Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Titanium”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Characterization of TiN, TiC and Ti(C,N) in titanium-alloyed ferritic chromium steels focusing on the significance of different particle morphologies

Titanium-alloyed ferritic chromium steels are a competitive option to classical austenitic stainless steels owing to their similar corrosion resistance. The addition of titanium significantly influences their final steel cleanliness. The present contribution focuses on the detailed metallographic characterization of titanium nitrides, titanium carbides and titanium carbonitrides with regard to their size, morphology and composition. The methods used are manual and automated Scanning Electron Microscopy with Energy Dispersive X-ray Spectroscopy as well as optical microscopy. Additional thermodynamic calculations are performed to explain the precipitation procedure of the analyzed titanium nitrides. The analyses showed that homogeneous nucleation is decisive at an early process stage after the addition of titanium. Heterogeneous nucleation gets crucial with ongoing process time and essentially influences the final inclusion size of titanium nitrides. A detailed investigation of the nuclei for heterogeneous nucleation with automated Scanning Electron Microscopy proved to be difficult due to their small size. Manual Scanning Electron Microscopy and optical microscopy have to be applied. Furthermore, it was found that during solidification an additional layer around an existing titanium nitride can be formed which changes the final inclusion morphology significantly. These layers are also characterized in detail. Based on these different inclusion morphologies, in combination with thermodynamic results, tendencies regarding the formation and modification time of titanium containing inclusions in ferritic chromium steels are derived. - Graphical abstract: Display Omitted - Highlights: • The formation and modification of TiN in the steel 1.4520 was examined. • Heterogeneous nucleation essentially influences the final steel cleanliness. • In most cases heterogeneous nuclei in TiN inclusions are magnesium based. • Particle morphology provides important information on inclusion formation.

36 MATERIALS SCIENCE↗

Enery Efficient Press and Sinter of Titanium Powder for Low-Cost Components in Vehicle Applications

This is the final technical report for the Department of Energy NETL project NT01931 Energy Efficient Press and Sinter of Titanium Powder for Low-Cost Components in Vehicle Applications. Titanium has been identified as one of the key materials with the required strength that can reduce the weight of automotive components and thereby reduce fuel consumption. Working with newly developed sources of titanium powder, Webster-Hoff will develop the processing technology to manufacture low cost vehicle components using the single press/single sinter techniques developed for iron based powder metallurgy today. Working with an automotive or truck manufacturer, Webster-Hoff will demonstrate the feasibility of manufacturing a press and sinter titanium component for a vehicle application. The project objective is two-fold, to develop the technology for manufacturing press and sinter titanium components, and to demonstrate the feasibility of producing a titanium component for a vehicle application. The lowest cost method for converting metal powder into a net shape part is the Powder Metallurgy Press and Sinter Process. The method involves compaction of the metal powder in a tool (usually a die and punches, upper and lower) at a high pressure (up to 60 TSI or 827 MPa) to form a green compact with the net shape of the final component. The powder in the green compact is held together by the compression bonds between the powder particles. The sinter process then converts the green compact to a metallurgically bonded net shape part through the process of solid state diffusion. The goal of this project is to expand the understanding and application of press and sinter technology to Titanium Powder applications, developing techniques to manufacture net shape Titanium components via the press and sinter process. In addition, working with a vehicle manufacturer, demonstrate the feasibility of producing a titanium component for a vehicle. This is not a research program, but rather a project to develop a process for press and sinter of net shape Titanium components. All of these project objectives have been successfully completed.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Production of Diesel Engine Turbocharger Turbine from Low Cost Titanium Powder

Turbochargers in commercial turbo-diesel engines are multi-material systems where usually the compressor rotor is made of aluminum or titanium based material and the turbine rotor is made of either a nickel based superalloy or titanium, designed to operate under the harsh exhaust gas conditions. The use of cast titanium in the turbine section has been used by Cummins Turbo Technologies since 1997. Having the benefit of a lower mass than the superalloy based turbines; higher turbine speeds in a more compact design can be achieved with titanium. In an effort to improve the cost model, and develop an industrial supply of titanium componentry that is more stable than the traditional aerospace based supply chain, the Contractor has developed component manufacturing schemes that use economical Armstrong titanium and titanium alloy powders and MgR-HDH powders. Those manufacturing schemes can be applied to compressor and turbine rotor components for diesel engine applications with the potential of providing a reliable supply of titanium componentry with a cost and performance advantage over cast titanium.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

A New Method for Low Cost Production of Titanium Alloys for Reducing Energy Consumption of Mechanical Systems

This project investigated an innovative manufacturing process intended to minimize the cost of production of titanium materials and components, and increase the adoption of Ti components for energy consuming applications, such as automobiles. A key innovation of the proposed manufacturing approach is a novel Ti powder sintering technology for making titanium materials with ultrafine grain microstructure in the as-sintered state with minimum, or an absence, of post-sintering processes. The new sintering technology is termed Hydrogen Sintering and Phase Transformations (HSPT), and constitutes a promising manufacturing technology that can be used to produce titanium (Ti) materials and components in a near-net-shape form, thus also minimizing machining costs. Our objective was to meet, or possibly surpass, the mechanical property levels for ASTM B348 Grade 5 for wrought Ti-6Al-4V. Although specific applications call for varying mechanical property requirements, ASTM B348 was created for the demanding applications of the aerospace industry, and is the established standard for Ti-6Al-4V. While the primary goal was to meet, or exceed this standard, the team also had the goal of demonstrating this could be done at a significantly lower cost of production. Interim goals of the project were to fully develop this novel sintering process, and provide sufficient baseline testing to make the method practical and attractive to industry. By optimizing the process parameters for the sintering of titanium hydride (TiH 2 ) powders in a hydrogen atmosphere and controlling the phase transformations during and after sintering, the HSPT process was expected to reduce the energy consumption, and thus cost, of making Ti alloys and fabricating Ti components. The process was designed such that no high temperature melting is required for producing Ti alloys; little or no post-sintering processing is needed for producing desired microstructures (and therefore enhanced mechanical properties), and finally, minimum machining is needed to fabricate finished Ti components. An energy analysis within this report provides more detail, but calculated values indicate that the HSPT process is less than half as energy intensive as conventional wrought processing, while producing mechanical properties that are comparable. In addition to the energy savings anticipated from the industrial production of Ti components, a second prong of energy savings resides in the use phase of components produced, primarily from use in the transportation sector. Titanium has a number of material qualities appropriate for the auto industry, particularly low mass and corrosion resistance. By reducing the weight of automobiles and other vehicles, energy costs and CO 2 production will be reduced over the lifetime of the vehicles, and components in corrosive environments on vehicles, such as exhaust systems and other under carriage parts, may not have to be replaced during a vehicle’s lifetime. Our analysis indicates that by replacing only 5.6 kg of steel parts in an auto with Ti components across the entire US fleet would save approximately 486 million gallons of gasoline per year. This correlates to a reduction of 3.6 million metric tons of CO 2 per year. The potential for replacing many more of the steel parts in automobiles with lighter weight titanium components is clear. The project was very successful overall, meeting all milestones and surpassing project goals in terms of mechanical properties and microstructures produced. In addition to tensile properties, fatigue properties were emphasized in the project work. Powder metallurgy processes often have porosity to some degree in their final microstructure, and porosity is a well-known cause of crack initiation and low fatigue performance. Although many automobile applications do not undergo fatigue stress regimes, many others do encounter cyclic stress, and design criteria in the latter case require good fatigue properties. Production and testing of HSPT parts showed excellent tensile properties and fracture toughness, and fatigue properties that exceeded all previously reported powder metallurgy Ti methods, overlapping with wrought processed values. Fatigue limits exceeded 500 MPa and tensile strength exceeded 1,000 MPa while maintaining good ductility. Microstructures produced during the project period easily surpassed pre-project expectations. In addition to producing very fine grains in the as-sintered state (without post sintered thermo-mechanical work), porosity was reduced and industrially relevant microstructures previously undemonstrated in any other powder metallurgy titanium method were produced using HSPT materials. These microstructures, both bi-modal and globularized, were produced with simple post-sinter heat treatments, but without the need for energy intensive mechanical work. The employed heat treatments expanded the available mechanical property range (tensile strength vs. ductility) of the HSPT system in Ti-6Al-4V. The project has resulted in the publication, thus far, of five refereed journal articles and five conference proceedings papers, as well as a patent application, two dissertations and a master’s thesis. Two additional journal articles are currently under review, and at least three others are currently in preparation, with several additional students anticipated to graduate within the coming year. Presentations and papers were a particular focus of the second half of the project, once significant experimentation had been performed and analyzed. As part of our efforts to disseminate information of our results, the Ti research teams within Prof. Fang’s and Prof. Chandran’s research groups had a strong presence at the 13th World Conference on Ti, August 16-20, 2015, in San Diego. Several research groups in the US and in Europe are now performing experiments using the HSPT process. Accompanying efforts to bring HSPT to the Ti community at large, and industry in particular, work has continued with our partners and with other interested industrial Ti users and producers, including Boeing and GKN (a major powder metallurgy parts manufacturer). Commercialization has been a central focus of the final phase of the project, and Reading Alloys signed a provisional licensing agreement in summer of 2015. They are currently seeking an appropriate customer with which to pursue initial parts manufacturing efforts. Other licensing options and partners are continuing to be pursued. The promise of lightweight, strong and corrosion resistant Ti alloys with long fatigue lifetimes for automobile or transportation applications has been the vision of the metal industry since titanium came to the attention of scientists and engineers. The sole limitation of realizing these goals has been cost, which is primarily a function of energy used in production. The HSPT process was shown through this work to be capable of realizing this goal, and facilitating the practical use of titanium in US automotive and other industries.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Low-Cost Titanium Casting Technology

This is the final report of "Low-Cost Titanium Casting Technology" project. Titanium alloys have attracted increasing attentions as structural materials for high performance and weight-sensitive applications in aerospace and biomedical fields. However, in mass-production of civil applications like automotive components, titanium alloys are scarcely used due to the unaffordable costs in manufacturing compared with other metallic materials, such as aluminum, magnesium and steel. Therefore, there is a need to reduce the manufacturing cost of titanium alloys so that titanium alloys can be more competitive in terms of property and cost considerations. In this 4-year project, we started from exploring new low-cost titanium alloy systems with the guidance of Integrated Computational Materials Engineering – Calculation of Phase Diagram (ICME-CALPHAD) framework, and determined several promising alloy systems, alloying elements including Ti-Al-Fe-Mn-B-C, that can allow further development (lab-scale and industry-scale) in the future. During the new alloy system exploration, considerable amount of scientific work was completed regarding CALPHAD modeling, microstructure morphology, mechanical properties, and processing of the new alloy systems. The relevant ternary titanium alloy systems, Ti-Al-Mn and Ti-Al-Fe, were examined and reassessed both computationally and experimentally, leading to more comprehensive understanding of these alloy systems. Based on this above study, a new low-cost casting titanium alloy was developed, Ti-6Al-5Fe-0.05B-0.05C (designated as T65-0.05BC), which has competitive as-cast strength level with current commercial titanium alloys but relatively low ductility. However, in this project, since the target application, automotive engine connecting rod, is a fatigue-limited component and does not require high ductility, this alloy shall suffice as the deliverable alloy in this project. After designing and confirming the potent of the new alloy, we designed and built a lab-scale manufacturing equipment aided by computational tools at OSU labs to conceptually prove that this alloy can be manufactured with permanent mold casting, which is low-cost and potentially a mass production process. We produced a lab-scale prototype connecting rod demonstrating the capability of permanent mold casting of this new alloy.

36 MATERIALS SCIENCE↗

Production of Diesel Engine Turbocharger Turbine from Low Cost Titanium Powder [CRADA Final Report for CRADA Number NFE-11-03486]

The objective of this Cooperative Research and Development Agreement (CRADA) between UT-Battelle and Queen City Forging Co., is to produce turbocharger turbine rotors. Turbochargers in commercial turbo-diesel engines are multi-material systems where usually the compressor rotor is made of aluminum or titanium based material and the turbine rotor is made of either a nickel based superalloy or titanium, designed to operate under the harsh exhaust gas conditions. The use of cast titanium in the turbine section has been used by Cummins Turbo Technologies since 1997. Having the benefit of a lower mass than the superalloy based turbines; higher turbine speeds in a more compact design can be achieved with titanium. In an effort to improve the cost model, and develop an industrial supply of titanium componentry that is more stable than the traditional aerospace based supply chain, the Contractor has developed component manufacturing schemes that use economical Armstrong™ titanium and titanium alloy powders and MgR-HDH powders. Those manufacturing schemes can be applied to compressor and turbine rotor components for diesel engine applications with the potential of providing a reliable supply of titanium componentry with a cost and performance advantage over cast titanium.

Muth, Thomas R↗

Oxynitrided Surface Layer Produced On Ti6Al4V Titanium Alloy Under Low Temperature Glow Discharge Conditions For Medical Applications

In spite that titanium oxides increase biocompatibility of titanium implants but their functional life is limited due to the problems arising from brittles and metalosis. Therefore technology, that allow to produce composite surface layer with controlled microstructure, chemical and phase composition and surface morphology on titanium alloy and eliminates the oxides disadvantages has been existing till now is searched. The requirements of titanium and its alloys implants can be fulfill by the low-temperature glow discharge assisted oxynitriding.The paper describes the surface layer of TiO{sub 2}+TiN+Ti{sub 2}N+{alpha}Ti(N) type produced at temperature 680 deg. C that preserves mechanical properties of titanium alloy Ti6Al4V. Characteristics of produced diffusion multi-phase surface layers in range of phase composition, microstructure (SEM, TEM, XRD) and its properties, such as frictional wear resistance are presented. The biological properties in dependency to the applied sterilization method are also analyzed.Properties of produced surface layers are discussed with reference to titanium alloy. The obtained data show that produced surface layers improves titanium alloy properties both frictional wear and biological. Preliminary in vitro examinations show good biocompatibility and antithrombogenic properties.

36 MATERIALS SCIENCE↗

Study of the Biocompatibility of Titanium-Niobium Implants by the Parameters of Their Osseointegration under Experimental Conditions

Superelastic titanium alloys (titanium-niobium-zirconium and titanium-niobium-tantalum) are considered to be the more advantageous choice for dental implants than titanium alloys due to their physico-mechanical properties close to those of the bone tissue. Morphological studies of the biocompatibility of these alloys in comparison with titanium were carried out in vivo. Scanning electron microscopy and microprobe elemental analysis of the tissue along the interface between the bone and titanium/superelastic titanium alloys showed similar morphology and elemental composition both on days 30 (poorly mineralized connective tissue was detected in sites of contact with titanium alloy samples) and 90 after surgery (the surface of the titanium alloy samples was covered with mineralized tissue similar by its composition to the surrounding bone).

60 APPLIED LIFE SCIENCES↗

Methods of producing a titanium alloy product

A method for producing a particulate titanium alloy product can include preparing a composite particulate oxide mixture with TiO2 powder and at least one alloying element powder. The composite particulate oxide mixture can be co-reduced using a metallic reducing agent under a hydrogen atmosphere at a reduction temperature for a reduction time sufficient to produce a hydrogenated titanium alloy product. The hydrogenated titanium alloy product can then be heat treated under a hydrogen atmosphere and a heat treating temperature to reduce pore size and specific surface area to form a heat treated hydrogenated titanium product. The heat treated hydrogenated titanium product can be deoxygenated to reduce residual oxygen to less than 0.2 wt % to form a deoxygenated hydrogenated titanium product as a particulate. The deoxygenated hydrogenated titanium product can optionally be dehydrogenated to form the titanium alloy product as a particulate.

Fang, Zhigang Zak↗

Vacancies in ordered and disordered titanium monoxide: Mechanism of B1 structure stabilization

The electronic structure and stability of three phases of titanium monoxide TiO{sub y} with B1 type of the basic structure have been studied. Cubic phase without structural vacancies, TiO, and two phases with structural vacancies, monoclinic Ti{sub 5}O{sub 5} and cubic disordered TiO{sub 1.0}, was treated by means of first-principles calculations within the density functional theory with pseudo-potential approach based on the plane wave's basis. The ordered monoclinic phase Ti{sub 5}O{sub 5} was found to be the most stable and the cubic TiO without vacancies the less stable one. The role of structural vacancies in the titanium sublattice is to decrease the Fermi energy, the role of vacancies in the oxygen sublattice is to contribute to the appearance of Ti–Ti bonding interactions through these vacancies and to reinforce the Ti–Ti interactions close to them. Listed effects are significantly pronounced if the vacancies in the titanium and oxygen sublattices are associated in the so called “vacancy channels” which determine the formation of vacancy ordered structure of monoclinic Ti{sub 5}O{sub 5}-type. - Graphical abstract: Changes in total DOS of titanium monoxide when going from vacancy-free TiO to TiO with disordered structural vacancies and to TiO with ordered structural vacancies. Highlights: • Ordered monoclinic Ti{sub 5}O{sub 5} is the most stable phase of titanium monoxide. • Vacancy-free TiO is the less stable phase of the titanium monoxide. • Ordering of oxygen vacancies leads to the appearance of Ti–Ti bonding interactions. • Titanium vacancies contribute significantly to the decreasing of the Fermi energy.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Controlled synthesis of titania using water-soluble titanium complexes: A review

The development of human society has led to the increase in energy and resources consumption as well as the arising problems of environmental damage and the toxicity to the human health. The development of novel synthesis method which tolerates utilization of toxic solvents and chemicals would fulfill the demand of the society for safer, softer, and environmental friendly technologies. For the past decades, a remarkable progress has been attained in the development of new water-soluble titanium complexes (WSTC) and their use for the synthesis of nanocrystalline titanium dioxide materials by aqueous solution-based approaches. The progress of synthesis of nanocrystalline titanium dioxide using such WSTCs is reviewed in this work. The key structural features responsible for the successfully controlled synthesis of TiO{sub 2} are discussed to provide guidelines for the morphology-controlled synthesis. Finally, this review ends with a summary and some perspectives on the challenges as well as new directions in this fascinating research. - Graphical abstract: The progress of synthesis of nanocrystalline titanium dioxide using water-soluble titanium complexes is reviewed in this work. The key structural features responsible for the successfully controlled synthesis of TiO{sub 2} are discussed to provide guidelines for the morphology-controlled synthesis. - Highlights: • The progress of the synthesis of novel water-soluble titanium complexes is reviewed. • Water-soluble titanium complexes are versatile precursor for synthesis of TiO{sub 2}. • The key structural features responsible for the controlled synthesis are discussed. • TiO{sub 2} with unusual shapes and complex patterns can be synthesized.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Hydrogen effect on the morphology and structure of 3D porous titanium in the HFCVD-diamond growth environment

Titanium hydride was obtained from hydrogenation process on pure titanium (Ti) using a hot filament chemical vapor deposition reactor. The Ti samples were produced from powder metallurgy technique and present three-dimensional porosity. The experimental parameters of the hydrogenation process were controlled in a similar way as those for diamond growth. The pressure inside the reactor was kept at 6.6 kPa for a H{sub 2} flow rate of 100 sccm and hydrogenation time of 1 hour. The distance from the filaments to the Ti surface was kept at 5 mm. Hydrogenation processes were carried out at different temperatures of 773, 873, 973 and 1073 K. The morphology of the titanium hydrides was studied by scanning electron microscopy. The images showed an increase in the roughness titanium surface as well as the formation of cracks due to the hydride titanium precipitation. The structure of these titanium hydrides was analyzed by X-ray diffraction, performed through {theta}-2{theta} scans from 1 to 15{sup o} grazing incident angle. The results revealed that the temperature enhanced the titanium hydride concentration in the samples with a predominant precipitation of TiH phase for the four temperatures studied. - Highlights: {yields} Hydrogen quickly spread out in the Ti matrix reacting and generating TiH phases. {yields} The higher the hydrogenation temperature the higher the amount of TiH formation. {yields} The volume increasing associated with the TiH formation caused tensions in the Ti metallic matrix. {yields} The TiH increases the Ti surface roughness influencing the grain size reduction.

36 MATERIALS SCIENCE↗

A detailed analysis of the energy levels configuration existing in the band gap of supersaturated silicon with titanium for photovoltaic applications

The energy levels created in supersaturated n-type silicon substrates with titanium implantation in the attempt to create an intermediate band in their band-gap are studied in detail. Two titanium ion implantation doses (10{sup 13 }cm{sup -2} and 10{sup 14 }cm{sup -2}) are studied in this work by conductance transient technique and admittance spectroscopy. Conductance transients have been measured at temperatures of around 100 K. The particular shape of these transients is due to the formation of energy barriers in the conduction band, as a consequence of the band-gap narrowing induced by the high titanium concentration. Moreover, stationary admittance spectroscopy results suggest the existence of different energy level configuration, depending on the local titanium concentration. A continuum energy level band is formed when titanium concentration is over the Mott limit. On the other hand, when titanium concentration is lower than the Mott limit, but much higher than the donor impurity density, a quasi-continuum energy level distribution appears. Finally, a single deep center appears for low titanium concentration. At the n-type substrate, the experimental results obtained by means of thermal admittance spectroscopy at high reverse bias reveal the presence of single levels located at around E{sub c}-425 and E{sub c}-275 meV for implantation doses of 10{sup 13 }cm{sup −2} and 10{sup 14 }cm{sup −2}, respectively. At low reverse bias voltage, quasi-continuously distributed energy levels between the minimum of the conduction bands, E{sub c} and E{sub c}-450 meV, are obtained for both doses. Conductance transients detected at low temperatures reveal that the high impurity concentration induces a band gap narrowing which leads to the formation of a barrier in the conduction band. Besides, the relationship between the activation energy and the capture cross section values of all the energy levels fits very well to the Meyer-Neldel rule. As it is known, the Meyer-Neldel rule typically appears in processes involving multiple excitations, like carrier capture and emission in deep levels, and it is generally observed in disordered systems. The obtained Meyer-Neldel energy value, 15.19 meV, is very close to the value obtained in multicrystalline silicon samples contaminated with iron (13.65 meV), meaning that this energy value could be associated to the phonons energy in this kind of substrates.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Causal Factors of Weld Porosity in Gas Tungsten Arc Welding of Powder Metallurgy Produced Titanium Alloys

ORNL undertook an investigation using gas tungsten arc (GTA) welding on consolidated powder metallurgy (PM) titanium (Ti) plate, to identify the causal factors behind observed porosity in fusion welding. Tramp element compounds of sodium and magnesium, residual from the metallothermic reduction of titanium chloride used to produce the titanium, were remnant in the starting powder and were identified as gas forming species. PM-titanium made from revert scrap where sodium and magnesium were absent, showed fusion weld porosity, although to a lesser degree. We show that porosity was attributable to hydrogen from adsorbed water on the surface of the powders prior to consolidation. The removal / minimization of both adsorbed water on the surface of titanium powder and the residues from the reduction process prior to consolidation of titanium powders, are critical to achieve equivalent fusion welding success similar to that seen in wrought titanium produced via the Kroll process.

Gas Tungsten Arc Welding↗

High energy X-ray diffraction study of a dental ceramics–titanium functional gradient material prepared by field assisted sintering technique

A functional gradient material with eleven layers composed of a dental ceramics and titanium was successfully consolidated using field assisted sintering technique in a two-step sintering process. High energy X-ray diffraction studies on the gradient were performed at High Energy Material Science beamline at Desy in Hamburg. Phase composition, crystal unit edges and lattice mismatch along the gradient were determined applying Rietveld refinement procedure. Phase analysis revealed that the main crystalline phase present in the gradient is α-Ti. Crystallinity increases stepwisely along the gradient with a decreasing increment between every next layer, following rather the weight fraction of titanium. The crystal unit edge a of titanium remains approximately constant with a value of 2.9686(1) Å, while c is reduced with increasing amount of titanium. In the layer with pure titanium the crystal unit edge c is constant with a value of 4.7174(2) Å. The lattice mismatch leading to an internal stress was calculated over the whole gradient. It was found that the maximal internal stress in titanium embedded in the studied gradient is significantly smaller than its yield strength, which implies that the structure of titanium along the whole gradient is mechanically stable. - Highlights: • High energy XRD studies of dental ceramics–Ti gradient material consolidated by FAST. • Phase composition, crystallinity and lattice parameters are determined. • Crystallinity increases stepwisely along the gradient following weight fraction of Ti. • Lattice mismatch leading to internal stress is calculated over the whole gradient. • Internal stress in α-Ti embedded in the gradient is smaller than its yield strength.

36 MATERIALS SCIENCE↗

Characterization of the porous structures of the green body and sintered biomedical titanium scaffolds with micro-computed tomography

The present research was aimed at gaining an understanding of the porous structure changes from the green body through water leaching and sintering to titanium scaffolds. Micro-computed tomography (micro-CT) was performed to generate 3D models of titanium scaffold preforms containing carbamide space-holding particles and sintered scaffolds containing macro- and micro-pores. The porosity values and structural parameters were determined by means of image analysis. The result showed that the porosity values, macro-pore sizes, connectivity densities and specific surface areas of the titanium scaffolds sintered at 1200 °C for 3 h did not significantly deviate from those of the green structures with various volume fractions of the space holder. Titanium scaffolds with a maximum specific surface area could be produced with an addition of 60–65 vol% carbamide particles to the matrix powder. The connectivity of pores inside the scaffold increased with rising volume fraction of the space holder. The shrinkage of the scaffolds prepared with > 50 vol% carbamide space holder, occurring during sintering, was caused by the reductions of macro-pore sizes and micro-pore sizes as well as the thickness of struts. In conclusion, the final porous structural characteristics of titanium scaffolds could be estimated from those of the green body. - Highlights: •Porous structures of green body and sintered titanium scaffolds was studied. •Porous structures of both samples were quantitatively characterized with micro-CT. •Porous structures of scaffolds could be controlled from the green body. •Shrinkage mechanisms of titanium scaffolds during sintering was established.

36 MATERIALS SCIENCE↗

A new route for the synthesis of titanium silicalite-1

Graphical abstract: Well-prepared TS-1 was synthesized by an innovative procedure using inexpensive reagents such as fumed silica and TPABr as structure-directing agent. This is the first time when highly crystalline TS-1 is obtained in basic medium, using sodium hydroxide as HO{sup -} ion source required for the crystallization process. Hydrolysis of titanium source has been prevented by titanium complexation with acetylacetone before structuring gel. Highlights: Black-Right-Pointing-Pointer TS-1 was obtained using cheap reagents as fumed silica and tetrapropylammonium bromide. Black-Right-Pointing-Pointer First time NaOH was used as source of OH{sup -} ions required for crystallization process. Black-Right-Pointing-Pointer The hydrolysis Ti alkoxides was controlled by Ti complexation with 2,4-pentanedione. -- Abstract: A new and efficient route using inexpensive reagents such as fumed silica and tetrapropylammonium bromide is proposed for the synthesis of titanium silicalite-1. High crystalline titanium silicalite-1 was obtained in alkaline medium, using sodium hydroxide as HO{sup -} ion source required for the crystallization process. Hydrolysis of titanium source with formation of insoluble oxide species was prevented by titanium complexation with before structuring gel. The final solids were fully characterized by powder X-ray diffraction, scanning electron microscopy, Fourier transform infrared, ultraviolet-visible diffuse reflectance, Raman and atomic absorption spectroscopies, as well as nitrogen sorption analysis. It was found that a molar ratio Ti:Si of about 0.04 in the initial reaction mixture is the upper limit to which well formed titanium silicalite-1 with channels free of crystalline or amorphous material can be obtained. Above this value, solids with MFI type structure containing both Ti isomorphously substituted in the network and extralattice anatase nanoparticles inside of channels is formed.

36 MATERIALS SCIENCE↗

Formation mechanism of anodic titanium oxide in mixed electrolytes

Highlights: • Compact anodic titanium oxide (CATO) and anodic TiO{sub 2} nanotubes (ATNTs) were compared. • A distinct transform from CATO films into the porous ATNTs was observed firstly. • FESEM evidences for oxygen bubble mould effect were provided firstly. • Formation mechanisms for different titanium oxide films are confirmed consistent. - Abstract: The formation mechanism of anodic TiO{sub 2} nanotubes (ATNTs) remains mysterious and complicated. Usually, ATNTs are fabricated in pure NH{sub 4}F electrolytes rather than mixed electrolytes and Ti anodizations are carried out under potentiostatic rather than galvanostatic conditions. In this work, anodizations under the potentiostatic and galvanostatic conditions are conducted. The formation processes of titanium oxide film in different mixed electrolytes are explored in detail. By changing the mass ratios of oxalic acid and ammonium fluoride, different kinds of anodic titanium oxide films are fabricated: the compact anodic titanium oxide (CATO) films, transient-state anodic titanium oxide films and porous films (ATNTs). A distinct transform from CATO films into ATNTs was observed. Cavities within oxide and hemispheric bottoms are found, confirming the presence of oxygen bubble mould. Based on the electronic current and ionic current model, a consistent formation mechanism for three kinds of anodic titanium oxide films in mixed electrolytes is proposed.

36 MATERIALS SCIENCE↗