Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Etching”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Nanoscale Editing of Multi and Single Layer Tungsten Disulfide via Gas‐Assisted Focused Electron Beam Induced Etching for Device Prototyping

Focused electron beam induced etching (FEBIE) with XeF 2 (xenon difluoride) precursor is conducted on multi-layer exfoliated WS 2 (tungsten disulfide) and monolayer WS 2 grown by chemical vapor deposition (CVD). The films are characterized by atomic force microscopy (AFM) and Raman and photoluminescence (PL) spectroscopy post-etching. The etch rates/efficiencies are reported as a function of electron beam energy, current, dwell time, and XeF 2 pressure. Bulk film Raman spectra are unchanged post-FEBIE, indicating minimal subsurface damage. Monolayer WS 2 shows a decrease in Raman and PL intensity post-FEBIE, with a dose-to-clear of ≈2 nC µm −2 . The study reveals regimes affected by the various mass transport contributions such as refresh time and the ratio of electrons/XeF 2 . Spontaneous etching was discovered during FEBIE of large patterned areas due to the long frame/refresh times. Density functional theory and ab initio molecular dynamics simulations compares desorption of SF x and WF x molecules from pristine WS 2 basal planes and pore edges, revealing the spontaneous etching is consistent with etching of partially etched monolayers during each frame. Single-line etching width of 21 nm, and patterning flakes into 100 nm wide channels are demonstrated. In conclusion, this work demonstrates the possibility of editing WS 2 flakes into electronic devices of arbitrary dimensions for semiconductor applications.

2D materials↗

Anisotropic Etching of Hexagonal Boron Nitride and Graphene: Question of Edge Terminations

Here, chemical vapor deposition (CVD) has been established as the most effective way to grow large area two-dimensional materials. Direct study of the etching process can reveal subtleties of this competing with the growth reaction and thus provide the necessary details of the overall growth mechanism. Here we investigate hydrogen-induced etching of hBN and graphene and compare the results with the classical kinetic Wulff construction model. Formation of the anisotropically etched holes in the center of hBN and graphene single crystals was observed along with the changes in the crystals' circumference. We show that the edges of triangular holes in hBN crystals formed at regular etching conditions are parallel to B-terminated zigzags, opposite to the N-terminated zigzag edges of hBN triangular crystals. The morphology of the etched hBN holes is affected by a disbalance of the B/N ratio upon etching and can be shifted toward the anticipated from the Wulff model N-terminated zigzag by etching in a nitrogen buffer gas instead of a typical argon. For graphene, etched hexagonal holes are terminated by zigzag, while the crystal circumference is gradually changing from a pure zigzag to a slanted angle resulting in dodecagons.

2D materials↗

Silver ion mediated shape control of platinum nanoparticles: Removal of silver by selective etching leads to increased catalytic activity

A procedure has been developed for the selective etching of Ag from Pt nanoparticles of well-defined shape, resulting in the formation of elementally-pure Pt cubes, cuboctahedra, or octahedra, with a largest vertex-to-vertex distance of {approx}9.5 nm from Ag-modified Pt nanoparticles. A nitric acid etching process was applied Pt nanoparticles supported on mesoporous silica, as well as nanoparticles dispersed in aqueous solution. The characterization of the silica-supported particles by XRD, TEM, and N{sub 2} adsorption measurements demonstrated that the structure of the nanoparticles and the mesoporous support remained conserved during etching in concentrated nitric acid. Both elemental analysis and ethylene hydrogenation indicated etching of Ag is only effective when [HNO{sub 3}] {ge} 7 M; below this concentration, the removal of Ag is only {approx}10%. Ethylene hydrogenation activity increased by four orders of magnitude after the etching of Pt octahedra that contained the highest fraction of silver. High-resolution transmission electron microscopy of the unsupported particles after etching demonstrated that etching does not alter the surface structure of the Pt nanoparticles. High [HNO{sub 3}] led to the decomposition of the capping agent, polyvinylpyrollidone (PVP); infrared spectroscopy confirmed that many decomposition products were present on the surface during etching, including carbon monoxide.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A statistical approach to optimization of alumina etching in a high density plasma

Inductively coupled plasma (ICP) reactive ion etching of Al{sub 2}O{sub 3} with fluorine-based gas chemistry in a high density plasma reactor was carried out in an initial investigation aimed at data storage applications. A statistical design of experiments was implemented to optimize etch performance with respect to process variables such as ICP power, platen power, direct current (dc) bias, and pressure. Both soft photoresist masks and hard metal masks were investigated in terms of etch selectivity and surface properties. The reverse power dependence of dc bias on the ratio of ICP to platen power was elucidated. Etch mechanisms in terms of physical and ion enhanced chemical etchings were discussed. The F-based chemistry greatly enhances the etch rate of alumina compared to purely physical processes such as ion milling. Etch rates as high as 150 nm/min were achieved using this process. A practical process window was developed for high etch rates, with reasonable selectivity to hard masks, with the desired profile, and with low substrate bias for minimal damage.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Insights into the reactive ion etching mechanism of nanocrystalline diamond films as a function of film microstructure and the presence of fluorine gas

Inhomogeneous etching of nanocrystalline diamond (NCD) films, which produces nanopillars during reactive ion etching process, is problematic to the microfabrication of NCD films for the sensor and actuator applications. Thus, its origin was investigated for various initial microstructures of the NCD films, SF{sub 6}/O{sub 2} gas ratios during etching, and plasma powers. The etched NCD film surface roughness became more pronounced (leading to larger pillar diameters and heights) for larger initial microstructural features (larger grain and cluster sizes), particularly at low plasma powers. The surface roughening was significantly reduced with the addition of SF{sub 6}, almost disappearing at SF{sub 6}/O{sub 2} of 5% to 10%. These results indicate that the etch rate was locally enhanced at the interfaces between grains or clusters, and the etch rate disparity between intragranular and intergranular (or cluster) carbons increased with decreasing ion energy, implying a chemical reaction rate-limited etching mechanism. The role of SF{sub 6} could be explained to reduce the energy barrier for the chemical reaction of intragranular carbons. Here we suggest that the etching rate is limited by an energy barrier that could be reduced by defect generation during ion bombardment or by catalytic radicals.

36 MATERIALS SCIENCE↗

Optimization of graphene dry etching conditions via combined microscopic and spectroscopic analysis

Single-layer graphene structures and devices are commonly defined using reactive ion etching and plasma etching with O{sub 2} or Ar as the gaseous etchants. Although optical microscopy and Raman spectroscopy are widely used to determine the appropriate duration of dry etching, additional characterization with atomic force microscopy (AFM) reveals that residual graphene and/or etching byproducts persist beyond the point where the aforementioned methods suggest complete graphene etching. Recognizing that incomplete etching may have deleterious effects on devices and/or downstream processing, AFM characterization is used here to determine optimal etching conditions that eliminate graphene dry etching residues.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Fabrication of ultra-high aspect ratio silicon nanopores by electrochemical etching

We report on the formation of ultra-high aspect ratio nanopores in silicon bulk material using photo-assisted electrochemical etching. Here, n-type silicon is used as anode in contact with hydrofluoric acid. Based on the local dissolution of surface atoms in pre-defined etching pits, pore growth and pore diameter are, respectively, driven and controlled by the supply of minority charge carriers generated by backside illumination. Thus, arrays with sub-100 nm wide pores were fabricated. Similar to macropore etching, it was found that the pore diameter is proportional to the etching current, i.e., smaller etching currents result in smaller pore diameters. To find the limits under which nanopores with controllable diameter still can be obtained, etching was performed at very low current densities (several μA cm{sup −2}). By local etching, straight nanopores with aspect ratios above 1000 (∼19 μm deep and ∼15 nm pore tip diameter) were achieved. However, inherent to the formation of such narrow pores is a radius of curvature of a few nanometers at the pore tip, which favors electrical breakdown resulting in rough pore wall morphologies. Lowering the applied bias is adequate to reduce spiking pores but in most cases also causes etch stop. Our findings on bulk silicon provide a realistic chance towards sub-10 nm pore arrays on silicon membranes, which are of great interest for molecular filtering and possibly DNA sequencing.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Quantum cascade laser based monitoring of CF{sub 2} radical concentration as a diagnostic tool of dielectric etching plasma processes

Dielectric etching plasma processes for modern interlevel dielectrics become more and more complex by the introduction of new ultra low-k dielectrics. One challenge is the minimization of sidewall damage, while etching ultra low-k porous SiCOH by fluorocarbon plasmas. The optimization of this process requires a deeper understanding of the concentration of the CF{sub 2} radical, which acts as precursor in the polymerization of the etch sample surfaces. In an industrial dielectric etching plasma reactor, the CF{sub 2} radical was measured in situ using a continuous wave quantum cascade laser (cw-QCL) around 1106.2 cm{sup −1}. We measured Doppler-resolved ro-vibrational absorption lines and determined absolute densities using transitions in the ν{sub 3} fundamental band of CF{sub 2} with the aid of an improved simulation of the line strengths. We found that the CF{sub 2} radical concentration during the etching plasma process directly correlates to the layer structure of the etched wafer. Hence, this correlation can serve as a diagnostic tool of dielectric etching plasma processes. Applying QCL based absorption spectroscopy opens up the way for advanced process monitoring and etching controlling in semiconductor manufacturing.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

A comparative study of capacitively coupled HBr/He, HBr/Ar plasmas for etching applications: Numerical investigation by fluid model

Fluid model has been applied to perform a comparative study of hydrogen bromide (HBr)/He and HBr/Ar capacitively coupled plasma discharges that are being used for anisotropic etching process. This model has been used to identify the most dominant species in HBr based plasmas. Our simulation results show that the neutral species like H and Br, which are the key player in chemical etching, have bell shape distribution, while ions like HBr{sup +}, Br{sup +}, which play a dominant rule in the physical etching, have double humped distribution and show peaks near electrodes. It was found that the dilution of HBr by Ar and/or He results in an increase in electron density and electron temperature, which results in more ionization and dissociation and hence higher densities of neutral and charged species can be achieved. The ratio of positive ion flux to the neutral flux increases with an increase in additive gas fraction. Compare to HBr/He plasma, the HBr/Ar plasma shows a maximum change in the ion density and flux and hence the etching rate can be considered in the ion-assisted and in the ion-flux etch regime in HBr/Ar discharge. The densities of electron and other dominant species in HBr/Ar plasma are higher than those of HBr/He plasma. The densities and fluxes of the active neutrals and positive ions for etching and subsequently chemical etching versus physical sputtering in HBr/Ar and HBr/He plasmas discharge can be controlled by tuning gas mixture ratio and the desire etching can be achieved.

74 ATOMIC AND MOLECULAR PHYSICS↗

Tin removal from extreme ultraviolet collector optics by inductively coupled plasma reactive ion etching

Tin (Sn) has the advantage of delivering higher conversion efficiency compared to other fuel materials (e.g., Xe or Li) in an extreme ultraviolet (EUV) source, a necessary component for the leading next generation lithography. However, the use of a condensable fuel in a lithography system leads to some additional challenges for maintaining a satisfactory lifetime of the collector optics. A critical issue leading to decreased mirror lifetime is the buildup of debris on the surface of the primary mirror that comes from the use of Sn in either gas discharge produced plasma (GDPP) or laser produced plasma (LPP). This leads to a decreased reflectivity from the added material thickness and increased surface roughness that contributes to scattering. Inductively coupled plasma reactive ion etching with halide ions is one potential solution to this problem. This article presents results for etch rate and selectivity of Sn over SiO{sub 2} and Ru. The Sn etch rate in a chlorine plasma is found to be much higher (of the order of hundreds of nm/min) than the etch rate of other materials. A thermally evaporated Sn on Ru sample was prepared and cleaned using an inductively coupled plasma etching method. Cleaning was confirmed using several material characterization techniques. Furthermore, a collector mock-up shell was then constructed and etching was performed on Sn samples prepared in a Sn EUV source using an optimized etching recipe. The sample surface before and after cleaning was analyzed by atomic force microscopy, x-ray photoelectron spectroscopy, and Auger electron spectroscopy. The results show the dependence of etch rate on the location of Sn samples placed on the collector mock-up shell.

36 MATERIALS SCIENCE↗

Plasma etching of Hf-based high-k thin films. Part III. Modeling the reaction mechanisms

A generalized etch rate model was formulated to describe metal oxide etching in complex plasma chemistries, based on the understanding gained from detailed plasma characterization and experimental investigation into the metal oxide etching mechanisms. Using a surface site balance-based approach, the correct etch rate dependencies on neutral-to-ion flux ratio, ion energy, competing deposition and etching reaction pathways, and film properties were successfully incorporated into the model. The applicability of the model was assessed by fitting to experimental etch rate data in both Cl{sub 2} and BCl{sub 3} chemistries. Plasma gas phase analysis as well as etch and deposition rate measurements were used to calculate initial values and appropriate ranges for model parameter variation. Physically meaningful parameter values were extracted from the modeling fitting to the experimental data, thereby demonstrating the applicability of this model in assessing the plasma etching of other complex materials systems.

36 MATERIALS SCIENCE↗

Mixing-layer kinetics model for plasma etching and the cellular realization in three-dimensional profile simulator

In this article the major kinetics models for plasma-surface interactions were reviewed highlighting their strengths and limitations. As a subset of reactive-site modeling, mixing-layer kinetics model was developed based upon the assumption of random atomic mixing in the top surface layer. The translation of the layer enabled the modeling of both etching and deposition. A statistical concept, nearest-neighbor bonding probability, was defined to express the concentration of any surface moieties with the surface elemental composition. A lumped set of reactions was adopted to carry on the overall physichemical processes including ion incorporation, neutral adsorption, physical sputtering, ion-enhanced etching, dangling bond generation and annihilation, and spontaneous etching. The rate coefficients were fitted to the experimental etching yields at various beam etching conditions. The good match between the kinetics modeling and the experimental results verified the capability of the mixing-layer model of predicting the poly-Si etching in chlorine plasma at various operating conditions. Then the kinetics model was incorporated into the three-dimensional Monte Carlo profile simulator. The concept of the mixing layer was simulated by a cellular-based model through composition averaging among neighboring cells. The reactions were sorted out in terms of ion initiated and neutral initiated, respectively, as discrete events. The reaction rates were calculated based upon the cellular composition and used as probabilities to remove particles from the cell. Results showed that the profile simulation combined with the kinetics, the numeric kinetics model, and the experimental etching yields are in quantitative agreement, which demonstrated the accuracy of kinetics after incorporation into the profile simulation. The simulation was compared to the published research work comprehensively including the etching yields, surface compositions, and dominant product distributions.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Highly selective etching of silicon nitride to physical-vapor-deposited a-C mask in dual-frequency capacitively coupled CH{sub 2}F{sub 2}/H{sub 2} plasmas

A multilevel resist (MLR) structure can be fabricated based on a very thin amorphous carbon (a-C) layer ( congruent with 80 nm) and Si{sub 3}N{sub 4} hard-mask layer ( congruent with 300 nm). The authors investigated the selective etching of the Si{sub 3}N{sub 4} layer using a physical-vapor-deposited (PVD) a-C mask in a dual-frequency superimposed capacitively coupled plasma etcher by varying the process parameters in the CH{sub 2}F{sub 2}/H{sub 2}/Ar plasmas, viz., the etch gas flow ratio, high-frequency source power (P{sub HF}), and low-frequency source power (P{sub LF}). They found that under certain etch conditions they obtain infinitely high etch selectivities of the Si{sub 3}N{sub 4} layers to the PVD a-C on both the blanket and patterned wafers. The etch gas flow ratio played a critical role in determining the process window for infinitely high Si{sub 3}N{sub 4}/PVD a-C etch selectivity because of the change in the degree of polymerization. The etch results of a patterned ArF photoresisit/bottom antireflective coating/SiO{sub x}/PVD a-C/Si{sub 3}N{sub 4} MLR structure supported the idea of using a very thin PVD a-C layer as an etch-mask layer for the Si{sub 3}N{sub 4} hard-mask pattern with a pattern width of congruent with 80 nm and high aspect ratio of congruent with 5.

36 MATERIALS SCIENCE↗

Defect formation during chlorine-based dry etching and their effects on the electronic and structural properties of InP/InAsP quantum wells

The general objective is the investigation of the defects formed by dry etching tools such as those involved in the fabrication of photonic devices with III–V semiconductors. Emphasis is put on plasma exposures with chlorine-based chemistries. In addition to identifying these defects and describing their effects on the electro-optic and structural properties, the long-term target would be to predict the impact on the parameters of importance for photonic devices, and possibly include these predictions in their design. The work is first centered on explaining the experimental methodology. This methodology starts with the design and growth of a quantum well structure on indium phosphide, including ternary indium arsenide/phosphide quantum wells with graded arsenic/phosphor composition. These samples have then been characterized by luminescence methods (photo- and cathodoluminescence), high-resolution transmission electron microscopy, and secondary ion mass spectrometry. As one of the parameters of importance in this study, the authors have also included the doping level. The samples have been exposed to the etching plasmas for “short” durations that do not remove completely the quantum wells, but change their optical signature. No masking layer with lithographic features was involved as this work is purely oriented to study the interaction between the plasma and the samples. A significant difference in the luminescence spectra of the as-grown undoped and doped samples is observed. A mechanism describing the effect of the built-in electric field appearing as a consequence of the doping profile is proposed. This mechanism involves quantum confined Stark effect and electric-field induced carrier escape from the quantum wells. In the following part, the effects of exposure to various chlorine-based plasmas were explored. Differences are again observed between the undoped and doped samples, especially for chemistries containing silicon tetrachloride. Secondary ion mass spectrometry indicates penetration of chlorine in the structures. Transmission electron microscopy is used to characterize the quantum well structure before and after plasma bombardment. By examining carefully the luminescence spectral properties, the authors could demonstrate the influence of the etching plasmas on the built-in electric field (in the case of doped samples), and relate it to some ionic species penetrating the structures. Etching plasmas involving both chlorine and nitrogen have also been studied. The etching rate for these chemistries is much slower than for some of the silicon tetrachloride based chemistries. Their effects on the samples are also very different, showing much reduced effect on the built-in electric field (for the doped samples), but significant blue-shifts of the luminescence peaks that the authors attributed to the penetration of nitrogen in the structures. Nitrogen, in interstitial locations, induces mechanical compressive stress that accounts for the blue-shifts. Finally, from the comparison between secondary ion mass spectrometry and luminescence spectra, the authors suggest some elements for a general mechanism involved in the etching by chloride-chemistries, in which a competition takes place between the species at the surface, active for the etching mechanism, and the species that penetrate the structure, lost for the etching process, but relevant in terms of impact on the electro-optic and structural features of the exposed materials.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

High temperature isotropic and anisotropic etching of silicon carbide using forming gas

Plasma-etched micropillars in 4H-SiC were etched in forming gas (4% H2, 96% N2) at 1500, 1550, and 1600 °C at 2.4 and 9.4 standard liters per min (slm). At 2.4 slm, oxygen from the aluminum oxide components of the tube furnace oxidized the SiC surface, and the pillars etched isotropically. Additionally, at 9.4 slm, the pillars etched crystallographically at 1500 and 1550 °C, and sharp 4H-SiC needless with tips as narrow as 15 nm were produced. The lateral etch rates of both 4H- and 6H-SiC were measured with the a-plane etching faster than the m-plane at 1500 and 1550 °C. At 1600 °C, the m-plane and a-plane etch at comparable rates. Due to the difference in etch rates between the m-plane and a-plane, convex surfaces tend to produce facets parallel to the a-plane, while concave surfaces produce facets parallel to the m-plane.

42 ENGINEERING↗

HF-based etching processes for improving laser damage resistance of fused silica optical surfaces

The effect of various HF-based etching processes on the laser damage resistance of scratched fused silica surfaces has been investigated. Conventionally polished and subsequently scratched fused silica plates were treated by submerging in various HF-based etchants (HF or NH{sub 4}F:HF at various ratios and concentrations) under different process conditions (e.g., agitation frequencies, etch times, rinse conditions, and environmental cleanliness). Subsequently, the laser damage resistance (at 351 or 355 nm) of the treated surface was measured. The laser damage resistance was found to be strongly process dependent and scaled inversely with scratch width. The etching process was optimized to remove or prevent the presence of identified precursors (chemical impurities, fracture surfaces, and silica-based redeposit) known to lead to laser damage initiation. The redeposit precursor was reduced (and hence the damage threshold was increased) by: (1) increasing the SiF{sub 6}{sup 2-} solubility through reduction in the NH4F concentration and impurity cation impurities, and (2) improving the mass transport of reaction product (SiF{sub 6}{sup 2-}) (using high frequency ultrasonic agitation and excessive spray rinsing) away from the etched surface. A 2D finite element crack-etching and rinsing mass transport model (incorporating diffusion and advection) was used to predict reaction product concentration. The predictions are consistent with the experimentally observed process trends. The laser damage thresholds also increased with etched amount (up to {approx}30 {micro}m), which has been attributed to: (1) etching through lateral cracks where there is poor acid penetration, and (2) increasing the crack opening resulting in increased mass transport rates. With the optimized etch process, laser damage resistance increased dramatically; the average threshold fluence for damage initiation for 30 {micro}m wide scratches increased from 7 to 41 J/cm{sup 2}, and the statistical probability of damage initiation at 12 J/cm{sup 2} of an ensemble of scratches decreased from {approx}100 mm{sup -1} of scratch length to {approx}0.001 mm{sup -1}.

42 ENGINEERING↗

Comparison of the structural and optical properties of porous In{sub 0.08}Ga{sub 0.92}N thin films synthesized by electrochemical etching

This paper presents the structural and optical study of porous (1 µm) In{sub 0.08}Ga{sub 0.92}N synthesized by photoelectrochemical etching under various conditions. Field emission scanning electron microscope and atomic force microscope images showed that the pre-etched thin films have a sufficiently smooth surface over a large region with wurtzite structure. The roughness increased with an increase in etching duration. The blue shift phenomenon was measured for photoluminescence emission peaks at 300 K. The energy band gap increased to be 3.18 and 3.16 eV for post-etched films at ratios of 1:4 and 1:5, respectively. At the same time, the photoluminescence intensities of the post-etched thin films indicated that the optical properties have been enhanced. - Graphical abstract: PL spectra of the as-grown and porous In{sub 0.08}Ga{sub 0.92}N under various etching duration. - Highlights: • Nanoporous structures of In{sub 0.08}Ga{sub 0.92}N. • The roughness of the porous thin films increased with an increase in etching durations. • No phase segregation in XRD pattern. • Blue shifts were observed in the PL spectra of the post-etched films.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Edge-Controlled Growth and Etching of Two-Dimensional GaSe Monolayers

Understanding the atomistic mechanisms governing the growth of two-dimensional (2D) materials is of great importance in guiding the synthesis of wafer-sized, single-crystalline, high-quality 2D crystals and heterostructures. Etching, in many cases regarded as the reverse process of material growth, has been used to study the growth kinetics of graphene. In this paper, we explore a growth–etching–regrowth process of monolayer GaSe crystals, including single-crystalline triangles and irregularly shaped domains formed by merged triangles. We show that the etching begins at a slow rate, creating triangular, truncated triangular, or hexagonally shaped holes that eventually evolve to exclusively triangles that are rotated 60° with respect to the crystalline orientation of the monolayer triangular crystals. The regrowth occurs much faster than etching, reversibly filling the etched holes and then enlarging the size of the monolayer crystals. A theoretical model developed based on kinetic Wulff construction (KWC) theory and density functional theory (DFT) calculations accurately describe the observed morphology evolution of the monolayer GaSe crystals and etched holes during the growth and etching processes, showing that they are governed by the probability of atom attachment/detachment to/from different types of edges with different formation energies of nucleus/dents mediated by chemical potential difference Δμ between Ga and Se. Finally, our growth–etching–regrowth study provides not only guidance to understand the growth mechanisms of 2D binary crystals but also a potential method for the synthesis of large, shape-controllable, high-quality single-crystalline 2D crystals and their lateral heterostructures.

36 MATERIALS SCIENCE↗