Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FILM”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Oxide Ceramic Films Grown on 55Ni-45Ti for NASA and Department of Defense Applications: Unidirectional Sliding Friction and Wear Evaluation

An investigation was conducted to examine the friction and wear behavior of the two types of oxide ceramic films furnished by the U.S. Army Research Laboratory, Development and Engineering Center (ARDEC) under Space Act Agreement SAA3 567. These two types of oxide ceramics were grown on 55Ni-45Ti (60 wt% Ni and 40 wt% Ti) substrates: one was a TiO2 with no other species (designated the B film) and the other was a TiO2 with additional species (designated the G film). Unidirectional ball-on-disk sliding friction experiments were conducted with the oxide films in contact with sapphire at 296 K (23 C) in approx. 50-percent relative humidity laboratory air in this investigation. All material characterization and sliding friction experiments were conducted at the NASA Glenn Research Center. The results indicate that both films greatly improve the surface characteristics of 55Ni-45Ti, enhancing its tribological characteristics. Both films decreased the coefficient of friction by a factor of 4 and increased wear resistance by a two-figure factor, though the B film was superior to the G film in wear resistance and endurance life. The levels of coefficient of friction and wear resistance of both films in sliding contact with sapphire were acceptable for NASA and Department of Defense tribological applications. The decrease in friction and increase in wear resistance will contribute to longer wear life for parts, lower energy consumption, reduced related breakdowns, decreased maintenance costs, and increased reliability.

Miyoshi, Kazuhisa↗

High-Temperature Superconducting/Ferroelectric, Tunable Thin-Film Microwave Components

At the NASA Lewis Research Center, ferroelectric films such as SrTiO3 and Ba(sub x)Sr(sub 1-x)TiO3, are being used in conjunction with YBa(sub 2)Cu(sub 3)O(sub 7-delta) high-temperature superconducting thin films to fabricate tunable microwave components such as filters, phase shifters, and local oscillators. These structures capitalize on the variation of the dielectric constant of the ferroelectric film upon the application of a direct-current electric field, as well as on the low microwave losses of high-temperature superconductors relative to their conventional conductor counterparts. For example, the surface resistance for a YBa(sub 2)Cu(sub 3)O(sub 7-delta) thin film at 10 GHz and 77 K is more than two orders of magnitude lower than that of copper or gold at the same temperature and frequency. SrTiO3 and Ba(sub x)Sr(sub 1-x)TiO3 films are used because their crystal structure and lattice parameters are similar to those of YBa(sub 2)Cu(sub 3)O(sub 7-delta), thus enabling the growth of highly textured YBa(sub 2)Cu(sub 3)O(sub 7-delta) films with high critical current densities (i.e., greater than 1 MA/sq cm) on the underlying ferroelectric film, or alternatively, of highly textured ferroelectric film on the underlying YBa(sub 2)Cu(sub 3)O(sub 7-delta) film.

Miranda, Felix A.↗

Pulsed Laser Deposition of High Temperature Protonic Films

Pulsed laser deposition has been used to fabricate nanostructured BaCe(0.85)Y(0.15)O3- sigma) films. Protonic conduction of fabricated BaCe(0.85)Y(0.15)O(3-sigma) films was compared to sintered BaCe(0.85)Y(0.15)O(3-sigma). Sintered samples and laser targets were prepared by sintering BaCe(0.85)Y(0.15)O(3-sigma) powders derived by solid state synthesis. Films 1 to 8 micron thick were deposited by KrF excimer laser on porous Al2O3 substrates. Thin films were fabricated at deposition temperatures of 700 to 950 C at O2 pressures up to 200 mTorr using laser pulse energies of 0.45 - 0.95 J. Fabricated films were characterized by X-ray diffraction, electron microscopy and electrical impedance spectroscopy. Single phase BaCe(0.85)Y(0.15)O(3-sigma) films with a columnar growth morphology are observed with preferred crystal growth along the [100] or [001] direction. Results indicate [100] growth dependence upon laser pulse energy. Electrical conductivity of bulk samples produced by solid state sintering and thin film samples were measured over a temperature range of 100 C to 900 C. Electrical conduction behavior was dependent upon film deposition temperature. Maximum conductivity occurs at deposition temperature of 900 oC; the electrical conductivity exceeds the sintered specimen. All other deposited films exhibit a lower electrical conductivity than the sintered specimen. Activation energy for electrical conduction showed dependence upon deposition temperature, it varied

Dynys, Fred W.↗

Spray Chemical Vapor Deposition of Single-Source Precursors for Chalcopyrite I-III-VI2 Thin-Film Materials

Thin-film solar cells on flexible, lightweight, space-qualified substrates provide an attractive approach to fabricating solar arrays with high mass-specific power. A polycrystalline chalcopyrite absorber layer is among the new generation of photovoltaic device technologies for thin film solar cells. At NASA Glenn Research Center we have focused on the development of new single-source precursors (SSPs) for deposition of semiconducting chalcopyrite materials onto lightweight, flexible substrates. We describe the syntheses and thermal modulation of SSPs via molecular engineering. Copper indium disulfide and related thin-film materials were deposited via aerosol-assisted chemical vapor deposition using SSPs. Processing and post-processing parameters were varied in order to modify morphology, stoichiometry, crystallography, electrical properties, and optical properties to optimize device quality. Growth at atmospheric pressure in a horizontal hotwall reactor at 395 C yielded the best device films. Placing the susceptor closer to the evaporation zone and flowing a more precursor-rich carrier gas through the reactor yielded shinier-, smoother-, and denser-looking films. Growth of (112)-oriented films yielded more Cu-rich films with fewer secondary phases than growth of (204)/(220)-oriented films. Post-deposition sulfur-vapor annealing enhanced stoichiometry and crystallinity of the films. Photoluminescence studies revealed four major emission bands and a broad band associated with deep defects. The highest device efficiency for an aerosol-assisted chemical vapor deposited cell was one percent.

Hepp, Aloysius F.↗

Synthesis of Poly-Silicon Thin Films on Glass Substrate Using Laser Initiated Metal Induced Crystallization of Amorphous Silicon for Space Power Application

Poly-silicon thin films on glass substrates are synthesized using laser initiated metal induced crystallization of hydrogenated amorphous silicon films. These films can be used to fabricate solar cells on low cost glass and flexible substrates. The process starts by depositing 200 nm amorphous silicon films on the glass substrates. Following this, 200 nm of sputtered aluminum films were deposited on top of the silicon layers. The samples are irradiated with an argon ion cw laser beam for annealing. Laser power densities ranging from 4 to 9 W/cm2 were used in the annealing process. Each area on the sample is irradiated for a different exposure time. Optical microscopy was used to examine any cracks in the films and loss of adhesion to the substrates. X-Ray diffraction patterns from the initial results indicated the crystallization in the films. Scanning electron microscopy shows dendritic growth. The composition analysis of the crystallized films was conducted using Energy Dispersive x-ray Spectroscopy. The results of poly-silicon films synthesis on space qualified flexible substrates such as Kapton are also presented.

Abu-Safe, Husam H.↗

Validation of Supersonic Film Cooling Modeling for Liquid Rocket Engine Applications

Topics include: upper stage engine key requirements and design drivers; Calspan "stage 1" results, He slot injection into hypersonic flow (air); test articles for shock generator diagram, slot injector details, and instrumentation positions; test conditions; modeling approach; 2-d grid used for film cooling simulations of test article; heat flux profiles from 2-d flat plate simulations (run #4); heat flux profiles from 2-d backward facing step simulations (run #43); isometric sketch of single coolant nozzle, and x-z grid of half-nozzle domain; comparison of 2-d and 3-d simulations of coolant nozzles (run #45); flowfield properties along coolant nozzle centerline (run #45); comparison of 3-d CFD nozzle flow calculations with experimental data; nozzle exit plane reduced to linear profile for use in 2-d film-cooling simulations (run #45); synthetic Schlieren image of coolant injection region (run #45); axial velocity profiles from 2-d film-cooling simulation (run #45); coolant mass fraction profiles from 2-d film-cooling simulation (run #45); heat flux profiles from 2-d film cooling simulations (run #45); heat flux profiles from 2-d film cooling simulations (runs #47, #45, and #47); 3-d grid used for film cooling simulations of test article; heat flux contours from 3-d film-cooling simulation (run #45); and heat flux profiles from 3-d and 2-d film cooling simulations (runs #44, #46, and #47).

Morris, Christopher I.↗

Wear Potential Due to Low EHD Films During Elevated Temperatures

An earlier study showed that EHD films could be accurately measured in a running bearing and that the EHD film eventually runs-in to a steady state value [1]. In the present paper, we report on additional tests conducted on bearings with more lubricants, wider speeds, and higher temperatures. The new results consistently show that all lubricants tested, including MAC-based lubricants have EHD film levels that are lower than model predictions in some situations. In addition, the MAC lubricants studied have lower film thickness than traditional hydrocarbons. Figure 1 is taken from [1] and shows room temperature data of MAC oil and Corey 100 oil, illustrating the smaller EHD film results when using this MAC oil. Since higher temperatures produce lower films by changing the viscosity, the concern we have is that the EHD films may be too small to prevent ball/race metal contact and resulting wear at lower speeds. Best bearing practices would have the EHD film thickness be at least three (3) times the composite surface roughness. In this paper, we will present measured EHD thicknesses of lubricant films at speeds up to several thousand RPM for bearing bore sizes from as low as 6 mm (0.2 in) to as large as 35 mm (1.4 in) using MAC, Corey and KG-80. Ambient temperatures from room temperature to 52C (125F) are used. Testing was done with the base oils as well as formulated greases. Greases eventually ran in to the same EHD values as the base oil but took longer times to get there. The results clearly indicate that wear is very possible in all steel bearings when using MAC lubricants and that this condition worsens with higher temperatures and smaller bearing size.

Leville, Alan↗

Slippery Lubricant-Infused Silica Nanoparticulate Film Processing for Anti-Biofouling Applications

Microbial biofilm build-up in water distribution systems can pose a risk to human health and pipe material integrity. The impact is more devastating in space stations and to astronauts due to the isolation from necessary replacement parts and medical resources. As a result, there is a need for coatings to be implemented onto the inner region of the pipe to minimize the adherence and growth of biofilms. Lubricant-infused surfaces has been one such interesting material for anti-biofouling applications in which their slippery property promotes repellence to many liquids and thus prevents bacterial adherence. Textured and porous films are suitable substrate candidates to infuse and contain the lubricant. However, there is little investigation in utilizing a nanoporous thin film as the substrate material for lubricant infusion. A nanoporous film has high porosity within the structure which can promote greater lubricant infusion and retention. The implementation as a thin film structure aids to reduce material consumption and cost. In our study, we utilized a well-studied nanoporous thin film fabricated via layer-by-layer assembly of polycations and colloid silica and calcination for greater stability. The film was further functionalized to promote fluorinated groups upon the surface and pores of the film, which then could interact with a fluorinated lubricant. The pristine nanoporous film was characterized to determine its morphology, thickness, wettability, and porosity. The lubricant-infused film was then tested for its lubricant layer stability upon various washing conditions and its performance against bacterial biofilm adherence as a result of its slippery and thus anti-biofouling property.

biofilm↗

Temperature Mapping Above and Below Air Film-Cooled Thermal Barrier Coatings Using Phosphor Thermometry

Thermal barrier coatings (TBCs) are typically used in conjunction with air film cooling to maximize overall cooling effectiveness and reliability while minimizing sacrifices in engine performance. The effects of thermal barrier coating (TBC) thermal protection and air film cooling effectiveness have usually been studied separately; however, their contributions to combined cooling effectiveness are interdependent and are not simply additive. The combined cooling effectiveness is always less than the sum of the cooling effectiveness of stand-alone TBC protection and stand-alone air film cooling. These diminishing returns arise because adding the thermally insulating TBC between the cooling air and the surface to be cooled reduces the air film cooling effectiveness and because the air film cooling reduces the heat flux through the TBC and therefore reduces the temperature difference sustained across the TBC thickness. Due to these considerations, combined cooling effectiveness must be measured to achieve an optimum balance between TBC thermal protection and air film cooling. In this investigation, temperature mapping above and below air film-cooled TBCs was performed using luminescence lifetime imaging-based phosphor thermometry. Measurements were performed in the NASA GRC Mach 0.3 burner rig on a TBC-coated plate using a scaled-up cooling hole geometry where both the hot mainstream gas temperature and the blowing ratio were varied. Surface temperature maps were obtained from a Cr-doped GdAlO3 thermographic phosphor deposited on the surface of the electron-beam vapor-deposited yttria-stabilized zirconia (YSZ) TBC. From separate plates, temperature maps from the bottom of the TBC were obtained from a thin Er-doped YSZ layer integrated into the TBC below the overlying undoped YSZ. Procedures for temperature and cooling effectiveness mapping above and below the air film-cooled TBC surface are described. Most importantly, these measurements enable mapping the combined cooling effectiveness below the TBC, which is more important than surface cooling effectiveness when there is a barrier coating between the hot mainstream gas and the surface that needs thermal protection. Advantages of the luminescence lifetime imaging method over infrared thermography, as well as its limitations to steady-state conditions are discussed.

cooling effectiveness.↗

Optical and Electrical Properties of Reactively Sputtered TiN, ZrN, and HfN Thin Films

Thin films of titanium, zirconium, and hafnium nitride are prepared by DC magnetron reactive sputtering at room temperature on fused silica, optical glass, and silicon substrates. Deposition parameters are investigated in order to obtain stoichiometric films. The optical and electrical properties of the films as a function of nitrogen partial pressure are determined. The results show that an inverse correlation exists between the optical reflectance and the electrical resistivity of the films. Ellipsometer data for all three films show that their refractive index in the visible spectrum is decreased by increasing the film thickness while the extinction coefficient is unchanged. Thin films of TiN have the lowest room temperature resistivity relative to ZrN and HfN thin films.

Reactive↗

Thin-Film Embedded Sensors for Battery Health Monitoring

Hybrid or all-electric aircraft are being developed as the next generation of aircraft to both allow new forms of aviation and decrease environmental impact. Since these types of aircraft are based on high-capacity battery technology, safe operation of these batteries becomes increasingly important. In particular, the potential for battery failure due to uncontrolled chemical reactions resulting in thermal runaway, catastrophic failure, and battery fires must be addressed in order for such battery technology to have the level of safety needed for standard aviation implementation. Efforts to ensure battery safety often involve engineering solutions that seek to contain rather than prevent such events by early detection. Such approaches increase the system weight and decrease the power per unit mass provided by the battery system. Existing methods for measuring battery parameters to determine the battery state-of-health are limited. These methods include electrical measurements of the cell current and/or voltage output as well as temperature measurements taken externally on the cell surface. Such external temperature measurements are limited in their ability to provide early warning of impending battery failure. In response, an effort to develop sensors operating internal to battery for health monitoring has been ongoing in the NASA Sensor-based Prognostics to Avoid Runaway Reactions & Catastrophic Ignition (SPARRCI) project. The basic approach associated with this sensor work is the deposition of thin film sensors on the battery separator located between the anode and cathode of the battery. These thin film sensors are then monitored to determine changes in battery parameters and health. Microfabrication techniques are employed to minimize the overall impact of the sensors on battery operation through the implementation of sensors with minimal size, weight, and power consumption. The thickness of the films, which are fabricated through physical vapor deposition (sputtering), are on the order of thousands of angstroms and can have minimal surface area. Thin film sensors for system health management have been implemented for a many decades on complex components for aerospace applications. However, the application of thin films of this type on a battery separator for internal battery monitoring applications has not previously been demonstrated to our knowledge. This paper describes the development of sensors for the internal battery monitoring through the use of thin film sensor technology. Thin metal films were successfully deposited on a battery separator polymer material with good adherence and electrical continuity. Multiple types of sensors have been deposited, as well as lead connections from the sensor to the edge of the separator material. The ability of these thin film sensors immersed in electrolyte to perform multiple types of battery parameter measurements has been demonstrated. For example, a multiparameter sensor system measured multiple properties simultaneously inside of a pouch cell over a wide temperature range. Further, real time measurement of interior temperature changes in a battery pouch cell with an integrated interior temperature sensor was demonstrated. These changes include detecting a fault in the battery (shorting) in situ with rapid response time (less than a minute) corresponding to a more limited response by a temperature sensor mounted externally. Other aspects of monitoring battery health were also explored, such as real-time measurement of simulated dendrite growth/metal deposition by sensor on separator material demonstrated. Future efforts will include improvements in the durability of the sensor structure to allow introduction of the approach into standard battery fabrication techniques. Overall, this work is a step forward in providing a method to prevent catastrophic battery failures and provide a foundation for safer, lighter, and higher energy batteries for the electric aircraft industry.

thin film battery health↗

A review of film boiling at cryogenic temperatures.

Film boiling occurs in the quenching of metals, the chilling of biological species, the regenerative cooling of rockets, and the cooling down of a cryogenic fuel tank. Occasionally film boiling is also found in a nuclear reactor or in a cryomagnet. Aspects of film boiling involving an unconstrained liquid mass are considered, giving attention to the evaporation time, the Leidenfrost temperature, solid-liquid contacts, the thermal properties of the solid, effects of coating or scale, wettability, the metastable condition, and the velocity effect on drops. Developments discussed with regard to pool boiling are related to vertical surfaces, film boiling from horizontal surfaces, film boiling from a horizontal cylinder, film boiling from a sphere, and film boiling of helium. Processes of film boiling in a channel are also analyzed.

Hsu, Y. Y.↗

Liquid film demonstration experiment Skylab SL-4

The liquid film demonstration experiment performed on Skylab 4 by Astronaut Gerald Carr, which involved the construction of water and soap films by boundary expansion and inertia, is discussed. Results include a 1-ml globule of water expanded into a 7-cm-diameter film as well as complex film structures produced by inertia whose lifetimes are longer in the low-g environment. Also discussed are 1-g acceleration experiments in which the unprovoked rupture of films was photographed and film lifetimes of stationary and rotated soap films were compared. Finally, there is a mathematical discussion regarding minimal surfaces, an isoperimetric problem, and liquid films.

Darbro, W.↗

Morphological growth of sputtered MoS2 films

Sputtered MoS2 films from 300 A to 20,000 A thick were deposited on metal and glass surfaces. The substrate effects such as surface temperature, finish, pretreatment and chemistry as they affect the film formation characteristics were investigated by optical, electron transmission, electron diffraction, and scanning electron microscopy. Substrate temperature and surface chemistry were found to be the prime variables as to the formation of a crystalline or amorphous film. The friction characteristics are strictly influenced by the type of film formed. Surface chemistry and surface pretreatment account for compound formation and corresponding grain growth, which directly affect the adhesion characteristics, resulting in poor adherence. The type of surface finish (topography) as related to scratches, impurities, inhomogeneities, etc., are favorable nucleation sites for the growth of isolated and complex nodules within the film, and various complex surface overgrowths on the film. These nodular growth features have progressively more undesirable effects on the film behavior as the film thickness increases.

Spalvins, T.↗

Water depth penetration film test

As part of the National Aeronautics and Space Administration Earth Resources Program, a comparative and controlled evaluation of nine film-filter combinations was completed to establish the relative effectiveness in recording water subsurface detail if exposed from an aerial platform over a typical water body. The films tested, with one exception, were those which prior was suggested had potential. These included an experimental 2-layer positive color film, a 2-layer (minus blue layer) film, a normal 3-layer color film, a panchromatic black-and-white film, and a black-and-white infrared film. Selective filtration was used with all films.

Lockwood, H. E.↗

Feasibility demonstration for electroplating ultra-thin polyimide film

The effect of electrodeposition variables on film thickness was investigated using a dilute polyimide solution as a bath into which aluminum (as foil or as a vapor deposited coating) was immersed. The electrodeposited film was dried for 2 hours at 93 C (primarily to remove solvent) and cured for 18 hours at 186 C. Infrared studies indicate that imide formation (curing) occurs at 149 C under vacuum. From a conceptual viewpoint, satisfactory film metallized on one side can be obtained by this method. The cured ultra thin polyimide film exhibits properties equivalent to those of commercial film, and the surface appearance of the strippable polyimide film compares favorably with that of a sample of commercial film of thicker gauge. The feasibility of manufacturing approximately one million sq m of ultra thin film capable of being joined to fabricate an 800 m by 9 800 m square from starting material 0.5 to 1 m wide for space erectable structures was demonstrated.

Schneier, R.↗

Progress towards high efficiency polycrystalline thin-film GaAs AMOS solar cells

Results of Ge film recrystallization using focused laser beams and GaAs film growth on such layers in the making of high efficiency thin-film AMOS solar cells are discussed. Since a conversion efficiency of 14% was obtained for an AMOS cell fabricated on sliced bulk polycrystalline GaAs, high efficiency cells are being developed by chemically vapor-depositing GaAs films on previously recrystallized evaporated Ge films to minimize the grain boundary (GB) effects. Schottky barrier solar cells made on sliced polycrystalline GaAs wafers were studied to investigate the effects of grain boundaries on cell properties and the potential efficiency of GaAs thin-film cells. Ge film recrystallization and the chemical vapor deposition (CVD) of the 2 to 3 micron thick GaAs films are described. AMOS solar cells with 100 Angstrom thick Ag metallization were made on CVD GaAs/recrystallized Ge/W substrates with an energy conversion efficiency of 8%.

Yeh, Y. C. M.↗

Fire resistant films for aircraft applications

Alternative sandwich panel decorative films were investigated as replacements for the polyvinyl fluoride currently used in aircraft interiors. Candidate films were studied for flammability, smoke emission, toxic gas emission, flame spread, and suitability as a printing surface for the decorative acrylic ink system. Several of the candidate films tested were flame modified polyvinyl fluoride, polyvinylidene fluoride, polyimide, polyamide, polysulfone, polyphenylsulfone, polyethersulfone, polybenzimidazole, polycarbonate, polyparabanic acid, polyphosphazene, polyetheretherketon, and polyester. The films were evaluated as pure films only, films silk-screened with an acrylic ink, and films adhered to a phenolic fiberglass substrate. Films which exhibited the highest fire resistant properties included PEEK polyetheretherketon, Aramid polyamide, and ISO-BPE polyester.

Kourtides, D. A.↗