Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “HYDRIDES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Correlating Thermodynamic and Kinetic Hydricities of Rhenium Hydrides

The kinetics of hydride transfer from Re( R bpy)(CO) 3 H (bpy = 4,4'-R-2,2'-bipyridine; R = OMe, t Bu, Me, H, Br, COOMe, CF 3 ) to CO 2 and seven different cationic N-heterocycles were determined. Additionally, the thermodynamic hydricities of complexes of the type Re( R bpy)(CO) 3 H were established primarily using computational methods. Linear free-energy relationships (LFERs) derived by correlating thermodynamic and kinetic hydricities indicate that, in general, the rate of hydride transfer increases as the thermodynamic driving force for the reaction increases. Kinetic isotope effects range from inverse for hydride transfer reactions with a small driving force to normal for reactions with a large driving force. Hammett analysis indicates that hydride transfer reactions with greater thermodynamic driving force are less sensitive to changes in the electronic properties of the metal hydride, presumably because there is less buildup of charge in the increasingly early transition state. Bronsted α values were obtained for a range of hydride transfer reactions and along with DFT calculations suggest the reactions are concerted, which enables the use of Marcus theory to analyze hydride transfer reactions involving transition metal hydrides. It is notable, however, that even slight perturbations in the steric properties of the Re hydride or the hydride acceptor result in large deviations in the predicted rate of hydride transfer based on thermodynamic driving forces. This indicates that thermodynamic considerations alone cannot be used to predict the rate of hydride transfer, which has implications for catalyst design.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Stability of zirconium hydride

This reports complete Milestone M2.2.1 Stability of zirconium hydride: Experimental investigation of the hydrogen concentration of encapsulated zirconium hydride before and after joining. In this milestone, we first report the successful fabrication of crack-free bulk zirconium hydride by using the ORNL static hydriding system. The fabricated hydride was characterized by using X-ray diffraction (XRD) and X-ray computed tomography (XCT). XRD results showed that the δ-phase zirconium hydride, α-zirconium, and ε-phase hydride were present. XCT confirmed the absence of the internal cracking. The hydrogen concentration was determined by the weight change before and after hydrogen loading, given the fact that the oxide phase was not found during XRD analysis. Two metallic cladding materials, i.e., molybdenum and FeCrAl, were selected to encapsulate the fabricated zirconium hydride pellets. Demonstration capsules were designed and machined. Mo crucible was successfully sealed by using a combination of electron beam welding and gas tungsten arc welding. Due to the undesired neutronics property of Mo, further investigation of this cladding material was not pursued. Electron beam welding and laser beam welding were employed to seal the FeCrAl capsules. XRD were performed on the zirconium hydride before and after the sealing. The results showed that the welding process has negligible impact on the hydrogen content in the FeCrAl-canned zirconium hydride. The presented work fulfilled the proposed work under this milestone and paves a pathway to fabricate single-phase zirconium hydride and to develop robust cladding materials to can bulk zirconium hydride.

36 MATERIALS SCIENCE↗

Sensitivity study of hydrogen Soret transport in yttrium Hydride-Based nuclear fuel

Yttrium hydride is an excellent solid neutron moderator material for high temperature nuclear reactor applications due to its high hydrogen density and exceptional hydride stability at high temperatures. Despite these attractive characteristics, the details of how hydrogen behaves within yttrium hydride while temperature gradients exist are still not well understood. The evolution of the hydrogen composition profile resulting from a temperature gradient requires knowledge of hydrogen’s heat of transport, a critical parameter that has not yet been measured for this material. In this work, we perform hydride redistribution, hydrogen dissociation, and hydrogen leakage calculations while varying the Soret heat of transport of hydrogen in yttrium hydride to elucidate the sensitivity of hydride stability under temperature gradients to this parameter. This study analyzes hydride stability of a hypothetical uranium-yttrium hydride nuclear fuel design during operation of a high temperature liquid metal-cooled nuclear reactor. Assuming U-YH x could be fabricated in a physically stabilized manner, this fuel system can likely maintain hydride stability while operating at very high power densities and temperatures. We find that even though the hydrogen dissociation pressure in the gas gap does vary by several percent as the heat of transport temperature parameter is varied, the hydrogen content in the U-YH x fuel meat is relatively insensitive to this parameter over the course of a high burnup fuel cycle; this is due to yttrium hydride’s excellent hydrogen retention under the high temperature conditions considered here. Here, this suggests that hydride stability analyses are insensitive to the value of the Soret heat of transport in U-YH x under steady state liquid metal-cooled reactor conditions. However, the susceptibility to internal gas overpressurization-induced stress-rupture of the cladding during a high temperature transient is more sensitive to this parameter due to the non-linear dependence of hydrogen gas dissociation pressure vs. composition and temperature.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Low-Cost Metal Hydride Thermal Energy Storage System for Concentrating Solar Power Systems

The objective of this research was to evaluate and demonstrate a metal hydride-based TES system for use with a CSP system. A unique approach has been applied to this project that combines our modeling experience with the extensive material knowledge and expertise at both SRNL and Curtin University (CU). Because of their high energy capacity and reasonable kinetics many metal hydride systems can be charged rapidly. Metal hydrides for vehicle applications have demonstrated charging rates in minutes and tens of minutes as opposed to hours. This coupled with high heat of reaction allows metal hydride TES systems to produce very high thermal power rates (approx. 1kW per 6-8 kg of material). A major objective of this work is to evaluate some of the new metal hydride materials that have recently become available. A problem with metal hydride TES systems in the past has been selecting a suitable high capacity low temperature metal hydride material to pair with the high temperature material. A unique aspect of metal hydride TES systems is that many of these systems can be located on or near dish/engine collectors due to their high thermal capacity and small size. The primary objective of this work is to develop a high enthalpy metal hydride that is capable of reversibly storing hydrogen at high temperatures (> 650 °C) and that can be paired with a suitable low enthalpy metal hydride with low cost materials. Furthermore, a demonstration of hydrogen cycling between the two hydride beds is desired.

25 ENERGY STORAGE↗

Technology Enabling Zero-EPZ Micro Modular Reactors: Fabrication of Zirconium Hydride with Controlled Hydrogen Loading

This report completes Milestone M2.2.2 - ZrH pellet fabricated with controlled hydride loading: ZrH1.5±0.1 single phase pellets fabricated with controlled and thermally stable hydride loading. Hydrogen content to be quantified and single-phase confirmed by X-ray diffraction. In this milestone, we report the successful fabrication of delta-phase zirconium hydride pellets using the ORNL bulk metal hydriding system. The successful deployment of zirconium hydride moderator in advanced reactors requires development of a consistent and affordable production pathway along with implementation of a hydrogen retention solution throughout the reactor life. Fabrication of delta-phase zirconium hydride is challenging since the absorption of a large amount of hydrogen into alpha-zirconium induces significant volume expansion and the present hydrogen concentration gradient results in cracking. A fully programmable hydriding system with continuous hydrogen partial pressure and flow control to facilitate processing of massive metal hydride has been developed at ORNL. In this report, the working principle of the hydriding system will be introduced. Characterization of the produced zirconium hydride includes X-ray powder diffraction to identify the present phases and X-ray Computed Tomography to visualize the internal microstructure (including cracks). The results indicate that single delta-phase zirconium hydride pellets with various sizes have been successfully produced.

36 MATERIALS SCIENCE↗

Developing Capability for Hydride Moderator Manufacturing to Facilitate Thermal Spectrum Design Options

This report provides a summary of efforts to develop the capability to fabricate massive crack-free yttrium hydride samples to support thermal spectrum design options for the Transformational Challenge Reactor (TCR) in FY2019. The challenges to fabricating massive, crack-free single-phase yttrium hydride are discussed. By using a modified static hydriding system, we have successfully demonstrated the fabrication of crack-free yttrium hydride, guided by the well-established thermodynamics of the binary yttriumhydrogen system. The presence of α-phase yttrium in the fabricated yttrium hydride necessitates employing temperature-pressure isochore cooling at the end of the hydriding process. Thus, a fully programmable hydriding system with continuous hydrogen partial pressure and flow control coordinated with precise temperature control has been designed to facilitate processing of massive, crack-free metal hydrides with the desired H/Y atom ratio. The new system is capable of fabricating yttrium hydride samples that will be used to establish a complete database of yttrium hydride to support the application of yttrium hydride as a high-performance moderator material in the TCR and other nuclear systems.

36 MATERIALS SCIENCE↗

Microstructure of surface cerium hydride growth sites

Samples of cerium were exposed to hydrogen under controlled conditions causing cerium hydride sites to nucleate and grow on the surface. The hydriding rate was measured in situ, and the hydrides were characterised using secondary ion mass spectrometry, scanning electron microscopy, and optical microscopy. The results show that the hydriding rate proceeded more quickly than earlier studies. Characterisation confirmed that the hydrogen is confined to the sites. The morphology of the hydrides was confirmed to be oblate, and stressed material was observed surrounding the hydride, in a number of cases lathlike features were observed surrounding the hydride sites laterally with cracking in the surface oxide above them. It is proposed that during growth the increased lattice parameter of the CeH{sub 2} induces a lateral compressive stress around the hydride, which relieves by the ca. 16% volume collapse of the γ-Ce to α-Ce pressure induced phase transition. Cracking of the surface oxide above the laths reduces the diffusion barrier to hydrogen reaching the metal/oxide interface surrounding the hydride site and contributes to the anisotropic growth of the hydrides.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Hydriding performances and modeling of a small-scale ZrCo bed

In order to evaluate the performance of the hydriding of a ZrCo bed, a small-scale getter bed of ZrCo was designed and fabricated. The results show that the hydriding time at room temperature was somewhat shorter than that at higher temperatures of ZrCo and that the performance of hydriding at low temperatures of ZrCo was better than that at high temperatures of ZrCo. The experimental results of the hydrogen pressure of hydriding (ZrCoH{sub 2.8}) at different temperatures were in agreement with the computed values using a numerical modeling equation but with a small difference during the first 10 minutes of the hydriding of ZrCo. The model is based on the Kozeny-Carman equation. The effect of a helium blanket on hydriding was measured and analyzed. The hydriding with no helium blanket in the primary vessel of ZrCo is much faster than that with a helium blanket. The hydriding at a helium concentration of 8% is slower than that at 0%. As the helium concentration increases, the hydriding of ZrCo decreases. The experimental results of the hydriding with 0 %, 4%, and 8% of helium concentration are in agreement with the calculated values but with minimal differences during the first 10 minutes.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Mechanical testing of hydrided fuel cladding

During light water reactor operations, hydrogen is generated from the oxidation of zirconium alloy materials. This hydrogen can be absorbed into the cladding and form zirconium hydrides. At high temperatures and hoop stresses, these normally circumferential oriented hydrides in high burnup used nuclear fuel (HB-UNF) may reorient in the radial direction and affect the mechanical properties of the cladding. Understanding these changes in mechanical properties will aid in analyzing how UNF will perform during storage and transportation. Systems, presented in the article, have been designed to introduce hydrides into cladding specimens, to reorient cladding hydrides, and to test and measure the mechanical properties of these specimens. The hydriding systems consist of a tube furnace capable of pre-hydriding cladding specimens and reorienting cladding hydrides and surface conditioning equipment. Mechanical testing (i.e., tensile, compression, and burst testing) will be performed on both pre-hydrided cladding and cladding with reoriented hydrides, and the results will be compared with those of as-manufactured cladding. Tensile and compression testing will be performed using a 5 kilo-pound load frame; burst testing will be performed on a purpose-built test system. Strain is measured with a digital image correlation (DIC) system. DIC is a real time optical measurement technique that utilizes high-definition imagery to measure object deformation. It is planned that tensile, compression, and burst testing of cladding with reoriented hydrides will begin this year.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Quantifying the stress state in the vicinity of a δ-hydride in α-zirconium

In zirconium alloys, precipitation of a hydride generally introduces internal stresses in the surrounding matrix. This study aims at understanding the role of internal stresses on the formation, growth and arrangement of δ-hydrides in α-zirconium. To this end, a Fast Fourier Transform based discrete dislocation dynamics technique is used to quantify both internal stresses induced during the formation of a hydride and the relief of the internal stresses by dislocation nucleation from the hydride-matrix interface. Overall, this work reveals that stress relaxation is localized in very small regions around the δ-hydride ( 300 nm). Further, it is proposed that the dislocations nucleated from the hydride-matrix interface could act as loci for the nucleation of new hydrides, thereby rationalizing experimentally observed hydride stacks. Finally, quantifying the stress relaxation resulting from dislocation nucleation reveals that diagonal components of the internal stress inside the hydride remain very high, i.e., >3.0 GPa. We find that this suggests that additional dissipative processes, intrinsic to the hydride, are necessary to diminish the aforementioned internal stress.

36 MATERIALS SCIENCE↗

Results of NDE Technique Evaluation of Clad Hydrides

This report fulfills the M4 milestone, M4FT-14IN0805023, Results of NDE Technique Evaluation of Clad Hydrides, under Work Package Number FT-14IN080502. During service, zirconium alloy fuel cladding will degrade via corrosion/oxidation. Hydrogen, a byproduct of the oxidation process, will be absorbed into the cladding and eventually form hydrides due to low hydrogen solubility limits. The hydride phase is detrimental to the mechanical properties of the cladding and therefore it is important to be able to detect and characterize the presence of this constituent within the cladding. Presently, hydrides are evaluated using destructive examination. If nondestructive evaluation techniques can be used to detect and characterize the hydrides, the potential exists to significantly increase test sample coverage while reducing evaluation time and cost. To demonstrate the viability this approach, an initial evaluation of eddy current and ultrasonic techniques were performed to demonstrate the basic ability to these techniques to detect hydrides or their effects on the microstructure. Conventional continuous wave eddy current techniques were applied to zirconium based cladding test samples thermally processed with hydrogen gas to promote the absorption of hydrogen and subsequent formation of hydrides. The results of the evaluation demonstrate that eddy current inspection approaches have the potential to detect both the physical damage induced by hydrides, e.g. blisters and cracking, as well as the combined effects of absorbed hydrogen and hydride precipitates on the electrical properties of the zirconium alloy. Similarly, measurements of ultrasonic wave velocities indicate changes in the elastic properties resulting from the combined effects of absorbed hydrogen and hydride precipitates as well as changes in geometry in regions of severe degradation. However, for both approaches, the signal responses intended to make the desired measurement incorporate a number of contributing parameters. These contributing factors need to be recognized and a means to control them or separate their contributions will be required to obtain the desired information.

36 MATERIALS SCIENCE↗

Hydriding, Oxidation, and Ductility Evaluation of Cr-Coated Zircaloy-4 Tubing

Accident-tolerant fuel concepts have been developed recently in diverse research programs. Recent research has shown clear advantages of Cr-coated Zr cladding over bare cladding tubes regarding oxidation behavior under the design basis loss-of-coolant accident condition. However, limited data are available about the hydriding behavior of the Cr coating. For that purpose, Cr-coated Zricaloy-4 tubes were tested to investigate the effects of hydriding, oxidation, and postquench ductility behavior on coated Zr cladding. A high-power impulse magnetron sputtering (HiPIMS) process was used to produce a high-density coating on the Zircaloy-4 tube surface. Coated and uncoated Zircaloy-4 tube specimens underwent one-sided hydriding in a tube furnace filled with pure hydrogen gas at 425 °C. The tubing specimen ends were sealed with Swagelok plugs before the hydriding runs. For uncoated specimens, H analysis of the hydrided specimens indicated that the H content increased as the test time and initial pressure increased. However, almost no change was observed for the coated specimens that were hydrided under the same test conditions. After one-sided hydriding, the hydrided coated and uncoated specimens were exposed to steam at high temperatures for two-sided oxidation studies to simulate accident conditions. The coated specimens showed a slower oxidation: oxygen pickup was 50% lower than the uncoated specimens tested under the same conditions. Ring compression testing was performed to evaluate the embrittlement behavior of the Cr-coated specimens after hydriding and oxidation. The results indicated that the HiPIMS coating provides excellent protection from hydriding and oxidation at high temperatures.

36 MATERIALS SCIENCE↗

Fabrication of yttrium hydride for high-temperature moderator application

We report given the superior thermal stability and highly attainable hydrogen density, yttrium hydride is an excellent high-temperature moderator material in advanced thermal neutron spectrum reactors that require small core volumes. Large-scale, crack-free, bulk yttrium hydride is in high demand; however, fabrication of yttrium hydride is challenging and has not been demonstrated for nearly half century. The associated challenges are discussed herein. In response to these challenges, a hydriding system was designed and constructed at Oak Ridge National Laboratory and was used to successfully fabricate crack-free yttrium hydride in complex geometries at large scales. This was accomplished by precisely controlling the hydrogen’s partial pressure and the retort temperature, which was informed by the well-established thermodynamic properties of the binary H–Y system. Hydrogen content in as-fabricated hydride was determined by weight change, an approach which was considered reliable based on the use of ultra–high-purity yttrium, the absence of oxide phases up to levels detectable using x-ray diffraction (XRD), and the significant weight gain. Hydrogen distribution along one yttrium hydride rod was evaluated with XRD analysis on materials extracted from different locations on the rod. The results indicated a relatively homogeneous hydrogen distribution along the hydride rod, with <3% uncertainty in the fraction of the δ-phase hydride. In addition, significant efforts are being dedicated to establish a complete database summarizing the thermomechanical and physical properties of as-fabricated yttrium hydride and the irradiation response to facilitate its deployment as a high-temperature moderator in advanced nuclear reactors.

36 MATERIALS SCIENCE↗

The Density of Uranium Hydride Formed Under Mechanical Load

The conversion of uranium metal (ρ = 19 g/cc) to uranium hydride (theoretical ρ = 11 g/cc) results in a large volumetric expansion due to both the density decrease and the substantial porosity of the hydride if not volumetrically constrained. This transformation from a monolithic solid to a particulate material can generate substantial forces when the growing hydride impacts a nearby target. The resulting displacement of the target is dependent upon both its resistance to motion and the strength of the growing hydride. We have observed columns of growing uranium hydride apply forces of hundreds to thousands of pounds to flex high-strength cantilever beams, and have measured applied forces of over 5000 pounds when growing hydride columns impacted rigid targets. The force/displacement behavior of growing uranium hydride was originally modeled by finite element methods to develop an elastic, perfectly plastic constitutive model of UH 3 . The UH 3 constitutive model was then applied to simulate the response of components impacted by growing uranium hydride. More recently we have used an experimental apparatus that simultaneously and independently provides measurement of applied force and target displacement during uranium hydride formation. These efforts confirm previous work and allow for increased confidence in modeling results. The design, testing, and experimental results using such an apparatus over a variety of system stiffnesses and with a variety of sample sizes has been completed. This work extended our understanding of UH 3 growth dynamics and mechanics and enabled the development of a higher fidelity constitutive Drucker-Prager model for UH 3 , and greater confidence in predictions of component behavior in systems impacted by uranium hydride formation.

36 MATERIALS SCIENCE↗

Fatigue Testing and Characterization of Pre-hydrided Zircaloy-4 Cladding Tubes

The solubility of hydrogen in Zircaloy-4 (Zry-4) at the cladding operating temperature is near 100 wt. ppm. Above this solubility limit, excess hydrogen precipitates as δ-hydride platelets in the cladding material. Because of the effect of the thermal gradient across the cladding thickness on the migration and precipitation of hydrogen, hydride rims are often observed at the cladding outer surface; under excessive corrosion conditions hydride blisters are possible. It is well known that the fatigue of metal alloys, especially high cycle fatigue, is sensitive to the status of surface including the microstructure, roughness, and residual stress. Thus, the question considered herein, is whether excessive hydrogen pickup modifies the microstructure such that it has a degradation effect on the fatigue performance of cladding during operation. This report describes the evaluation of fatigue performance of a pre-hydrided Zry-4 cladding. A commercial Zry-4 was polished and pre-hydrided to 800 ppm and 1300 ppm H contents. The fatigue testing was conducted under strain control at 5 Hz with fully-reversed bending by using a cyclic integrated reversible bending fatigue tester (CIRFT). Six specimens with 1300 ppm and one specimen with 800 ppm were tested. Significant variation in test results were observed. While two of the 1300 ppm specimens failed with less than 1 ×10 5 cycles (at 0.32% and 0.41%), the four other samples did not fail over the strain amplitude range of 0.25% to 0.38%. Interestingly, the fracture initiation site of the failed samples was on the outside diameter (OD) surface rather than on the inside diameter (ID) surface as is typical for the as-polished cladding. This suggested a degrading effect of the hydriding process. Subsequently, three of the unfailed specimens were then further tested at ~0.43% to observe where failure initiation occurred. Significant variation was also observed in these three specimens. One specimen failed at ~9000 cycles while the two others failed at 43000 and 1.06 ×10 5 cycles. The performance here correlated to the location of failure initiation; failure initiated on the OD in the sample that failed after 9000 cycles while it initiated on the ID in the sample that failed after 43000 and 1.06 ×10 5 cycles. Flat features at the OD initiation sites suggest a brittle hydride feature on the surface of those samples was the cause of the degradation in fatigue performance, though the overall hydrogen levels in all samples was similar. A summary of all the observations is provided below: • The un-failed specimens with 1300 ppm H were cycled to failure with a higher amplitude near 0.43%. In addition, the fatigue-treated specimen tended to have a longer fatigue at the same induced amplitude. • Fractography revealed a mixed failure mode for the pre-hydrided specimen. Particularly, the specimen with fracture initiation site (FIS) located on the outer diameter surface of tube tended to have a shorter fatigue life than that of FIS on the inner diameter surface. • Etched cross section was shown to have hydride platelets aligned with tube longitudinal axis as expected, and the density of hydrides is at the similar level as in literature data. Meanwhile, a LECO procedure was applied for hydrogen concentration measurement, which showed the measured hydrogen contents are close to the nominal value. • With the polished cladding tube as baseline, O’Donnell-Lager (O-L) analysis showed that a decrease of about 50% in reduction-of-area (RA) would be needed for the O-L fitting to the fatigue data of 1300 ppm cladding. The suggestion for the next steps is provided.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Hydride structures in Ti-aluminides subjected to high temperature and hydrogen pressure charging conditions

The distribution and chemistry of hydrides produced in single and dual phase alloys with a composition near TiAl have been investigated by using a combination of TEM and X-ray diffraction techniques. The alloys were exposed at 650 C to 13.8 MPa of gaseous H2 for 100 h. In the single-phase gamma alloy, large hydrides preferentially nucleated on the grain boundaries and matrix dislocations and a population of small hydrides was distributed throughout the matrix. X-ray and electron diffraction patterns from these hydrides indicated that they have an fcc structure with a lattice parameter of 0.45 nm. EDAX analysis of the hydrides showed that they were enriched in Ti. The hydrides were mostly removed by vacuum annealing at 800 C for 24 h. On dissolution of the hydrides, the chemistry of hydride-free regions of the grain boundary returned to the matrix composition, suggesting that Ti segregation accompanied the hydride formation rather than Ti enrichment causing the formation of the hydride.

Legzdina, D.↗

Hydrided moderators for nuclear reactors

High temperature moderators for nuclear reactors and processes for their production are disclosed. The moderators include at least one hydrided metal and/or hydride metal allow, such as yttrium hydride, thorium hydride, yttrium-cerium hydride, yttrium-gadolinium hydride, yttrium calcium hydride, cerium hydride, etc. Such metal hydrides and/or hydride alloys may have high thermal stability, a relatively low thermal neutron absorption cross section, the ability to retain hydrogen over a large temperature range, and have good mechanical properties. Such moderators may induce spectral shift in reactors which, in turn, magnifies the Doppler reactivity temperature coefficient. Such moderators to thermalize neutrons may also enhance fuel utilization and cost-effectiveness of the reactor while keeping the core portable.

Dasari, Venkateswara Rao↗

Measurement and modeling of strain fields in zirconium hydrides precipitated at a stress concentration

Hydrogen adsorption into zirconium, as a result of corrosion in aqueous environments, leads to the precipitation of a secondary brittle hydride phase. These hydrides tend to first form at stress concentrations such as fretting flaws or cracks in engineering components, potentially degrading the structural integrity of the component. One mechanism for component failure is a slow crack growth mechanism known as Delayed Hydride Cracking (DHC), where hydride fracture occurs followed by crack arrest in the ductile zirconium matrix. The current work employs both an experimental and a modeling approach to better characterize the effects and behavior of hydride precipitation at such stress concentrations. Strains around stress concentrations containing hydrides were mapped using High Energy X-ray Diffraction (HEXRD). These studies highlighted important differences in the behavior of the hydride phase and the surrounding zirconium matrix, as well as the strain associated with the precipitation of the hydride. A finite element model was also developed and compared to the X-ray strain mapping results. This model provided greater insight into details that could not be obtained directly from the experimental approaches, as well as providing a framework for future modeling to predict the effects of hydride precipitation under varied conditions.

08 HYDROGEN↗