At least 145 records · Page 8

Dioxygen activation by non-adiabatic oxidative addition to a single metal center [O 2 activation by non-adiabatic oxidative addition to a single metal center]

A chromium(I) dinitrogen complex reacts rapidly with O 2 to form the mononuclear dioxo complex [Tp tBu,Me Cr V (O) 2 ] (Tp tBu,Me =hydrotris(3- tert -butyl-5-methylpyrazolyl)borate), whereas the analogous reaction with sulfur stops at the persulfido complex [Tp tBu,Me Cr III (S 2 )]. The transformation of the putative peroxo intermediate [Tp tBu,Me Cr III (O 2 )] (S= 3 / 2 ) into [Tp tBu,Me Cr V (O) 2 ] (S= 1 / 2 ) is spin-forbidden. The minimum-energy crossing point for the two potential energy surfaces has been identified. Finally, although the dinuclear complex [(Tp tBu,Me Cr) 2 (μ-O) 2 ] exists, mechanistic experiments suggest that O 2 activation occurs on a single metal center, by an oxidative addition on the quartet surface followed by crossover to the doublet surface.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

AFRL Additive Manufacturing Modeling Series: Challenge 4, In Situ Mechanical Test of an IN625 Sample with Concurrent High-Energy Diffraction Microscopy Characterization

In this work, we describe 3D characterization of an additively manufactured Inconel 625 nickel-base superalloy specimen conducted during a uniaxial tension test using a suite of nondestructive x-ray techniques. High-energy diffraction microscopy in both near- and far-field modalities are employed in situ to track evolution of the material orientation and stress–strain fields at six points during the mechanical test, and these data streams are registered with micro-computed tomography reconstructions which probe the material density. This data volume was matched to a multi-modal serial sectioning characterization of the specimen taken after loading, described in this article’s companion. Twenty-eight grains which were monitored throughout the experiment were selected to form the basis for AFRL AM Modeling Series Challenge 4, Microscale Structure-to-Properties.

36 MATERIALS SCIENCE↗

Directional and oscillating residual stress on the mesoscale in additively manufactured Ti-6Al-4V Mesoscale and anisotropic residual stress in additive manufacturing of Ti-6Al-4V

In additive manufacturing of metals as compared to conventional processing, the directional track-by-track and layer-by-layer nature of the fabrication process can lead to residual stresses that locally are both directionally and spatially heterogeneous. Much of the existing literature has focused either on the macroscale residual stress inside the entire part, or on the microscale residual stresses that are created around a scan vector, thereby neglecting the intermediate length-scale of the different layers. The objective of this research is to investigate such mesoscale residual stress distributions across several layers in Ti-6Al-4V components produced by laser metal deposition process. The incremental centre hole drilling and incremental slitting methods provide measurements with excellent spatial resolution within and across the layer length scale. Here in this work, the two methods complemented each other to quantify both mesoscale and directional variations of residual stress that correlate with the deposition pattern. Lastly, our findings also provide strong evidence that an oscillatory residual stress variation persists even after thermal cycling that occurs during deposition of subsequent layers.

36 MATERIALS SCIENCE↗

Tensile properties, strain rate sensitivity, and activation volume of additively manufactured 316L stainless steels [Tensile properties of 316L stainless steels made by laser powder-bed-fusion additive manufacturing]

The tensile properties of additively manufactured (AM) metals and alloys are among the most important variables that impact the potential applications of these materials. Here we examine and report on the tensile properties of AM 316L stainless steels fabricated by the laser powder-bed-fusion (L-PBF) technique, via twelve sets of optimized laser processing parameters that produce materials with density >98.8 ± 0.10%. A heterogeneous microstructure is observed in all L-PBF samples, including microscopic features such as dislocations, cellular walls, elemental segregations, local misorientations, impurities, precipitates, and a large fraction of low-angle grain boundaries (2-10°, ~40–60%). The derived average grain size defined by high-angle grain boundaries (>10°) is ~30–50 μm. Tensile testing reveals a yield strength ranging from 552 to 635 MPa and a tensile-elongation-to-failure (TEF) of 0.09–0.42 for directly-printed samples, whereas these values are 592–690 MPa and 0.29–0.50 for samples machined from the as-built rectangular thin plates. In all samples, we observe a variation of tensile yield strength within ~15% but not the TEF, suggesting marginal microstructural changes despite a wide range of laser processing parameters. The large scatter of TEF in directly-printed samples originates from the sensitivity of thin gauge geometry (~2 mm 2 cross-section area) to the built-in flaws. We measured a substantially higher strain rate sensitivity (m~0.02–0.03) of L-PBF 316L compared to the coarse-grained counterparts (~0.006), together with a small activation volume of ~20–30b3 (where b is the Burgers vector of 316L). In conclusion, these deformation kinetics parameters suggest that the tensile plasticity of L-PBF 316L is controlled by a much finer microstructural length scale than the measured grain size, consistent with the high strength and juxtaposed nano- to macro-structures seen in these materials. Strategies to optimize the tensile properties of AM materials are discussed.

36 MATERIALS SCIENCE↗

Residual stress accumulation in large-scale Ti-6Al-4V wire-arc additive manufacturing

Large-scale additive manufacturing (AM) is of interest in the manufacturing industry to produce components of dimensions on the order of hundreds of millimeters to meters in scale. Wire-arc AM (WAAM) of Ti-6Al-4V (Ti64) is an attractive technique for large-scale AM in the aerospace industry, give the high strength-to-weight ratio of the material and high deposition rate of the process. However, due to the large scale, significant distortion and residual stresses are developed in the material during deposition and cooling, potentially leading to part failure. WAAM of a prototypical large-scale Ti64 machine tool component is studied in this work via finite element analysis (FEA). Element activation/deactivation technique is employed to simulate deposition and the resulting distortion and residual stress (RS) predictions are analyzed to evaluate the possibility of crack formation. Significant distortion (∼10 mm) and RS (>1300 MPa) is predicted, suggesting the formation of cracks and possible crack propagation into the build region. Incorporation of fillets significantly reduces RS concentration regions, thus reducing the possibility of part failure. Material deposition sequence also affects the RS pattern in the build.

Mathews, Ritin↗

Real-Time Defect Correction in Large-Scale Polymer Additive Manufacturing via Thermal Imaging and Laser Profilometer

Defects can result in a failed part and are costly in terms of time and material. This cost is even greater in the context of large-scale additive manufacturing where the objects can be very large. As a result, a great deal of research has focused on defect identification and mitigation. To address defects during object construction, researchers at Oak Ridge National Laboratory’s Manufacturing Demonstration Facility investigated an in-situ control system comprised of two sensors: a thermal camera and laser profilometer. This control system adjusted material flow and build speed to mitigate three types of defects: low layer times, underfill, and overfill. Several test objects were constructed. The control system was found to adjust build parameters to handle low layer times of approximately 15 seconds and height deviations from -100% underfill (the absence of a layer) to 50% overfill. Within two layers, height deviations could be returned to within 10% of the expected layer height. Further, preliminary results suggest the system can compensate for uneven build surfaces.

Borish, Michael↗

Characterization and nondestructive inspection of additively manufactured materials

Additively manufactured (AM) components often exhibit significant discontinuities and indications without a clear understanding of how they might affect the mechanical properties of a part during qualification and service. This uncertainty is unacceptable for the design and manufacturing of most aerospace components. Current research in both mechanical testing and nondestructive evaluation involves developing methods for characterizing and inspecting AM components as the use of such materials continues to rise. Although several AM manufacturing methods have been developed in recent decades, this paper focuses on AM production-ready processes for a direct metal laser sintering (DMLS) powder bed fusion machine and will provide background on Sandia National Laboratories’ research efforts in this area. Tensile bar samples manufactured using the DMLS powder bed fusion method were inspected in this study, and the results of ultrasonic spectroscopy for assessing internal flaws will be presented. A combination of material property evaluation, microstructural characterization, and nondestructive inspection techniques will also be described. Finally, the results obtained from these material evaluation methods assist in determining inspection limits and methods for qualifying AM materials.

36 MATERIALS SCIENCE↗

A fully coupled thermal–microstructural–mechanical finite element process model for directed energy deposition additive manufacturing of Ti–6Al–4V

A fully coupled thermal–microstructural–mechanical finite element modelling framework is developed to investigate the distortion and residual stresses during directed energy deposition (DED) of multi-phase Ti–6Al–4V alloy. The Johnson–Cook constitutive model is used to predict the yield strength of each phase as a function of strain, strain rate and temperature where the flow stress is calculated by a linear mixing rule based on the volumetric phase fractions. A thin-walled rectangular sample is chosen as the reference geometry and the results are compared with experimentally measured in situ thermal history and distortion data, where a reasonable agreement is achieved. The proposed modelling framework with physics-based material constitutive model provides useful information for a better understanding of process–microstructure–property relations in additive manufacturing by DED.

Tunay, Merve↗

Theoretical Considerations for Improving the Pulse Power of a Battery through the Addition of a Second Electrochemically Active Material

Here, porous electrode theory is used to conduct case studies for when the addition of a second electrochemically active material can improve the pulse-power performance of an electrode. Case studies are conducted for the positive electrode of a sodium metal-halide battery and the graphite negative electrode of a lithium “rocking chair” battery. The replacement of a fraction of the nickel chloride capacity with iron chloride in a sodium metal-halide electrode and the replacement of a fraction of the graphite capacity with carbon black in a lithium-ion negative electrode were both predicted to increase the maximum pulse power by up to 40%. In general, whether or not a second electrochemically active material increases the pulse power depends on the relative importance of ohmic-to-charge transfer resistances within the porous structure, the capacity fraction of the second electrochemically active material, and the kinetic and thermodynamic parameters of the two active materials.

25 ENERGY STORAGE↗