losses. The high-density samples displayed improved performance in hot hydrogen by minimizing porous sites and reducing areas of direct contact with hydrogen gas, leading to reduced mass losses. Variations in sample density proved to induce large changes in mass loss rates, increasing them up to 90%. The compositions with higher UC content reported the largest mass losses in the study. The loss of uranium occurred primarily at the surfaces exposed to the hot hydrogen where changes in the lattice constant confirmed losses exceeding 50% of the initial UC content in higher compositions, specifically to U 0.3 Zr 0.7 C y . XRD analyses revealed the presence of UH 3 in U 0.3 Zr 0.7 C y suggesting that metallic uranium formed inside the sample as a product of carbon losses. High-density U x Zr x-1 C y fuel with UC concentrations at or below 20 at.% UC exhibited stability and negligible density changes in a high temperature hydrogen environment.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Evaluation of high-temperature properties of binary, eutectic Ni-X alloys (X = B, Ca, Ce, La, Y, Zr)

We investigated the high-temperature behavior of binary eutectic nickel-base alloys with low-solubility elements, towards developing alloys with new combinations of structural and functional (e.g. thermal or corrosion) properties. Based on thermodynamic screening, we cast binary near-eutectic Ni-B, Ni-Ca, Ni-Ce, Ni-La, Ni-Y, and Ni-Zr alloys and characterized their microstructure and high-temperature properties. All alloys (except Ni-Ca) contain a fine eutectic microstructure, containing submicron alternating lamellae of γ-Ni and continuous intermetallic phases. The eutectic microstructure did not significantly coarsen at 700°C (except for Ni-B), but measurably coarsened in all alloys at 900°C, most quickly in Ni-B, followed by Ni-Ce, Ni-La, Ni-Y, and Ni-Zr. Coarsening in these alloys occurs by fault migration; diffusion within the intermetallic, and its interfacial energy, likely influence coarsening kinetics. At room-temperature, all alloys possess negligible ductility due to the continuous, brittle intermetallic. At 700 and 900°C, the Ni-Zr alloy showed the best combination of strength and ductility. Oxidation experiments at 900°C on Ni-Zr and Ni-Ce revealed heavy internal oxidation of the continuous intermetallic phase. Overall, the Ni-Zr alloy showed good high-temperature coarsening resistance and strength, though ductility and oxidation resistance require improvement for use in structural applications. Possible routes for improving alloy properties via additive manufacturing are discussed.

Ekaputra, Clement [ORNL] (ORCID:0000000307166479)↗

A high strength Al-2Ni-0.5Zr conductor alloy fabricated via laser powder bed fusion

There is a current need for new aluminum alloy design strategies to target applications requiring high strength and conductivity with reductions in mass. A new lightweight Al-2Ni-0.5Zr (wt. %) conductor alloy was fabricated using laser powder bed fusion. A design of experiments probed the alloy's solidification cracking susceptibility. It was observed that solidification cracking was generally reduced with fast scan speeds, above 1500 mm/s, and smaller hatch spacings. The different cooling rates throughout the melt pool produced a heterogeneous distribution of cellular and equiaxed Al 3 Ni precipitates in the as-printed alloy. Additionally, the rapid solidification characteristic of laser powder bed fusion created a super-saturated Zr solid solution. An aging heat treatment at 375 °C for 24 h imparted strengthening through the precipitation of L1 2 -Al 3 Zr nanoprecipitates, which counteracted the softening caused by the fragmentation and coarsening of Al 3 Ni precipitates. The yield strength increased from 138 MPa in the as-printed condition to 168 MPa after aging, while the ductility remained constant at ∼21%. The aging treatment simultaneously increased the electrical conductivity from 40.8% IACS (International Annealed Copper Standard) to 53.5% IACS. Modeling of the strengthening mechanisms and electrical conductivity contributions rationalized the simultaneous increase in strength and conductivity upon aging. Furthermore, the strengthening efficacy of the Al 3 Ni and L1 2 -Al 3 Zr precipitates, combined with the low Ni and Zr solubility in the FCC Al matrix, facilitated both high strength and electrical conductivity. Overall, the combination of strength and electrical conductivity positions this alloy as a suitable choice for additively manufactured lightweight conductors.

Additive manufacturing↗

From Cation Order to Disorder: Unlocking Ion Transport Pathways in Li–Zn–Zr–Cl Halospinels

Lithium metal chloride halospinels of the general formula Li 2 MCl 4 are a promising class of earth-abundant ion conductors for all-solid-state batteries. However, poor roomtemperature ionic conductivity has historically limited their use in practical applications. Here, we substitute Zr 4+ into Li 2 ZnCl 4 along the series Li 2−2x/3 Zn 1−x Zr 2x/3 Cl 4 (x = 0, 0.1, 0.3, 0.4, 0.6, 0.9, and 1.0) to understand how cation disorder and vacancy tuning impact ion transport in “normal” halospinels. Aliovalent Zr 4+ substitution increases ionic conductivity by nearly 5 orders of magnitude, from 1.320(3) × 10 −9 S cm −1 in Li 2 ZnCl 4 to 6.74(1)× 10 −5 S cm −1 for x = 0.6. Average and local structure characterization through synchrotron X-ray diffraction (SXRD) and neutron pair distribution function (nPDF) analysis reveal that Zr 4+ redistributes the Zn 2+ and Li + sublattices into previously unoccupied interstitial sites, which form new low-energy hopping pathways that facilitate ion transport. We rationalize the dramatic rearrangement of the cation local structure by considering the coordination preferences of the cations and the potential electrostatic penalties incurred by the higher-valent Zr 4+ cations. This work delivers an atomistic understanding of substitution-induced cation disorder and ion transport properties in a new family of earth-abundant halospinels.

Cardoza, Abby M. [Colorado School of Mines, Golden↗

Revisiting the role of Zr doping in Ni-rich layered cathodes for lithium-ion batteries

We report the realization of high performance Ni-rich layered cathodes remains a challenge because of the multiple degradation factors that concurrently operate during battery cycling. In particular, depletion of oxygen charge and consequent lattice oxygen instability at deep charge state accelerate the subsequent chemomechanical degradation mechanisms. Among the proposed methodologies, doping has proven to be effective in enhancing the cathode cycle life by stabilizing the layered structure. Herein, we achieved the electrochemically stabilized Ni-rich LiNi 0.92 Co 0.04 Mn 0.04 O 2 through Zr doping, resulting in a 15% increase of the capacity retention after 100 cycles. In-depth investigations are conducted to unveil the effects of Zr doping on the layered cathode, and in particular, the critical role of Zr doping on the lattice oxygen stability is systematically studied. By combining state-of-the-art magnetometer characterization, X-ray analysis, and first-principles calculation, we reveal that Zr doping positively contributes the to lattice oxygen stability by alleviating the oxygen charge loss at deep charge, thereby improving the cathode electrochemical reversibility. Our findings provide an insight into the Zr doping mechanism and help to design the Ni-rich layered oxides for future applications.

25 ENERGY STORAGE↗

Unveiling the mechanism of the photocatalytic reduction of CO 2 to formate promoted by porphyrinic Zr-based metal–organic frameworks

A complete picture of the reaction mechanism responsible for the photocatalytic reduction of CO 2 into formate promoted by the Zr-based porphyrinic MOF-545 (PCN-222) in acetonitrile/triethanolamine (CH 3 CN/TEOA) solutions is provided for the first time by combining experimental and computational approaches. Firstly, we combined the metalation of the porphyrin linkers and the synthesis under microwave conditions of nano-sized materials (150–200 nm) to reach one of the highest CO 2 RR activities under visible light irradiation reported so far for a MOF-based catalyst in terms of formate production (identified in all cases as the sole product), i.e., 6000 μmol g –1 after 4 h for the NanoMOF-545(Fe). A thorough mechanistic study of CO 2 RR is provided afterwards, which elucidated the respective roles of TEOA, porphyrin linkers and Zr 6 -nodes. Photophysical measurements of both metalated and unmetalated MOFs excluded the prevailing belief of ligand-to-Zr 6 cluster charge-transfer state formation, while bulk photolysis proved that the porphyrinic linkers of the MOF promote the photooxidation of TEOA under catalytic conditions. DFT calculations allowed characterization with atomistic detail of a novel reaction mechanism whereby TEOA˙ radicals generated photochemically at the porphyrinic linkers play the crucial role of transferring a formal hydride to a CO 2 molecule activated on a Zr IV center, which acts as a Lewis acid. Notably, this mechanism backed by additional experimental assays explains the experimental activity trends observed upon metalation, on the basis of the ability of the materials to accomplish the photo-oxidation of TEOA. Here, while elucidating the reaction pathways at work in Zr 6 -based MOFs with chromophore linkers, the findings reported herein pinpoint new mechanistic features capable of rationalizing other light-driven reactions making use of TEOA (or structurally related donors) and ultimately, inspire the bottom-up design of new catalysts and catalytic routes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Elucidation of Ce/Zr ratio effects on the physical properties and catalytic performance of CuO x /Ce y Zr 1− y O 2 catalysts

Although cerium oxide (CeO 2 ) is widely used as a catalyst support, its limited defect sites and surface oxygen vacancy/mobility should be improved. The incorporation of zirconium (Zr) in the cerium (Ce) lattice is shown to increase the number of oxygen vacancies and improve catalytic activity. Using a fixed surface density (SD) of copper (∼2.3 Cu atoms per nm 2 ) as a surface species, the role of the support (Ce y Zr 1−y O 2 (y = 1.0, 0.9, 0.6, 0.5, and 0.0)) and defect site effects in the CO oxidation reaction was investigated. Spectroscopic (e.g., Raman, XRD, XPS) and microscopic (e.g., SEM-EDX, HR-TEM) characterization techniques were applied to evaluate the defect sites, crystallite size, lattice parameters, chemical composition, oxidation states of elements and microstructure of the catalysts. Here, the CO oxidation reaction with varied CO : O 2 ratios (1 : 5, 1 : 1, and 1 : 0.5 (stoichiometric)) was used as a model reaction to describe the relationship between the structure and the catalytic performance of each catalyst. Based on the characterization results of Ce y Zr 1−y O 2 materials, the addition of Zr causes physical and chemical changes to the overall material. The inclusion of Zr into the structure of CeO 2 decreased the overall lattice parameter of the catalyst and increased the number of defect sites. The prepared catalysts were able to reach complete CO conversion (∼100%) at low temperature conditions (<200 °C), each showing varied reaction activity. The difference in CO oxidation activity was then analyzed and related to the structure, wherein Cu loading, surface oxygen vacancies, reduction–oxidation ability, CuO x –support interaction and oxygen mobility in the catalyst were the crucial descriptors.

36 MATERIALS SCIENCE↗

In situ study of microstructure evolution and α → ω phase transition in annealed and pre-deformed Zr under hydrostatic loading

The detailed study of the effect of the initial microstructure on its evolution under hydrostatic compression before, during, and after the irreversible α → ω phase transformation and during pressure release in Zr using in situ x-ray diffraction is presented. Two samples were studied: one is plastically pre-deformed Zr with saturated hardness and the other is annealed. Phase transformation α → ω initiates at lower pressure for a pre-deformed sample but for a volume fraction of ω Zr, c > 0.7, a larger volume fraction is observed for the annealed sample. This implies that the proportionality between the athermal resistance to the transformation and the yield strength in the continuum phase transformation theory is invalid; an advanced version of the theory is outlined. Phenomenological plasticity theory under hydrostatic loading is outlined in terms of microstructural parameters, and plastic strain is estimated. During transformation, the first rule is suggested, i.e., the average domain size, microstrain, and dislocation density in ω Zr for c < 0.8 are functions of the volume fraction, c of ω Zr only, which are independent of the plastic strain tensor prior to transformation and pressure. The microstructure is not inherited during phase transformation. Surprisingly, for the annealed sample, the final dislocation density and the average microstrain after pressure release in the ω phase are larger than for the severely pre-deformed sample. The results suggest that an extended experimental basis is required for the predictive models for the combined pressure-induced phase transformations and microstructure evolutions.

36 MATERIALS SCIENCE↗

Phase diagrams and polarization reversal in nanosized Hf x Zr 1–x O 2–y

To describe the polar properties of nanosized Hf x Zr 1–x O 2–y , we evolve the “effective” Landau–Ginzburg–Devonshire (LGD) model based on the parametrization of the Landau expansion coefficients for polar and antipolar orderings. We have shown that the effective LGD model can predict the influence of screening conditions and size effects on phase diagrams, polarization reversal, and structural properties of nanosized Hf x Zr 1–x O 2–y of various shapes and sizes. To verify the model, we use the available experimental results for Hf x Zr 1–x O 2 thin films and oxygen-deficient HfO2–y nanoparticles prepared under different annealing conditions. X-ray diffraction, which was used to determine the phase composition of the HfO 2–y nanoparticles, revealed the formation of a ferroelectric orthorhombic phase in them. Micro-Raman spectroscopy was used to explore the correlation of lattice dynamics and structural changes that depend on the oxygen vacancy concentration in the HfO 2–y nanoparticles. Since our approach allows us to determine the conditions (shape, sizes, Zr content, and/or oxygen vacancy amount) for which nanosized Hf x Zr 1–x O 2–y are ferroelectric or antiferroelectric, we hope that the obtained results are useful for creation of next generation Si-compatible ferroelectric gate oxide nanomaterials.

36 MATERIALS SCIENCE↗

In-field critical current and pinning mechanisms at 4.2 K of Zr-added REBCO coated conductors

The critical current and pinning mechanisms at 4.2 K have been studied over a magnetic field range of 0–14 T for Zr-added (0, 5 and 15 mol.%) REBa 2 Cu 3 O 7-x (REBCO and RE = rare earth) coated conductors fabricated by advanced metal organic chemical vapor deposition (A-MOCVD). It is found that the (Ba + Zr)/Cu content in Zr-added (5 and 15 mol.%) REBCO affects the critical current at 77 K, 0 T as well as density, continuity and shape of BaZrO 3 (BZO) self-assembled nanocolumns and RE 2 O 3 in-plane precipitates that significantly enhance the pinning force density Fp(H) as well as isotropic pinning landscape at 4.2 K. In addition to bell-shape dependence of critical current density, J c , at 4.2 K with (Ba + Zr)/Cu content we observed an unusual Fp(H) behavior correlated to particular type of pinning centers, morphology and distribution that have been revealed by TEM microstructure analysis. By fitting the Dew–Hughes equation of the pinning force density Fp(H) at 4.2 K we extract the scaling behaviors of the Fp(H) associated with the competition of pinning mechanisms driven by vertically-aligned BZO nanorods and in-plane RE 2 O 3 pinning defects. This result sheds light on approaches towards interactive control of strong and isotropic pinning centers in Zr-added REBa 2 Cu 3 O 7-x (REBCO and RE = rare earth) coated conductors, and especially understanding the correlation between microstructural characteristics and vortex pinning mechanisms at 4.2 K in high magnetic fields.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Pinning Characteristics of Zr and Hf- Added REBCO Coated Conductors Made by Advanced MOCVD in Low-to-High Magnetic Fields

BaMO 3 (M=Zr, Hf) pinning centers introduced in REBa 2 Cu 3 O 7-x (REBCO and RE = rare earth) coated conductors yield superior performance in high magnetic fields. We present the critical current density J c over a temperature range of 4.2-77 K and magnetic fields of 0-14 T (B || c-axis), of 5-15 mol.% Zr- and Hf-added REBCO 4+ μm thick film tapes fabricated by advanced metal organic chemical vapor deposition (A-MOCVD). The morphology of self-assembled BMO nanorods aligned along c-axis is found to be dependent on the Zr/Hf content. We also observe a correlation between the density of RE 2 O 3 in-plane nano-precipitates and the continuity and concentration of BMO nanorods in films of different Ba content. It is found that the (Ba+M)/Cu (M=Zr, Hf) content in REBa 2 Cu 3 O 7-x affects the shape of pinning force density curves over a wide magnetic field range and temperatures below 20 K. Another remarkable observation is the similarity in the critical current properties of Hf and Zr -added REBCO films as function of (Ba+M)/Cu content at intermediate to high range of (Ba+M)/Cu content. As a result, a quantitative analysis of pinning efficiency and correlation with the microstructure of Zr and Hf- added REBCO coated conductors is discussed.

2G high-temperature superconductor (2G-HTS)↗

Microstructure and Hard Magnetic Properties of Sm 1-x Zr x (Fe,Co) 11.3-y Ti 0.7 By Ingots and Thick Melt-Spun Ribbons

Permanent magnets made from Sm(Fe,Co) 12 -based compounds are being actively pursued through nanostructuring and powder metallurgy. This study was aimed at the development of hard magnetic properties in bulk as-cast alloys and in melt-spun alloys for very low wheel speeds. Slower solidification rates and alloying with Zr promote the tetragonal ThMn 12 -type crystal structure, whereas higher solidification rates and alloying with B replace the ThMn 12 structure type with the TbCu 7 structure type. When introduced simultaneously, Zr and B dramatically reduce the alloy solidification rates required for both the refinement of the 1:12 crystallites and their replacement with the 1:7 phase. In bulk arc-melted alloys, this allowed for a microstructure of separated 1:12 crystallites 1–3 μm in size, although, because of the ferromagnetic nature of a minority phase, the coercivity of these fine-grained alloys reached only 0.73 kOe. A moderately accelerated solidification further refined the 1:12 crystallites and increased the coercivity; a Sm 0.7 Zr 0.4 (Fe,Co) 10.8 Ti 0.7 B 0.5 alloy exhibited a coercivity of 1.5 kOe and a maximum energy product of 3.4 MGOe when it was melt-spun into a 0.26-mm-thick ribbon. A more rapid solidification suppressed the 1:12 phase and after annealing at 800–850 °C, the alloys modified with Zr and B developed reasonably high coercivity and maximum energy product even when melt-spun at a wheel speed of 6 m/s. For the above-mentioned alloy, these values were 4.1 kOe and 7.8 MGOe, respectively. Further, a similarly processed very-Sm-lean Sm 0.5 Zr 0.6 (Fe,Co) 10.6 Ti 0.7 B 0.7 alloy exhibited a remanence of 8.8 kG and an energy product of 7.4 MGOe.

36 MATERIALS SCIENCE↗

DISSOLUTION OF SURROGATE U-Zr FUEL USING ALNIFLEX CONDITIONS

Non-aluminum clad spent nuclear fuel (NASNF) stored in L Basin at the Savannah River Site (SRS) is widely varied in fuel composition, design, packaging, and physical condition. The complexity of the NASNF inventory presents significant challenges, and technology development is necessary for successful disposition. One such fuel in the inventory is metallic uranium-zirconium (U-Zr) alloy fuel, the focus of this study. Electrolytic or nitric acid only dissolution of metallic U-Zr alloy can form insoluble zirconium oxide, which results in up to 52% loss of U to insoluble solids, and can be subject to potentially uncontrolled oxidation reactions [1, 2]. The AlNiflex process was determined to be a viable dissolution flowsheet for the U-Zr alloy fuel. Under a narrow set of solution concentrations, a combination of hydrofluoric acid (HF), nitric acid (HNO3), aluminum nitrate (Al(NO3)3), and hexavalent chromium can safely dissolve U-Zr intermetallic alloys, keep Zr soluble, and not significantly corrode stainless steel (SS) vessels [3, 4.

Gogolski, Jarrod M. [Savannah River National Labor↗

A critical analysis of U-Pu-Zr phase transitions using calorimetric, microstructural, and phase equilibria data

Metallic fuels consisting primarily of uranium, plutonium, and zirconium (U-Pu-Zr) are a leading material candidate for fast-spectrum nuclear reactors. Early demonstration programs proved the principle of safe and efficient fast reactor operation, however there is still considerable uncertainty regarding the phase equilibria and microstructural evolution across the ternary composition space. Quantitative phase formation and identification measurements are scarce and often incomplete, with studies reporting either phase transition temperatures or phase identification data, but not both from the same specimens. In this study, we critically compared experimental and calculated phase transition data and correlated with the microstructure and phase characterization data of as-cast and annealed U-Pu-Zr alloys. Differential scanning calorimetry (DSC) was used to measure phase transitions in the subsolidus regions (723−948 K) of three ternary U-Pu-Zr alloys with similar plutonium concentrations but various U/Zr ratios. Due to sluggish kinetics and narrow ranges of phase stability, complex peaks required the use of a Frazier-Suzuki peak fitting algorithm to deconvolute and calculate transition peak temperatures and enthalpies. We also identified trends of phase transition behavior by critically comparing our DSC data with previous phase transition measurements as well as historical and calculated phase equilibrium diagrams. In conclusion, this provides a critical approach for benchmarking and assessing the quality of new U-Pu-Zr phase equilibria data prior to its incorporation into nuclear material databases.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Materials Data on Zr(MnGe)6 by Materials Project

ZrMn6Ge6 crystallizes in the hexagonal P6/mmm space group. The structure is three-dimensional. Zr is bonded to eight Ge atoms to form distorted edge-sharing ZrGe8 hexagonal bipyramids. There are two shorter (2.76 Å) and six longer (2.96 Å) Zr–Ge bond lengths. Mn is bonded in a 12-coordinate geometry to six Ge atoms. There are a spread of Mn–Ge bond distances ranging from 2.51–2.67 Å. There are three inequivalent Ge sites. In the first Ge site, Ge is bonded in a 8-coordinate geometry to one Zr, six equivalent Mn, and one Ge atom. The Ge–Ge bond length is 2.62 Å. In the second Ge site, Ge is bonded in a 12-coordinate geometry to three equivalent Zr and six equivalent Mn atoms. In the third Ge site, Ge is bonded in a 6-coordinate geometry to six equivalent Mn atoms.

36 MATERIALS SCIENCE↗

Materials Data on Zr(Se2Cl3)2 by Materials Project

Zr(SeCl3)2(Se)2 crystallizes in the orthorhombic Pccn space group. The structure is one-dimensional and consists of eight selenium molecules and two Zr(SeCl3)2 ribbons oriented in the (1, 1, 0) direction. In each Zr(SeCl3)2 ribbon, Zr2+ is bonded in an octahedral geometry to six Cl1- atoms. There are two shorter (2.45 Å) and four longer (2.52 Å) Zr–Cl bond lengths. Se1+ is bonded in a bent 120 degrees geometry to two Cl1- atoms. There are one shorter (2.97 Å) and one longer (2.99 Å) Se–Cl bond lengths. There are three inequivalent Cl1- sites. In the first Cl1- site, Cl1- is bonded in a single-bond geometry to one Zr2+ atom. In the second Cl1- site, Cl1- is bonded in a single-bond geometry to one Zr2+ and one Se1+ atom. In the third Cl1- site, Cl1- is bonded in a single-bond geometry to one Zr2+ and one Se1+ atom.

36 MATERIALS SCIENCE↗

Materials Data on Zr(TeCl)6 by Materials Project

Zr(TeCl2)3(Te)3 crystallizes in the orthorhombic Pbcm space group. The structure is one-dimensional and consists of twelve tellurium molecules and two Zr(TeCl2)3 ribbons oriented in the (0, 0, 1) direction. In each Zr(TeCl2)3 ribbon, Zr4+ is bonded in an octahedral geometry to six Cl1- atoms. There are a spread of Zr–Cl bond distances ranging from 2.45–2.53 Å. There are two inequivalent Te+0.33+ sites. In the first Te+0.33+ site, Te+0.33+ is bonded in a water-like geometry to two equivalent Cl1- atoms. Both Te–Cl bond lengths are 3.13 Å. In the second Te+0.33+ site, Te+0.33+ is bonded in a single-bond geometry to one Cl1- atom. The Te–Cl bond length is 3.09 Å. There are four inequivalent Cl1- sites. In the first Cl1- site, Cl1- is bonded in a 2-coordinate geometry to one Zr4+ and one Te+0.33+ atom. In the second Cl1- site, Cl1- is bonded in a single-bond geometry to one Zr4+ atom. In the third Cl1- site, Cl1- is bonded in a single-bond geometry to one Zr4+ atom. In the fourth Cl1- site, Cl1- is bonded in a distorted water-like geometry to one Zr4+ and one Te+0.33+ atom.

36 MATERIALS SCIENCE↗

Materials Data on Zr(Se2Cl3)2 by Materials Project

Zr(SeCl3)2(Se)2 crystallizes in the tetragonal P4_2/ncm space group. The structure is one-dimensional and consists of eight selenium molecules and two Zr(SeCl3)2 ribbons oriented in the (1, 1, 0) direction. In each Zr(SeCl3)2 ribbon, Zr2+ is bonded in an octahedral geometry to six Cl1- atoms. There are two shorter (2.46 Å) and four longer (2.52 Å) Zr–Cl bond lengths. Se1+ is bonded in a bent 120 degrees geometry to two equivalent Cl1- atoms. Both Se–Cl bond lengths are 2.99 Å. There are two inequivalent Cl1- sites. In the first Cl1- site, Cl1- is bonded in a single-bond geometry to one Zr2+ and one Se1+ atom. In the second Cl1- site, Cl1- is bonded in a single-bond geometry to one Zr2+ atom.

36 MATERIALS SCIENCE↗