Effects of Thiocyanate on Anodic Dissolution of Iron, Chromium, Nickel and Type 304 Stainless Steel: I. Electrochemical Measurements and Surface Morphology

Recently published work investigated themechanism of the catalytic effect of thiocyanate on the active dissolution of ferritic stainless steel (Type 430 stainless steel). This work has been extended to Type 304 stainless steel. Potentiostatic and impedance measurements were performed on pure iron, pure chromium, pure nickel and Type 304 stainless steel in 1 M sulfate solutions at pH = 2.5 and pH= 0. As proposed for Type 430 stainless steel, the catalytic effect of thiocyanate on anodic dissolution of Type 304 stainless steel also appears to be primarily caused by the increased dissolution rate of chromium, counteracting the formation of the Cr-O-Cr passivating network at ledges. Nickel does contribute to the corrosion resistance of Type 304 stainless steel in the presence of thiocyanate, but its beneficial effect appears to be secondary to that of chromium.

36 MATERIALS SCIENCE↗

In-situ Characterization of Cast Stainless Steel Microstructures

Cast austenitic stainless steel (CASS) that was commonly used in U.S. nuclear power plants is a coarse-grained, elastically anisotropic material. The engineering properties of CASS made it a material of choice for selected designs of nuclear power reactor systems. However, the fabrication processes result in a variety of coarse-grain microstructures that are difficult to inspect ultrasonically, largely due to detrimental effects of wave interactions with the microstructure. To address the inspection needs, new approaches that are robust to these phenomena are being sought. However, overcoming the deleterious effects of the coarse-grained microstructure on the interrogating ultrasonic beam will require knowledge of the microstructure and the corresponding acoustic properties of the material, for potential optimization of inspection parameters to enhance the probability of detecting flaws. The goal of improving the reliability and effectiveness of ultrasonic inspection of CASS specimens can therefore potentially be achieved by first characterizing the microstructure of the component. The characterization of CASS microstructure must be done in-situ, to enable dynamic selection and optimization of the ultrasonic inspection technique. This paper discusses the application of ultrasonic measurement methods for classifying the microstructure of CASS components, when making measurements from the outside surface of the pipe or component. Results to date demonstrate the potential of ultrasonic and electromagnetic measurements to classify the material type of CASS for two consistent microstructures-equiaxed-grain material and columnar-grain material.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Crystallography of intergranular corrosion in sensitized austenitic stainless steel

Highlights: • Intergranular corrosion (IGC) in stainless steel was crystallographically discussed. • Grain boundaries (GBs) were classified based on the coincidence site lattice (CSL). • Influence of the Σ value on their IGC susceptibility had a wide range scatter. • IGC susceptibility was characterized by the Σ value and unit cell area of CSL GBs. - Abstract: This study deals with the susceptibility to intergranular corrosion (IGC) in type 304 austenitic stainless steel from a crystallographic viewpoint. An IGC test was conducted using oxalic acid and sensitized stainless steel, whose crystal orientation was analyzed by electron backscattered diffraction (EBSD). GBs were classified according to the misorientation of adjacent grains, and subclassified using the Σ value based on the coincidence site lattice (CSL) model. The width of corroded groove was measured for each GB category, and the effect of GB category on the susceptibility to IGC was examined. Then, the area of the unit cell of CSL boundaries was used to characterize the susceptibility to IGC of CSL boundaries. It was found that no IGC occurred in low-angle GBs with a misorientation of 15°, the width of corroded groove at each Σ boundary exhibited large scatter. The relationship between the width and unit cell area was characterized by a sigmoid curve, and the susceptibility to IGC was well described by the unit cell area.

36 MATERIALS SCIENCE↗

Thermal Aging Degradation of Cast Stainless Steels in LWR Systems

Cast austenitic stainless steels (CASSs) have been extensively used for the large components of light water reactor (LWR) power plants such as primary coolant piping and pump casing. Since a large number of massive CASS components are installed in every modern nuclear power plant, any significant degradation of CASS components will raise serious concerns on the integrity of the entire power plant. Upon the presumption that the replacement cost of such massive components is prohibitive, therefore, thorough scientific understanding and systematic monitoring the thermal aging degradation of CASS components should be essential requirements for assessing the plant safety. In the past few decades many researches have concluded that the formation of Cr-rich α-phase by Spinoidal decomposition of δ-ferrite phase, which is formed in high temperature region during cooling, is the primary mechanism for the thermal embrittlement. Cracking mechanism in the thermally-embrittled duplex stainless steels consists of cleavage initiation at ferrite and crack propagation via separation of ferrite-austenite interphase. It has been known, however, that such thermal aging embrittlement is observed only in accelerated aging conditions and the cast stainless steel grades used in nuclear plants have performed well without experiencing real embrittlement. It has been speculated that long-term thermal aging for ≥ 60 years could lead to further decomposition of designed phases and increase of precipitation. This will result in significantly increased susceptibility to embrittlement or other degradation due to thermal aging-radiation synergistic effect, irradiation-induced degradation, stress-corrosion cracking, and general corrosion. Currently, therefore, the thermal embrittlement of CASS components is one of the most serious concerns for extended operation of nuclear power plants. A scientific research is underway to address the issues related to the thermal aging degradation of CASS components. The research aims to provide knowledge-based conclusive prediction for the integrity of the CASS components of LWR power plants during extended operation up to and beyond 60 years. This presentation intends to provide an introductory overview on the thermal aging phenomena in LWR relevant conditions and discussion on the measurements of mechanical property degradation after accelerated and LWR relevant thermal aging treatments. First, the thermal aging effect on toughness is discussed in terms of the causes of embrittlement and influential parameters. Second, the talk will include a comprehensive discussion on the thermal aging effects in different CASS grades (i.e., CF3, CF3M, CF8, and CF8M), which will focus on the influence of alloying elements such as molybdenum and carbon. Third, approximate analysis on thermal reaction in CASS was carried out using Arrhenius equation to decide the effective temperature range for accelerated aging experiments to simulate 60 and 80 years of services in limited time frame. The results will provide valuable insights in the degree of thermal aging. Fourth, calculation on equilibrium precipitation was performed for model CASS alloys using the CALPHAD program, and the results will be used to describe the precipitation behaviors in association with the degradation in mechanical properties. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Development of nano-structured duplex and ferritic stainless steels by pulverisette planetary milling followed by pressureless sintering

Nano-structured duplex and ferritic stainless steel powders are prepared by planetary milling of elemental Fe, Cr and Ni powder for 40 h and then consolidated by conventional pressureless sintering. The progress of milling and the continuous refinement of stainless steel powders have been confirmed by means of X-ray diffraction and scanning electron microscopy. Activation energy for the formation of duplex and ferritic stainless steels is calculated by Kissinger method using differential scanning calorimetry and is found to be 159.24 and 90.17 KJ/mol respectively. Both duplex and ferritic stainless steel powders are consolidated at 1000, 1200 and 1400 °C in argon atmosphere to study microstructure, density and hardness. Maximum sintered density of 90% and Vickers microhardness of 550 HV are achieved for duplex stainless steel sintered at 1400 °C for 1 h. Similarly, 92% sintered density and 263 HV microhardness are achieved for ferritic stainless steel sintered at 1400 °C. - Highlights: • Synthesized duplex and ferritic stainless steels by pulverisette planetary milling • Calculated activation energy for the formation of duplex and ferritic stainless steels • Studied the effect of sintering temperature on density, hardness and microstructure • Duplex stainless steel exhibits 90% sintered density and microhardness of 550 HV. • Ferritic stainless steel shows 92% sintered density and 263 HV microhardness.

36 MATERIALS SCIENCE↗

Effects of Static Recrystallization and Precipitation on Mechanical Properties of 00Cr12 Ferritic Stainless Steel

The 00Cr12 ferritic stainless steel samples were isothermally held at different temperatures in the range of 700 °C to 1000 °C to investigate the effect of static recrystallization and precipitation on mechanical properties, such as microhardness, tensile strength, and yield strength. The results show that the formation of the fine recrystallized grain, as well as precipitation, coarsening, and dissolution of the second-phase particles, influences the mechanical properties remarkably. The fine recrystallized grain can provide a positive grain boundary-strengthening effect in the sample under a relatively high holding temperature. Coarsening and dissolution of M{sub 23}C{sub 6} result in partial depletion of precipitate hardening. In contrast, the size and number density of MX particles are almost constant, regardless of the holding temperature; therefore, it can provide a better precipitation-hardening effect.

36 MATERIALS SCIENCE↗

Stainless Steel Coating Test Report

A process was developed to coat 316L stainless steel pieces having very low levels of fixed contamination on their surface (~100 dpm/100 cm²). The coating process served to significantly decrease the likelihood of any fixed contamination becoming loose contamination due to physical shocks. Prior to coating, the stainless steel was etched with a commercial methane sulfonic acid (MSA) solution in a heated ultrasonic bath, rinsed with deionized water, cleaned with a basic detergent solution, and then rinsed with deionized water. The MSA etched the surface of the stainless-steel pieces, creating a more favorable surface on which the coating could adhere. Due to the short timeline of the project, only commercially available clear coating products were considered. The clear coating had to be wear-resistant, shock resistant, radiation resistant, and have high adhesion to the surface of the stainless steel. Adhesion of coatings to stainless steel is notoriously difficult. A commercial, high molecular weight polymer coating was found that met these requirements. The adhesion properties of this coating to stainless steel are very good, and are significantly improved by the etching process. The etching process results in a higher surface area that is free of debris and other residues, making the surface much more wetable, and at the same time creating a favorable surface topography for adhesion. The polymer in its uncured form is a low viscosity liquid. It can be applied by brush or pipette, and it cures in air alone, but heat is required to speed up curing and attain the highest performance of the cured polymer. As the project progressed, the project team became interested in the composition of the selected commercial polymer coating, and in ways that this polymer coating could be made more wear resistant and potentially more radiation resistant. Nano-particle addition was chosen as the preferred way to achieve higher performance. Therefore, a series of tests were planned and performed. This report summarizes these tests, and presents the results.

36 MATERIALS SCIENCE↗

Recrystallization and modification of the stainless-steel surface relief under photonic heat load in powerful plasma discharges

Targets made of ITER-grade 316L(N)-IG stainless steel and Russian-grade 12Cr18Ni10Ti stainless steel with a close composition were exposed at the QSPA-T plasma gun to plasma photonic radiation pulses simulating conditions of disruption mitigation in ITER. After a large number of pulses, modification of the stainless-steel surface was observed, such as the formation of a wavy structure, irregular roughness, and cracks on the target surface. X-ray and optic microscopic analyses of targets revealed changes in the orientation and dimensions of crystallites (grains) over a depth of up to 20 μm for 316L(N)-IG stainless steel after 200 pulses and up to 40 μm for 12Cr18Ni10Ti stainless steel after 50 pulses, which is significantly larger than the depth of the layer melted in one pulse (∼10 μm). In a series of 200 tests of ITER-grade 316L(N)-IG ITER stainless steel, a linear increase in the height of irregularity (roughness) with increasing number of pulses at a rate of up to ∼1 μm per pulse was observed. No alteration in the chemical composition of the stainless-steel surface in the series of tests was revealed. A model is developed that describes the formation of wavy irregularities on the melted metal surface with allowance for the nonlinear stage of instability of the melted layer with a vapor/plasma flow above it. A decisive factor in this case is the viscous flow of the melted metal from the troughs to tops of the wavy structure. The model predicts saturation of the growth of the wavy structure when its amplitude becomes comparable with its wavelength. Approaches to describing the observed stochastic relief and roughness of the stainless-steel surface formed in the series of tests are considered. The recurrence of the melting-solidification process in which mechanisms of the hill growth compete with the spreading of the material from the hills can result in the formation of a stochastic relief.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Marine Atmospheric Corrosion of Additively Manufactured Stainless Steels

Additively manufactured (AM) stainless steels exhibit numerous microstructural differences compared to their wrought counterparts, such as Cr enriched dislocation cell structures. The influence these unique features have on a SSs corrosion resistance are still under investigation with most current works limited to laboratory experiments. The work herein shows the first documented study of AM 304L and 316L exposed to a severe marine environment on the eastern coast of Florida with comparisons made to wrought counterparts. Coupons were exposed for 21 months and resulted in significant pitting corrosion to initiate after 1 month of exposure for all conditions. At all times, the AM coupons exhibited lower average and maximum pit depths than their wrought counterparts. After 21 months, pits on average were 4 μm deep for AM 316L specimen and 8 μm deep for wrought specimen. Pits on the wrought samples tended to be nearly hemispherical and polished with some pits showing crystallographic attack while pits on AM coupons exhibited preferential attack at melt pool boundaries and the cellular microstructure.

36 MATERIALS SCIENCE↗

In-situ Characterization of Cast Stainless Steel Microstructures

Cast austenitic stainless steel (CASS) was commonly used in selected designs of nuclear power reactor systems for corrosion resistance and enhanced durability in service. CASS materials are generally coarse-grained and elastically anisotropic in nature, and are consequently difficult to inspect ultrasonically, largely due to detrimental effects of ultrasonic wave interactions with the coarse-grain microstructures. To address the inspection needs for these materials, new approaches that are robust to these phenomena are being developed. However, to enhance the probability of detecting flaws, knowledge of the microstructure and the corresponding acoustic properties of the material may be required. This paper discusses the application of ultrasonic backscatter measurement methods for classifying the microstructure of CASS components, when making measurements from the outside surface of the pipe or component. Results to date from laboratory experiments demonstrate the potential of these measurements to classify the material type of CASS for two homogeneous microstructures—equiaxed-grain material or columnar-grain material. Measurements on mixed or banded microstructures also show correlation with the estimated volume-fraction of columnar grains in the material. However, several operational issues will need to be addressed prior to applying this method for in-situ characterization of CASS microstructure.

CASS↗

Methods for the In-Situ Characterization of Cast Austenitic Stainless Steel Microstructures

Cast austenitic stainless steel (CASS) that was commonly used in U.S. nuclear power plants is a coarse-grained, elastically anisotropic material. Its engineering properties made it a material of choice for selected designs of nuclear power reactor systems. However, the fabrication processes result in a variety of coarse-grain microstructures that make current ultrasonic in-service inspection of components quite challenging. To address inspection needs, new ultrasonic inspection approaches are being sought. However, overcoming the deleterious and variable effects of the microstructure on the interrogating ultrasonic beam may require knowledge of the microstructure, for potential optimization of inspection parameters to enhance the probability of detection (POD). The ability to classify microstructure type (e.g. polycrystalline or columnar) has the potential to guide selection of optimal NDE approaches. This paper discusses the application of ultrasonic and electromagnetic methods for classifying CASS microstructures, when making measurements from the outside surface of the component. Results to date demonstrate the potential of these measurements to discriminate between two consistent microstructures - equiaxed-grain material versus columnar-grain material. The potential for fusion of ultrasonic and electromagnetic measurements for in-situ microstructure characterization in CASS materials will be explored.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Stainless Steel to Titanium Bimetallic Transitions

In order to use stainless steel piping in an LCLS-II (Linac Coherent Light Source Upgrade) cryomodule, stainless steel to titanium bimetallic transitions are needed to connect the stainless steel piping to the titanium cavity helium vessel. Explosion bonded stainless steel to titanium transition pieces and bimetallic transition material samples have been tested. A sample transition tube was subjected to tests and x-ray examinations between tests. Samples of the bonded joint material were impact and tensile tested at room temperature as well as liquid helium temperature. The joint has been used successfully in horizontal tests of LCLS-II cavity helium vessels and is planned to be used in LCLS-II cryomodules. Results of material sample and transition tube tests will be presented.

43 PARTICLE ACCELERATORS↗

Hydrogen effects on the deformation and slip localization in a single crystal austenitic stainless steel

Hydrogen is known to embrittle austenitic stainless steels, which are widely used in high-pressure hydrogen storage and delivery systems, but the mechanisms that lead to such material degradation are still being elucidated. The current work investigates the deformation behavior of single crystal austenitic stainless steel 316L through combined uniaxial tensile testing, characterization and atomistic simulations. Thermally precharged hydrogen is shown to increase the critical resolved shear stress (CRSS) without previously reported deviations from Schmid’s law. Molecular dynamics simulations further expose the statistical nature of the hydrogen and vacancy contributions to the CRSS in the presence of alloying. Slip distribution quantification over large in-plane distances (> 1 mm), achieved via atomic force microscopy (AFM), highlights the role of hydrogen increasing the degree of slip localization in both single and multiple slip configurations. The most active slip bands accumulate significantly more deformation in hydrogen precharged specimens, with potential implications for damage nucleation. For $\langle$110$\rangle$ tensile loading, slip localization further enhances the activity of secondary slip, increases the density of geometrically necessary dislocations and leads to a distinct lattice rotation behavior compared to hydrogen-free specimens, as evidenced by electron backscatter diffraction (EBSD) maps. Finally, the results of this study provide a more comprehensive picture of the deformation aspect of hydrogen embrittlement in austenitic stainless steels.

36 MATERIALS SCIENCE↗

Effect of Surface Treatment on the Surface Characteristics of AISI 316L Stainless Steel

The ability of 316L stainless steel to maintain biocompatibility, which is dependent upon the surface characteristics, is critical to its effectiveness as an implant material. The surfaces of mechanically polished (MP), electropolished (EP) and plasma treated 316L stainless steel coupons were characterized by X-ray Photoelectron Spectroscopy (XPS) and Auger Electron Spectroscopy (AES) for chemical composition, Atomic Force Microscopy for surface roughness, and contact angle measurements for critical surface tension. All surfaces had a Ni concentration that was significantly lower than the bulk concentration of -43%. The Cr content of the surface was increased significantly by electropolishing. The surface roughness was also improved significantly by electropolishing. Plasma treatment had the reverse effect - the surface Cr content was decreased. It was also found that the Cr and Fe in the surface exist in both the oxide and hydroxide states, with the ratios varying according to surface treatment.

Trigwell, Steve↗

Long-term corrosion evaluation of stainless steels in Space Shuttle iodinated resin and water

The effects of stainless steel exposure to iodinated water is a concern in developing the Integrated Water System (IWS) for Space Station Freedom. The IWS has a life requirement of 30 years, but the effects of general and localized corrosion over such a long period have not been determined for the candidate materials. In 1978, Umpqua Research Center immersed stainless steel 316L, 321, and 347 specimens in a solution of deionized water and the Space Shuttle microbial check valve resin. In April 1990, the solution was chemically analyzed to determine the level of corrosion formed, and the surface of each specimen was examined with scanning electron microscopy and metallography to determine the extent of general and pitting corrosion. This examination showed that the attack on the stainless steels was negligible and never penetrated past the first grain boundary layer. Of the three alloys, 316L performed the best; however, all three materials proved to be compatible with an aqueous iodine environment. In addition to the specimens exposed to aqueous iodine, a stainless steel specimen (unspecified alloy) was exposed to moist microbial check valve resin and air for a comparable period. This environment allowed contact of the metal to the resin as well as to the iodine vapor. Since the particular stainless steel alloy was not known, energy dispersive spectroscopy was used to determine that this alloy was stainless steel 301. The intergranular corrosion found on the specimen was limited to the first grain boundary layer.

Krohn, Douglas D.↗

Methods of Measuring Residual Stresses in Additively Manufactured 316L Stainless Steel

The microstructure of AM 316L stainless steel Is different from steel manufactured using conventional methods e.g. casting and forging. Data on the effects of residual stresses in the structural integrity and importance of AM parts (fatigue behavior) must be quantified. Evaluate different methods and identify a viable process for determining residual stresses in 316L stainless steel. Next step is to conduct measurements of residual stresses of samples fabricated by different manufacturers.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Corrosion of 316L & 316H stainless steel in molten LiF-NaF-KF (FLiNaK)

The corrosion behavior of 316L and 316H stainless steels (low and high carbon, respectively) in molten LiF-NaF-KF (FLiNaK) salt at 700 °C for 500 h has been investigated. Tests were performed in 316L stainless steel, pyrolytic boron nitride, and glassy carbon capsule materials. The capsule material had a notable effect on the corrosion behavior of the two stainless steels. Further, the modes of corrosion for the two types of stainless steel in various capsule materials were classified into three categories, namely, uniform surface recession, selective grain boundary Cr dissolution, and the dissolution of Cr in the bulk grains. By most metrics, the 316H stainless steel exhibited slightly superior corrosion resistance, while by others the two stainless steels were comparable. These differences in corrosion behavior are attributed to the differences in grain size and the degree of sensitization.

36 MATERIALS SCIENCE↗