Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Silicon anodes”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Robust Polymer Electrolytes For Flexible Energy Storage (CRADA Final Report)

As part of the Cyclotron Road program, Anthro Energy investigated the formulation, synthesis, and application of advanced supramolecular compounds for lithium-ion batteries. Anthro Energy developed and tested formulations and chemistries to create polymeric materials with improved mechanical strength, safety, and electrochemical performance. These materials were explored for use in next-generation batteries with a variety of form factors. Initially, Anthro Energy tested these materials to create flexible and deformable batteries, which are in high demand for the wearable/flexible electronics industry. In future work, Anthro Energy’s materials may be applied to create rigid structural batteries, or to enable novel chemistries such as silicon anodes or lithium metal anodes. In the process of testing the company’s unique lithium-ion cells, Anthro Energy explored the development and utilization of novel cell components, cell architectures, and testing protocols. These next-generation flexible and structural batteries may eventually enable new categories of electronic devices.

25 ENERGY STORAGE↗

Electrolyte formulations for electrochemical cells containing a silicon electrode

Additives to electrolytes that enable the formation of comparatively more robust SEI films on silicon anodes. The SEI films in these embodiments are seen to be more robust in part because the batteries containing these materials have higher coulombic efficiency and longer cycle life than comparable batteries without such additives.

25 ENERGY STORAGE↗

Electrolyte formulations for electrochemical cells containing a silicon electrode

Additives to electrolytes that enable the formation of comparatively more robust SEI films on silicon anodes. The SEI films in these embodiments are seen to be more robust in part because the batteries containing these materials have higher coulombic efficiency and longer cycle life than comparable batteries without such additives. The additives preferably contain a nitrate group.

25 ENERGY STORAGE↗

Electrolyte formulations for electrochemical cells containing a silicon electrode

Additives to electrolytes that enable the formation of comparatively more robust SEI films on silicon anodes. The SEI films in these embodiments are seen to be more robust in part because the batteries containing these materials have higher coulombic efficiency and longer cycle life than comparable batteries without such additives.

Zhu, Ye↗

Composition-Nanoarchitecture-Performance Analysis of High Energy Density Electrodeposited Silicon for Lithium-Ion Battery Anodes

Electrodeposition of silicon (Si) was previously demonstrated as a promising method for fabricating 3D-structured lithium-ion battery anodes. However, the relationship between the electrochemical performance and chemical composition of the relatively impure electrodeposited silicon is not well understood. Here, we report the electrodeposition of a Si-dominant active material (EDEP-Si) onto 3D-structured nickel (Ni) scaffolds and systematically compare the electrochemical properties, elemental composition, atomistic Si coordination, and molecular structure of EDEP-Si with high-purity amorphous Si grown via static chemical vapor deposition. Despite the considerable amount of carbon (9–11 at %) and oxygen (42–44 at %) present in EDEP-Si, the cycling stability and high reversible specific capacity are remarkably similar to those of CVD-Si on a silicon basis (~2400 mA h/g-Si after 100 cycles). The primary difference is that EDEP-Si exhibits reduced cycling efficiency over the first 10–20 cycles. Reactions between carbon and, more importantly, oxygen in EDEP-Si with lithium are likely responsible for the reduced early cycle performance and lower capacity of the total deposit. Finally, our observations suggest ultrapure Si is not necessary for high electrochemical access to reversible charge storage, although limiting the presence of incorporated impurity species would improve energy density and first cycle efficiency.

25 ENERGY STORAGE↗

Investigating the impact of preparation routes on the properties of copper-decorated silicon particles as anode materials for lithium-ion batteries

In recent years, the calendar life of Si has been recognized as a significant issue that must be addressed prior to technology deployment: The carbon conductive additive is a potential source of parasitic side reactions. However, carbon remains essential due to the low electronic conductivity of Si. In this study, we investigate the use of Cu as a conductive additive and potential alternative to carbon. Some Cu-decorated silicon particles (Si Cu ) were prepared using physical vapor deposition (PVD) via sputtering and high-energy milling. Other Si Cu particles were prepared by using a solution method and examined briefly. The milling method caused Cu to appear as island-like features on the Si surface, whereas the PVD method initially produced similar island-like features that gradually developed into a continuous coating around the Si as sputtering time increased. Electrodes fabricated from Si Cu exhibited lower overall resistivity, demonstrating the beneficial effect of Cu in improving electronic percolation through the electrode. Electrochemical tests showed that the milled SiCu exhibited higher capacity retention, improved rate capability, and lower overpotential. Furthermore, Si Cu coupled with an NMC811 cathode exhibited lower leakage currents compared with the baseline silicon, indicating that incorporating Cu provided an additional advantage of minimizing parasitic currents in the cells.

25 ENERGY STORAGE↗

Improving Lithium Metal Composite Anodes with Seeding and Pillaring Effects of Silicon Nanoparticles

Metallic lithium (Li) anodes are crucial for the development of high specific energy batteries yet plagued by their poor cycling efficiency. Electrode architecture engineering is vital for maintaining a stable anode volume and suppress Li corrosion during cycling. In this paper, a reduced graphene oxide “host” framework for Li metal anodes is further optimized by embedding silicon (Si) nanoparticles between the graphene layers. They serve as Li nucleation seeds to promote Li deposition within the framework even without pre-stored Li. Meanwhile, the LixSi alloy particles serve as supporting “pillars” between the graphene layers, enabling a minimized thickness shrinkage after full stripping of metallic Li. Combined with a Li compatible electrolyte, 99.4% Coulombic efficiency over ~600 cycles is achieved, and stable cycling of a Li||NMC532 full cell for ~380 cycles with negligible capacity decay is realized.

Wang, Hansen↗

Quantifying lithium loss in amorphous silicon thin-film anodes via titration-gas chromatography

Silicon with a high theoretical capacity (3,579 mAh/g) is a promising anode candidate for lithium-ion batteries. However, commercialization is still impeded by low Coulombic efficiency, caused by solid electrolyte interphase (SEI) formation and trapped lithium (Li)-silicon (Si) alloy during repeated volume change. Quantifying capacity losses from each factor is crucial to formulate rational design strategies for further improvement. In this work, titration-gas chromatography and cryogenic transmission electron microscopy are applied to characterize the evolution of trapped Li-Si alloy and SEI growth in a silicon thin-film anode. It is found that continuous growth of the SEI is the dominant factor for lithium inventory loss during cycling, with only a marginal increase in trapped Li-Si alloy. This study offers a quantitative approach to differentiate Li in the SEI from trapped Li in Li-Si alloy through a silicon thin-film anode, providing unique insights into identifying critical bottlenecks for developing Si anodes.

25 ENERGY STORAGE↗

Effect of Si Content on Extreme Fast Charging Behavior in Silicon–Graphite Composite Anodes

Commercial Li-ion batteries typically incorporate a small amount of high-capacity silicon (Si)-based materials in the composite graphite-based anode to increase the energy density of the battery. However, very little is known about the effects of Si on the fast-charging behavior of composite anodes. Herein, we examine the effects of the Si/graphite ratio in the composite anode on the fast-charging behavior of full cells. We show that addition of Si increases the rate capability from 1C to 8C and improves the capacity retention in early cycles at 6C due to reduced overpotential in constant current charging cycles. The impacts of Si content on fast-charging aging were identified by Post-Test characterization. Despite realizing benefits of available capacity and reduced Li plating at 6C, silicon–electrolyte interactions lead the time-dependent cell performance to fade quickly in the long term. The Post-Test analysis also revealed the thickening of the electrode and nonuniform distribution of electrolyte decomposition products on the Si-containing anodes, as well as the organic-rich solid electrolyte interphase (SEI), which are the factors behind cell degradation. Our study sheds insight on the advantages and disadvantages of Si/graphite composite anodes when they are used in fast-charging applications and guides further research in the area by designing an optimized composition of Si incorporated in a mature graphite matrix.

25 ENERGY STORAGE↗

3D Carbon Coating Enabled High‐capacity and Stable Micro‐sized Silicon Suboxide‐graphite Blended Anodes for Practical Lithium‐ion Batteries

Abstract Silicon oxide (SiO x ) is a promising anode candidate of lithium‐ion batteries (LIBs) owing to its extremely high specific capacity. However, the low initial Coulombic efficiency (ICE) and rapid capacity degradation of SiO x , triggered by the enormous volume variation upon repeated (de)lithiation, gravely hinder its practical use. Herein, two mass‐produced micro‐sized SiO x @C composites with obviously different morphologies for commercial LIBs are reported. Particularly, the SiO x ‐graphite blended anode (SiO x @3D‐G‐Gr) based on SiO x wrapped by three‐dimensional (3D) carbon layers (SiO x @3D‐G) exhibits a capacity of 519 mAh g −1 , an ICE of 90.0 % and a capacity retention of 83.4 % at 0.2 C over 100 cycles. which is far exceeding its counterpart SiO x @C‐H‐Gr (65.7 %). The obtained impressive properties of SiO x @3D‐G originate from the critical contribution of 3D carbon layers, which serves as the effective stress buffer and protective layer as well as the strong networks for electron/Li + transport. Accordingly, the full‐cell based on SiO x @3D‐G‐Gr anode and commercial LiCoO 2 cathode delivers a capacity of 803 mAh and an excellent capacity retention of 95.6 % (616 mAh, 96.6 % for graphite, respectively) at 1 C over 100 cycles with a stabilized CE of nearly 100 %. The micro‐sized SiO x @3D‐G showing a promising prospect in the commercial‐grade anodes in LIBs.

Electrochemistry↗

Electrodes and lithium ion cells with high capacity anode materials

High capacity silicon based anode active materials are described for lithium ion batteries. These materials are shown to be effective in combination with high capacity lithium rich cathode active materials. Supplemental lithium is shown to improve the cycling performance and reduce irreversible capacity loss for at least certain silicon based active materials. In particular silicon based active materials can be formed in composites with electrically conductive coatings, such as pyrolytic carbon coatings or metal coatings, and composites can also be formed with other electrically conductive carbon components, such as carbon nanofibers and carbon nanoparticles. Additional alloys with silicon are explored.

Lopez, Herman A.↗

Intrinsic chemical reactivity of solid-electrolyte interphase components in silicon–lithium alloy anode batteries probed by FTIR spectroscopy

Herein we report the solid reaction products from the chemical reaction of aprotic battery electrolyte and three purported components of the Si-based anode SEI : SiO 2 nanoparticles (NPs), lithium silicate (Li x SiO y ) powders, and Si NPs. We use FTIR and classical molecular dynamics/density functional perturbation theory to assess the solid products remaining with these model materials after exposure to electrolyte. The absence of electrochemical bias provides a view of the chemical speciation resulting from early-stage chemical reactivity during battery assembly as well as under open circuit storage conditions. We believe these species represent the initial stages of SEI growth and predict they likely drive subsequent chemical and electrochemical reactions by controlling molecular interactons at the Si active material interface. We find that nominally equivalent materials react differently even before any electrochemistry is performed (e.g., acidic SiO 2 dissolves whereas alkaline SiO 2 is relatively robust), and derive new understanding of the chemical species that could and could not form stable SEI components in Si-based anodes. These results can be used to inform how to passivate Si anode surfaces and potentially generate an artificially engineered SEI that would be stable and enable next-generation battery anodes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Crack-Free Silicon Monoxide as Anodes for Lithium-Ion Batteries

The volume expansion of Si and SiO particles was investigated using a single-particle battery assembled with a focused ion beam and scanning electron microscopy (FIB-SEM) system. Single Si and SiO particles were galvanostatically charged and discharged as in real batteries. Microstructural changes of the particles were monitored in situ using FIB-SEM from two different angles. The results revealed that the volume expansion of micrometer size particle SiO was not only much smaller than that of Si, but it also kept its original shape with no sign of cracks. Additionally, this isotropic mechanical property of a SiO particle can be attributed to its microstructure: nanosized Si domains mixed with SiO 2 domains. The nanosized Si domains can mitigate the anisotropic swelling caused by the orientation-dependent lithium-ion insertion; the surrounding SiO 2 domains can act as a buffer to further constrain the localized anisotropic swelling.

25 ENERGY STORAGE↗

Dual functionality of over-lithiated NMC for high energy silicon-based lithium-ion batteries

Owing to their high specific capacity and suitably low operating potential, silicon-based anodes are an attractive alternative to graphite in next-generation lithium-ion batteries. However, silicon anodes suffer from low initial coulombic efficiency and fast capacity decay, limiting their widespread application. Pre-lithiation strategies are highly appealing to compensate for irreversible active lithium loss and to boost the cell energy density. In this work, we maximize the cell energy density by direct pre-lithiation of the NMC (LiNi 0.5 Mn 0.3 Co 0.2 O 2 ) cathode to Li 1+x NMCO 2 without introducing inactive deadweight to either electrode. First, we demonstrate that Li 1+x NMCO 2 can be synthesized chemically, via reaction between NMC and lithium napthalide, and electrochemically. The NMC cathode is tolerant of a one-time over-lithiation up to 60 mA h g NMC -1 , giving capacity retention on par with untreated NMC in half cell electrochemical cycling. Using synchrotron X-ray absorption spectroscopy (ex situ) and diffraction (in situ), we demonstrate that higher amounts of over-lithiation lead to local structure distortion – driven by transition metal reduction to Jahn–Teller active Mn 3+ and Co 2+ – as well as bulk structural hysteresis during over-lithiation and layer “buckling” that increases the amount of lithium extracted from the structure in the charged state. The Li 1+x NMCO 2 with low-to-moderate over-lithiation capacity (23, 46, and 70 mA h g NMC -1 ) is proven to be a highly effective dual-purpose lithium source and cathode material in full cell tests with a commercially relevant Si–graphite anode. These cells show higher capacity, superior cycle life, and improved coulombic efficiencies when compared to those with stoichiometric NMC cathodes. Finally, this study introduces a new and simple method to pre-lithiate layered transition metal oxide cathodes, opening up new possibilities for the development of high energy density lithium-ion batteries with next-generation anodes.

25 ENERGY STORAGE↗

Progress Towards Extended Cycle Life Si-based Anodes: Investigation of Fluorinated Local High Concentration Electrolytes

Silicon (Si) anodes are promising candidates for Li-ion batteries due to their high specific capacity and low operating potential. Implementation has been challenged by the significant Si volume changes during (de)lithiation and associated growth/regrowth of the solid electrolyte interphase (SEI). In this report, fluorinated local high concentration electrolytes (FLHCEs) were designed such that each component of the electrolyte (solvent, salt, diluent) is fluorinated to modify the chemistry and stabilize the SEI of high (30%) silicon content anodes. FLHCEs were formulated to probe the electrolyte salt concentration and ratio of the fluorinated carbonate solvents to a hydrofluoroether diluent. Higher salt concentrations led to higher viscosities, conductivities, and contact angles on polyethylene separators. Electrochemical cycling of Si-graphite/NMC622 pouch cells using the FLHCEs delivered up to 67% capacity retention after 100 cycles at a C/3 rate. Post-cycling X-ray photoelectron spectroscopy (XPS) analyses of the Si-graphite anodes indicated the FLHCEs formed a LiF rich solid electrolyte interphase (SEI). The findings show that the fluorinated local high concentration electrolytes contribute to stabilizing the Si-graphite electrode over extended cycling.

36 MATERIALS SCIENCE↗

Understanding and Enhancing Silicon Nanoparticle Distribution during Electrode Processing

Silicon-dominant anodes are of great interest because of their potential to boost the cell-level energy of state-of-the-art Li-ion batteries. While silicon materials have been extensively studied, understanding interactions at the electrode level has recieved little attention, especially the coating process of Si particles, which plays an equally important role in unlocking the full potential of silicon anodes. Herein, the electrode processing of a Si-dominated anode (52.8 wt%, 3.5–4.5 mAh cm −2 ) is being investigated to understand the relationship of processing on the morphology and properties of Si anodes at the electrode level. It has been found that almost-undetectable Si agglomerates easily form during electrode processing, which grow into largeprotrusions after lithiation and trigger potential internal shorting and self-discharge problems. A facile slurry filtration step is proposed to homogenize the particle distribution within Si-dominant electrodes which improves the electrochemical performance and storage stability of Si-based Li ion batteries.

Wu, Bingbin↗

Hierarchical porous silicon structures with extraordinary mechanical strength as high-performance lithium-ion battery anodes

Abstract Porous structured silicon has been regarded as a promising candidate to overcome pulverization of silicon-based anodes. However, poor mechanical strength of these porous particles has limited their volumetric energy density towards practical applications. Here we design and synthesize hierarchical carbon-nanotube@silicon@carbon microspheres with both high porosity and extraordinary mechanical strength (>200 MPa) and a low apparent particle expansion of ~40% upon full lithiation. The composite electrodes of carbon-nanotube@silicon@carbon-graphite with a practical loading (3 mAh cm −2 ) deliver ~750 mAh g −1 specific capacity, <20% initial swelling at 100% state-of-charge, and ~92% capacity retention over 500 cycles. Calendered electrodes achieve ~980 mAh cm −3 volumetric capacity density and <50% end-of-life swell after 120 cycles. Full cells with LiNi 1/3 Mn 1/3 Co 1/3 O 2 cathodes demonstrate >92% capacity retention over 500 cycles. This work is a leap in silicon anode development and provides insights into the design of electrode materials for other batteries.

25 ENERGY STORAGE↗