Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CASTING MOLDS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Improving the performance of high-strength steel castings by specialized cooling

The influence of microcooling and external cooling on the structure and mechanical properties of moderately alloyed high-strength special-purpose steel and also on the morphology of its nonmetallic inclusions is investigated. The properties of castings obtained in different molds and in different conditions are compared. The influence of hybrid (external and internal) modification of the casting process on the quality of heavy housing castings is investigated.

42 ENGINEERING↗

Epoxy-resin patterns speed shell-molding of aluminum parts

Half patterns cast from commercial epoxy resin containing aluminum powder are used for shell-molding of aluminum parts. The half patterns are cast in plastic molds of the original wooden pattern. Ten serviceable sand resin molds are made from each epoxy pattern.

Source record↗

Influence of Electropulsing Treatment on the Initial Solidification of Molten Steel During Continuous Casting

An electropulsing-assisted mold simulator (EPMS) technique was developed to investigate the effect of pulsed electric current on the initial solidification behavior of molten steel during the process of continuous casting. The results indicated that the variation of mold hot surface temperatures in the meniscus area decreased from 375.8 K to 394 K for the case without electropulsing treatment (EPT) to 363.5 K to 377.3 K for the one with EPT. The mold surface heat fluxes fluctuated around the baseline of 0.83 and 2.42 MW/m{sup 2} in the cases with and without EPT, respectively, which indicated that a higher thermal resistance between the initial shell and copper mold was introduced by employing the EPT. The crystal fraction of slag films increased from 69.8 to 77.9 pct, whereas the grain size of mold flux film decreased, when compared the case of EPT treatment with the benchmark one, which suggested that the pulsed electric current promotes the movement of molten clusters and particles, leading to the enhancement of mold flux crystallization and the improvement of thermal resistance. Moreover, the solidification structure of steel along the direction of solidification (from the mold to melt) includes a fine chilled grain layer close to the mold, a columnar dendrite layer in the middle, and equiaxed grains next to the melt core, in which a compacted microstructure with smaller secondary dendrite arm spacing was observed in the case of the EPT. The results demonstrate that the EPT could refine the as-cast solidification microstructure.

36 MATERIALS SCIENCE↗

Energy-Saving Melting and Revert Reduction Technology (E-SMARRT), Task 5.3: Casting Porosity-Free Grain Refined Magnesium Alloys

The objective of this project was to identify the root causes for micro-porosity in magnesium alloy castings and recommend remedies that can be implemented in production. Three casting magnesium alloys were used to determine the causes of porosity that is a common problem in the magnesium casting industry. These alloys were AM50A, AM60A, and AZ91D, and all were grain refined with C 2 Cl 6 . Gas porosity was found to have little effect if proper degassing methods and foundry practices were used. It was found that sound gating practice, directional solidification towards the riser and generous risering should always dominate in order to produce sound castings. In sand cast magnesium, thermal gradients were found to be an important indicator of heat transfer in the mold. A minimum thermal gradient was found for each alloy that would produce sound castings. There were 2.02°C/cm for AM50A, 1.99°C/cm for AM60A, and 1.97°C/cm for AZ91D. If these gradients are met or exceeded when an area of the casting reaches 50°C below the liquidus for the alloy, the casting will be free of shrinkage porosity in that area. The cooling rates measured during casting magnesium alloys in a pre-heated step permanent mold ranged from 12°F/min in the three inches thick step to 200o F/min in the one inch step. The effect of the cooling rate on the grain size and the mechanical properties was noticeable but not substantial. Grain refining with C 2 Cl 6 had a marked effect on the grain size of the permanent mold step casting. It reduced it by 10-15% in AM50A and by a factor of six in AZ91E from 300 µm to around 55 µm. The mechanical properties of both permanent mold cast AZ91E and AM50A were improved by grain refinement. The most prominent increase was in the elongation of AM50A that more than doubled from 8% to 17%. Computer simulation of porosity was conducted for a well gated commercial wheel casting. The simulation did not predict significant porosity in the wheel. The mechanical testing of tensile specimens excised from the wheel indeed confirmed good properties, in line with the specifications for this alloy. Evidence of minimal micro-porosity was detected in sections cut from the wheel and investigated under optical microscopy. This finding confirms the key role played by utilizing optimal gating and risering practices in minimizing porosity in magnesium castings.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Method for casting polyethylene pipe

Short lengths of 7-cm ID polyethylene pipe are cast in a mold which has a core made of room-temperature-vulcanizable (RTV) silicone. Core expands during casting and shrinks on cooling to allow for contraction of the polyethylene.

Elam, R. M., Jr.↗

Effect of Nozzle Port Angle on Transient Flow and Surface Slag Behavior During Continuous Steel-Slab Casting

Undesirable flow variations can cause severe instabilities at the interface between liquid mold flux and molten steel across the mold top-region during continuous steel casting, resulting in surface defects in the final products. A three-dimensional Large Eddy Simulation (LES) model using the volume of fluid method for the slag and molten steel phases is validated with plant measurements, and applied to gain new insights into the effects of nozzle port angle on transient flow, top slag/steel interface movement, and slag behavior during continuous slab casting under nominally steady conditions. Upward-angled ports produce a single-roll flow pattern with lower surface velocity, due to rapid momentum dissipation of the spreading jet. However, strong jet wobbling from the port leads to greater interface variations. Severe level drops allow easy entrapment of liquid flux by the solidifying steel shell at the meniscus. Sudden level rises may also be detrimental, leading to overflow of the solidified meniscus region. Downward-angled ports produce a classic double-roll pattern with less jet turbulence and a more stable interface everywhere except near the narrow faces. Finally, the flow patterns, surface velocity, and level predicted from the validated LES model are compared with steady-state standard k-ε model predictions.

36 MATERIALS SCIENCE↗

Pressure Rig for Repetitive Casting

Equipment life increased by improved insulation. New design cuts time of preparation for casting from several days to about 1 hour. Savings due to elimination of lengthy heating and drying operations associated with preparation of ceramic mold. Quality of casting improved because moisture in cavity eliminated by use of insulating material, and more uniform pressure applied to process. Commercial blanket insulator protects components from heat, increasing life of pressure rig and enabling repeated use. Improved heat protection allows casting of brass and other alloys with higher melting temperatures in pressure rig.

Vasquez, P.↗

High-Strength Aluminum Casting Alloy for High-Temperature Applications (MSFC Center Director's Discretionary Fund Final Project No. 97-10)

A new aluminum-silicon alloy has been successfully developed at Marshall Space Flight Center that has a significant improvement in tensile strength at elevated temperatures (550 to 700 F). For instance, the new alloy shows in average tensile strength of at least 90 percent higher than the current 390 aluminum piston alloy tested at 500 F. Compared to conventional aluminum alloys, automotive engines using the new piston alloy will have improved gas mileage, and may produce less air pollution in order to meet the future U.S. automotive legislative requirements for low hydrocarbon emissions. The projected cost for this alloy is less than $0.95/lb, and it readily allows the automotive components to be cast at a high production volume with a low, fully accounted cost. It is economically produced by pouring molten metal directly into conventional permanent steel molds or die casting.

Lee, J. A.↗

Experimental Study of the Mold Flow Induced by a Swirling Flow Nozzle and Electromagnetic Stirring for Continuous Casting of Round Blooms

This study focuses on an experimental investigation of the fluid flow in round bloom continuous casting using a 1:3 model of the industrial casting process. A swirling flow nozzle, represented by the specific design of the RHI Magnesita GYRONOZZLE, is used to produce a swirling motion in the cylindrical mold. The test section is integrated into the Mini-LIMMCAST facility at HZDR, which is operated at room temperature using the ternary alloy GaInSn. Systematic measurements of horizontal and vertical velocity profiles are performed by means of the Ultrasound Doppler Velocimetry. The second part of the study focuses on the interaction between the flow driven by the GYRONOZZLE and concurrent electromagnetic stirring in the mold (M-EMS) by applying rotating magnetic fields (RMFs) at different magnetic flux densities. The effect of the GYRONOZZLE on the flow pattern inside the mold is examined with and without superimposed RMFs and compared to those of a standard single-port nozzle. The measurements reveal that the GYRONOZZLE induces a swirling flow in the whole mold. It is further shown that the influence of a simultaneously applied RMF is mainly restricted to the lower part of the mold since the transport of angular momentum to the top is suppressed by the jets pouring out from the GYRONOZZLE.

36 MATERIALS SCIENCE↗

Glovebox Advanced Casting System Casting Optimization

Casting optimization in the GACS included three broad areas; casting of U-10Zr pins, incorporation of an integral FCCI barrier, and development of a permanent crucible coating. U-10Zr casting was improved over last year’s results by modifying the crucible design to minimize contact with the colder mold. Through these modifications casting of a three pin batch was successful. Incorporation of an integral FCCI barrier also was optimized through furnace chamber pressure changes during the casting cycle to reduce gas pressures in the mold cavities which led to three full length pins being cast which incorporated FCCI barriers of three different thicknesses. Permanent crucible coatings were tested against a base case; 1500°C for 10 minutes in a U-20Pu-10Zr molten alloy. None of the candidate coating materials showed evidence of failure upon initial visual examination. In all areas of work a large amount of characterization will be needed to fully determine the effects of the optimization activities. The characterization activities and future work will occur next year.

36 MATERIALS SCIENCE↗

Preparation of cast aluminum alloy-mica particle composites

A method for making aluminum-mica particle composites is presented in which mica particles are stirred in molten aluminum alloys followed by casting in permanent molds. Magnesium is added either as an alloying element or in the form of pieces to the surface of the alloy melts to disperse up to 3 wt% mica powders in the melts and to obtain high recoveries of mica in the castings. The mechanical properties of the aluminum alloy-mica composite decrease with increasing mica content; however, even at 2.2% it has a tensile strength of 14.22 kg/sq mm with 1.1% elongation, a compression strength of 42.61 kg/sq mm, and an impact strength of 0.30 kgm/sq cm. Cryogenic and self-lubricating bearing are mentioned applications.

Deonath, MR.↗

Commercialization of NASA's High Strength Cast Aluminum Alloy for High Temperature Applications

In this paper, the commercialization of a new high strength cast aluminum alloy, invented by NASA-Marshall Space Flight Center, for high temperature applications will be presented. Originally developed to meet U.S. automotive legislation requiring low- exhaust emission, the novel NASA aluminum alloy offers dramatic improvement in tensile and fatigue strengths at elevated temperatures (450 F-750 F), which can lead to reducing part weight and cost as well as improving performance for automotive engine applications. It is an ideal low cost material for cast components such as pistons, cylinder heads, cylinder liners, connecting rods, turbo chargers, impellers, actuators, brake calipers and rotors. NASA alloy also offers greater wear resistance, dimensional stability, and lower thermal expansion compared to conventional aluminum alloys, and the new alloy can be produced economically from sand, permanent mold and investment casting. Since 2001, this technology was licensed to several companies for automotive and marine internal combustion engines applications.

Lee, Jonathan A.↗

Casting Characteristics of High Cerium Content Aluminum Alloys

This paper compares the castability of the near eutectic aluminum-cerium alloy system to the aluminum-silicon and aluminum-copper systems. The alloys are compared based on die filling capability, feeding characteristics and tendency to hot tear in both sand cast and permanent mold applications. The castability ranking of the binary Al–Ce systems is as good as the aluminum-silicon system with some deterioration as additional alloying elements are added. In alloy systems that use cerium in combination with common aluminum alloying elements such as silicon, magnesium and/or copper, the casting characteristics are generally better than the aluminum-copper system. In general, production systems for melting, de-gassing and other processing of aluminum-silicon or aluminum-copper alloys can be used without modification for conventional casting of aluminum-cerium alloys.

36 MATERIALS SCIENCE↗

Energy Saving Melting andRevert Reduction Technology (E0SMARRT): Predicting Pattern Tooling and Casting Dimension for Investment Casting

The investment casting process is an expendable mold process where wax patterns of the part and rigging are molded, assembled, shelled and melted to produce a ceramic mold matching the shape of the component to be cast. Investment casting is an important manufacturing method for critical parts because of the ability to maintain dimensional shape and tolerances. However, these tolerances can be easily exceeded if the molding components do not maintain their individual shapes well. In the investment casting process there are several opportunities for the final casting shape to not maintain the intended size and shape, such as shrinkage of the wax in the injection tool, the modification of the shape during shell heating, and with the thermal shrink and distortion in the casting process. Studies have been completed to look at the casting and shell distortions through the process in earlier phases of this project. Dr. Adrian Sabau at Oak Ridge National Labs performed characterizations and validations of 17-4 PH stainless steel in primarily fused silica shell systems with good agreement between analysis results and experimental data. Further tasks provided material property measurements of wax and methodology for employing a viscoelastic definition of wax materials into software. The final set of tasks involved the implementation of the findings into the commercial casting analysis software ProCAST, owned and maintained by ESI Group. This included: o the transfer of the wax material property data from its raw form into separate temperature-dependent thermophysical and mechanical property datasets o adding this wax material property data into an easily viewable and modifiable user interface within the pre-processing application of the ProCAST suite, namely PreCAST o and validating the data and viscoelastic wax model with respect to experimental results

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Dynamic Wetting of High-Al Steel by CaO-SiO{sub 2}- and CaO-Al{sub 2}O{sub 3}-Based Mold Fluxes

Wetting of steel by mold fluxes affects the surface quality of steel products. Reaction between [Al] and mold fluxes in the continuous casting of high-Al steel leads to a dynamic interfacial phenomenon. This work investigated the wetting of the high-Al steel substrate by CaO-SiO{sub 2}-based and CaO-Al{sub 2}O{sub 3}-based mold fluxes. The interfacial tensions were estimated and related to their high-temperature structures. The interface morphology revealed that CaO-SiO{sub 2}-based mold flux and CaO-Al{sub 2}O{sub 3}-based mold flux with CaO/Al{sub 2}O{sub 3} = 1 exhibited deep reaction zones in the steel substrates and irregular flux/steel interfaces, while CaO-Al{sub 2}O{sub 3}-based mold fluxes with CaO/Al{sub 2}O{sub 3} = 2 and 3 showed smooth interfaces and superficial reaction zones. The sedation of dynamic wetting behavior in Samples 3 and 4 was related to the high viscosity in the flux droplet after the initial composition change, which led to the stabilization of the interface.

36 MATERIALS SCIENCE↗

A Low-Cost Lightweight Entropic Alloy with High Strength

In this study, a series of lightweight Al–Mg system entropic alloys containing Zn, Cu, and Si were designed based on the order/disorder or entropy, and eutectic concepts. The alloys of Al{sub 58.5}Mg{sub 31.5}Zn{sub 4.5}Cu{sub 4.5}Si{sub 1}; Al{sub 63}Mg{sub 27}Zn{sub 4.5}Cu{sub 4.5}Si{sub 1}; Al{sub 66.7}Mg{sub 23.3}Zn{sub 4.5}Cu{sub 4.5}Si{sub 1}; Al{sub 80}Mg{sub 14}Zn{sub 2.7}Cu{sub 2.7}Si{sub 0.6}; Al{sub 85}Mg{sub 10.5}Zn{sub 2.025}Cu{sub 2.025}Si{sub 0.45}; and Al{sub 90}Mg{sub 7}Zn{sub 1.35}Cu{sub 1.35}Si{sub 0.3} were prepared by induction melting under a high-purity argon atmosphere and then casted into stainless steel molds. The microstructures which were tested in the as-cast state exhibited multiphases and contained apparent volume fractions of intermetallic compounds and solid solutions. Then, the compressive mechanical properties of the alloys were measured, and high fracture strengths of 577, 677, 590, 498, 814, and 794 MPa, respectively, were determined. Strong hardening phenomena were observed in the Al{sub 80}Mg{sub 14}Zn{sub 2.7}Cu{sub 2.7}Si{sub 0.6}, Al{sub 85}Mg{sub 10.5}Zn{sub 2.025}Cu{sub 2.025}Si{sub 0.45}, and Al{sub 90}Mg{sub 7}Zn{sub 1.35}Cu{sub 1.35}Si{sub 0.3} alloys at room temperature, with amazing plasticity percentages of 13.8, 24.8, and 32.7%, respectively. The property differences in the lightweight alloys were analyzed using the following parameters: the critical values of the enthalpy of mixing; atomic size differences; ratio of entropy to enthalpy; valence electron concentration (VEC); and Pauling electronegativity difference. Finally, three of the aforementioned parameters (atomic size difference, enthalpy of mixing, and Pauling electronegativity difference) were regarded in this study as the crucial rules for the lightweight multicomponent alloys.

36 MATERIALS SCIENCE↗

Magnetic properties and microstructure of bulk Nd-Fe-B magnets solidified in magnetic field

The Nd-Fe-B bulk magnets with a slab shape of 0.9 x 4 x 15 mm{sup 3} were prepared by injection casting into a copper mold. The effects of applying a magnetic field during the casting process on the magnetic properties and microstructure of Nd{sub 9.5}Fe{sub 71.5}Ti{sub 2.5}Zr{sub 0.5}Cr{sub 1}B{sub 14.5}C{sub 0.5} alloy have been studied. The results show that the sample cast with magnetic field has a stronger (00L) texture of Nd{sub 2}Fe{sub 14}B phase with the c-axis perpendicular to the slab plane than the sample cast without magnetic field. The intensity of the texture weakens from surface to inner region of the bulk magnets. Applying a magnetic field during the casting process is helpful to refine the grain size effectively. As a result, the magnetic properties are improved from B{sub r} = 5.8 kG, {sub i}H{sub c} = 6.5 kOe, and (BH){sub max} = 5.9 MGOe for thesample cast without magnetic field to B{sub r} = 6.1 kG, {sub i}H{sub c} = 10.3 kOe, and (BH){sub max} = 7.3 MGOe for the sample cast with a 3.7 kOe magnetic field.

36 MATERIALS SCIENCE↗

Improved ceramic slip casting technique

A primary concern in modern fluid dynamics research is the experimental verification of computational aerothermodynamic codes. This research requires high precision and detail in the test model employed. Ceramic materials are used for these models because of their low heat conductivity and their survivability at high temperatures. To fabricate such models, slip casting techniques were developed to provide net-form, precision casting capability for high-purity ceramic materials in aqueous solutions. In previous slip casting techniques, block, or flask molds made of plaster-of-paris were used to draw liquid from the slip material. Upon setting, parts were removed from the flask mold and cured in a kiln at high temperatures. Casting detail was usually limited with this technique -- detailed parts were frequently damaged upon separation from the flask mold, as the molded parts are extremely delicate in the uncured state, and the flask mold is inflexible. Ceramic surfaces were also marred by 'parting lines' caused by mold separation. This adversely affected the aerodynamic surface quality of the model as well. (Parting lines are invariably necessary on or near the leading edges of wings, nosetips, and fins for mold separation. These areas are also critical for flow boundary layer control.) Parting agents used in the casting process also affected surface quality. These agents eventually soaked into the mold, the model, or flaked off when releasing the case model. Different materials were tried, such as oils, paraffin, and even an algae. The algae released best, but some of it remained on the model and imparted an uneven texture and discoloration on the model surface when cured. According to the present invention, a wax pattern for a shell mold is provided, and an aqueous mixture of a calcium sulfate-bonded investment material is applied as a coating to the wax pattern. The coated wax pattern is then dried, followed by curing to vaporize the wax pattern and leave a shell mold of the calcium sulfate-bonded investment material. The shell mold is cooled to room temperature, and a ceramic slip is poured therein. After a ceramic shell of desired thickness has set up in the shell mold, excess ceramic slip is poured out. While still wet, the shell mold is peeled from the ceramic shell to expose any delicate or detailed parts, after which the ceramic shell is cured to provide a complete, detailed, precision ceramic article without parting lines.

Buck, Gregory M.↗