Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SEI”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Solvation Rule for Solid-Electrolyte Interphase Enabler in Lithium-Metal Batteries

Despite the exceptionally high energy density of lithium metal anodes, the practical application of lithium-metal batteries (LMBs) is still impeded by the instability of the interphase between the lithium metal and the electrolyte. To formulate a functional electrolyte system that can stabilize the lithium-metal anode, the solvation behavior of the solvent molecules must be understood because the electrochemical properties of a solvent can be heavily influenced by its solvation status. Here, we unambiguously demonstrated the solvation rule for the solid-electrolyte interphase (SEI) enabler in an electrolyte system. In this study, fluoroethylene carbonate was used as the SEI enabler due to its ability to form a robust SEI on the lithium metal surface, allowing relatively stable LMB cycling. The results revealed that the solvation number of fluoroethylene carbonate must be ≥ 1 to ensure the formation of a stable SEI in which the sacrificial reduction of the SEI enabler subsequently leads to the stable cycling of LMBs.

25 ENERGY STORAGE↗

An Inorganic-Rich Solid Electrolyte Interphase for Advanced Lithium-Metal Batteries in Carbonate Electrolytes

In carbonate electrolytes, the organic-inorganic solid electrolyte interphase (SEI) formed on the lithium (Li) metal anode surface is strongly bonded to Li and experiences the same volume change as Li, thus it undergoes continuous cracking/reformation during plating/stripping cycles. Here we report, an inorganic-rich SEI is designed on a Li metal surface to reduce its bonding energy with Li metal by dissolving 4 M concentrated LiNO 3 in dimethyl sulfoxide (DMSO) as an additive for a fluoroethylene carbonate (FEC) based electrolyte. Due to the aggregate structure of NO 3 - ions and its participation in the primary Li + solvation sheath, abundant Li 2 O, Li 3 N, and LiN x O y grains are formed in the resulting SEI, in addition to the uniform LiF distribution from the reduction of PF 6 - ions. The inorganic-rich SEI’s weak bonding (high interface energy) to Li can effectively promote Li diffusion along the SEI/Li interface and prevent Li dendrite penetration into the SEI. As a result, our designed carbonate electrolyte enables a Li anode to achieve a high Li plating/stripping CE of 99.55% (1 mA cm -2 , 1.0 mAh cm -2 ) and the electrolyte also enables a Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) full cell (2.5 mAh cm -2 ) to retain 75%of its initial capacity after 200 cycles with an outstanding CE of 99.83%.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Resolving Graphite‐Electrolyte Interphase of Lithium‐Ion Batteries using Air‐Tight Ambient Mass Spectrometry

Abstract The formation of a stable solid electrolyte interphase (SEI) at graphite electrode is necessary for lithium‐ion batteries (LIB) to prevent excessive degradation of electrolytes. Until now, the exact organic composition of SEI has not been decisively determined with lithium ethylene mono‐carbonate (LEMC) being one of the debated components. An air‐tight ambient mass spectrometry (MS) platform is developed to directly characterize the air‐sensitive organic components present in SEI. Ionization occurs via a solvent‐free field‐induced process at atmospheric pressure. Our experimental data, based on tandem MS analysis, revealed LEMC to be the major organic component in SEI. This result resolves a long‐standing mystery surrounding the composition of native SEI in LIB, where no trace of the other debated compound, lithium ethylene dicarbonate, was detected. The energetics of fragmentation of LEMC and the corresponding stabilities of various ionic species detected during the air‐tight ambient MS analysis were calculated using density functional theory (DFT). Our findings confirmed favorable protonation energies and suggested the molecular structures for many of the detected species. Solvent (i. e., ethylene carbonate)‐induced stabilization effects observed during the ionization process were also confirmed by DFT. The reported study encourages the routine use of ambient mass spectrometry to characterize both anodic and cathodic electrodes of all battery types as well as to study other air‐sensitive materials in their native state.

25 ENERGY STORAGE↗

Automatic Generation of Chemical Mechanisms for Electrochemical Systems: Solid Electrolyte Interphase Formation in Lithium Batteries

Electrolytes in many lithium ion batteries decompose at the low potentials near the anode. The decomposition products form a layer termed the solid electrolyte interphase (SEI). The composition and growth of the SEI layer significantly affect both the capacity fade and safety of lithium ion batteries. However, SEI formation and growth kinetics are not well understood. In this work, we present an extension of the Reaction Mechanism Generator (RMG) software to automatically generate mechanisms for SEI formation. We extend RMG’s solvation correction framework to account for kinetic solvent effects and demonstrate the accuracy of our technique. We calculate thermochemical parameters for 252 species and rate coefficients for 69 reactions, most with associated solvation corrections. This and additional quantum chemistry data are used to extend RMG’s thermodynamic group additivity and solute parameter estimation schemes to handle lithiated species and add 14 new reaction families to RMG. RMG is additionally extended to simulate electrocatalytic systems. Lastly, we demonstrate RMG on the decomposition of acetonitrile and ethylene carbonate near a battery anode. Furthermore, while this framework does not yet resolve individual ions, as appropriate thermochemistry estimators are not available, and thus, cannot yet resolve more complex electrochemical pathways, RMG is able to generate reasonable pathways for SEI formation that match literature pathways and products. In particular, RMG identifies a new important reaction pathway that is not present in literature.

Chemical reactions↗

Resolving Current-Dependent Regimes of Electroplating Mechanisms for Fast Charging Lithium Metal Anodes

Poor fast-charge capabilities limit the usage of rechargeable Li metal anodes. Understanding the connection between charging rate, electroplating mechanism, and Li morphology could enable fast-charging solutions. In this report we develop a combined electroanalytical and nanoscale characterization approach to resolve the current-dependent regimes of Li plating mechanisms and morphology. Measurement of Li + transport through the solid electrolyte interphase (SEI) shows that low currents induce plating at buried Li||SEI interfaces, but high currents initiate SEI-breakdown and plating at fresh Li||electrolyte interfaces. The latter pathway can induce uniform growth of {110}-faceted Li at extremely high currents, suggesting ion-transport limitations alone are insufficient to predict Li morphology. At battery relevant fast-charging rates, SEI-breakdown above a critical current density produces detrimental morphology and poor cyclability. Thus, prevention of both SEI-breakdown and slow ion-transport in the electrolyte is essential. This mechanistic insight can inform further electrolyte engineering and customization of fast-charging protocols for Li metal batteries.

25 ENERGY STORAGE↗

Surface SiO 2 Thickness Controls Uniform-to-Localized Transition in Lithiation of Silicon Anodes for Lithium-Ion Batteries

Silicon is a promising anode material for lithium-ion batteries because of its high capacity, but its widespread adoption has been hampered by a low cycle life arising from mechanical failure and the absence of a stable solid–electrolyte interphase (SEI). Understanding SEI formation and its impact on cycle life is made more complex by the oxidation of silicon materials in air or during synthesis, which leads to SiO x coatings of varying thicknesses that form the true surface of the electrode. Here, the lithiation of SiO 2 -coated Si is studied in a controlled manner using SiO 2 coatings of different thicknesses grown on Si wafers via thermal oxidation. SiO 2 thickness has a profound effect on lithiation: below 2 nm, SEI formation followed by uniform lithiation occurs at positive voltages versus Li/Li + . Si lithiation is reversible, and SiO 2 lithiation is largely irreversible. Above 2 nm SiO 2 , voltammetric currents decrease exponentially with SiO 2 thickness. For 2–3 nm SiO 2 , SEI formation above 0.1 V is suppressed, but a hold at low or negative voltages can initiate charge transfer whereupon SEI formation and uniform lithiation occur. Cycling of Si anodes with an SiO 2 coating thinner than 3 nm occurs at high Coulombic efficiency (CE). If an SiO 2 coating is thicker than 3–4 nm, the behavior is totally different: lithiation at positive voltages is strongly inhibited, and lithiation occurs at poor CE and is highly localized at pinholes which grow over time. As they grow, lithiation becomes more facile and the CE increases. Pinhole growth is proposed to occur via rapid transport of Li along the SiO 2 /Si interface radially outward from an existing pinhole, followed by the lithiation of SiO 2 from the interface outward.

25 ENERGY STORAGE↗

Impact of dual-layer solid-electrolyte interphase inhomogeneities on early-stage defect formation in Si electrodes

While intensive efforts have been devoted to studying the nature of the solid-electrolyte interphase (SEI), little attention has been paid to understanding its role in the mechanical failures of electrodes. Here we unveil the impact of SEI inhomogeneities on early-stage defect formation in Si electrodes. Buried under the SEI, these early-stage defects are inaccessible by most surface-probing techniques. With operando full field diffraction X-ray microscopy, we observe the formation of these defects in real time and connect their origin to a heterogeneous degree of lithiation. This heterogeneous lithiation is further correlated to inhomogeneities in topography and lithium-ion mobility in both the inner- and outer-SEI, thanks to a combination of operando atomic force microscopy, electrochemical strain microscopy and sputter-etched X-ray photoelectron spectroscopy. Our multi-modal study bridges observations across the multi-level interfaces (Si/LixSi/inner-SEI/outer-SEI), thus offering novel insights into the impact of SEI homogeneities on the structural stability of Si-based lithium-ion batteries. Severe structural deformation during (de)lithiation is the main factor limiting the stability of Si anodes in Li-ion batteries. Here, a multi-modal approach is used to visualize these deformations in their early-stage and link them to inhomogeneities in the dual-layer solid-electrolyte interphase.

25 ENERGY STORAGE↗

Real-time mass spectrometric characterization of the solid–electrolyte interphase of a lithium-ion battery

Solid-electrolyte interphase (SEI) is a key component that dictates the performance of most electrochemical devices, but the understanding of its chemistry and structure has been limited by the lack of in-situ tools. In this work, we report SEI live-formation in Li-ion battery under operando condition with liquid secondary ion mass spectrometry (SIMS), which, in combination with molecular dynamics (MD) simulation, presents the first dynamic picture with molecular-accuracy about this key component. Before any interphasial chemistry occurs during the initial charging, an electric double layer forms at the electrode-electrolyte interface via the self-assembly of solvent molecules directed by both Li+ and potential of the electrified surface. Such double layer structure predicts the eventual interphasial chemistries formed from the electrolytes, where the negatively-charged electrode surface repels salt anions from the inner-Helmholtz layer and results in an inner SEI that is thin, dense and inorganic in nature but LiF-depleted. It was this dense layer that exercises the major functions of an interphase, i.e., conducting Li+ but insulating electrons. An outer layer that is electrolyte-permeable and organic-rich appears after formation of the inner SEI. In highly-concentrated electrolyte, the presence of LiF in the inner-SEI is raised due to the high population of salt anions in the double layer. These real-time observations at nano-scale reveal in general sense how an interphase inherits chemistry from inner-Helmholtz layer structure, and establish guidelines in engineering desirable interphases for the future battery chemistries.

Zhou, Yufan↗

Analysis of an all-solid state nanobattery using molecular dynamics simulations under an external electric field

Present Li-ion battery (LIB) technology requires strong improvements in performance, energy capacity, charging-time, and cost to expand their application to e-mobility and grid storage. Li-metal is one of the most promising materials to replace commercial anodes such as graphite because of its 10 times higher specific capacity. However, Li-metal has high reactivity with commercial liquid electrolytes; thus, new solid materials are proposed to replace liquid electrolytes when Li-metal anodes are used. We present a theoretical analysis of the charging process in a full nanobattery, containing a LiCoO 2 cathode, a Li 7 P2S 8 I solid-state electrolyte (SSE), a Li-metal anode as well as Al and Cu collectors for the cathode and anode, respectively. In addition, we added a Li 3 P/Li 2 S film as a solid electrolyte interphase (SEI) layer between the Li-anode and SSE. Thus, we focus this study on the SEI and SSE. We simulated the charging of the nanobattery with an external voltage by applying an electric field. We estimated temperature profiles within the nanobattery and analyzed Li-ion transport through the SSE and SEI. Here, we observed a slight temperature rise at the SEI due to reactions forming $PS_{3}^{–}$ and $P_{2}S_{7}^{4}$$^{–}$ fragments at the interfaces; however, this temperature profile changes due to the charging current under the presence of the external electric field ε = 0.75 V Å –1 . Without the external field, the calculated open-circuit voltage (OCV) was 3.86 V for the battery, which is within the range of values of commercial cobalt-based LIBs. This voltage implies a spontaneous fall of available Li-ions from the anode to the cathode (during discharge). The charge of this nanobattery requires overcoming the OCV plus an additional voltage that determines the charging current. Thus, we applied an external potential able to neutralize the OCV, plus an additional 1.6 V to induce the transport of Li + from the cathode up to the anode. Several interesting details about Li + transport paths through the SSE and SEI are discussed.

25 ENERGY STORAGE↗

Solvent oligomerization pathways facilitated by electrolyte additives during solid-electrolyte interphase formation

The solid–electrolyte interphase (SEI) layer formation is known to play an important role in determining the lifetime of lithium-ion batteries. A thin, stable SEI layer is linked to overall improved battery performance and longevity, however, the factors and mechanisms that lead to optimal SEI morphology and composition are not well understood. Inclusion of electrolyte additives (fluoroethylene carbonate, FEC; and vinylene carbonate, VC) is often necessary for improving SEI characteristics. To understand how these electrolyte additives impact SEI formation, we employed molecular dynamics (MD) and density functional theory (DFT) simulations to study the reaction networks and oligomerization pathways, respectively, for three systems containing ethylene carbonate (EC), a lithium ion, and FEC or VC. MD simulations suggest radical oligomerization pathways analogous to traditional oligomerization with nucleophilic alkoxide species via SN1 reaction mechanisms. Both S N 1 and S N 2 mechanisms were studied for all three systems using DFT. Oligomerization reactions were studied with both a standard alkoxide species and a ring-opened EC radical as the nucleophiles and EC, FEC, and VC as the electrophiles. For all cases, FEC and VC exhibited lower free energy barriers and more stable adducts when compared with EC. We conclude that one of the role of additives is to modify the oligomerization process of EC by introducing branching points (FEC) or termination points (VC).

25 ENERGY STORAGE↗

Interfacial solvation-structure regulation for stable Li metal anode by a desolvation coating technique

Rechargeable lithium (Li) metal batteries face challenges in achieving stable cycling due to the instability of the solid electrolyte interphase (SEI). The Li-ion solvation structure and its desolvation process are crucial for the formation of a stable SEI on Li metal anodes and improving Li plating/stripping kinetics. This research introduces an interfacial desolvation coating technique to actively modulate the Li-ion solvation structure at the Li metal interface and regulate the participation of the electrolyte solvent in SEI formation. Through experimental investigations conducted using a carbonate electrolyte with limited compatibility to Li metal, the optimized desolvation coating layer, composed of 12-crown-4 ether-modified silica materials, selectively displaces strongly coordinating solvents while simultaneously enriching weakly coordinating fluorinated solvents at the Li metal/electrolyte interface. This selective desolvation and enrichment effect reduce solvent participation to SEI and thus facilitate the formation of a LiF-dominant SEI with greatly reduced organic species on the Li metal surface, as conclusively verified through various characterization techniques including XPS, quantitative NMR, operando NMR, cryo-TEM, EELS, and EDS. The interfacial desolvation coating technique enables excellent rate cycling stability (i.e., 1C) of the Li metal anode and prolonged cycling life of the Li||LiCoO 2 pouch cell in the conventional carbonate electrolyte (E/C 2.6 g/Ah), with 80% capacity retention after 333 cycles.

42 ENGINEERING↗

Atomistic modeling of LiF microstructure ionic conductivity and its influence on nucleation and plating

We report the formation and degradation of the solid electrolyte interphase (SEI) and its underlying transport properties play an essential role in the overall performance of lithium-ion batteries. This paper presents classical molecular dynamics studies on polycrystalline inorganic lithium fluoride (LiF) layers to model and predict the SEI transport properties. The ionic conductivity is obtained from the lithium-ion diffusivity in polycrystalline structures of LiF using the Nernst-Einstein relation. The predicted molecular dynamics data are used in a continuum scale phase-field model to evaluate the plating kinetics under fast charging conditions. The analysis emphasizes that the SEI ionic conductivity properties impact the plating dynamics, where SEI's low ion conductivity value is prone to large plating and subsequent capacity degradation. The combination of atomic and continuum scale studies shown herein lays a foundation to tune in SEI transport properties to decrease the amount of lithium plating and improve the performance of fast-charging batteries.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Engineering Solid Electrolyte Interphase Composition by Assessing Decomposition Pathways of Fluorinated Organic Solvents in Lithium Metal Batteries

Studies have shown fluorinated electrolyte solvents can form desirable solid electrolyte interphase (SEI) in lithium metal batteries. In this study, we develop a detailed mechanistic understanding of two high performing electrolytes, Fluoroethylene Carbonate (FEC) and Difluoroethylene Carbonate (DFEC) to demonstrate minimal structural variations can lead to different decomposition products, and thereby the nature of the SEI. Using density functional theory (DFT) calculations, we find different initial bond-breaking mechanisms between FEC and DFEC. We develop free energy diagrams for the decomposition pathways including both electrochemical and chemical steps. Using the computational Li electrode, we identify the largest limiting potential of 1.77 V for FEC decomposition, associated with the formation of lithium fluoride, lithium oxide and FEC oligomers, and 1.53 V for DFEC, which correspond to the formation of polymerized vinylene carbonate and lithium fluoride. We suggest the formation of oligomers in the case of FEC instead of long polymers may lead to better SEI compactness. We also demonstrate the SEI components of FEC and DFEC are not stable on typical cathode voltage (3.87 V). This study presents a unified electrocatalytic perspective on SEI formation and decomposition.

25 ENERGY STORAGE↗

The Solid Electrolyte Interphase Dispersion Can Predict Cycle and Calendar Lifetimes in Silicon Anodes for Lithium-Ion Batteries

The solid electrolyte interphase (SEI) plays a critical role in lithium-ion battery (LIB) anodes. It is responsible for passivating the reactive surface of lithiated anodes against degradation of the electrolyte which enables long cycle and calendar lifetimes for LIBs. This role is especially important in high energy density anodes like silicon, that undergo massive volumetric changes during electrochemical cycling. The mechanism by which the SEI performs this role, however, is not clear which makes designing an SEI to passivate silicon anodes impossible. Through decades of research, dozens of chemical species have been identified within the SEI ranging from inorganic solids to polymeric coatings all of which simultaneously exist in a 'mosaic' composition at the anode surface. This mosaic creates a highly dispersive environment in which electrostatic screening of the anode surface from the electrolyte is not always complete. Here, we present an electrochemical technique to directly test the dispersion at the anode surface. We use this technique to screen more than 20 different electrolytes against silicon anodes and find correlations between both the cycle life and calendar life. The insights from this study offer a new framework to think about the SEI and a rapid screening method to test novel electrode/electrolyte combinations.

battery↗

Dendrite Growth Morphology Modeling in Liquid and Solid Electrolytes

The main goal of this project is to develop a multi-scale modeling approach that connects micron-scale phase-field models and atomic-scale density functional theory (DFT)-based simulations via parameter- and relationship-passing in order to predict Li-metal dendrite morphology evolution, in both liquid and solid electrolytes. The key hypothesis of the DFT-informed phase-field multiscale modeling approach is that it can capture the electrochemical-mechanical driving forces and incorporate the roles of nano-meter-thin solid electrolyte interphase (SEI) in liquid electrolytes as well as of the microstructures of micro-meter-thick solid electrolytes (SEs) for all-solid-state batteries. In this project, we have formulated and implemented phase-field models to incorporate the electrochemical driving forces in liquid electrolytes and then incorporate mechanical driving forces to simulate dendrite growth in solid electrolytes with resolved microstructures. We have implemented two treatments for the SEI: an explicit model to include the microstructure of the SE or SEI in the phase field model and an implicit model to simulate the impact of nano-meter thick SEI in liquid electrolytes by varying the electrode/electrolyte interfacial properties. The key interfacial properties, including the electronic and ionic transport properties, the charge transfer reaction kinetics, and mechanical properties, were computed by DFT-based calculations. At the DFT-based model, one key advancement is to directly predict the charge transfer reaction kinetics at a complex Li/SEI/electrolyte interface by linking DFT with density functional tight binding (DFTB) calculations. As the main accomplishments, we have demonstrated two successful predictions in both solid electrolyte and liquid electrolyte based on this multiscale approach. The predicted intergranular Li dendrite growth in LLZO revealed the importance of trapped electrons at internal interfaces in the microstructure of LLZO. The predicted electroplating morphology of mossy Li and faceted Mg agreed well with experiments. The insights provided by the multiscale model and the model enabled electrolyte and SEI design will accelerate the development of Li-metal electrode for high energy density batteries, that meet DOE’s target on cell density (>350 Wh/kg) and cost below $100/kWhuse for EV applications.

25 ENERGY STORAGE↗

Understanding Solid-Electrolyte Interphase Formation at the Lithium Metal Anode of Lithium-Sulfur Batteries

Lithium-sulfur (Li-S) batteries are one of the most promising chemistries for the next generation of energy storage devices. In a standard Li-S cell, the metallic lithium anode is an essential component of the battery due to its low density, extremely high theoretical specific capacity, and very low negative electrochemical potential. However, several challenges related to the use of Li metal have prevented this battery technology from becoming commercially available. For instance, Li-anodes are highly reactive, which results in the continuous decomposition of the electrolyte and the formation of the solid-electrolyte interphase (SEI) layer. This, combined with the non-uniform deposition of Liions during plating at the anode surface, can seriously affect the performance, cycling, and safety of the battery. In addition, it has been suggested that a controlled SEI formation at the metallic Li anode can yield enhanced battery performance. Hence, a comprehensive understanding of how the SEI layer is formed can help elucidate improvements in this battery technology. In this work, the formation of the SEI layer in Li-S batteries is investigated using density functional theory (DFT) and ab initio molecular dynamics (AIMD) simulations. The stability of liquid organic-based electrolyte components, salt concentration, electron-rich environments, and the use of inorganic solid-state electrolyte (SSE) materials are explored in order to provide molecular-level fundamental insights into how the nature and composition of the electrolyte can alter the initial stages of the SEI formation. The products of electrolyte decomposition and electro-/chemical reaction pathways of liquid electrolyte component such as solvent and salts are predicted from AIMD simulations of electrolyte-anode interfaces. Energetics of reactions from DFT ground-state optimizations are also presented to confirm the decomposition mechanisms. Some significant differences are then drawn regarding the use of low and high salt concentrations. Simulations under electron-rich environments show additional multielectron electrochemical reactions of solvent and salt decomposition taking place due to the excess of electrons and the presence of radical anions in the solution. Finally, the initial stages of formation, stability, and main constituents of interfaces between Li-metal and Sbased electrodes with sulfide-based SSEs are characterized in detail.

25 ENERGY STORAGE↗

Enabling 4C Fast Charging of Lithium–Ion Batteries by Coating Graphite with a Solid–State Electrolyte

Enabling fast-charging (≥4C) of lithium-ion batteries is an important challenge to accelerate the adoption of electric vehicles. However, the desire to maximize energy density has driven the use of increasingly thick electrodes, which hinders rate capability. Herein, atomic layer deposition is used to coat a single-ion conducting solid electrolyte (Li 3 BO 3 -Li 2 CO 3 ) onto postcalendered graphite electrodes, forming an artificial solid-electrolyte interphase (SEI). When compared to uncoated control electrodes, the solid electrolyte coating: 1) eliminates natural SEI formation during preconditioning; 2) decreases interphase impedance by >75% compared to the natural SEI; and 3) extends cycle life under 4C charging conditions, enabling retention of 80% capacity after 500 cycles (compared to 12 cycles in the uncoated control) in pouch cells with >3 mAh cm –2 loading. Furthermore, this work demonstrates that 4C charging without Li plating can be achieved through purely interfacial modification without sacrificing energy density and sheds new light on the role of the SEI in Li plating and fast-charge performance.

25 ENERGY STORAGE↗

Performance degradation due to anodic failure mechanisms in lithium-ion batteries

Here, we report a mechano-chemical model for anodic degradation during fast-charging of nickel-manganese-cobalt (NMC)/graphite (C) cell due to SEI growth, lithium plating/stripping, dead lithium storage, and film fracture of composite SEI and plated lithium film. Degradation of the battery is analyzed for a range of charging rates from 1 to 6 C-rates, and the influence of plating mechanisms – lithium plating and dead lithium deposition and recovery during stripping – on the film resistance of the anode are accounted for in the model. Dynamic evolution of the interfacial properties is modeled using rule-of-mixture approach. Model predictions of plating associated stress fields are used to compute critical energy release rate for film cracking. The results indicate an increased tendency of fracture for thinner SEI film with lithium plating at higher charging rates. The process of reforming the cracked film absorbs a significant portion of the electrode current thereby reducing the cell capacity and plating efficiency. The mechano-chemical model provides an extensive analytical framework for understanding the synergistic coupling of anodic degradation mechanisms, prognosticating conditions of SEI failure, and evaluating the capacity fade and efficiency of lithium-ion battery.