Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Tensile Testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,387 records · Page 77

Mechanical rolling and annealing of wire-arc additively manufactured stainless steel plates

Thin walls of 304L stainless steel were fabricated by wire-arc additive manufacturing (WAAM) followed by post build thermomechanical processing to modify the as built microstructure and properties. The walls were made using a high-deposition-rate robotically controlled gas-metal arc welding system and were characterized using optical microscopy and tensile tested for mechanical properties. Post processing consisted of mechanical rolling the walls to 25% and 40% strains, followed by annealing at 1050°C to demonstrate a wide range of properties. Results show that WAAM can be used to build custom sized semi-finished parts or blanks that can later be thermomechanically processed to increase strength and ductility through recrystallization of the as built microstructure, and/or processed into desired shapes with improved mechanical properties.

304L stainless steel↗

High strength kiloampere Bi 2 Sr 2 CaCu 2 O x cables for high-field magnet applications

Multifilamentary Ag-sheathed Bi 2 Sr 2 CaCu 2 O x (Bi-2212) wire can carry sufficient critical current density J c for the development of powerful superconducting magnets. But, the range of its applications is limited by the low mechanical strength of the Ag/Bi-2212 strand. A potential solution is to cable Ag/Bi-2212 wire with high-strength materials that are compatible with the Bi-2212 heat treatment in an oxygen atmosphere. Past attempts have not always been successful, because the high-strength materials reacted with Bi-2212 wires, significantly reducing their J c . We examined the nature of reactions occurring when Ag/Bi-2212 wires are heat-treated in direct contact with several commonly used high-strength alloys and a new Fe-Cr-Al alloy. INCONEL X750 and INCONEL 600 resulted in significant J c loss, whereas Ni80-Cr caused little or no J c loss; however, all of them formed chromium oxide that subsequently reacted with silver, creating cracks in the silver sheath. We found that Fe-Cr-Al did not show significant reactions with Ag/Bi-2212 strands. Scanning electron microscopy (SEM) and energy dispersive x-ray (EDS) examinations revealed that the Fe-Cr-Al alloy benefits from the formation of a uniform, crack-free, continuous alumina layer on its surface that does not react with Ag and that helps minimize the Cu loss found with INCONEL X750 and INCONEL 600. We then fabricated prototype 6-around-1 cables with six Bi-2212 strands twisted and transposed around an Fe-Cr-Al alloy core coated with TiO 2 . After standard 1 bar melt processing, the cable retained 100% of the total current-carrying capability of its strands, and, after a 10 bar overpressure processing, the cable reached a total current of 1025 A at 4.2 K and 10 T. Tensile tests showed that Fe-Cr-Al becomes brittle after being cooled to 4.2 K, whereas INCONEL X750 remains ductile and retains a modulus of 183 GPa. Finally. we proposed new cable designs that take advantage of the chemical compatibility of Fe-Cr-Al and high strength of INCONEL X750 for various high-field magnet applications.

43 PARTICLE ACCELERATORS↗

Modeling of irradiation hardening of iron after low–dose and low–temperature neutron irradiation

Irradiation hardening is a prominent low-temperature degradation phenomena in materials, and is characterized both by an irradiation-induced increase in yield strength along with the loss of ductility. In this paper, a reaction–diffusion cluster dynamics model is used to predict the distribution of vacancy and interstitial clusters in iron following low-temperature (<373 K) and low-dose (<0.1 dpa) neutron irradiation. The predicted microstructure evolutions of high-purity iron samples are compared to published experimental data (positron annihilation spectroscopy and transmission electron microscopy) and show good agreement for neutron irradiation in this regime. The defect cluster distributions are then coupled to a dispersed barrier hardening model that assumes a strength factor, α, which varies with cluster type and size to compute the yield strength increase; the results of which agree reasonably well with tensile tests performed in previous studies. Furthermore, the modeling results presented here compare quite well to the experimental observations in the low-dose regime, and provide insight into the underlying microstructure–property relationships and the need for spatially dependent modeling to accurately predict the saturation behavior of yield strength changes observed experimentally at higher dose levels.

36 MATERIALS SCIENCE↗

Microstrip patch antenna for simultaneous strain and temperature sensing

A patch antenna, consisting of a radiation patch, a dielectric substrate, and a ground plane, resonates at distinct fundamental frequencies that depend on the substrate dielectric constant and the dimensions of the radiation patch. Since these parameters change with the applied strain and temperature, this study investigates simultaneous strain and temperature sensing using a single antenna that has two fundamental resonant frequencies. The theoretical relationship between the antenna resonant frequency shifts, the temperature, and the applied strain was first established to guide the selection of the dielectric substrate, based on which an antenna sensor with a rectangular radiation patch was designed and fabricated. A tensile test specimen instrumented with the antenna sensor was subjected to thermo-mechanical tests. Experiment results validated the theoretical predictions that the normalized antenna resonant frequency shifts are linearly proportional to the applied strain and temperature changes. As a result, an inverse method was developed to determine the strain and temperature changes from the normalized antenna resonant frequency shifts, yielding measurement uncertainty of 0.4 °C and 17.22 μϵ for temperature and strain measurement, respectively.

01 COAL, LIGNITE, AND PEAT↗

Mechanical characterization of Bi-2212 composite winding pack samples for high-field superconducting magnet design

Bi₂Sr₂CaCu₂O8−x (Bi-2212) multi-filament round wire is a high-temperature superconductor (HTS) capable of carrying high transport currents, which makes it suitable for high-field magnet applications. However, its weak Ag–Mg sheath leaves it vulnerable to mechanical stress, posing challenges for high-field magnet design. To better understand and improve mechanical stress management in Bi-2212 winding packs, we conducted an experimental study evaluating the axial stress–strain behavior of five winding pack configurations with varying insulation materials, reinforcement strategies, and construction quality. Using uniaxial tensile testing at 77 K, we measured Young’s modulus and Poisson’s ratio for each composition. Our results show that pure alumina braid insulation and co-wind reinforcements significantly enhance stiffness compared to aluminosilicate braids, with more than 2.5 times increased winding pack Young’s modulus. Rule of mixtures analysis further quantified the contribution of non-wire composite components to overall stiffness. These findings highlight the critical role of insulation material selection and reinforcement design in optimizing Bi-2212 coil performance under stress, providing a foundation for improved mechanical models and more reliable high-field HTS magnet designs.

Bi-2212 magnet↗

Direct ink write multi-material printing of PDMS-BTO composites with MWCNT electrodes for flexible force sensors

Here, with recent advances of additive manufacturing technology, direct ink write (DIW) printing has allowed to incorporate multi-material printing of various materials with freedom of design and complex geometric shapes to complete functional sensors in a one-step fabrication. This paper introduces the use of DIW 3D printing of polydimethylsiloxane (PDMS) with barium titanate (BTO) filler as stretchable composites with tunable piezoelectric properties that can be used for force sensors applications. To improve the bonding between stretchable piezoelectric composites and electrodes, multi-walled carbon nanotubes was included in the fabrication of electrodes at a fixed ratio of 11 wt. %. The alignment of the BTO dipoles was achieved through corona poling method, which applies an electric charge on the surface layer of the functional material, aligning the dipoles in the desired direction and thus gaining the piezoelectricity. Different BTO mixing ratios (10–50 wt. %) were evaluated in order to obtain tunable piezoelectric properties and compare the sensitivity with respect their elastic properties. Tensile testing and piezoelectric testing were carried out to characterize mechanical and piezoelectric properties. Results showed that fabricated PDMS with 50 wt. % BTO gave the highest piezoelectric coefficient (d 33 ) of 11.5 pC N -1 and with an output voltage of 385 mV under compression loading of >200 lbF. This demonstrates feasibility of using multi-material DIW printing to fabricate piezoelectric force sensors with integrated electrodes in one-step without compromising the flexibility of the material.

36 MATERIALS SCIENCE↗

Reversible Movement of Homogenously Nucleated Dislocations in a {beta}-Titanium Alloy

We demonstrate reversible movement of (1/2)[110](110) dislocation loops generated from nanodisturbances in a {beta}-titanium alloy. High resolution transmission electron microscope observations during an in situ tensile test found three reversible deformation mechanisms, nanodisturbances, dislocation loops and martensitic transformation, that are triggered in turn with increasing applied stress. All three mechanisms contribute to the nonlinear elasticity of the alloy. The experiments also revealed the evolution of the dislocation loops to disclination dipoles that cause severe local lattice rotations.

36 MATERIALS SCIENCE↗

Dispersed SiC nanoparticles in Ni observed by ultra-small-angle X-ray scattering

In this paper, a metal-ceramic composite, nickel reinforced with SiC nanoparticles, was synthesized and characterized for its potential application in next-generation molten salt nuclear reactors. Synchrotron ultra-small-angle X-ray scattering (USAXS) measurements were conducted on the composite. The size distribution and number density of the SiC nanoparticles in the material were obtained through data modelling. Scanning and transmission electron microscopy characterization were performed to substantiate the results of the USAXS measurements. Tensile tests were performed on the samples to measure the change in their yield strength after doping with the nanoparticles. Finally, the average interparticle distance was calculated from the USAXS results and is related to the increased yield strength of the composite.

36 MATERIALS SCIENCE↗

FTIR Investigation of EVA Chemical Bonding Environment and Its Impact on Debond Energy

The chemical makeup of ethylene vinyl acetate (EVA) interfaces in photovoltaic (PV) modules is probed via Fourier-transform infrared spectroscopy (FTIR) to determine the impact of the EVA formulation on the adhesion degradation. EVA samples laminated with glass particles are used to demonstrate the effect of damp heat exposure on the glass-EVA interface, showing that increasing silane content increases chemical stability. Delamination interfaces created in one cell modules demonstrate a high correlation between the siloxane bonding at the silicon cell-EVA interface and the debond energy. A significant decrease in debond energy after UV exposure is also shown to be due in part to decreasing siloxane bond density at the interface. However, FTIR results indicated contributions to the adhesion beyond the chemical interface, and a basic tensile test indicates increasing bulk mechanical properties with increasing silane. These results demonstrate the importance of the EVA formulation on its adhesion performance and long-term reliability. Furthermore, it is shown that FTIR is a capable technique for assessing and quantifying chemical mechanisms within PV modules. These results can then be used to more effectively model module lifetimes and to better design polymer systems for PV modules.

14 SOLAR ENERGY↗

Survey of Mechanical Durability of PV Backsheets

The ability to maintain mechanical properties after applied environmental stress is a good indicator for long term durability of a backsheet. This work surveys a set of 56 backsheet films, some of which are known to fail in the field and evaluates them utilizing the proposed photovoltaic weathering standard IEC 62788-7-2. While the complete study examined optical reflectance characterization, tensile testing, dielectric testing, and a mandrel bend test, this paper focuses on the mandrel bend test results. All seven of the transparent specimens failed. A polyamide based backsheet known to fail in the field did not fail the bend test. It is believed that the field failure is due to an interaction with the encapsulant and/or the cyclic mechanical exposure experienced in the field. When cracks occur, they happen predominantly in the polyethylene terephthalate for transparent backshees or the 'E' layer for opaque films, never in a fluoropolymer layer.

14 SOLAR ENERGY↗

Oxidation and microstructure of SiC f /SiC composites in moist air up to 1600°C by X‐ray tomographic characterization

Abstract SiC f /SiC composites that possess PyC or BN interface layers were fabricated and then oxidized in moist air at 1000, 1200, 1400, and 1600°C. High‐resolution CT was used for capturing 3D images and quantifying the SiC phase, mesophase, and voids. The oxidation behavior and microstructural evolution of SiC f /SiC with PyC or BN interface are discussed in this study. The microstructure of the SiC f /SiC with a PyC layer was seriously damaged in moist air at high temperature, whereas the BN interface layer enhanced the oxidation resistance of the SiC f /SiC. These results are also confirmed by using XRD, oxidation mass gain, tensile testing, and SEM measurements. The results of the oxidation behavior and microstructural evolution for SiC f /SiC oxidized in dry air are also compared with the results of this study. Comparing the SiC f /SiC with a PyC interface layer, the composite with a BN interface layer oxidized in moist air exhibits a high void growth rate and a low SiO 2 grain growth rate from 1000 to 1600°C. This work will provide guidance for predicting the service life of SiC f /SiC for multiscale damage rate models of materials at a local scale and will also provide guidance on the life service design of SiC f /SiC materials.

Lu, Zilong↗

Combined thermographic phosphor and digital image correlation (TP + DIC) for simultaneous temperature and strain measurements

We report thermographic phosphors (TP) are combined with stereo digital image correlation (DIC) in a novel diagnostic, TP + DIC, to measure full-field surface strains and temperatures simultaneously. The TP + DIC method is presented, including corrections for nonlinear CMOS camera detectors and generation of pixel-wise calibration curves to relate the known temperature to the ratio of pixel intensities between two distinct wavelength bands. Additionally, DIC is employed not only for strain measurements but also for accurate image registration between the two cameras for the two-colour ratio method approach of phosphoric thermography. TP + DIC is applied to characterize the thermo-mechanical response of 304L stainless steel dog bones during tensile testing at different strain rates. The dog bones are patterned for DIC with Mg 3 F 2 GeO 4 :Mn (MFG) via aerosol deposition through a shadow mask. Temperatures up to 425°K (150°C) and strains up to 1.0 mm/mm are measured in the localized necking region, with conservative noise levels of 10°K and 0.01 mm/mm or less. Finally, TP + DIC is compared to the more established method of combining infrared (IR) thermography with DIC (IR + DIC), with results agreeing favourably. Three topics of continued research are identified, including cracking of the aerosol-deposited phosphor DIC features, incomplete illumination for pixels on the border of the phosphor features, and phosphor emission evolution as a function of applied substrate strain. This work demonstrates the combination of phosphor thermography and DIC and lays the foundation for further development of TP + DIC for testing in combined thermo-mechancial environments.

304L stainless steel↗

Crystal plasticity analysis of stress partitioning mechanisms and their microstructural dependence in advanced steels

Two-phase advanced steels contain an optimized combination of high yield strength and large elongation strain at failure, as a result of stress partitioning between a hard phase (martensite) and a ductile phase (ferrite or austenite). Provided with strong interfaces between the constituent phases, the failure in the brittle martensite phase will be delayed by the surrounding geometric constraints, while the rule of mixture will dictate a large strength of the composite. To this end, the microstructural design of these composites is imperative especially in terms of the stress partitioning mechanisms among the constituent phases. Based on the characteristic microstructures of dual phase and multilayered steels, two polycrystalline aggregate models are constructed to simulate the microscopic lattice strain evolution of these materials during uniaxial tensile tests. By comparing the lattice strain evolution from crystal plasticity finite element simulations with advanced in situ diffraction measurements in literature, this study investigates the correlations between the material microstructure and the micromechanical interactions on the intergranular and interphase levels. Finally, it is found that although the applied stress will be ultimately accommodated by the hard phase and hard grain families, the sequence of the stress partitioning on grain and phase levels can be altered by microstructural designs. Implications of these findings on delaying localized failure are also discussed.

36 MATERIALS SCIENCE↗

Additive Manufacturing of Porous Ceramics With Foaming Agent

The macro-porous ceramics has promising durability and thermal insulation performance. As porous ceramics find more and more applications across many industries, a cost-effective and scalable additive manufacturing technique for fabricating macro-porous ceramics is highly desirable. Herein, we reported a facile additive manufacturing approach to fabricate porous ceramics and control the printed porosity. Several printable ceramic inks were prepared, and the foaming agent was added to generate gaseous bubbles in the ink, followed by the direct ink writing and the ambient-pressure and room-temperature drying to create the three-dimensional geometries. In this work, a set of experimental studies were performed to optimize the printing quality. The results revealed the optimal process parameters for printing the foamed ceramic ink with a high spatial resolution and fine surface quality. Varying the concentration of the foaming agent enables the controllability of the structural porosity. The maximum porosity can reach 85%, with a crack-free internal porous structure. The tensile tests showed that the printed macro-porous ceramics possessed enhanced durability with the addition of fiber. With a high-fidelity three-dimensional (3D) printing process and the precise controllability of the porosity, we showed that the printed samples exhibited a remarkably low thermal conductivity and durable mechanical strength.

36 MATERIALS SCIENCE↗

Experimental Characterization of Hygrothermal Aging: Competition Between Thermo-Oxidation and Hydrolysis Phenomena

Abstract In this work, we have presented a comparison between effects of accelerated thermo-oxidative, hydrolytic and hygrothermal aging on the mechanical and chemical properties of a polyurethane based (PUB) adhesive. The adhesive is a flexible adhesive which is extensively used in automobile industry as a glass sealant. During service life it gets exposed to the hygrothermal environment and the integrity of matrix interface is most vulnerable. This study focuses on weighing and comparing effects of different aging environments on material behavior; and it shows that hygrothermal aging environment results as a competition between two sub-aging phenomena i.e., thermo-oxidation and hydrolytic aging. Samples were exposed to 0%RH, 80%RH and submerged condition in distilled water. Uni-axial tensile tests, and cross-link density analysis by swelling test were carried out on as-received and aged samples. The aging process was conducted at three different temperatures (60°C, 80°C and 95°C) and for four different exposure durations of 1, 10, 30, and 90 days. This work confirms that the effect of hygrothermal aging is a result of competition between thermo-oxidation and hydrolytic aging environments. The total mechanical and environmental damage incurred by specimens is a collaborative effect of all exposure environments involved i.e., aging time, temperature, oxygen, water and humidity. The results are in agreement with the chemical test outcomes as well.

Shaafaey, Mamoon↗

Effect of Dual Environment Aging on Flexible Polyurethane Based Adhesive

Abstract Environmental degradation of adhesives naturally increases with the intensity of the ambient weathering agents involved. During service life, these materials are never subjected to a constant environmental loading. Real-time applications expose the material to multiple weather conditions, ranging from dry to humid or fully wet conditions. While some understanding exists about aging environments in isolation, we intend to investigate the effect of multiple environments on the constitutive behavior of the materials in question. The extent of damage can be accessed by analyzing the changes in constitutive behavior and toughness of aged material. Therefore, this aging experiment was designed around two-way aging regimes involving combinations of thermo-oxidation, hydrolytic and hygrothermal aging environments. We selected a polyurethane based flexible adhesive which is commonly used in the automotive industry as a glass sealant. The aged specimens were subjected to uniaxial tensile tests, and variation in material toughness and constitutive behavior was analyzed to ascertain the mechanics involved in the case of each environmental exposure. We outlined how different environments affect the material in isolation and how they interact with other weathering conditions. This study will help better understand and model the damage mechanics involved in exposure to multiple environmental conditions.

Shaafaey, Mamoon↗

Independence of Environmental and Mechanical Damages on Silicone Adhesive Stored in a Thermo-Oxidative Environment

Abstract Elastomeric polymer materials hold a special place in today’s industrial sectors with respect to structural application needs. Low quality materials are detrimental to industries like aerospace, and automotive engineering. Assessment of the durability of elastomers for structural applications has been of much interest among the literary circles for decades and new materials keep outperforming the existing ones. Polymeric adhesives are one of the most abundantly used materials in these industries. All polymeric materials get damaged when in contact with aggressive environments in presence of high temperature and oxygen. Commonly referred to as thermo-oxidation, this environment exposes the material to heat and oxidation reactions in presence of oxygen. Resultantly, during service life, the damage to the polymer matrix is primarily caused by two factors: mechanical damage and environmental aging. Environmental aging is an irreversible phenomenon caused by changes in the molecular structure while mechanical damage maintains the shape of the polymer matrix, and the deterioration is mostly due to polymer chain mobility. Environmental aging can be caused by a single environmental agent or by a synergized impact of several environmental elements. Increasing temperature is found to be proportional to decreasing tensile strength and toughness of material. The rate and extent of degradation can be accessed by scrutinizing the changes in constitutive behavior of material through mechanical and chemical properties. Accelerated thermal aging is among the most common modes of process related degradation, leading generally to chain scission, and crosslinking phenomena and reduced resistance to fracture stress, and strain. In this experimental study, our goal is to separate the environmental degradation from mechanical damage. A silicone-based adhesive was aged in thermo-oxidative at (0%RH) aging environment. The damage and decay mechanisms have been used to draw a distinction between environmental degradation and mechanical damage. Material characterization included uniaxial tensile test (failure and cyclic) and scanning electron microscopy (SEM) tests on as-received and aged samples. Aging was conducted at three different temperatures (60°C, 80°C and 95°C) and six different exposure durations (1, 3, 10, 30, 90 and 200 days). This work confirms that environmental damage is superposed on top of the mechanical damage, and thus, they are separable. The total mechanical and environmental damage is a synergized effect of all exposure conditions and parameters involved i.e., aging time, temperature, and oxygen. The chemistry and mechanics of the polymer degradation were found to be in good agreement with each other.

Alazhary, Sharif↗

Coupled diffusion-deformation-damage model for polymers used in hydrogen infrastructure

The soft materials used in the infrastructure of hydrogen storage and distribution systems are vulnerable because exposure to high-pressure hydrogen can lead to mechanical damage and property degradation. Some materials, such as polymers, can undergo mechanical failure due to a phenomenon wherein hydrogen gas diffuses through the polymer chains and occupies preexisting cavities or voids inside the polymer material. If the hydrogen gas pressure is reduced more quickly than hydrogen can diffuse back out of the polymer which is necessary for some applications, the trapped hydrogen gas instead escapes by rupturing the material, causing surface blistering or permanent damage. In this study, a continuum mechanics-based fully coupled diffusion-deformation model with damage is developed to predict the stress distribution and damage propagation while the polymer undergoes rapid decompression failure. The hyperelastic material model, along with the maximum principal strain failure theory, was chosen for this study as it represents the nonlinear material response with brittle failure observed in uniaxial tensile tests perfectly. EPDM polymer was chosen for this study because of its commercial availability and common use in hydrogen storage and distribution system. It has superior mechanical properties, high and low temperature resistance, and certain compounds work well in hydrogen gas. This work is useful for design engineers to alter the parameters while manufacturing polymer composites to increase their performance in a high-pressure hydrogen environment.

Kulkarni, Shank S.↗