Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MARTENSITE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Crystallographic stability of the BCC phase during quenching of metastable beta titanium alloy Ti-5553 and comparison of structural criteria for the predictive capability of α” martensite

This work evaluates the compositional standard currently developed for Ti-5553 powder and explores the metastable β region for sensitivity to martensitic formation during rapid quenching from the melt. Ti-5553 is a beta-stabilized titanium alloy that is increasingly being used in additive manufacturing applications. A series of alloys within the Ti-5553 compositional space was processed using two-piston spat quenching to perform rapid solidification and quenching for each of these alloy compositions. Typical empirical models such as molybdenum equivalency are not able to fully separate the retained BCC and martensitic compositions. Further, the use of thermodynamic data to estimate the transformation energy needed to form martensite can differentiate the alloys and provide a metric to further develop compositional limits for metastable beta titanium alloy development.

36 MATERIALS SCIENCE↗

In-situ determination of austenite and martensite formation in 13Cr6Ni2Mo supermartensitic stainless steel

In-situ analysis of the phase transformations in a 13Cr6Ni2Mo supermartensitic stainless steel (X2CrNiMoV13-5-2) was carried out using a thermo-magnetic technique, dilatometry and high temperature X-ray diffractometry (HT-XRD). A combination of the results obtained by the three applied techniques gives a valuable insight in the phase transformations during the austenitization treatment, including subsequent cooling, of the 13Cr6Ni2Mo supermartensitic stainless steel, where the magnetic technique offers a high accuracy in monitoring the austenite fraction. It was found by dilatometry that the austenite formation during heating takes place in two stages, most likely caused by partitioning of Ni into austenite. The in-situ evolution of the austenite fraction is monitored by high-temperature XRD and dilatometry. The progress of martensite formation during cooling was described with a Koistinen-Marburger relation for the results obtained from the magnetic and dilatometer experiments. Enhanced martensite formation at the sample surface was detected by X-ray diffraction, which is assumed to be due to relaxation of transformation stresses at the sample surface. Due to the high alloy content and high thermodynamic stability of austenite at room temperature, 4 vol.% of austenite was found to be stable at room temperature after the austenitization treatment. - Highlights: Black-Right-Pointing-Pointer We in-situ analyzed phase transformations and fractions of a 13Cr6Ni2Mo SMSS. Black-Right-Pointing-Pointer Higher accuracy of the austenite fraction was obtained from magnetic technique. Black-Right-Pointing-Pointer Austenite formation during heating takes place in two stages. Black-Right-Pointing-Pointer Enhanced martensite formation at the sample surface detected by X-ray diffraction.

36 MATERIALS SCIENCE↗

Determination of dislocation density by electron backscatter diffraction and X-ray line profile analysis in ferrous lath martensite

The microstructure and the dislocation density in as-quenched ferrous lath martensite were studied by different methods. The blocks, packets and variants formed due to martensitic transformation were identified and their sizes were determined by electron backscatter diffraction (EBSD). Concomitant transmission electron microscopy (TEM) investigation revealed that the laths contain subgrains with the size between 50 and 100 nm. A novel evaluation procedure of EBSD images was elaborated for the determination of the density and the space distribution of geometrically necessary dislocations from the misorientation distribution. The total dislocation density obtained by X-ray diffraction line profile analysis was in good agreement with the value determined by EBSD, indicating that the majority of dislocations formed due to martensitic transformation during quenching are geometrically necessary dislocations.

36 MATERIALS SCIENCE↗

Martensite crystal structure in Ru-based high temperature shape memory alloys

Highlights: • A three level twinned microstructure is recognized in the β″ phase. • Wavy contrast boundaries which are typical for translation interfaces • Displacements are translations of tetragonal β′ phase, lost during transformation. • Six times bigger monoclinic cell is characterized by the disappearance of 5 translations. - Abstract: High temperature shape memory alloys RuNb and RuTa were investigated by X-ray diffraction in order to determine the structure of the low temperature β” martensite. Powder X-ray diffraction and Rietveld analysis confirm the monoclinic symmetry and allow a precise determination of the atom positions. The low temperature microstructure is the result of a martensitic transformation from a tetragonal β′ martensite. The analysis of how it is controlled by the space groups of the two phases and by their relative orientation is performed by transmission electron microscopy. A three level twinned microstructure is recognized in the β” phase. The investigation at the smallest scale twins reveals the presence of wavy contrast boundaries which are typical for translation interfaces. High resolution transmission electron microscopy images, accompanied by phase contrast imaging analysis, have been used to determine the translation vectors associated to the interfaces. These displacements are the translations of the tetragonal β′ phase which are lost during the transformation. The combination of X-ray diffraction and transmission electron microscopy investigation allows the suggestion of a global distortion mechanism that explains the atomic displacements in the β” form.

36 MATERIALS SCIENCE↗

Suppressing heating rate-dependent martensitic stabilization in ductile Cu-Al-Mn shape memory alloys by Ni addition: An experimental and first-principles study

Highlights: • Additional nearest neighbor bond between Ni and Al atoms was produced theoretically in the Cu-Al-Mn-Ni (Ni≤2 at.%) alloys. • Shape memory effect of Cu-Al-Mn alloys heated at 20 K/min was improved from 85% to 92% after the addition of 2 at.% Ni. • Addition of 2 at.% Ni can suppress heating rate-dependent martensitic stabilization in Cu-Al-Mn alloys heated at 0.01 K/min. - Abstract: The present paper aims to suppress the heating rate-dependent martensitic stabilization of ductile Cu-Al-Mn shape memory alloys through restricting the mobility and thus the behavior of vacancies. A combined study based on first-principles calculation and experimental results were presented to unveil the effect of Ni addition into ternary Cu-Al-Mn alloys on the bonding force between atoms. The results showed that additional nearest neighbor bond between Ni and Al atoms in quaternary Cu-Al-Mn-Ni alloys can be produced. The addition of Ni (≤2 at.%) into ternary Cu-Al-Mn alloys can not only efficiently increase the shape memory effect, but also suppress the occurrence of heating rate-dependent martensitic stabilization. The addition of 2 at.% Ni improved the shape memory effect of ternary Cu-Al-Mn alloys from 85% to 92% when heated at 20 k/min. The shape memory effect of ternary Cu-Al-Mn alloys dropped to 10% as the heating rate decreased to 1 K/min, but it remain at 92% even when the heating rate was sufficiently lowered to 0.01 K/min after the addition of 2 at.% Ni.

36 MATERIALS SCIENCE↗

Creep of MARBN-type 9Cr martensitic steel in gaseous CO 2 environment

Here, with an interest in moving from steam to supercritical CO 2 as the working fluid in advanced energy systems, it is important to study the mechanical response of structural alloys to CO 2 -containing environments. MARBN-type 9Cr martensitic steel was originally developed for application in boilers for supercritical and ultra-supercritical power plants where the steam temperature reaches 650 °C. In this research, a MARBN-type 9Cr martensitic steel designed and manufactured at NETL was creep tested in a gaseous CO 2 environment (i.e., 0.1 MPa at 650 °C), and the results are directly compared to creep tests conducted in air. It was found that environmentally-assisted cracking facilitated by carbide formation beneath the growing oxide accelerated failure in gaseous CO 2 . This work indicates that creep-oxidation interactions in advanced martensitic steels represent an important consideration for materials selection in supercritical CO 2 power cycles. Furthermore, this work confirms that more oxidation-resistant alloys will be required for the highest temperature portions of these systems.

36 MATERIALS SCIENCE↗

In-situ neutron diffraction investigation of two-stage martensitic transformation in a 13%Mn steel with serrated deformation

Two stage austenite →ε-martensite →α-martensite phase transformation, phase-specific lattice strain evolution and load sharing during tensile deformation of a 13%Mn hot-rolled austenitic steel are revealed by in-situ neutron diffraction. In conclusion, direct evidence is provided that serrated deformation behavior is attributed to discontinuous martensitic transformation.

Austenitic steel↗

Evidence of martensitic phase transitions in magnetic Ni-Mn-In thin films

Ni{sub 50}Mn{sub 35}In{sub 15} Heusler alloy thin films (with thicknesses of about 10 nm) have been grown on single crystal MgO and SrTiO{sub 3} (STO) (100) substrates using a laser-assisted molecular beam epitaxy method. Films of mixed austenitic and martensitic phases and of pure martensitic phase have been detected for those grown on MgO and STO substrates, respectively. Thermomagnetic curves were measured using a SQUID magnetometer and are consistent with those of off-stoichiometric In-based bulk Heusler alloys, including a martensitic transition at T = 315 K for films grown on MgO. The differences in the properties of the films grown on MgO and STO are discussed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Study of electroless Ni-W-P alloy coating on martensitic stainless steel

Electroless nickel phospor (Ni-P) is widely used in many industries due to their corrosion and wear resistance, coating uniformity, and ability to coat non-conductive surfaces. The unique properties of tungsten such as high hardness, higher melting point, lower coefficient of linear thermal expansion, and high tensile strength have created a lot of interest in developing ternary Ni-W-P alloys. This article presents the study of electroless Ni-W-P alloys coating using acid or alkaline bath on martensitic stainless steel. Nickel sulfate and sodium tungstate were used as nickel and tungsten sources, respectively, and sodium hypophosphite was used as a reducing agent. Acid or alkaline bath refer to bath pH condition was adjusted by adding sulfuric acid. Martensitic stainless steel was immersed in Ni-W-P bath for 15, 30, and 60 minutes. The substrate of martensitic stainless steel was subjected to pre-treatment (polishing and cleaning) and activation prior to electroless plating. The plating characteristics were investigated for concentration ratio of nickel and hypophosphite (1:3), sodium tungstate concentration 0,1 M, immersion time (15 min, 30 min, 60 min), and bath condition (acid, alkaline). The electroless Ni-W-P plating was heat treated at 400°C for 1 hour. Deposits were characterized using scanning electron microscope (SEM) and corrosion measurement system (CMS).

36 MATERIALS SCIENCE↗

Magnetostructural martensitic transformations with large volume changes and magneto-strains in all-d-metal Heusler alloys

The all-d-metal Mn{sub 2}-based Heusler ferromagnetic shape memory alloys Mn{sub 50}Ni{sub 40−x}Co{sub x}Ti{sub 10} (x = 8 and 9.5) are realized. With a generic comparison between d-metal Ti and main-group elements in lowering the transformation temperature, the magnetostructural martensitic transformations are established by further introducing Co to produce local ferromagnetic Mn-Co-Mn configurations. A 5-fold modulation and (3, −2) stacking of [00 10] of martensite are determined by X-ray diffraction and HRTEM analysis. Based on the transformation, a large magneto-strain of 6900 ppm and a large volume change of −2.54% are observed in polycrystalline samples, which makes the all-d-metal magnetic martensitic alloys of interest for magnetic/pressure multi-field driven applications.

36 MATERIALS SCIENCE↗

Phonon-deformational generalized ginzburg-landau functionals for describing martensite transitions between FCC and BCC structures in metals

A method is developed for theoretical description of martensite transitions between fcc and bcc phases of metals based on generalized Ginzburg-Landau functionals (GGLFs), in which the transformation parameters are the 'phonon' parameter describing relative slips of close-packed atomic planes and fcc lattice deformations in the region of a martensite inclusion. General expressions are proposed for calculating the deformational contributions to the GGLF. Local strains and local elastic moduli in the region of martensite inclusions are estimated numerically. The possibility of constructing phenomenological expressions for the GGLF using interpolations of available experimental data on the structure and elastic moduli in the fcc and bcc phases is discussed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structure of tetragonal martensite in the In{sub 95.42}Cd{sub 4.58} cast alloy

The structure of martensite in the In{sub 95.42}Cd{sub 4.58} alloy has been studied by metallography, X-ray diffraction, dilatometry, and transmission electron microscopy. It has been shown that a massive structure built of colonies of tetragonal lamellar plates divided by a twin boundary {101}FCT is formed in the alloy under cooling below the martensite FCC → FCT transition temperature. The alloy recrystallizes after a cycle of FCT → FCC → FCT transitions with a decrease in the grain size by several times compared with the initial structure such fashion that the size of massifs and individual martensite lamella in the massif correlates with the change in the size of the alloy grain. Using thermal cycling, it has been revealed that the alloy tends to stabilize the high-temperature phase.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Development of Novel Ferritic-Martensitic Steels with Superior Creep Properties for Power Plant Applications

A creep resistant martensitic steel, CPJ-7, was developed with an operating temperature approaching 650°C. Subsequently, another creep resistant martensitic steel, JMP, was designed with the potential to operate at, or slightly above, 650°C. This report describes the development of these alloys from early iterations of CPJ steels to the final CPJ-7 formulation as well as the more heat resistant JMP steel formulation. The design originated from computational modeling for phase stability and precipitate strengthening using fifteen constituent elements. Approximately forty heats of CPJ and ten of JMP, each weighing ~7 kg, were vacuum induction melted. A computationally optimized heat treatment schedule was developed to homogenize the ingots prior to hot forging and rolling prior to final normalization and tempering. Overall, wrought and cast versions of CPJ-7 present superior creep properties when compared to wrought and cast versions of COST alloys for steam turbine and wrought and cast versions of P91/92 for boiler applications. For instance, the Larson Miller Parameter curve for CPJ-7 at 650°C almost coincides with that of COST E at 620°C. The prolonged creep life was attributed to slowing down the process of the destabilization of the MX and M 23 C 6 precipitates at 650°C. On the other hand, the cast version of CPJ-7 also revealed superior mechanical performance, well above commercially available cast 9% Cr martensitic steel or derivatives, especially for creep life at 650°C. The casting process employed slow cooling to simulate the conditions of a thick wall full-size steam turbine casing but utilized a separate homogenization step prior to final normalization and tempering. To advance the development of CPJ-7 for commercial applications, a process was used to scale up the production of the alloy using vacuum induction melting (VIM) and electroslag remelting (ESR), which underlined the importance of melt processing control of intentionally designed minor and trace elements in these advanced alloys. Following the work on CPJ-7, the JMP steels were designed with higher Co for increased solid solution strengthening, Si for oxidation resistance and increased W (with low Mo content) for matrix strength and stability as well as solid solution strengthening. The JMP steels showed increases in creep life compared to CPJ-7 between 118 to 150% at 650°C for testing at various stresses between 138 MPa and 207 MPa. On a Larson-Miller plot, the performance of the JMP steels surpasses that of state-of-the-art MARBN and other MARBN-type steels. The influence of various elements within the composition of the alloys on the microstructure and mechanical properties are discussed. This report presents approximately 420,000 h of in-house creep testing, the equivalent of almost 50 years of cumulative creep tests.

36 MATERIALS SCIENCE↗

Effect of tailored martensitic transformation in a thick weld: Residual stresses mitigation, heterogeneous microstructure, and mechanical properties

The residual stresses, microstructural heterogeneities, and mechanical properties were extensively examined in a 25 mm thick weld consisting of two regions which respectively undergo phase transformation at relatively low (100 °C) temperature (LTT) and high (670 °C) temperature (HTT) during cooling. Due to the LTT martensitic transformation, which features a transformation strain of ~4000 με, large compressive residual stress (−510 MPa) was generated as confirmed by neutron diffraction and contour method. Meanwhile, significant heterogeneities were observed in terms of the chemical composition, yield strength, and microhardness across the interface between the LTT and HTT regions. The dependency of martensitic transformation starting temperature (M{sub s}) on chemical composition is empirically formulated, and it reveals that the dependency of M{sub s} on the Ni and Cr compositions becomes stronger when the temperature is lower than 200 °C. The maximum change of residual stresses (σ{sub x}{sup max}) exponentially decreases as M{sub s} decreases in the manner of σ{sub x}{sup max} = 97.5 exp(M{sub s}/227)-649. The fracture behavior was found highly dependent upon the volume fraction of retained austenite influenced by M{sub s}. While a ductile fracture mode was found in the cellular LTT region containing relatively higher amount of retained austenite (~10%), the interface shows transgranular brittle fracture features and sub-cracking due to the relatively small amount of retained austenite and the predominant martensite constituent.

36 MATERIALS SCIENCE↗

Austenite formation and cementite dissolution during intercritical annealing of a medium-manganese steel from a martensitic condition

In the present study, in situ high-energy X-ray diffraction (HEXRD), dilatometry, and metallography were conducted for the purpose of understanding microstructure evolution during intercritical annealing of a Fe-0.19C-4.39Mn steel from a martensitic initial condition. Three different simulations for austenite growth and solute partitioning during isothermal holding were conducted using the DICTRA™ module of Thermo-Calc®. The microstructures after intercritical annealing exhibit film-like retained austenite; however, in situ HEXRD indicates that retained austenite in the initial martensitic microstructure had decomposed upon heating to the isothermal holding temperature, suggesting that film-like austenite may be generated during intercritical annealing via nucleation and growth of new austenite and without necessarily preserving initial retained austenite films in the martensitic microstructure. Metallography and in situ HEXRD also indicate that cementite had formed upon heating but did not readily dissolve during an 1800 s isothermal hold although considerable growth of austenite had occurred during the isothermal hold, suggesting that austenite nucleation and initial growth during intercritical annealing does not solely occur due to carbon partitioning. A simulation incorporating cementite suggests that the increase in austenite fraction during intercritical annealing initially occurs in association with Mn partitioning followed by austenite growth induced by gradual cementite dissolution.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of high Mn-containing ferritic-martensitic alloys exposed to cyclical thermal treatment

Substantial residual tensile stress tends to accumulate in currently available high-Cr ferritic martensitic steels that are subjected to cyclical heat treatment, which leads to premature brittle fracture. By tailoring the alloy composition, this thermal cycling can be exploited to induce a high number density of nanoprecipitates and phase transformations countering residual tensile stresses. In this work, three new variants of ferritic-martensitic steels have been designed with computational thermodynamics to meet the goals of mitigating residual tensile stresses by lowering martensite start temperatures and of enhancing mechanical strength and irradiation sink strength by increasing the number density of nanoprecipitates. Furthermore, ctenast materials were subjected to cyclical heat treatment. The thermally cycled samples were evaluated with mechanical testing and microstructural analysis to identify the optimal composition in which figures of merit include low residual stress and a high density of nanoscale MX (M = metal, X = C/N) precipitates, leading to high yield strength with reasonable ductility. The noticeably higher density of nanoprecipitates in the optimal alloy favor its higher yield strength, which is supported by the microstructure-derived yield strength calculation and precipitation kinetics simulation.

36 MATERIALS SCIENCE↗

Two-step deformation-induced martensitic transformation in additively manufactured High-Si stainless steel

Deformation-induced phase transformation in the additively manufactured (AM) Fe–18Cr–8Ni-5.5Si (in wt.%) alloy was analyzed using the in-situ electron backscattered diffraction (EBSD) record during uniaxial tensile testing in a scanning electron microscope (SEM). Analysis of EBSD data was focused to investigate phase transformation behavior during deformation with consideration of mechanical interactions among phases and grains in the ultrafine AM microstructure. The initial EBSD phase map illustrated that the as-built microstructure was a duplex structure consisting of major austenite (γ) and minor ferrite phases, some of which showed non-traditional orientation relationship since the rapid solidification in the AM process has produced non-equilibrium state in phase formation. In the deformed as-built AM alloy, the two-step martensitic transformation (γ→ε→α´) was identified as the main deformation-induced transformation mechanism. Martensitic transformation steps were found to be associated with glides of Shockley partial dislocations on closed packed (111) planes under the influence of atomic disturbance in the γ and ε phases, respectively. Using the closed-packed plane pole figures and unit cell orientations, their evolutions and mechanisms accompanying with the transformation were analyzed. Finally, the results indicate that one variant of ε-martensite forms from their parent γ phase, while two variants of α´ form from their parent ε phase.

36 MATERIALS SCIENCE↗

Boundaries for martensitic transition of 7 Li under pressure

We report that physical properties of lithium under extreme pressures continuously reveal unexpected features. These include a sequence of structural transitions to lower symmetry phases, metal-insulator-metal transition, superconductivity with one of the highest elemental transition temperatures, and a maximum followed by a minimum in its melting line. The instability of the bcc structure of lithium is well established by the presence of a temperature-driven martensitic phase transition. The boundaries of this phase, however, have not been previously explored above 3 GPa. All higher pressure phase boundaries are either extrapolations or inferred based on indirect evidence. Here we explore the pressure dependence of the martensitic transition of lithium up to 7 GPa using a combination of neutron and X-ray scattering. We find a rather unexpected deviation from the extrapolated boundaries of the hR3 phase of lithium. Furthermore, there is evidence that, above ~3 GPa, once in fcc phase, lithium does not undergo a martensitic transition.

36 MATERIALS SCIENCE↗