Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CREEP”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Creep deformation and cavitation in an additively manufactured Al-8.6Cu-0.4Mn-0.9Zr (wt%) alloy

Creep deformation and cavitation were investigated at 300 ºC in both tension and compression for an additively manufactured Al-8.6Cu-0.5Mn-0.9Zr (wt%) alloy in the as-fabricated state and after various aging treatments (aging at 300 °C/200 h or 350 °C/24 h and overaging at 400 °C/200 h). Creep mechanisms at 300 °C were determined by relating the measured creep response to corresponding microstructural and X-ray computed tomography observations. In compression, alloys in the as-fabricated and two aging conditions exhibited similarly high creep resistance. Overaging (400 °C/200 h) led to substantial coarsening of intragranular θ-Al2Cu precipitates and an expected drop in their Orowan strengthening contribution. In tension, minimum strain rates comparable to those in compression were obtained at any given stress; however, upon accumulation of some plastic strain in the matrix, creep cavities started to form, leading to accelerated tertiary stage creep deformation and rupture. Cavitation occurred exclusively along melt pool boundaries due to locally enhanced diffusion enabled by (i) large grain-boundary area in adjacent fine-grained zones and (ii) localization of creep strain in nearby heat-affected zones. Although cavity growth was initially diffusion-controlled, its rate was determined by matrix creep rate, consistent with constrained cavity growth mechanisms. This study reveals how microstructural complexities induced by the additive manufacturing process affect the creep and cavitation behavior of Al-Cu-Mn-Zr alloys. The underlying creep and cavitation mechanisms uncovered in this study point to pathways that improve the high-temperature properties of additively manufactured alloys.

36 MATERIALS SCIENCE↗

Creep behavior of an additively manufactured 9Cr steel in the as-built condition

Limited studies have evaluated the creep behavior of additively manufactured (AM) ferritic-martensitic (FM) steels. This work investigated the creep behavior of a 9Cr FM steel fabricated by powder blown directed energy deposition (DED) technique. Here, the creep testing at 550–650 °C and 150 MPa for the specimens along the deposition direction in the as-built condition, together with corresponding microstructural characterization, revealed a threshold temperature between 600 and 625 °C, below which the steel has creep resistance comparable with Grade 91 cross-welds and noticeably greater than 9Cr-1Mo steel. The threshold temperature distinguishes the creep behavior in two regimes differentiated in creep activation energy, creep deformation, and failure mechanism. Unlike the creep rupture surface ~45° from the loading direction when tested above the threshold temperature, the creep rupture for testing below the threshold temperature resembles type IV failure in the cross-welds of ferritic steels. The DED-induced layer structure in the as-built steel played a significant role on the change of creep behavior.

36 MATERIALS SCIENCE↗

Creep and microstructural processes in a low-alloy 2.25%Cr1.6%W steel (ASTM Grade 23)

A low-alloy 2.25%Cr1%Mo steel (ASTM Grade 22) has been greatly improved by the substitution of almost all of the 1%Mo by 1.6%W. The improved material has been standardized as P/T23 steel (Fe–2.25Cr–1.6W–0.25V–0.05Nb–0.07C). The present investigation was conducted on T23 steel in an effort to obtain a more complete description and understanding of the role of the microstructural evolution and deformation processes in high-temperature creep. Constant load tensile creep tests were carried out in an argon atmosphere in the temperature range 500–650 °C at stresses ranging from 50 to 400 MPa. It was found that the diffusion in the matrix lattice is the creep-rate controlling process. The results of an extensive transmission electron microscopy (TEM) analysis programme to investigate microstructure evolution as a function of temperature are described and compared with the thermodynamic calculations using the software package Thermo-Calc. The significant creep-strength drop of T23 steel after long-term creep exposures can be explained by the decrease in dislocation hardening, precipitation hardening and solid solution hardening due to the instability of the microstructure at high temperature. - Highlights: • The constant load creep tests of T23 steel were carried out at 500–650 °C. • The stress exponents of the creep rate correspond to power law (dislocation) creep. • Diffusion in the matrix lattice is the creep-rate controlling process. • The microstructure instability is the main creep degradation process in T23 steel.

36 MATERIALS SCIENCE↗

Microstructural investigation of oxide dispersion strengthened alloy 617 after creep rupture at high temperature

Highlights: • The creep related microstructural evolution of ODS-617 at 950 °C under 25 MPa was investigated. • Dispersion of nanoscale Y-Al-O particles contributed to the superior creep properties of the ODS-617. • The creep mechanism of the ODS-617 at 950 °C under 25 MPa was Coble creep. • Cracks preferentially developed around the large rod-like AlN particles, resulting in the brittle creep fracture mode. - Abstract: Oxide dispersion strengthened (ODS) alloys have been widely considered as candidate structural materials for advanced nuclear reactors because of their good high temperature properties and irradiation resistance. In this study, the creep properties of oxide dispersion strengthened Alloy 617 (ODS-617) was examined at 950 °C under 25 MPa in the air. Conventional Alloy 617 tested under the same conditions was included for comparison. The ODS-617 exhibited superior creep resistance, including a much longer rupture life of 8533 h and a steady-state creep rate of 8.9 × 10{sup −8} (1/s), which was two orders of magnitude lower than that of the conventional alloy. The lower steady-state creep rate was related to the dispersion of nano-sized Y-Al-O particles, which may impede grain boundary diffusion. It seems that cracks preferentially developed near some large rod-like AlN particles, resulting in the brittle creep fracture mode.

36 MATERIALS SCIENCE↗

The Fundamental Creep Behavior Model of Gr.91 Alloy by ICME Approach (Final Report)

The current project mainly focused on the fundamental creep cracking mechanism of the Grade 91 system during the operation conditions in the advanced technologies FE power plants and build the link among Composition-Processing Parameters-Phase Stability-Microstructure-Creep Resistance. A model based on computational thermodynamics and diffusion kinetics will be developed to provide guidance on how to improve the creep resistance of the alloy system. The PI mainly investigate the Gr.91 base alloy and weldment with the Integrated Computational Materials Engineering (ICME) approach. The long-term goal of the proposed program is to develop a model for creep and fatigue resistant alloys with different elemental systems, compositions, and processing parameters of weldment and heat-treatment. In addition, new creep and fatigue resistant alloys are to be designed based on the predictions from the model. The computational as well as experimental results include three sections: 1) The compositional optimization and secondary phases evaluation regarding the creep resistance in Grade 91 steel through the CALPHAD approach. In this section, the formation of the critical secondary phases, M23C6, MX and Z-phase were well predicted based on many conditions like the temperature as well as compositions. Meanwhile, the role of different alloying elements was also considered as they will directly affect the formation of the secondary phases mentioned above based on the compositional evolution of the alloying elements. 2) An investigation of Creep Resistance in Grade 91 Steel through Computational Thermodynamics. We systematically considered the evolution of the four critical temperatures, Ac3, Ac1, the threshold of M23C6 and Z-phase, on basis of the computational approach. Meanwhile, the equilibrium cooling as well as Scheil simulations were also considered to perform further predictions based on the different cooling rates. 3) Creep lifetime and microstructural evolution of the Grade 91 steel. In this part, mainly experimental approach was performed on the real creep test from the beginning of the commercial Gr.91 alloys. The alloys were normalized, tempered, welded (Gleeble) and PWHT and finally subjected to the creep lifetime analyses. Finally, all the samples after each process were further characterized based on the OM, XRD and SEM technique to draw final conclusions.

01 COAL, LIGNITE, AND PEAT↗

Creep-fatigue behavior of alloy 617 - 18581

Alloy 617 is the leading candidate material for the intermediate heat exchanger for the very high temperature reactor (VHTR). It is thought that creep-fatigue resistance is likely to be the life-limiting material property for this application. As part of evaluating the behavior of this material in the expected service conditions, creep fatigue testing of Alloy 617 was performed at 850 and 950 deg. C for several strain ranges and hold times. Creep-fatigue degradation was observed, characterized by reduced cycles to failure when a hold time was added at peak tensile strain, compared to fatigue values. At 850 deg. C, increasing the tensile hold duration continued to degrade the creep fatigue resistance, at least to the investigated strain controlled hold time of up to 60 minutes at the 0.3% strain range and 240 minutes at the 1.0% strain range. At 950 deg. C, the creep fatigue cycles to failure are not further reduced with increasing hold duration, indicating saturation occurs at relatively short hold times. The creep and fatigue damage fractions have been calculated using the ASME methodology and plotted on a creep fatigue interaction D diagram. The impact of selecting different parameters on calculation of the creep damage fraction has been evaluated and will be discussed in this paper. Additional damage fractions from creep fatigue tests at 800 and 1000 deg. C on a different heat of Alloy 617 have been determined and are plotted on the D diagram along with results of the current testing. The combined data represent a comprehensive evaluation of Alloy 617 behavior under the ASME methodology and result in a consistent creep-fatigue damage envelope. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Effects of W on creep behaviors of novel Nb-bearing high nitrogen austenitic heat-resistant cast steels at 1000 °C

Highlights: • The synergistic CALPHAD and experimental approaches are adopted. • Creep behaviors of high nitrogen austenitic alloys are investigated at 1000 °C. • Creep properties are improved through the W solid solution strengthening. • W additions promote the formation of (Cr,Fe,W){sub 23}C{sub 6} instead of (Cr,Fe,W){sub 7}C{sub 3}. • (Cr, W)-rich precipitates severely degrade the creep properties. - Abstract: Recently, there is an urgent demand from automotive industries to develop new austenitic heat-resistant cast steels that withstand exhaust gas temperatures as high as 1000 °C. In this study, the effect of W additions on the creep behavior of a series of Nb-bearing high nitrogen austenitic heat-resistant cast steels was investigated at 1000 °C and 50 MPa. Microstructures before and after creep rupture tests were carefully characterized to illustrate the microstructural evolution during creep deformation. Microstructural analyses revealed that the W addition did not affect the formation of primary Nb(C,N), whereas significantly promoted the precipitation of primary (Cr, W)-rich phases, particularly those cellular structures along grain boundaries. The W solid solution strengthening and the secondary precipitation strengthening of submicron-scale (Cr, W)-rich phase improved the creep resistance of the alloys through increasing the hardness of γ-austenite and pinning the dislocations. However, the primary cellular (Cr, W)-rich structures significantly accelerated the nucleation and propagation of creep cracks along grain boundaries, thereby increasing the creep rate and decreasing the creep life.

36 MATERIALS SCIENCE↗

Improving creep resistance of Al-0.27Zr-0.08Sn (wt%) via cold swaging while maintaining high electrical conductivity

This study investigates the effect of mechanical cold work (0, 50, and 90% cross-sectional area reduction via swaging) on the creep properties of cast aluminum alloys with high electrical conductivity including high-purity Al (HP-Al), Al-0.15Zr (Al-Zr), and Al-0.27Zr-0.08Sn (Al-Zr-Sn, wt%). The Al-Zr alloy is strengthened by Zr in solid solution while the Al-Zr-Sn alloy is additionally strengthened by Al3Zr nanoprecipitates (8 nm diameter). After 90% cold swaging, the alloys exhibit grains elongated along the swaging direction with their widths ranging between 8 and 152 μm perpendicular to the swaging direction. Creep testing at 200 °C shows that the minimum creep rate of all 90% swaged alloys shows high sensitivity to stress, which can be modeled via a threshold stress σth. Increasing swaging magnitude from 0 to 50 to 90% in Al-Zr-Sn improves the creep resistance without reducing electrical conductivity. The formation of subgrains, increased dislocation density, and columnar grain structure in swaged alloys all enhance creep resistance. HP-Al swaged to 90% exhibits much lower creep resistance (σth = 18 MPa) due to subgrain coarsening and the absence of precipitates compared to Al-Zr (σth = 40 MPa) and Al-Zr-Sn (σth = 40 MPa), which maintain stable subgrain structures and benefit from solid solution strengthening and Al3Zr nanoprecipitates, respectively. Although Al3Zr precipitates are known to stabilize the deformed microstructure by pinning grain-boundaries, this work demonstrates that Zr in solid solution alone can effectively stabilize the deformed microstructure resulting in enhanced creep resistance. This effect of Zr solute on stabilizing grain boundaries for creep performance was not previously well-defined in the literature. Despite similar creep performances of Al-Zr and Al-Zr-Sn, the latter shows 70% higher room-temperature microhardness and slightly improved electrical conductivity (56%IACS (International Annealed Copper Standard) vs. 57%IACS, respectively). This work provides new insights into creep mechanisms of cold-worked Al–Zr alloys that will guide the design of heat-resistant Al conductors for high-demand applications.

Coello ramirez, Ismael [Northwestern University,]↗

Creep Deformation in Vaca Muerta Shale From Nanoindentation to Triaxial Experiments

In this work, we tested samples cored from the Vaca Muerta shale reservoir using nanoindentation (2 min) and triaxial (12 hr) creep experiments in which confining pressure and differential stresses were <40 MPa. In all cases, we observed transient creep wherein strain increased as the logarithm of time. Creep was always compactional, led to increased moduli, was triggered by changes in either hydrostatic or deviatoric stress, and occurred under loads well below the failure stress. Our results are consistent with yield cap models proposed to describe shear-enhanced compaction of sandstones and carbonates, assuming that the yield surface depends on strain rate. We compared our results to earlier studies that observed the transition from transient creep to approximately constant strain rate behavior. If short-term creep can be quantified by a creep modulus, $C$, and long-term creep, after a transition time, $t_c$, by a linear viscosity, $η$, then $η = Ct_c$. Owing to heterogeneity, the local values of Young's and creep moduli, E and C, measured during nanoindentation, varied by several orders of magnitude. Simple averaging of the indentation results overestimated E and C, as compared to their triaxial counterparts. The kinetics of log time creep, which is seen in various materials and loading circumstances, has been represented by a simple conceptual model incorporating the interplay of viscoelastic elements with widely distributed characteristic times. Thus, we argue that log time creep is an emerging phenomenon, independent of the identities of the underlying physical mechanisms.

58 GEOSCIENCES↗

Computational Design of Creep-Resistant Alloys and Experimental Validation in Ferritic Superalloys

A new class of ferritic superalloys containing B2-type zones inside parent L21-type precipitates in a disordered solid-solution matrix, also known as a hierarchical-precipitate strengthened ferritic alloy (HPSFA), has been developed for high-temperature structural applications in fossil-energy power plants. These alloys were designed by the addition of the Ti element into a previously-studied NiAl-strengthened ferritic alloy (denoted as FBB8 in this study). In the present research, systematic investigations, including advanced experimental techniques, first-principles calculations, and numerical simulations, have been integrated and conducted to characterize the complex microstructures and excellent creep resistance of HPSFAs. The experimental techniques include transmission-electron microscopy, scanningtransmission- electron microscopy, neutron diffraction, and atom-probe tomography, which provide detailed microstructural information of HPSFAs. Systematic tension/compression creep tests revealed that HPSFAs exhibit the superior creep resistance, compared with the FBB8 and conventional ferritic steels (i.e., the creep rates of HPSFAs are about 4 orders of magnitude slower than the FBB8 and conventional ferritic steels.) First-principles calculations include interfacial free energies, anti-phase boundary (APB) free energies, elastic constants, and impurity diffusivities in Fe. Combined with kinetic Monte- Carlo simulations of interdiffusion coefficients, and the integration of computational thermodynamics and kinetics, these calculations provide great understanding of thermodynamic and mechanical properties of HPSFAs. In addition to the systematic experimental approach and first-principles calculations, a series of numerical tools and algorithms, which assist in the optimization of creep properties of ferritic superalloys, are utilized and developed. These numerical simulation results are compared with the available experimental data and previous first-principles calculations, providing deep insight of creep mechanisms of the creep-resistant ferritic superalloys. With the above investigations, the HPSFA has been proved with superior creep resistance, and its microstructure, creep mechanism, and thermal/mechanical properties have been well studied and understood. In the future, HPSFAs with different additions and sizes of precipitates will be investigated and developed to further enhance the creep resistance of the ferritic superalloys and provide promising applications of the fossil-energy power plants.

Liaw, Peter↗

Characterization of Creep-Fatigue Crack Growth in Alloy 709 and Prediction of Service Lives in Nuclear Reactor Components (Final Report)

This final report summarizes the activities and results that were obtained by the research team working on the project “Characterization of Creep-Fatigue Crack Growth in Alloy 709 and Prediction of Service Lives in Nuclear Reactor Components”, DOE-NEUP Project 15-8623. This project was mainly concerned with the creep-fatigue crack growth characterization of austenitic stainless-steel Fe-20Cr-25Ni (Alloy 709). For this purpose, an array of experimental and computational activities was performed. The main goal of these activities was to describe and predict the crack growth behavior in Alloy 709 under different conditions of applied loading and temperature. Alloy 709 specimens were tested to describe both the uniaxial creep behavior and creep-fatigue crack growth rates at temperatures between 550°C and 700°C. Microstructure and fracture surface analysis was performed using several experimental techniques, and the defining features of crack growth propagation were identified and described. Thermodynamic and diffusion simulations were performed to understand the microstructure evolution of Alloy 709 at elevated temperatures, and to establish an aging schedule relevant for in-service conditions over extended periods. Experimental testing was performed on both as-received and aged Alloy 709 specimens. Two computational methods were developed to predict crack growth rates and remaining lives in specimens loaded under either fatigue of creep-fatigue. The first computational technique was the finite element method, while the second was strip-yield modeling. Both methods relied on the prediction of crack growth rates using the concept of plasticity-induced crack closure. Crack-tip opening loads were computed and used to perform crack growth rate predictions. The computational predictions matched well with the experimental results. The strip-yield model was shown to be an excellent predictive tool not only for crack growth in austenitic SS Alloy 709, but also in 316 SS, martensitic Cr-Mo steels, Ni-based alloys and Al-based alloys. The main conclusion of this study is that Alloy 709 exhibits excellent creep crack growth resistance at temperatures between 550°C and 700°C. In fact, the crack growth resistance of this alloy appears to be higher than that of 316 SS in similar testing conditions. Moreover, when creep loading with hold (dwell) times of 60s or 600s were intercalated every fatigue cycle, the crack growth rates did not change significantly. The conclusion is that the tests performed revealed that the crack growth is insignificant during the creep portion of a loading cycle, as compared with the crack growth during the fatigue portion of the cycle. In general, Alloy 709 shows excellent resistance to creep deformations and creep crack growth up to 700°C.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Relationship between Grain Size and Sample Thickness on the Creep-Rupture Performance of Thin Metallic Sheets of INCONEL Alloy 740H

A study was conducted on INCONEL® alloy 740H® to examine the role of grain size and sheet thickness on the alloy’s creep-rupture behavior. Three different starting sheet thicknesses were utilized and multiple heat-treatment conditions anticipated for compact heat exchanger (CHX) manufacturing were applied to produce a range of grain sizes. Creep-rupture testing was conducted at 750 °C for times up to about 6000 h and the results were compared to wrought databases. The data show that both creep strength and ductility were important factors in the overall creep performance of the sheets. Reductions in performance were observed due either to accelerated creep when grain size was fine or loss of rupture ductility when grain sizes approached the sheet thickness. Some combinations of heat-treatment and thickness were able to produce typical expected wrought creep properties. Historically a ‘rule-of-thumb’ requirement for creep testing suggests 3-5 grains per sample minimum dimension to ensure homogeneous behavior. This research shows that to ensure representative wrought creep performance (i.e. no effect of sample size), the sample minimum cross-section should be 10 times the average ASTM grain size. Statistical analysis of the microstructures suggests the population of larger grains as a controlling feature in creep failure.

14 SOLAR ENERGY↗

Molecular-dynamics study of diffusional creep in uranium mononitride

Uranium mononitride (UN) is a promising advanced nuclear fuel due to its high thermal conductivity and high fissile density. Yet, many aspects of its mechanical behavior and microstructural features are currently unknown. In this paper, molecular dynamics (MD) simulations are used to study UN's diffusional creep. Nanometer-sized polycrystals are used to simulate diffusional creep and to calculate an effective GB width. It is found that Nabarro-Herring creep is not dominant in the temperature range of 1700–2000 K and that the dominant diffusional creep mechanism is Coble creep with an activation energy of 2.28 ± 0.09 eV. A method is proposed to calculate the diffusional GB width and its temperature dependence in polycrystals. The effective GB width of UN is calculated as 2.69 ± 0.08 nm. This value fits very well with the prefactor of the phenomenological Coble creep formula. It is demonstrated that the most comprehensive thermal creep model for UN can be represented as the combination of our Coble creep model and the dislocation creep model proposed by Hayes et al.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

An accelerated framework for predicting creep rupture lifetimes in engineering alloys

Confidently predicting high-temperature deformation, including creep and creep rupture, is paramount for the design and commercialization of candidate materials for advanced nuclear energy systems. To accelerate creep quantification, we introduce a framework that enables rapid, cost-effective, and reliable prediction of creep rupture lifetimes, minimizing reliance on time-intensive bulk creep testing. Unlike conventional creep analysis, which requires extensive time and resources, our method leverages a maximum of four short-term bulk creep tests as training data for prediction. This framework combines high-throughput nanoindentation up to 700 °C with these targeted bulk tests to inform our creep rupture model in order to predict rupture lifetimes. The strong agreement between our predictions and conventional experimental data demonstrates the effectiveness of our approach for accelerated creep analysis and lifetime prediction of structural components in high-temperature applications. Our multi-pronged approach motivates further integration of computational tools and advanced instrumentation to establish a universal framework for understanding high-temperature material responses.

36 MATERIALS SCIENCE↗

Clarification of creep deformation mechanism in heat-affected zone of 9Cr steels with In Situ experiments

This work quantified nonuniform creep deformation across the heterogeneous heat-affected zone (HAZ) of Grade 91 steel with sophisticated experiments, including an electric-thermal finite element model–assisted Gleeble thermomechanical simulation and a high-temperature creep testing with in situ digital image correlation (DIC). High temperature creep properties of HAZ sub-zones were quantitatively measured by the DIC. Furthermore, by utilizing peak temperature, hardness, local creep strain, and underlying microstructures, creep deformation mechanisms in HAZ were further understood. DIC measurements reveal a creep-vulnerable zone (CVZ) exposed to a peak temperature of 932°C (close to A C3 ) in the intercritical HAZ experienced the fastest creep strength degradation instead of the soft zone with the lowest hardness prior to creep. The significantly reduced precipitation strengthening from misplacement of undissolved and coarsened M 23 C 6 carbides led to a faster recrystallization of tempered martensite in the CVZ. Weak untransformed tempered martensite (ferrite grains) stabilized by local Cr enrichment from dissolved M 23 C 6 also harmed the CVZ's creep resistance.

36 MATERIALS SCIENCE↗

Fundamental Understanding of Creep-Fatigue Interactions in 9Cr-1MoV Steel Welds. Final Report

Ferritic-martensitic steels constitute a vital class of materials for current and future generation of nuclear reactors as well as ultra supercritical coal fired power plants due to their superior creep resistant properties. One particular ferritic-martensitic steel, 9Cr-1MoV (Grade 91) is one of five materials approved for high temperature use in nuclear service by the American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (BPVC). Grade 91 is also a candidate material for proposed fission and fusion reactors such as the sodium cooled fast reactor (SFR). In service, Grade 91 components can be subjected to elevated temperatures and cyclic stresses, leading to the accumulation of creep-fatigue (CF) damage. While the monotonic creep properties of Grade 91 steels have been studied extensively, there is less knowledge concerning the mechanisms governing CF damage of this steel in the creep-dominated failure region. Moreover, the creep failure is especially pronounced in welded Grade 91 components, which are commonly joined using conventional arc welding techniques such as flux-cored arc welding (FCAW). In a Grade 91 weld, the creep failure typically occurs in the outer region of the heat affected zone (HAZ), specifically in the intercritical or fine-grained heat-affected zone (ICHAZ or FGHAZ), a phenomenon known as type IV failure. Currently, there exists a limited knowledge of CF damage mechanisms in Grade 91 welds. Improving the mechanistic understanding of the CF damage and failure of Grade 91 steel and its welds with inhomogeneous microstructure is crucial for the safety and design of key structural components in advanced, high-temperature reactors. The overall objectives of the project were to advance the state of knowledge and understanding of CF damage in both Grade 91 base metal and its welds, especially under loading conditions where creep is the dominant damage mechanism. Uncovering the mechanisms governing the creep-fatigue deformation and damage in Grade 91 base metal in creep-dominated region as well as type IV failure in Grade 91 welds contributes to a new knowledge that may lead to more accurate life prediction models than those currently in use. Moreover, the superior CF properties obtained by low heat input welding has a high potential to develop practical solutions to the premature failure of Grade 91 weld.

36 MATERIALS SCIENCE↗

The Role of Eta Phase Formation on the Creep Strength and Ductility of INCONEL Alloy 740 t 1023 k (750 Degrees C)

INCONEL alloy 740 is an age-hardenable nickel-based superalloy proposed for advanced ultrasupercritical steam boiler applications operating at high stress and long times above 973 K (700 C), where creep will be the dominate deformation mode. During high-temperature exposure, the alloy can form eta phase platelets that many have suggested may be detrimental to creep strength and ductility. In this study, creep-rupture tests were conducted on smooth and notched bars of INCONEL alloy 740 at 1023 K (750 C) for times up to 20,000 hours. Examination of the creep-rupture life, creep ductility, failure modes, and microstructure by quantitative electron microscopy shows that a small amount of eta phase does not diminish the creep performance. Applied stress appears to have a minor effect on the precipitation of the eta phase but not its growth rate. Based on the observation that the microstructure after 20,000 hours of creep exposure has reached equilibrium in comparison to thermodynamic calculations, it is concluded that 20,000 hour creep tests are adequate for prediction of long-term creep performance.

36 MATERIALS SCIENCE↗

An additively manufactured near-eutectic Al-Ce-Ni-Mn-Zr alloy with high creep resistance

A new additively manufactured (AM) Al-7.5Ce-4.5Ni-0.4Mn-0.7Zr (wt.%) near-eutectic alloy is reported, which shows unprecedented creep resistance up to 400 °C (a homologous temperature of 0.72). The eutectic solidification microstructure comprises ~ 27 vol% of coarsening-resistant second phase network with an ultrafine (<100 nm) inter-phase spacing. Both Mn and Zr contribute to creep resistance of the alloy. Small amount of Mn addition promotes selection of coarsening resistant phases without compromising the alloy processability. Zr not only improves hot-tearing resistance, but further enhances the second phase coarsening resistance resulting in improved creep resistance. Neutron diffraction performed during creep deformation reveals that the underlying mechanism for creep resistance in this alloy is impedance to dislocation motion stemming from the ultrafine eutectic solidification microstructure, whereas load transfer strengthening becomes less effective as the creep temperature increases. The second phase forms a continuous network in the as-fabricated condition, which is maintained during long-term creep at 300 °C. However, this network is fragmented into fine dispersoids at higher temperatures. It is proposed that the rate-limiting deformation mechanism at 300–400 °C is (i) dislocation climb for the alloy with fragmented second phase dispersoids and (ii) Orowan looping for the alloy with a continuous second phase network. In conclusion, the present design of an AM-processable multicomponent eutectic alloy with high creep resistance can be applied to other metallic systems exhibiting eutectic reactions, with expected extreme creep resistance.

36 MATERIALS SCIENCE↗