Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “WEAR”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Chameleon: An Adaptive Wear Balancer for Flash Clusters

NAND flash-based Solid State Devices (SSDs) offer the desirable features of high performance, energy efficiency, and fast growing capacity. Thus, the use of SSDs is increasing in distributed storage systems. A key obstacle in this context is that the natural unbalance in distributed I/O workloads can result in wear imbalance across the SSDs in a distributed setting. This, in turn can have significant impact on the reliability, performance, and lifetime of the storage deployment. Extant load balancers for storage systems do not consider SSD wear imbalance when placing data, as the main design goal of such balancers is to extract higher performance. Consequently, data migration is the only common technique for tackling wear imbalance, where existing data is moved from highly loaded servers to the least loaded ones. In this paper, we explore an innovative holistic approach, Chameleon, that employs data redundancy techniques such as replication and erasure-coding, coupled with endurance-aware write offloading, to mitigate wear level imbalance in distributed SSD-based storage. Chameleon aims to balance the wear among different flash servers while meeting desirable objectives of: extending life of flash servers; improving I/O performance; and avoiding bottlenecks. Evaluation with a 50 node SSD cluster shows that Chameleon reduces the wear distribution deviation by 81% while improving the write performance by up to 33%.

Zhao, Nannan↗

An Analytical Solution for the Initiation and Early Progression of Fretting Wear in Spherical Contacts

Abstract This article derives analytical solutions to calculate the wear volume at the initiation of fretting motion and its early progression over the first few oscillation cycles. The Archard-based model considers a deformable hemisphere that is contact with a deformable flat block. The material pairs investigated are special alloys, the Inconel 617/Incoloy 800H, and Inconel 617/Inconel 617. The analytical study begins with a unidirectional frictional sliding contact, where the local interfacial sliding distance and the nominal sliding distance at the initiation of gross slip are derived. The obtained analytical expressions for unidirectional sliding are then used to derive the corresponding wear volume for the initiation and early progression of gross slip and the wear volume for a general fretting cycle under elastic conditions. These analytical derivations are all verified by the finite element analysis (FEA). The FEA method and the analytical solutions render virtually identical results for both similar and dissimilar material pairs. The effects of plasticity on the wear volume under elastic–plastic conditions are also investigated. It is found that the fretting wear volumes obtained from the FEA simulations, which include plasticity, are close to those obtained from the analytical expressions for purely elastic regimes. All the results are presented in normalized forms, which can be easily generalized and applied to three-dimensional fretting wear of other material pairs.

Engineering↗

Computational Modeling of Graphite Degradation due to Molten Salt Infiltration and Wear

Molten-salt reactors (MSRs) represent a promising next-generation reactor design, with graphite serving as a moderator and/or reflector in several designs. However, due to limited experimental data and operational experience, a technical understanding of the structural integrity of graphite in molten salt environments remains incomplete. This report presents a modeling-based evaluation of graphite degradation in MSR environments, focusing on the effects of salt infiltration in fuel salt-based designs and surface wear in pebble bed reactor designs. The objective of this study is to enhance understanding of the structural integrity challenges posed by these degradation mechanisms and to provide a framework for assessing graphite behavior in MSRs. The first part of the report investigates the phenomenon of molten salt infiltration into graphite. This infiltration occurs when molten salt permeates the interconnected pore structure of the graphite moderator, driven by factors such as pressure differentials and the physical properties of both the salt and graphite. The infiltration process is influenced by characteristics of the pore structure, viscosity of the molten salt, and the interfacial energies between the graphite, salt, and the atmosphere within the graphite pore. Utilizing a coupled multiphysics modeling approach with Grizzly software, the study evaluates the stress induced by internal heat sources due to infiltration, which can lead to structural concerns. This evaluation is crucial for understanding how infiltration affects the mechanical integrity of graphite components in MSRs. The study considers the Molten-Salt Reactor Experiment (MSRE) graphite stringer geometry due to the availability of relevant data. Through detailed finite element analysis, the study examines stress distributions at varying infiltration percentages, revealing that stress levels increase with higher amounts of infiltration. Rare-event simulations, using the parallel subset simulation (PSS) framework, further quantify the failure probabilities under input uncertainties, with a user-specified failure metric. The PSS framework also identifies critical input parameters that significantly affect the stress values, including infiltration amount, thermal conductivity, and power density. Additionally, considering realistic reactor scenarios, the analysis was performed to account for the combined effects of radiation and infiltration, and modeling strategies on how to analyze new reactor designs or new graphite grades are discussed. The second part of the report focuses on wear mechanisms in pebble bed-based MSRs. As graphite fuel pebbles interact with the graphite reflector block, wear can result in material loss and the formation of surface defects, which may act as stress concentrators. A similar multiphysics modeling framework is employed to assess the impact of wear on the structural integrity of graphite components. This study considers a generic fluoride-cooled high-temperature reactor (gFHR) design due to the availability of comprehensive data. Worst-case scenario dimensions of the reflector blocks were analyzed under thermal and radiation conditions. Subsequently, wear in the form of idealized pits and grooves is modeled on the inner surface of the graphite block, with the maximum stress from previous simulations. The simulations show that groove-type defects are more detrimental than pits, leading to higher stress concentrations. Considering worst-case simulation scenarios and experimental wear rates, it was determined that the formation of a surface defect critical enough to affect the stress may not be possible in a gFHR design. Overall, the findings of this research contribute to the development of robust modeling tools for predicting graphite behavior under various operational conditions in MSRs.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Role of plastic deformation in wear of copper and copper - 10-percent-aluminum alloy in cryogenic fuels

High-purity copper specimens and a copper-aluminum (10%) alloy specimen were subjected to sliding against Type 440 C in cryogenic fuel environments. It was found that virtually all wear occurred by the plastic deformation of a recrystallized layer extending to about 10 micrometers below the wear scar surface of the copper or copper alloy. The wear debris was in the form of a layered structure adhering to the exit region of the wear scar. Measurements on the high purity copper specimens indicated that the wear rate was proportional to the applied load and to the sliding velocity squared. A physical model of the wear process is proposed to account for these observations.

Bill, R. C.↗

Polyimide film wear: Effect of temperature and atmosphere

Friction and wear experiments conducted on polyimide films bonded to 440C stainless steel disks indicated that a wear transition (from high wear to low wear) accompanied a friction transition (from high friction to low friction). In dry argon or dry air (less than 20 ppm H2O), the transition was found to occur at 40 plus or minus 10 C; when H20 was present in air (10,000 ppm H2O), the transition was found to be elevated to a temperature between 100 and 200 C. Wear rate calculations made at 25, 100, and 200 C indicated that film wear was relatively constant for particular experimental conditions; however, the rate was strongly dependent on temperature and atmosphere.

Fusaro, R. L.↗

Effect of atmosphere and temperature on wear, friction, and transfer of polyimide films

Friction and wear experiments conducted on polyimide films bonded to 440C stainless steel disks indicated that a wear transition (from high wear to low wear) accompanied the friction transition (from high friction to low friction). The transition was found to be atmosphere dependent as well as temperature dependent. Wear rate calculations indicated that at temperatures above the transition, wear could be up to 600 times less than at temperatures below the transition. Transfer to metallic riders was also investigated and found to be considerably different at temperatures above and below the transition.

Fusaro, R. L.↗

Studies of friction and wear characteristics of various wires for wire-brush skids

The friction and wear characteristics of 22 types and sizes of wires for potential use in wire-brush skids were studied. These characteristics were determined by placing brushes made from candidate wires on a belt sander whose moving belt simulated landing roll-out distance. At the same time, the drag force and wear behavior were monitored. Data were obtained over distances up to 3048 m (10,000 ft) at preselected bearing pressures of 172 to 1034 kPa (25 to 150 psi). In general, the friction coefficient developed by the candidate wires was found to be independent of bearing pressure and ranged between 0.4 and 0.6 under the test conditions of this investigation. The friction coefficient was not degraded when the surface was wetted and appears to be independent of wire diameter except perhaps when wire size is relatively large compared with the surface asperities. Generally, the high friction demonstrated by the soft materials was accompanied by high wear rates; conversely, the hard materials provided greater wear resistance but offered lower friction. For all test wires, the wear was shown to increase with increasing bearing pressure, in general, for the same bearing pressure, wear increased with increasing wire diameter and decreased when the surface was wetted.

Dreher, R. C.↗

Effect of atmosphere and temperature on wear, friction, and transfer of polyimide films

Friction and wear experiments conducted on polyimide films bonded to 440 C stainless steel disks indicated that a wear transition (from high wear to low wear) accompanied the friction transition (from high friction to low friction). The transition was found to be atmospheric dependent as well as temperature dependent. Wear rate calculations indicated that, at temperatures above the transition, wear could be up to 600 times less than at temperatures below the transition. Transfer to metallic riders was also investigated and found to be considerably different at temperatures above and below the transition.

Fusaro, R. L.↗

Fretting wear of iron, nickel, and titanium under varied environmental conditions

Fretting wear experiments were conducted on high purity iron, nickel and titanium in air under conditions of varied humidity and temperature, and in nitrogen. For iron and titanium, maximum fretting occurred at 10 and 30 percent relative humidity respectively. Nickel showed a minimum in fretting wear at about 10 percent relative humidity. With increasing temperature, all three metals initially showed reduced fretting wear, with increasing wear observed as temperatures increased beyond 200-300 C. For titanium, dramatically reduced fretting wear was observed at temperatures above 500 C, relatable to a change in oxidation kinetics. All three metals showed much less fretting wear in N2 with the presence of moisture in N2 having a proportionally stronger effect than in air.

Bill, R. C.↗

Fretting wear of iron, nickel, and titanium under varied environmental conditions

Fretting wear experiments were conducted on high-purity iron, nickel and titanium in air under conditions of varied humidity and temperature, and in nitrogen. For iron and titanium, maximum fretting occurred at 10 and 30 percent relative humidity respectively. Nickel showed a minimum in fretting wear at about 10% relative humidity. With increasing temperature, all three metals initially showed reduced fretting wear, with increasing wear observed as temperatures increased beyond 200-300 C. For titanium, dramatically reduced fretting wear was observed at temperatures above 500 C, relatable to a change in oxidation kinetics. All three metals showed much less fretting wear in N2 with the presence of moisture in N2 having a proportionally stronger effect than in air.

Bill, R. C.↗

Effect of gamma irradiation on the friction and wear of ultrahigh molecular weight polyethylene

The effect of sterilization gamma irradiation on the friction and wear properties of ultrahigh molecular weight polyethylene (UHMWPE) sliding against stainless steel 316L in dry air at 23 C is investigated, the results to be used in the development of artificial joints which are to surgically replace diseased human joints. A pin-on-disk sliding friction apparatus is used, a constant sliding speed in the range 0.061-0.27 m/s is maintained, a normal load of 1 kgf is applied with dead weight, and the irradiation dose levels are: 0, 2.5, and 5.0 Mrad. Wear and friction data and conditions for each of the ten tests are summarized, and include: (1) wear volume as a function of the sliding distance for the irradiation levels, (2) incremental wear rate, and (3) coefficient of friction as a function of the sliding distance. It is shown that (1) the friction and wear properties of UHMWPE are not significantly changed by the irradiation doses of 2.5 and 5.0 Mrad, (2) the irradiation increases the amount of insoluble gel as well as the amount of low molecular weight material, and (3) after run-in the wear rate is either steady or gradually decreases as a function of the sliding distance.

Jones, W. R.↗

Friction and wear of iron in sulfuric acid

Elemental iron sliding on aluminum oxide in aerated sulfuric acid concentrations ranging from very dilute (0.000007 N; i.e., 4 ppm) to very concentrated (96 percent acid) was studied. Load and reciprocating sliding speeds were kept constant. With the most dilute acid of 0.7 to 0.0002 N, a complex corrosion product formed that was friable and often increased friction and wear. At concentrations of 0.001 N, metal losses were essentially by wear alone. Because no buildup of corrosion products occurred, this acid concentration became the standard from which to separate metal loss from direct corrosion and mechanical wear losses. When the acid concentration was increased to 5 percent, the high corrosion rate of iron in sulfuric acid strongly dominated the total wear loss. This strong corrosion increased to 30 percent acid, and decreased somewhat at 50 percent in accordance with expectations. However, the low corrosion of iron expected at acid concentrations of 65 to 96 percent was not observed in the wear area. It is apparent that the normal passivating film was being worn away and a galvanic cell established which rapidly attached to the wear area.

Rengstorff, G. W. P.↗

Microstructures Associated with Wear

High strain associated with metal wear is discussed and macroscopic and fine microscopic aspects are included. Mechanisms for the production of debris which include extrusion of microfurrows, adhesive transfer, and fragmentation are outlined. The structure of near surface deformation zones, a thin transfer layer, is examined. The similarity among the size of fine wear debris particles, the structure of the transfer layer, and large wear flakes is shown. Differences in microstructure associated with dry wear and lubricated wear are pointed out. Some parallels and differences for classic high strain deformation and wear microstructures are discussed.

Glaeser, W. A.↗

Selected fretting-wear-resistant coatings for Ti-6 pct Al-4 pct V alloy

The ability of several wear-resistant coatings to reduce fretting in the Ti-6Al-4V alloy is investigated. The experimental apparatus and procedures for evaluating fretting in uncoated Ti-6Al-4V alloy and in the alloy with plasma-sprayed coatings, polymer-bonded coating, and surface treatments are described. The wear volume and wear rate for the alloys are measured and compared. It is concluded that Al2O3 with 13 percent TiO2, preoxidation and nitride surface treatments, and MoS2 sputtering result in wear-resistant surfaces; however, the polyimide coating is the most wear resistant coating in both dry and moist air, and it causes the least wear to the uncoated alloy surface.

Bill, R. C.↗

Experimentally determined wear behavior of an Al2O3-SiC composite from 25 to 1200 C

The sliding wear behavior of a self-mated alumina-silicon carbide whisker toughened composite was studied using optical, scanning electron (SEM) and transmission electron (TEM) microscopy. Because of its excellent strength and toughness properties this composite material is under consideration for use in heat engine applications for sliding contacts which operate at elevated temperatures. The composite's wear behavior and especially its wear mechanisms are not well understood. Pin-on-disk specimens were slid in air at 2.7 m/s sliding velocity, under a 26.5-N load, at temperatures 25 to 1200 C. Pin wear increased with increasing temperature. Based upon the microscopic analyses, the wear mechanism seems to be loosening of the reinforcing whiskers due to frictional and bulk heating. This leads to whisker pullout and increased wear.

Dellacorte, Christopher↗

Surface Chemistry, Friction, and Wear Properties of Untreated and Laser-Annealed Surfaces of Pulsed-Laser-Deposited WS(sub 2) Coatings

An investigation was conducted to examine the surface chemistry, friction, and wear behavior of untreated and annealed tungsten disulfide (WS2) coatings in sliding contact with a 6-mm-diameter 440C stainless-steel ball. The WS2 coatings and annealing were performed using the pulsed-laser-deposition technique. All sliding friction experiments were conducted with a load of 0.98 N (100 g), an average Hertzian contact pressure of 0.44 GPa, and a constant rotating speed of 120 rpm. The sliding velocity ranged from 31 to 107 mm/s because of the range of wear track radii involved in the experiments. The experiment was performed at room temperature in three environments: ultrahigh vacuum (vacuum pressure, 7X(exp -10) Pa), dry nitrogen (relative humidity, less than 1 percent), and humid air (relative humidity, 15 to 40 percent). Analytical techniques, including scanning electron microscopy (SEM), energy-dispersive x-ray spectroscopy (EDX), x-ray photo electron spectroscopy (XPS), surface profilometry, and Vickers hardness testing, were used to characterize the tribological surfaces of WS2 coatings. The results of the investigation indicate that the laser annealing decreased the wear of a WS2 coating in an ultrahigh vacuum. The wear rate was reduced by a factor of 30. Thus, the laser annealing increased the wear life and resistance of the WS2 coating. The annealed WS 2 coating had a low coefficient of friction (less than O.1) and a low wear rate ((10(exp -7) mm(exp 3)/N-m)) both of which are favorable in an ultrahigh vacuum.

Miyoshi, Kazuhisa↗

An Additive to Improve the Wear Characteristics of Perfluoropolyether Based Greases

The friction and wear characteristics of two formulated perfluoropolyether based greases were compared to their non-additive base greases. One grease was developed for the electronics industry (designated as GXL-296A) while the other is for space applications (designated as GXL-320A). The formulated greases (GXL-296B and GXL-320B) contained a proprietary antiwear additive at an optimized concentration. Tests were conducted using a vacuum four-ball tribometer. AISI 52100 steel specimens were used for all GXL-296 tests. Both AISI 52100 steel and 440C stainless steel were tested with the GXL-320 greases. Test conditions included: a pressure less than 6.7 x 10(exp )-4 Pa, a 200N load, a sliding velocity of 28.8 mm/sec (100 rpm) and room temperature (approximately equal to 23 C). Wear rates for each grease were determined from the slope of the wear volume as a function of sliding distance. Both non-additive base greases yielded relatively high wear rates on the order of 10(exp -8) cu mm using AISI 52100 steel specimens. Formulated grease GXL-296B yielded a reduction in wear rate by a factor of approximately 21, while grease GXL-320B had a reduction of approximately 12 times. Lower wear rates (-50%) were observed with both GXL-320 greases using 440C stainless steel. Mean friction coefficients were slightly higher for both formulated greases compared to their base greases. The GXL-296 series (higher base oil viscosity) yielded much higher friction coefficients compared to their GXL-320 series (lower base oil viscosity) counterparts.

Jones, David G. V.↗

Volatility and Wear Characteristics of a Variety of Liquid Lubricants for Space Applications

The vapor pressures and wear characteristics are critical properties for liquid lubricants to assure long-term reliability and performance in space applications. Vapor pressures, obtained using a Knudsen cell technique, and wear properties, obtained using a vacuum four-ball apparatus, were measured for a series of unformulated liquid lubricants. These included two multiply alkylated cyclopentanes (MACs) (X-1000 and X2000), two linear perfluoropolyalkylethers (PFPAEs) (Z-25 and 815Z), and four silahydrocarbons (a tri, a tetra, and two pentas). Vapor pressures were measured at three elevated temperatures (423, 448, and 498 K) and extrapolated to room temperature 298 K. The lowest 298 K vapor pressure of 5.7 x 10(exp -14) Pa was obtained with the PFPAE fluid (815Z) and the highest value with the low molecular weight MAC (X-1000) at 3.6 x 10(exp -7) Pa. In addition, vacuum wear rates were determined for some of the lubricants. The lowest wear rates (approximately 3 x 10(exp -11) cubic mm/mm) were observed for three of the silahydrocarbons while the highest wear rates (approximately 2 x 10(exp -9) cubic mm/mm) were observed with the two PFPAE fluids (Z-25 and 815Z). The MAC (X-2000) yielded a wear rate of about 10(exp -10) cubic mm/mm. The results indicated that the silahydrocarbon class of liquid lubricants offers the better potential for space applications.

Nguyen, QuynhGiao N.↗