Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “PERMITTIVITY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,423 records · Page 79

Structural and electrical characteristics of dysprosium-doped barium stannate titanate ceramics

Effects of dysprosium (Dy) amphoteric doping on the structural, dielectric and electric properties of barium stannate titanate (BTS) ceramics have been studied. X-ray diffraction analyses reveal that all Dy-doped BTS ceramics exhibit cubic perovskite structure until to 1 mol%. Dy doping at the A site shows lower solubility than that at the B site. SEM surface morphologies display that the Dy B site doping is beneficial for the compact and homogeneous grain distribution. The dielectric constant and loss tangent are reduced with increase of the doping levels. Impedance spectroscopy investigation demonstrates that all samples are insulating at room temperature. Doping alters the full resistive regions of pure BTS ceramics to Doped BTS with insulating grain boundaries and semiconducting bulk regions, but the doping contents has little effect on changing the electric structures.

36 MATERIALS SCIENCE↗

Electrical properties of vanadium tungsten oxide thin films

The vanadium tungsten oxide thin films deposited on Pt/Ti/SiO{sub 2}/Si substrates by RF sputtering exhibited good TCR and dielectric properties. The dependence of crystallization and electrical properties are related to the grain size of V{sub 1.85}W{sub 0.15}O{sub 5} thin films with different annealing temperatures. It was found that the dielectric properties and TCR properties of V{sub 1.85}W{sub 0.15}O{sub 5} thin films were strongly dependent upon the annealing temperature. The dielectric constants of the V{sub 1.85}W{sub 0.15}O{sub 5} thin films annealed at 400 {sup o}C were 44, with a dielectric loss of 0.83%. The TCR values of the V{sub 1.85}W{sub 0.15}O{sub 5} thin films annealed at 400 {sup o}C were about -3.45%/K.

36 MATERIALS SCIENCE↗

Synthesis of nanocrystalline magnesium titanate by an auto-igniting combustion technique and its structural, spectroscopic and dielectric properties

Nanocrystalline magnesium titanate was synthesized through an auto-ignited combustion method. The phase purity of the powder was examined using X-ray diffraction, thermo gravimetric analysis, differential thermal analysis, Fourier transform infrared spectroscopy and Raman spectroscopy. The transmission electron microscopy study showed that the particle size of the as-prepared powder was in between 20 and 40 nm. The nanopowder could be sintered to 98% of the theoretical density at 1200 {sup o}C for 3 h. The microstructure of the sintered surface was examined using scanning electron microscopy. The dielectric constant ({epsilon}{sub r}) of 16.7 and loss factor (tan {delta}) of the order of 10{sup -4} were obtained at 5 MHz when measured using LCR meter. The quality factor (Q{sub u} x f) 73,700 and temperature coefficient of resonant frequency ({tau}{sub f}) -44.3 ppm/{sup o}C, at 6.5 GHz are the best reported values for sintered pellets obtained from phase pure nanocrystalline MgTiO{sub 3} powder.

36 MATERIALS SCIENCE↗

Dielectric, electrical and magnetoelectric characterization of (x)Ni{sub 0.8}Zn{sub 0.2}Fe{sub 2}O{sub 4} + (1 - x)Pb{sub 0.93}La{sub 0.07}(Zr{sub 0.60}Ti{sub 0.40})O{sub 3} composites

The structural, electrical, dielectric, magnetic and magnetoelectric properties of (x)Ni{sub 0.8}Zn{sub 0.2}Fe{sub 2}O{sub 4} + (1 - x)Pb{sub 0.93}La{sub 0.07}(Zr{sub 0.60}Ti{sub 0.40})O{sub 3} (x = 0, 0.15, 0.30, 0.45 and 1) have been studied by means of various experimental techniques. Polycrystalline samples of this series have been prepared by the double sintering ceramic method. X-ray diffraction data analysis revealed purity of the composites. Microstructural analysis using scanning electron microscopy mode depicts the presence of two phases in contact with each other. Dielectric properties were studied at and well above room temperature. Temperature dependent variation of the dielectric constant show diffused phase transition which can be well described by fitting the Lorentz-type relation, {epsilon}{sub A}/{epsilon}=1+(T-T{sub A}){sup 2}/2{delta}{sub A}{sup 2}. Observation of well-saturated ferroelectric hysteresis loop and magnetic hysteresis loop for composites indicates that ferroelectric and magnetic ordering exist simultaneously at room temperature. The static value of magneto electric voltage coefficient ({alpha}{sub E}) has been studied as a function of magnetic field at room temperature for all the composites. The maximum value of {alpha}{sub E} is 7.53 mV/(cm Oe) for 85% PLZT-15% NZFO composites.

36 MATERIALS SCIENCE↗

Structural characterization and AC conductivity of bis tetrapropylammonium hexachlorado-dicadmate, [N(C{sub 3}H{sub 7}){sub 4}]{sub 2}Cd{sub 2}Cl{sub 6}

Synthesis, crystal structure, vibrational study, {sup 13}C, {sup 111}Cd CP-MAS-NMR analysis and electrical properties of the compound [N(C{sub 3}H{sub 7}){sub 4}]{sub 2}Cd{sub 2}Cl{sub 6}, are reported. The latter crystallizes in the triclinic system (space group P1-bar, Z = 2) with the following unit cell dimensions: a = 9.530(1) A, b = 11.744(1) A, c = 17.433(1) A, {alpha} = 79.31(1){sup o}, {beta} = 84.00(1){sup o} and {gamma} = 80.32(1){sup o}. Besides, its structure was solved using 6445 independent reflections down to R = 0.037. The atomic arrangement can be described by alternating organic and inorganic layers parallel to the (11-bar 0) plan, made up of tetrapropylammonium groups and Cd{sub 2}Cl{sub 6} dimers, respectively. In crystal structure, the inorganic layer, built up by Cd{sub 2}Cl{sub 6} dimers, is connected to the organic ones through van der Waals interaction in order to build cation-anion-cation cohesion. Impedance spectroscopy study, reported in the sample, reveals that the conduction in the material is due to a hopping process. The temperature and frequency dependence of dielectric constants of the single crystal sample has been investigated to determine some related parameters to the dielectric relaxation.

36 MATERIALS SCIENCE↗

Structural, spectroscopic and dielectric investigations on Ba{sub 8}Zn(Nb{sub 6-x}Sb{sub x})O{sub 24} microwave ceramics

Ba{sub 8}Zn(Nb{sub 6-x}Sb{sub x})O{sub 24} (x = 0, 0.3, 0.6, 0.9, 1.2, 1.5, 1.8 and 2.4) ceramics were prepared through the conventional solid-state route. The materials were calcined at 1250 {sup o}C and sintered in the range 1400-1425 {sup o}C. The structure of the system was analyzed by X-ray diffraction, Fourier transform infrared and Raman spectroscopic methods. The theoretical and experimental densities were calculated. The microstructure of the sintered pellets was analyzed using scanning electron microscopy. The low frequency dielectric properties were studied in the frequency range 50 Hz-2 MHz. The dielectric constant ({epsilon}{sub r}), temperature coefficient of resonant frequency ({tau}{sub f}) and the unloaded quality factor (Q{sub u}) are measured in the microwave frequency region using cavity resonator method. The {tau}{sub f} values of the samples reduced considerably with the increase in Sb concentration. The materials have intense emission lines in the visible region. The compositions have good microwave dielectric properties and photoluminescence and hence are suitable for dielectric resonator and ceramic laser applications.

36 MATERIALS SCIENCE↗

Effects of porous carbon additives and induced fluorine on low dielectric constant polyimide synthesized with an e-beam

We report the synthesis of a polyimide matrix with a low dielectric constant for application as an intercalation material between metal interconnections in electronic devices. Porous activated carbon was embedded in the polyimide to reduce the dielectric constant, and a thin film of the complex was obtained using the spin-coating and e-beam irradiation methods. The surface of the thin film was modified with fluorine functional groups to impart water resistance and reduce the dielectric constant further. The water resistance was significantly improved by the modification with hydrophobic fluorine groups. The dielectric constant was effectively decreased by porous activated carbon. The fluorine modification also resulted in a low dielectric constant on the polyimide surface by reducing the polar surface free energy. The dielectric constant of polyimide film decreased from 2.98 to 1.9 by effects of porous activated carbon additive and fluorine surface modification.

36 MATERIALS SCIENCE↗

Magnetic and dielectric study of R{sub 0.5}Sr{sub 0.5}MnO{sub 3} (R = Gd, Tb and Dy)

Magnetic and dielectric properties of perovskite manganites R{sub 0.5}Sr{sub 0.5}MnO{sub 3} (R = Gd, Tb and Dy) have been investigated. DC and AC magnetic measurements showed short-range glassy magnetic ordering at T{sub g} {approx} 40 K. Such ordering was observed by neutron diffraction and is ascribable to the size mismatch of R{sup 3+} and Sr{sup 3+} settled randomly at the same crystallographic site. Dielectric constants for each material were {approx}1000-10,000 between {approx}50 and {approx}300 K and showed broad maximums above T{sub g}. Dielectric dispersion showed poor coherency of the motion of polar regions, plausibly because of the size-mismatch effect; both the magnetic and dielectric properties of this system are governed by the randomness at the R/Sr site. The tan {delta} and EXAFS data suggest that the dielectric response is rooted in a transfer of the Mn-3d electrons.

36 MATERIALS SCIENCE↗

Dielectric properties of lead indium niobate ceramics synthesized by conventional solid state reaction method

Pyrochlore free lead indium niobate ceramics are successfully prepared using wolframite precursor by conventional solid state reaction method in air atmosphere, by adding an excess amount of MgO in PbO-InNbO{sub 4} mixture. The dielectric properties of lead indium niobate ceramic studied as a function of both temperature and frequency indicate relaxor ferroelectric behavior with maximum dielectric constant of 4310 at 40 {sup {omicron}}C for 1 kHz. Lowering of transition temperature and enhancement of dielectric constant at room temperature, compared to earlier reports, may be due to the diffusion of magnesium ion into the lead indium niobate. The saturation polarization P{sub s}, measured at room temperature, is found to be 22.5 {mu}C/cm{sup 2} for 40 kV/cm.

36 MATERIALS SCIENCE↗

Synthesis, dielectric behavior and impedance measurement studies of Cr-substituted Zn-Mn ferrites

Graphical abstract: Variation of dielectric constant with frequency. Research highlights: {yields} Sol-gel route synthesized spherical crystalline nanoparticles of ZnMn{sub 1-x}Cr{sub x}FeO{sub 4}. {yields} XRD, DTA, FTIR, SEM, dielectric and impedance study. {yields} The ferrites show concentration dependence of ac electrical conductivity. {yields} Impedance response is dominated by grain boundary behavior. -- Abstract: Nanocrystalline ZnMn{sub 1-x}Cr{sub x}FeO{sub 4} (1.0 {>=} x {>=} 0) ferrites were synthesized by sol-gel technique. X-ray diffraction (XRD) confirmed the formation of single phasic cubic spinel lattice for all the compositions studied. Lattice parameter shows a decreasing trend with an increase in Cr content in the compositions. Formation of spherical nanoparticles was revealed by scanning electron microscopy (SEM) analysis. Infrared spectroscopic studies revealed two main absorption bands in the range 400-800 cm{sup -1} arising due to tetrahedral (A) and octahedral (B) site vibrations. Dielectric constant, dielectric loss tangent, ac conductivity and complex impedance were measured as a function of frequency in the range 20 Hz to 1 MHz. Frequency dependence of dielectric constant shows dielectric dispersion due to the Maxwell-Wagner type of interfacial polarization. The role of chromium in modifying structural and dielectric properties of these ferrites has been explained.

36 MATERIALS SCIENCE↗

Enhanced characteristics of Ba{sub 5}SmTi{sub 3}Nb{sub 7}O{sub 30} ferroelectric nanocrystalline ceramic prepared by mechanical activation process: A comparative study

Graphical abstract: In the present work, structural, dielectric, ferroelectric, piezoelectric and pyroelectric properties of tungsten-bronze structured Ba{sub 5}SmTi{sub 3}Nb{sub 7}O{sub 30} ceramics, synthesized by mechanical activation and conventional solid-state reaction processes, have been studied with an objective of comparing the properties of the specimens synthesized by the two processes. The specimen prepared using mechanical activation process exhibits improved structural and electrical properties. Research highlights: {yields} In this report Ba{sub 5}SmTi{sub 3}Nb{sub 7}O{sub 30} compounds have been synthesized. {yields} Synthesis was carried out by mechanical activation and solid-state reaction processes. {yields} The mechanical activation process yields nanocrystalline specimen. {yields} The synthesized specimens were characterized for their electrical properties. {yields} A comparative study reveals that nanocrystalline specimen possesses superior properties. -- Abstract: In the present work, structural, dielectric, ferroelectric, piezoelectric and pyroelectric properties of tungsten-bronze structured Ba{sub 5}SmTi{sub 3}Nb{sub 7}O{sub 30} ceramics, synthesized by mechanical activation and conventional solid-state reaction processes, have been studied with an objective of comparing the properties of the specimens synthesized by the two processes. X-ray diffraction analysis shows the formation of the compound in an orthorhombic structure by both the processes. Scanning electron microscopy reveals the formation of a fine granular microstructure in the specimen synthesized by mechanical activation process compared to the specimen synthesized by conventional solid-state method. The specimen prepared using mechanical activation process exhibits improved electrical properties with higher dielectric constant, lower dielectric loss and higher resistivity. The effective remanent polarization (P{sup -bar{sub r}}) value, d{sub 33} value and pyroelectric coefficients are also observed to be higher in the sample synthesized by the mechanical activation process.

36 MATERIALS SCIENCE↗

Could binary mixture of Nd-Ni ions control the electrical behavior of strontium-barium M-type hexaferrite nanoparticles?

Research highlights: {yields} Strontium-barium hexaferrites (Sr{sub 0.5}Ba{sub 0.5}Fe{sub 12}O{sub 19}) in single magnetoplumbite phase solid structure are synthesized by the co-precipitation method. {yields} Structural and electrical properties of Nd-Ni substituted ferrites are investigated. {yields} These ferrite materials possess high electrical resistivity (108 {Omega} cm) that is essential to curb the eddy current loss, which is pre-requisite for surface mount devices. -- Abstract: Cationic substitution in M-type hexaferrites is considered to be an important tool for modification of their electrical properties. This work is part of our comprehensive study on the synthesis and characterization of Nd-Ni doped strontium-barium hexaferrite nanomaterials of nominal composition Sr{sub 0.5}Ba{sub 0.5-x}Nd{sub x}Fe{sub 12-y}Ni{sub y}O{sub 19} (x = 0.00-0.10; y = 0.00-1.00). Doping with this binary mixture modulates the physical and electrical properties of strontium-barium hexaferrite nanoparticles. Structural and electrical properties of the co-precipitated ferrites are investigated using state-of-the-art techniques. The results of X-ray diffraction analysis reveal that the lattice parameters and cell volume are inversely related to the dopant content. Temperature dependent DC-electrical resistivity measurements infer that resistivity of strontium-barium hexaferrites decreases from 1.8 x 10{sup 10} to 2.0 x 10{sup 8} {Omega} cm whereas the drift mobility, dielectric constant and dielectric loss tangent are directly related to the Nd-Ni content. The results of the study demonstrate a relationship between the modulation of electrical properties of substituted ferrites and nature of cations and their lattice site occupancy.

36 MATERIALS SCIENCE↗

Dielectric properties of Ba{sub 3-x}K{sub x}CaNb{sub 2}O{sub 9-{delta}} (0.5 < x < 1.25) (KBCN) double perovskites

Graphical abstract: Electrical conductivity, dielectric constant and dielectric loss of Ba{sub 1.75}K{sub 1.25}CaNb{sub 2}O{sub 9-{delta}} in air at 400-700 {sup o}C. Research highlights: {yields} We show the effectiveness of AC impedance spectroscopy to screen dielectric materials and to understand contributing effects on the dielectric properties of polycrystalline metal oxides. {yields} Unlike Ba{sub 3}CaNb{sub 2}O{sub 9}, Ba{sub 3-x}K{sub x}CaNb{sub 2}O{sub 9-{delta}} exhibits negligible grain-boundary and electrode effects to the total electrical properties and is consistent with perovskite-type K-doped BaZrO{sub 3}. {yields} Among the samples investigated, Ba{sub 1.75}K{sub 1.25}CaNb{sub 2}O{sub 9-{delta}} sintered at 1100 {sup o}C showed the highest dielectric constant of 65 at 10{sup 6} Hz and dielectric loss of 0.14 at 400 {sup o}C in air. -- Abstract: We report synthesis, structure and dielectric properties of double perovskite-type Ba{sub 3-x}K{sub x}CaNb{sub 2}O{sub 9-{delta}} (x = 0.5, 0.75, 1, 1.25) (KBCN). Powder X-ray diffraction (XRD) confirmed the formation of double perovskite-type structure and lattice constant decreases with increasing K in KBCN. AC impedance study showed a single semicircle over the investigated temperatures and frequencies in dry H{sub 2}, H{sub 2} + 3% H{sub 2}O, 3% H{sub 2}O + N{sub 2}, while two semicircles were observed at low temperatures in air, which could be attributed to bulk and grain-boundary contributions. Unlike un-doped BCN, KBCN exhibits negligible grain-boundary and electrode effects to the total electrical properties and is consistent with perovskite-type K-doped BaZrO{sub 3}. The bulk dielectric constant and dielectric loss were found to increase with increasing K content in KBCN and also found to change with sintering temperature. Among the samples investigated, Ba{sub 1.75}K{sub 1.25}CaNb{sub 2}O{sub 9-{delta}} sintered at 1100 {sup o}C showed the highest dielectric constant of 65 at 10{sup 6} Hz and dielectric loss of 0.14 at 400 {sup o}C in air. Isothermal dielectric constant and electrical conductivity at 1 MHz were found to be independent at elevated temperatures, while vary at low-frequency and low temperatures. Below 700 {sup o}C, dielectric constant and dielectric loss decreases with increasing frequency, whereas an opposite trend was observed for the electrical conductivity.

36 MATERIALS SCIENCE↗

Studies on the growth and physical properties of nonlinear optical crystal: 2-Amino-5-nitropyridinium-toluenesulfonate

Graphical abstract: 2-Amino-5-nitropyridinium-toluenesulfonate is identified as potential candidate for efficient frequency conversion. Research highlights: {yields} Single crystals of 2A5NPT have been grown from saturated solution. {yields} Powder test with Nd:YAG laser radiation shows a high second harmonic generation. {yields} Single shot and multiple shot surface laser damage thresholds are determined. {yields} The thermal parameters of 2A5NPT were measured by an improved photopyroelectric technique. {yields} The high value of damage threshold is related to the specific heat of the crystal which is reasonably high. -- Abstract: Single crystals of 2-amino-5-nitropyridinium-toluenesulfonate (2A5NPT) were grown by the slow cooling method. The unit cell dimensions were determined from single crystal X-ray diffraction studies. The thermal parameters - thermal diffusivity ({alpha}), thermal effusivity (e), thermal conductivity (K) and heat capacity (C{sub p}) of 2A5NPT were measured by an improved photopyroelectric technique at room temperature. Single and multiple shot experiments performed on the grown crystals for the second harmonic of pulsed Nd:YAG laser (532 nm) show that it exhibits a high laser damage threshold which is a favorable property for nonlinear optical applications. Dielectric constant and dielectric loss of the grown crystal were evaluated for the frequency range 1 kHz-1 MHz in the temperature region 40-130 {sup o}C. Hardness values were measured using Vickers hardness measurement.

36 MATERIALS SCIENCE↗

Low loss Sr{sub 1-x}Ca{sub x}La{sub 4}Ti{sub 5}O{sub 17} microwave dielectric ceramics

Highlights: {yields} New single phase highly dense (95%) microwave dielectric Sr{sub 1-x}Ca{sub x}La{sub 4}Ti{sub 5}O{sub 17} (0 {<=} x {<=} 1) ceramics were designed and processed. {yields} Theoretical density and molar volume decreased due to the substitution of small Ca{sup 2+} for large Sr{sup 2+}. {yields} As required for microwave dielectric applications, optimum properties (i.e. {epsilon}{sub r} {approx} 53.7, Qf{sub o} {approx} 11,532 GHz and {tau}{sub f} {approx} -1.4 ppm/{sup o}C) were achieved for Sr{sub 0.4}Ca{sub 0.6}La{sub 4}Ti{sub 5}O{sub 17} (x = 0.6). -- Abstract: Microwave dielectric ceramics in the Sr{sub 1-x}Ca{sub x}La{sub 4}Ti{sub 5}O{sub 17} (0 {<=} x {<=} 1) composition series were prepared through a solid state mixed oxide route. All the compositions formed single phase ceramics within the detection limit of in-house X-ray diffraction when sintered in the temperature range 1450-1580 {sup o}C. Theoretical density and molar volume decreased due to the substitution of Ca{sup 2+} for Sr{sup 2+} which was associated with a decrease in the dielectric constant ({epsilon}{sub r}) and temperature coefficient of resonant frequency ({tau}{sub f}) but an increase in quality factor, Qf{sub o}. Optimum properties were achieved for Sr{sub 0.4}Ca{sub 0.6}La{sub 4}Ti{sub 5}O{sub 17} which exhibited, {epsilon}{sub r} {approx} 53.7, Qf{sub o} {approx} 11,532 GHz and {tau}{sub f} {approx} -1.4 ppm/{sup o}C.

36 MATERIALS SCIENCE↗

Microstructural and electrical changes in nickel manganite powder induced by mechanical activation

Highlights: {yields} The influence of mechanical activation on microstructure evolution in the nickel manganite powder was investigated as well as electrical properties of the sintered samples. {yields} Structural refinement obtained by Topas-Academic software based on Rietveld analysis showed that the milling process remarkably changed the powder morphology and microstructure. {yields} SEM studies of sintered samples also revealed the strong influence of milling time on ceramics density (increases with milling time). {yields} The electrical properties of ceramic samples are clearly conditioned by terms of synthesis, in our case the time of mechanical activation. {yields} The highest density and higher values of dielectric constant were achieved at the sample activated for 45 min. -- Abstract: Nickel manganite powder synthesized by calcination of a stoichiometric mixture of manganese and nickel oxide was additionally mechanically activated in a high energy planetary ball mill for 5-60 min in order to obtain a pure NiMn{sub 2}O{sub 4} phase. The as-prepared powders were uniaxially pressed into disc shape pellets and then sintered for 60 min at 1200 {sup o}C. Changes in the particle morphology induced by mechanical activation were monitored using scanning electron microscopy, while changes in powder structural characteristics were followed using X-ray powder diffraction. The ac impedance spectroscopy was performed on sintered nickel manganite samples at 25 {sup o}C, 50 {sup o}C and 80 {sup o}C. It was shown that mechanical activation intensifies transport processes causing a decrease in the average crystallites size, while longer activation times can lead to the formation of aggregates, defects and increase of lattice microstrains. The observed changes in microstructures were correlated with measured electrical properties in order to define optimal processing conditions.

36 MATERIALS SCIENCE↗

Effect of Pb(Fe{sub 1/2}Nb{sub 1/2})O{sub 3} modification on dielectric and piezoelectric properties of Pb(Mg{sub 1/3}Nb{sub 2/3})O{sub 3}-PbZr{sub 0.52}Ti{sub 0.48}O{sub 3} ceramics

Highlights: {yields} 10 mol% PFN modified PMN-PZT relaxor ferroelectric ceramics were prepared by the conventional solid-state mixed-oxide technique, and their structure, dielectric and piezoelectric properties were studied. {yields} At the frequency of 1 kHz, the maximum dielectric constant at room temperature ({epsilon}{sub r}) was 3519 and maximum dielectric constant ({epsilon}{sub m}) was 20,475, corresponding to the (0.9 - x)PMN-0.1PFN-xPZT ceramic composition of x = 0.8. While the sample with composition of x = 0.3 possessed the maximum dielectric relaxor factor of {gamma} = 1.94. The Curie temperature T{sub c} could be higher than 300 {sup o}C around morphotropic phase boundary (MPB) area which is much higher than some other system. {yields} The largest d{sub 33} could be as high as 318 pC/N when x = 0.9. And the maximum remnant polarization P{sub r} was 28.3 {mu}C/cm{sup 2} at x = 0.4. -- Abstract: 10 mol% Pb(Fe{sub 1/2}Nb{sub 1/2})O{sub 3} (PFN) modified Pb(Mg{sub 1/3}Nb{sub 2/3})O{sub 3}-PbZr{sub 0.52}Ti{sub 0.48}O{sub 3} (PMN-PZT) relaxor ferroelectric ceramics with compositions of (0.9 - x)PMN-0.1PFN-xPZT (x = 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8 and 0.9) were prepared. X-ray diffraction investigations indicated that as-prepared ceramics were of pure perovskite phase and the sample with composition of x = 0.8 was close to morphotropic phase boundary (MPB) between rhombohedral and tetragonal phase. Dielectric properties of the as-prepared ceramics were measured, and the Curie temperature (T{sub c}) increased sharply with increasing PZT content and could be higher than 300 {sup o}C around morphotropic phase boundary (MPB) area. At 1 kHz, the sample with composition of x = 0.1 had the largest room temperature dielectric constant {epsilon}{sub r} = 3519 and maximum dielectric constant {epsilon}{sub m} = 20,475 at T{sub m}, while the sample with composition of x = 0.3 possessed the maximum dielectric relaxor factor of {gamma} = 1.94. The largest d{sub 33} = 318 pC/N could be obtained from as-prepared ceramics at x = 0.9. The maximum remnant polarization (P{sub r} = 28.3 {mu}C/cm{sup 2}) was obtained from as-prepared ceramics at x = 0.4.

36 MATERIALS SCIENCE↗

Synthesis, characterization, UV and dielectric properties of hexagonal disklike ZnO particles embedded in polyimides

Graphical abstract: The hexagonal disklike ZnO particles with a diameter of 300-500 nm were synthesized from zinc acetate and NaOH in water with citric acid. ZnO/polyimide composite films with different ZnO contents was prepared. The prepared zinc oxide-polyimide composites were characterized for their structure, morphology and thermal behavior. Composites with ZnO particle contents from 1 to 5 wt% show good transparency in the visible region and luminescent properties. Highlights: {yields} A series of novel ZnO/polyimide composite films with different ZnO contents was prepared. {yields} The ZnO was homogeneously dispersed in the PI matrix. {yields} The composites showed the low dielectric constant of 50 at 10{sup 6} Hz. {yields} Homogenous dispersion and the amount of ZnO particles contributed to the dielectric properties of composites. -- Abstract: A series of novel ZnO/polyimide composite films with different ZnO contents was prepared through incorporation hexagonal disklike ZnO particles into poly(amic acid) of the pre polymer of the polyimide. The hexagonal disklike ZnO particles with a diameter of 300-500 nm were synthesized from zinc acetate and NaOH in water with citric acid. The prepared zinc oxide-polyimide composites were characterized for their structure, morphology, and thermal behavior employing Fourier transform infrared spectroscopy, scanning electron micrograph, X-ray diffraction and thermal analysis techniques. Thermal analyses show that the ZnO particles were successfully incorporated into the polymer matrix and these ZnO/polymer composites have a good thermal stability. Scanning electron microscopy studies indicate the ZnO particles were uniformly dispersed in the polymer and they remained at the original size (300-500 nm) before immobilization. All composite films with ZnO particle contents from 1 to 5 wt% show good transparency in the visible region and luminescent properties.

36 MATERIALS SCIENCE↗