Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “HYDRATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,405 records · Page 78

Insight into elastic behavior of calcium silicate hydrated oxide (C-S-H) under pressure and composition effect

The present work relates to the study of structural and elastic properties of Tobermorite 11 A as a function of external pressure and composition in terms of calcium to silicon ratio. Basing on the lattice dynamics method, the main aim of this work is precisely to shed light, for the first time, on the high pressure structural phase transition in Tobermorite 11 A and the possible correlation with some elastic quantities. In order to check the transferability of the potentials used we have, additionally, performed a single calculation based on the density functional theory (DFT) for a pressure of 15 GPa in the case of Ca/Si = 1. The variation of the unit cell parameters with pressure indicates that Tobermorite 11 A undergoes a structural instability around 15 GPa along b-axis and around 20 GPa along a-axis which is confirmed from our calculations of X-Rays diffraction patterns at various pressure values. We have also observed the anisotropic character of the Tobermorite structure for both cases (Ca/Si = 1 and Ca/Si = 0.83). Our results show that around 20 GPa an important change appears in the elastic behaviour of Tobermorite. As pressure increases the calculated elastic quantities for Ca/Si = 1 became closer to those evaluated for Ca/Si = 0.83, which may stimulate further experimental and theoretical research on the matter.

36 MATERIALS SCIENCE↗

Acid attack on hydrated cement — Effect of mineral acids on the degradation process

During acid attack on concrete structural components, a degraded layer develops whose properties as a protective barrier are decisive for durability. {sup 29}Si NMR spectroscopy and {sup 27}Al NMR spectroscopy were used with XRD to investigate the degraded layer on hardened cement paste exposed to HCl and H{sub 2}SO{sub 4}. The layer comprises an amorphous silica gel with framework silicates, geminate and single silanol groups in which Si is substituted by Al. Amorphous Al(OH){sub 3} and Fe(OH){sub 3} are present. The gel forms by polycondensation and cross-linking of C-A-S-H chains at AlO{sub 4} bridging tetrahedra. In the transition zone between the degraded layer and the undamaged material, portlandite dissolves and Ca is removed from the C-A-S-H phases maintaining their polymer structure at first. With HCl, monosulphate in the transition zone is converted into Friedel's salt and ettringite. With H{sub 2}SO{sub 4}, gypsum precipitates near the degradation front reducing the thickness of the transition zone and the rate of degradation.

36 MATERIALS SCIENCE↗

Mapping high pH levels in hydrated calcium silicates

Data on the variability of pH levels in cement-based materials is essential for a better understanding of the early aging of materials and the long-term performance of concrete structures. Current approaches for measuring pH levels in concrete are inadequate with respect to radiometric range and resolution and spatial granularity. We report on a methodology for mapping pH levels in concrete utilizing a halochromic porphyrin sensor molecule that allows a simple measurement of surface values of pH level using a commercial digital camera setup. As proof of concept, cement paste, mortar, and concrete samples were subject to accelerated carbonation and then evaluated for pH profiles at different ages of degradation. Comparative tests on the same specimens were also conducted using phenolphthalein as the pH indicator. Spatial distribution of pH level from pH 11.0 to 13.5 was mapped at various levels of carbonation.

36 MATERIALS SCIENCE↗

Role of calcium on chloride binding in hydrated Portland cement–metakaolin–limestone blends

Chloride binding is investigated for Portland cement–metakaolin–limestone pastes exposed to CaCl{sub 2} and NaCl solutions. The phase assemblages and the amount of Friedel's salt are evaluated using TGA, XRD and thermodynamic modeling. A larger amount of Friedel's salt is observed in the metakaolin blends compared to the pure Portland cement. A higher total chloride binding is observed for the pastes exposed to the CaCl{sub 2} solution relative to those in the NaCl solution. This is reflected by the fact that calcium increases the quantity of Friedel's salt in the metakaolin blends by promoting the transformation of strätlingite and/or monocarbonate to Friedel's salt. Calcium increases also the amount of chloride in the diffuse layer of the C-S-H for the pure cement. A linear correlation between the total bound chloride and the uptake of calcium from the CaCl{sub 2} solution is obtained and found to be independent on the type of cement blend.

36 MATERIALS SCIENCE↗

Experimental determination of solubilities of di-calcium ethylenediaminetetraacetic acid hydrate [Ca2C10H12N2O8·7H2O(s)] in NaCl and MgCl2 solutions to high ionic strengths and its Pitzer model: Applications to geological disposal of nuclear waste and other low temperature environments

In this study, solubility measurements on di-calcium ethylenediaminetetraacetic acid [Ca 2 C 10 H 12 N 2 O 8 (s), abbreviated as Ca 2 EDTA(s)] as a function of ionic strength are conducted in NaCl solutions up to I = 5.0 mol•kg –1 and in MgCl 2 solutions up to I = 7.5 mol•kg –1 , at room temperature (22.5 ± 0.5oC).

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Corrigendum to “Experimental Determination of Solubilities of Di-calcium Ethylenediaminetetraacetic Acid Hydrate [Ca 2 C 10 H 12 N 2 O 8 •7H 2 O(s)] in NaCl and MgCl 2 Solutions to High Ionic Strengths and Its Pitzer Model: Applications to Geological Disposal of Nuclear Waste and Other Low Temperature Environments”

In the published version (Xiong et al., 2017), there was an error for the reaction coefficient for the dissolution reaction of Ca 2 C 10 H 12 N 2 O 8 •7H 2 O(s) in the database used for the modeling. In the database for the modeling, the coefficient for water (i.e., 7H 2 O) was inadvertently omitted.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗