Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Ni dissolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

135 records · Page 8

Structure/Interface Coupling Effect for High-Voltage LiCoO 2 Cathodes

LiCoO 2 (LCO) is widely applied in today's rechargeable battery markets for consumer electronic devices. However, LCO operations at high voltage are hindered by accelerated structure degradation and electrode/electrolyte interface decomposition. To overcome these challenges, co-modified LCO (defined as CB-Mg-LCO) that couples pillar structures with interface shielding are successfully synthesized for achieving high-energy-density and structurally stable cathode material. Benefitting from the "Mg-pillar" effect, irreversible phase transitions are significantly suppressed and highly reversible Li + shuttling is enabled. Interestingly, bonding effects between the interfacial lattice oxygen of CB-Mg-LCO and amorphous Co x B y coating layer are found to elevate the formation energy of oxygen vacancies, thereby considerably mitigating lattice oxygen loss and inhibiting irreversible phase transformation. Meanwhile, interface shielding effects are also beneficial for mitigating parasitic electrode/electrolyte reactions, subsequent Co dissolution, and ultimately enable a robust electrode/electrolyte interface. As a result, the as-designed CB-Mg-LCO cathode achieves a high capacity and excellent cycle stability with 94.6% capacity retention at an extremely high cut-off voltage of 4.6 V. We report these findings provide new insights for cathode material modification methods, which serves to guide future cathode material design.

25 ENERGY STORAGE↗

Additive engineering for robust interphases to stabilize high-Ni layered structures at ultra-high voltage of 4.8 V

Nickel-rich layered cathode materials promise high energy density for next-generation batteries when coupled with lithium metal anodes. However, the practical capacities accessible are far less than the theoretical values due to their structural instability during cycling, especially when charged at high voltages. Here we demonstrate that stable cycling with an ultra-high cut-off voltage of 4.8 V can be realized by using an appropriate amount of lithium difluorophosphate in a common commercial electrolyte. The Li||LiNi 0.76 Mn 0.14 Co 0.10 O 2 cell retains 97% of the initial capacity (235 mAh g -1 ) after 200 cycles. The cycling stability is ascribed to the robust interphase on the cathode. It is formed by lithium difluorophosphate decomposition, which is facilitated by the catalytic effect of transition metals. The decomposition products (Li 3 PO 4 and LiF) form a protective interphase. This suppresses transition metal dissolution and cathode surface reconstruction. It also facilitates uniform Li distribution within the cathode, effectively mitigating the strain and crack formation.

25 ENERGY STORAGE↗

Density functional modeling of the binding energies between aluminosilicate oligomers and different metal cations

Interactions between negatively charged aluminosilicate species and positively charged metal cations are critical to many important engineering processes and applications, including sustainable cements and aluminosilicate glasses. In an effort to probe these interactions, here we have calculated the pair-wise interaction energies (i.e., binding energies) between aluminosilicate dimer/trimer and 17 different metal cations M n+ (M n+ = Li + , Na + , K + , Cu + , Cu 2+ , Co 2+ , Zn 2+ , Ni 2+ , Mg 2+ , Ca 2+ , Ti 2+ , Fe 2+ , Fe 3+ , Co 3+ , Cr 3+ , Ti 4+ and Cr 6+ ) using a density functional theory (DFT) approach. Analysis of the DFT-optimized structural representations for the clusters (dimer/trimer + M n+ ) shows that their structural attributes (e.g., interatomic distances) are generally consistent with literature observations on aluminosilicate glasses. The DFT-derived binding energies are seen to vary considerably depending on the type of cations (i.e., charge and ionic radii) and aluminosilicate species (i.e., dimer or trimer). A survey of the literature reveals that the difference in the calculated binding energies between different M n+ can be used to explain many literature observations associated with the impact of metal cations on materials properties (e.g., glass corrosion, mineral dissolution, and ionic transport). Analysis of all the DFT-derived binding energies reveals that the correlation between these energy values and the ionic potential and field strength of the metal cations are well captured by 2nd order polynomial functions ( R 2 values of 0.99–1.00 are achieved for regressions). Given that the ionic potential and field strength of a given metal cation can be readily estimated using well-tabulated ionic radii available in the literature, these simple polynomial functions would enable rapid estimation of the binding energies of a much wider range of cations with the aluminosilicate dimer/trimer, providing guidance on the design and optimization of sustainable cements and aluminosilicate glasses and their associated applications. Finally, the limitations associated with using these simple model systems to model complex interactions are also discussed.

Gong, Kai↗

xLi2MnO3 (1-x)LiMeO2 and Li4Ti5O12 Cell Chemistry for Behind-the-Meter Storage Applications

Li- and Mn-rich layered oxide material (xLi2MnO3 (1-x)LiMeO2, Me = Ni, Mn, and etc., LMR-NM) is paired with Li4Ti5O12 (LTO) in a full cell and evaluated for the Behind-the-Meter Storage (BTMS) applications. The LMR-NM/LTO full cell shows very high capacities and excellent long-term cycle life. It delivers 192 mAh g-1 after 500 cycles at C/2 and 45 degrees C with a capacity retention of 75% and coulombic efficiency higher than 99.95%. It also has impressive rate capabilities. A capacity of 220 mAh g-1 is achieved at 2C which is 88 % of the initial capacity at C/10. The high cycling temperature clearly enhances electrochemical kinetics and activates more Li2MnO3 component, which gives high capacities, low cell impedance, and better rate capabilities. Moreover, it helps to form a relatively thick cathode-electrolyte interphase (CEI) film to suppress transition metal dissolution from the cathode surface. The upper cut-off voltage (UCV) of 3.0 V keeps the structural integrity of the cathode during cycling. A higher UCV of 3.2 V accelerates structural instabilities of the cathode as well as growth of the solid-electrolyte interphase (SEI) via transition metal dissolution and deposition on the anode surface. It results in higher cell impedance, worse capacity retention and faster capacity fade.

behind-the-meter storage↗

Speciation of Transition Metal Dissolution in Electrolyte from Common Cathode Materials

Abstract Significant capacity loss has been observed across extended cycling of lithium‐ion batteries cycled to high potential. One of the sources of capacity fade is transition metal dissolution from the cathode active material, ion migration through the electrolyte, and deposition on the solid‐electrolyte interphase on the anode. While much research has been conducted on the oxidation state of the transition metal in the cathode active material or deposited on the anode, there have been limited investigations of the oxidation state of the transition metal ions dissolved in the electrolyte. In this work, X‐ray absorption spectroscopy has been performed on electrolytes extracted from cells built with four different cathode active materials (LiMn 2 O 4 (LMO), LiNi 0.5 Mn 1.5 O 4 (LNMO), LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), and (x Li 2 MnO 3 *(1‐x) LiNi a Mn b Co c O 2 , with a+b+ c =1) (LMRNMC)) that were cycled at either high or standard potentials to determine the oxidation state of Mn and Ni in solution. Inductively coupled plasma‐mass spectrometry has been performed on the anodes from these cells to determine the concentration of deposited transition metal ions. While transition metal ions were found dissolved in all electrolytes, the oxidation state(s) of Mn and Ni were determined to be dependent on the cathode material and independent of cycling potential.

Rynearson, Leah↗

Interphase Engineering Enabled by Using a Separator with Electrochemically Active Carbazole Polymers for Lithium-Ion Batteries

Separators are generally considered inert components in lithium-ion batteries. In the past, some electroactive polymers have been successfully applied in separator modifications for overcharge protection or as acid scavengers. This study highlights the first use of two “electroactive” carbazole polymers (copolymer 9-phenyl-9H-carbazole-phenyl [PCP] and poly(9-vinylcarbazole) [PVC]), which were each applied separately as coatings on the cathode-facing side of commercial Celgard 2325 separators, respectively, to enhance the cycling performance of 0.3Li 2 MnO 3 ·0.7LiMn 0.5 Ni 0.5 O 2 //graphite (LMR-NM//Gr) full cells through interphase engineering. The team observed an irreversible polymer oxidation process of the carbazole-functionalized polymers—occurring only during the first charge—for the modified separator cells, and the results were confirmed by dQ/dV analysis, cyclic voltammetry measurements, and nuclear magnetic resonance characterizations. During this oxidation, carbazole polymers participate in the process of interphase formation, contributing to the improved cycling performance of LMR-NM//Gr batteries. Particularly, oxidation takes place at voltages of ~4.0 and ~3.5 V when PCP and PVC are used as separator coatings, which is highly irreversible. Further postmortem examinations suggest that the improvements using these modified separators arise from the formation of higher-quality and more inorganic SEI, as well as the beneficial CEI enriched in LixPOyFz. These interphases effectively inhibit the crosstalk effect by reducing TM dissolution.

carbazole↗

Deformation mechanisms in an additively manufactured dual-phase eutectic high-entropy alloy

Nanostructured metals and alloys often exhibit high strengths but at the expense of reduced ductility. Through harnessing the far-from-equilibrium processing conditions of laser powder-bed fusion (L-PBF) additive manufacturing, we develop a dual-phase nanolamellar structure comprised of FCC/L1 2 and BCC/B2 phases in a Ni 40 Co 20 Fe 10 Cr 10 Al 18 W 2 eutectic high-entropy alloy (EHEA), which exhibits a combination of ultrahigh yield strength (>1.4 GPa) and large tensile ductility (~17%). The deformation mechanisms of the additively manufactured EHEA are studied via in-situ synchrotron X-ray diffraction and high-resolution transmission electron microscopy. The high yield strength mainly results from effective blockage of dislocation motion by the high density of lamellar interfaces. The refined nanolamellar structures and low stacking fault energy (SFE) promote stacking fault (SF)-mediated deformation in FCC/L1 2 nanolamellae. The accumulation of abundant dislocations and SFs at lamellar interfaces can effectively elevate local stresses to promote dislocation multiplication and martensitic transformation in BCC/B2 nanolamellae. The cooperative deformation of the dual phases, assisted by the semi-coherent lamellar interfaces, gives rise to the large ductility of the as-printed EHEA. In addition, here we also demonstrate that post-printing heat treatment allows us to tune the non-equilibrium microstructures and deformation mechanisms. After annealing, the significantly reduced SFE and thicknesses of the FCC nanolamellae facilitate the formation of massive SFs. The dissolution of nano-precipitates in the BCC/B2 nanolamellae reduces spatial confinement and further promotes martensitic transformation to enhance work hardening. Our work provides fundamental insights into the rich variety of deformation mechanisms underlying the exceptional mechanical properties of the additively manufactured dual-phase nanolamellar EHEAs.

36 MATERIALS SCIENCE↗

Microstructural evolution in a precipitate-hardened (Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 ) 94 Ti 2 Al 4 multi-principal element alloy during high-pressure torsion

Multi-principal element alloys demonstrate high strength, thermal stability, and irradiation resistance, making them excellent candidate materials for applications in nuclear reactors and other harsh environments. Some studies have examined the use of high-pressure torsion to strengthen MPEAs through grain size reduction and strain hardening. However, no studies have investigated the effect of HPT on secondary phases (precipitates) within an MPEA. Two alloys, (Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 ) 94 Ti 2 Al 4 containing Ni(Ti, Al) B2 phase, and CrFe σ phase, and single-phase Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 , were fabricated by casting and heat treatment. Both alloys were then processed with HPT to study microstructural evolution. Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were used to characterize the alloys before and after HPT processing. HPT processing produced a nanocrystalline structure in both alloys, but (Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 ) 94 Ti 2 Al 4 exhibited a significantly smaller grain size and higher dislocation density than Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 , with corresponding higher hardness. Before HPT, the (Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 ) 94 Ti 2 Al 4 alloy consisted of large grain (~ 400 μm) and precipitates, including B2 of ~ 38 μm average size, B2 of ~ 0.7 μm average size, and small amounts of σ of ~ 1.5 μm average size. After HPT, the larger B2 precipitates were decreased in size and volume fraction, while the smaller B2 precipitates were completely dissolved; the σ precipitates appeared unaffected by HPT, likely due to their much higher hardness. Finally, observation of the B2 precipitate distribution along radial distance indicates that the strain caused the precipitates to fracture at intermediate strain (γ = 125) and dissolve at high strain (γ = 280).

36 MATERIALS SCIENCE↗

Atomic-scale constituting stable interface for improved LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathodes of lithium-ion batteries

Ascribed to their higher capacity and lower cost compared to conventional LiCoO 2 , the Ni-rich layered LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) is now considered as one promising cathode for lithium-ion batteries (LIBs). However, it still suffers from some evident performance degradation, especially under high cutoff voltages (i.e., >4.3 V versus Li/Li + ). The performance degradation typically is exhibited as capacity fading and voltage drop, mainly originating from an instable interface between the NMC622 and electrolyte as well as the evolution of the NMC structure. To improve the interfacial and structural stability of NMC cathodes, herein we deposited an ultrathin layer of Al 2 O 3 coatings (<5 nm) conformally over NMC622 composite electrodes directly using atomic layer deposition (ALD). It was found that, under different upper cutoff voltages (4.3, 4.5, and 4.7 V), the ALD Al 2 O 3 coatings enable enhanced performance of NMC622 cathodes with better cyclability and higher capacity. Particularly, the beneficial effects of the ALD Al 2 O 3 coatings are more remarkable at higher upper cutoff voltages (4.5 and 4.7 V). Furthermore, the ALD coatings can significantly improve the rate capability of NMC622. To this end, we utilized a suite of characterization tools and performed a series of electrochemical tests to clarify the effects of the ALD Al 2 O 3 coatings. This study revealed that the beneficial effects of the Al 2 O 3 ALD coatings are multiple: (i) serving as an artificial layer of solid electrolyte interphase to mitigate undesirable interfacial reactions; (ii) acting as a physical barrier to inhibit metal dissolution of NMC; and (iii) forming a reinforced networked overcoating to boost the mechanical integrity of NMC cathodes. This study is favorable for designing high-performance NMC cathodes.

25 ENERGY STORAGE↗