Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SAPPHIRE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,387 records · Page 77

Superconductivity in Nb-Sn Thin Films of Stoichiometric and Off-Stoichiometric Compositions

Binary Nb-Sn thin film samples were fabricated and characterized in terms of their composition, morphology, and superconducting properties. Nb-Sn was magnetron-sputtered onto heated R-plane sapphire substrates at 700 °C, 800 °C, and 900 °C, using a custom-built heater assembly. Samples were cut into strips, where each strip has a unique composition. For a subset of the samples, Nb-Sn was selectively etched away at an etching rate of 6 ± 1 nm/s using an aqueous solution of 3 vol. % hydrofluoric and 19 vol. % nitric acid. The sample composition was investigated with a scanning electron microscope with an X-ray energy dispersive spectroscopy detector. Surface and cross-section morphologies were investigated using scanning electron microscopy and scanning transmission electron microscopy, revealing a dense columnar poly-crystalline grain structure. X-ray diffraction measurements indicate a highly textured film that is (100) oriented out-of-plane and random in-plane. The critical temperature Tc (ranging from 9.8 to 17.9 K), critical magnetic field μ-0 H c2 (ranging from 12.5 to 31.3 T), residual resistivity ratio (RRR), and normal state resistivity ρ 0 were measured and found to be broadly consistent with literature data on bulk Nb- 3 Sn.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

First Results of the SRF Wafer Test Cavity for the Characterization of Superconductors

The wafer test cavity was designed as a short sample test system that could create a reproducible environment for the testing of superconducting materials above the Bardeen-Cooper- Schrieffer limit of niobium. The results of the sapphire test cavity showed that the dielectric was too lossy, and thus, the original design had to be altered to make operation feasible with current hardware and achieve ~200 mT. The new design was fabricated at Thomas Jefferson National Accelerator Facility and was cryogenically tested. After four tests, the cavity was able to produce a 6.6-mT field with a Q of 3.96 * 108. Although lower than anticipated, in comparison to other TE01 cavities, this result is quite encouraging. Multipacting and coupling were limitations, but current work is pursuing the elimination of these complications. This document will expound upon the new design, mathematical simulations, testing of the cavity, complications, results, and future work.

Pogue, Nathaniel J.↗

Temperature and Microstructural Effects on the Superconducting Properties of Niobium Thin Films

Here, superconducting thin films have a wide range of dc and RF applications, from detectors to superconducting radio frequency. Amongst the most used materials, niobium (Nb) has the highest critical temperature (TC) and highest lower critical field (HC1) of the elemental superconductors and can be deposited on a variety of substrates, making Nb thin films very appealing for such applications. Here, we present temperature-dependent dc studies on the critical temperature and critical fields of Nb thin films grown on copper and r-plane sapphire surfaces. Additionally, we correlate the dc superconducting properties of these films with their microstructure, which allows for the possibility of tailoring future films for a specific application.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Electroluminescence and Transmission Electron Microscopy Characterization of Reverse-Biased AlGaN/GaN Devices

Reverse-bias stress testing has been applied to a large set of more than 50 AlGaN/GaN high electron mobility transistors, which were fabricated using the same process but with different values of the AlN mole fraction and the AlGaN barrier-layer thickness, as well as different substrates (SiC and sapphire). Two sets of devices having different defect types and densities, related to the different growth conditions and the choice of nucleation layer, were also compared. When subjected to gate drain (or gate-to-drain and source short-circuited) reverse-bias testing, all devices presented the same time-dependent failure mode, consisting of a significant increase in the gate leakage current. This failure mechanism occurred abruptly during step-stress experiments when a certain negative gate voltage, or critical voltage, was exceeded or, during constant voltage tests, at a certain time, defined as time to breakdown. Electroluminescence (EL) microscopy was systematically used to identify localized damaged areas that induced an increase of gate reverse current. This current increase was correlated with the increase of EL intensity, and significant EL emission during tests occurred only when the critical voltage was exceeded. Focused-ion-beam milling produced cross-sectional samples suitable for electron microscopy observation at the sites of failure points previously identified by EL microscopy. In highdefectivity devices, V-defects were identified that were associated with initially high gate leakage current and corresponding to EL spots already present in untreated devices. Conversely, identification of defects induced by reverse-bias testing proved to be extremely difficult, and only nanometer-size cracks or defect chains, extending vertically from the gate edges through the AlGaN/GaN heterojunction, were found. No signs of metal/semiconductor interdiffusion or extended defective areas were visible.

Cullen, David A↗

Hf-Doped Ni-Al2O3 Interfaces at Equilibrium

In this study, a series of dewetting experiments of pure and Hf-doped Ni films on sapphire and HfO2 substrates were conducted in order to measure the change in interface energy of the Ni-Al2O3 interface in the presence of Hf, and to study Hf interfacial segregation. It was found that Hf oxidizes under the conditions of the experiment (P(O2)=10-20atm.), and that the presence of HfO2 at the Ni-Al2O3 interface increases the interface energy from 2.16 0.2 to 2.7 0.4 [J/m2]. This result contradicts several theoretical studies that predict that Hf segregates to the interface to stabilize it thermodynamically. The solubility of Hf in bulk Ni was found to be significantly lower than the value reported in the equilibrium phase diagram.

Meltzman, Hila↗

Influence of partial charge on the material removal rate during chemical polishing

A partial charge-based chemical polishing model has been developed, which can serve as metric for describing the relative polishing material removal rate for different combinations of slurries and workpieces. A series of controlled polishing experiments utilizing a variety of colloidal polishing slurries (SiO 2 , CeO 2 , ZrO 2 , MgO, Sb 2 O 5 ) and optical materials [single crystals of Al 2 O 3 (sapphire), SiC, Y 3 Al 5 O 12 (YAG), CaF 2 , and LiB 3 O 5 (LBO); a SiO 2 -Al 2 O 3 -P 2 O 5 -Li 2 O glass ceramic (Zerodur); and glasses of SiO 2 :TiO 2 (ULE), SiO 2 (fused silica), and P 2 O 5 -Al 2 O 3 -K 2 O-BaO (Phosphate)] was performed and its material removal rate was measured. As previously proposed by Cook (J Non-Cryst Solids. 1990;120:152), for many polishing systems, the removal rate is governed by a series of chemical reactions which include the formation of a surface hydroxide, followed by condensation of that hydroxyl moiety with the polishing particle, and a subsequent hydrolysis reaction. The rate of condensation can often be the rate limiting step, thus it can determine the polishing material removal rate. By largely keeping the numerous other factors that influence material removal rate fixed (such as due to particle size distributions, interface interactions, pad topography, kinematics, and applied pressure), the material removal rate is shown to scale exponentially with the partial charge difference (δ wp-s ) between the workpiece and polishing slurry particle for many of the slurry-workpiece combinations indicating that condensation rate is the rate limiting step. The partial charge (δ) describes the equilibrium distribution of electron density between chemically bonded atoms and is related to the electronegativity of the atoms chemically bonded to one another. This partial charge model also explains the age-old experimental finding of why cerium oxide is the most effective polishing slurry for chemical removal of many workpieces. Finally, some of the slurry-workpiece combinations that did not follow the partial charge dependence offer insight to other removal mechanisms or rate limiting reaction pathways.

36 MATERIALS SCIENCE↗

Nanoplastic removal function and the mechanical nature of colloidal silica slurry polishing

The nanomechanical deformations on a broad range of optical material surfaces (single crystals of Al 2 O 3 [sapphire], SiC, Y 3 Al 5 O 12 [YAG], CaF 2 , and LiB 3 O 5 [LBO]; a SiO 2 –Al 2 O 3 –P 2 O 5 –Li 2 O glass-ceramics [Zerodur]; and glasses of SiO 2 :TiO 2 [ULE], SiO 2 [fused silica], and P 2 O 5 –Al 2 O 3 –K 2 O–BaO [Phosphate]) near the elastic-plastic load boundary have been measured by nanoindentation and nanoscratching to mimic the nanoplastic removal caused by a single slurry particle during polishing. Nanoindenation in air was performed to determine the workpiece hardness at various loads using a commercial nanoindenter with a Berkovich tip. Similarly, an atomic force microscope (AFM) with a stiff diamond coated tip (150 nm radius) was used to produce nanoplastic scratches in air and aqueous environments over a range of applied loads (~20-170 μN). The resulting nanoplastic deformation of the nanoscratches were used to calculate the removal function (i.e., depth per pass) which ranged from 0.18 to 3.6 nm per pass for these materials. A linear correlation between the nanoplastic removal function and the polishing rate (using a fixed polishing process with colloidal silica slurry on a polyurethane pad) of these materials was observed implying that: (a) the polishing mechanism using colloidal silica slurry can be dominated by mechanical rather than chemical interactions; and (b) the nanoplastic removal function, as opposed to interface particle interactions, is the controlling factor for the polishing material removal rate. Furthermore, this correlation is consistent with the Ensemble Hertzian Multi-Gap (EHMG) microscopic material removal rate model described previously. The nanoplastic removal depth was also found to correlate to the measured nanoindentation hardness (H1) of the optical material, scaling as H 1 -3.5 . Two-dimensional (2D) finite element analysis simulations of nanoindentation showed a similar nonlinear dependence of plastic deformation with the workpiece material hardness. The findings of this study are used to determine an effective Preston coefficient for the material removal rate expression and enhance the predictive nature of the nanoplastic polishing rate for various materials utilizing their material properties.

36 MATERIALS SCIENCE↗

Lateral cracks during sliding indentation on various optical materials

A series of static and sliding indentation (ie, scratching) was performed and characterized on a wide range of optical workpiece materials [single crystals of Al 2 O 3 (sapphire), SiC, Y 3 Al 5 O 12 (YAG), CaF 2 , and LiB 3 O 5 (LBO); a SiO 2 –Al 2 O 3 –P 2 O 5 –Li 2 O glass ceramic (Zerodur); and glasses of SiO 2 :TiO 2 (ULE), SiO 2 (fused silica), and P 2 O 5 –Al 2 O 3 –K 2 O–BaO (Phosphate)] at various applied loads using various indenters (Vickers, 10 µm conical, and 200 µm conical). Despite having different load dependencies, the lateral crack depth formed during sliding indentation quantitatively scales with that formed during static indentation, explaining why static indentation has been historically effective in describing various grinding parameters. Depending on the indenter geometry, the amount of residual trench damage (plastic deformation and local fracturing) during sliding indentation was often enhanced by more than an order of magnitude compared with static indentation. A simple ploughing scratch model, which considers both tangential and normal stresses (where the tangential stress is amplified by relatively small tangential contact area), explains this enhancement and other observed trends. Accounting for the high correlation between residual trench depth and volumetric fracturing, the model is extended to estimate the amount of fracture damage as a function of the material properties of the workpiece, indenter geometry, and applied load. Such a model has utility in the design of optimized grinding processes, particularly the abrasive geometry. Finally, at higher loads (>1 N), lateral cracks were often observed to preferentially propagate in the forward scratching direction, as opposed to perpendicular to the scratch as typically observed. High-speed imaging of the scratch process confirms that these cracks propagate ahead of the sliding indenter during the scratching event. Finite element stress analysis suggests the ploughing frictional forces increase the mode I tensile stresses at the leading edge of the sliding indenter explaining the direction of crack propagation of such cracks.

36 MATERIALS SCIENCE↗

Optical characteristics of nanocrystalline Al{sub x}Ga{sub 1−x}N thin films deposited by hollow cathode plasma-assisted atomic layer deposition

Gallium nitride (GaN), aluminum nitride (AlN), and Al{sub x}Ga{sub 1−x}N films have been deposited by hollow cathode plasma-assisted atomic layer deposition at 200 °C on c-plane sapphire and Si substrates. The dependence of film structure, absorption edge, and refractive index on postdeposition annealing were examined by x-ray diffraction, spectrophotometry, and spectroscopic ellipsometry measurements, respectively. Well-adhered, uniform, and polycrystalline wurtzite (hexagonal) GaN, AlN, and Al{sub x}Ga{sub 1−x}N films were prepared at low deposition temperature. As revealed by the x-ray diffraction analyses, crystallite sizes of the films were between 11.7 and 25.2 nm. The crystallite size of as-deposited GaN film increased from 11.7 to 12.1 and 14.4 nm when the annealing duration increased from 30 min to 2 h (800 °C). For all films, the average optical transmission was ∼85% in the visible (VIS) and near infrared spectrum. The refractive indices of AlN and Al{sub x}Ga{sub 1−x}N were lower compared to GaN thin films. The refractive index of as-deposited films decreased from 2.33 to 2.02 (λ = 550 nm) with the increased Al content x (0 ≤ x ≤ 1), while the extinction coefficients (k) were approximately zero in the VIS spectrum (>400 nm). Postdeposition annealing at 900 °C for 2 h considerably lowered the refractive index value of GaN films (2.33–1.92), indicating a significant phase change. The optical bandgap of as-deposited GaN film was found to be 3.95 eV, and it decreased to 3.90 eV for films annealed at 800 °C for 30 min and 2 h. On the other hand, this value increased to 4.1 eV for GaN films annealed at 900 °C for 2 h. This might be caused by Ga{sub 2}O{sub 3} formation and following phase change. The optical bandgap value of as-deposited Al{sub x}Ga{sub 1−x}N films decreased from 5.75 to 5.25 eV when the x values decreased from 1 to 0.68. Furthermore, postdeposition annealing did not affect the bandgap of Al-rich films.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Study of the effects of GaN buffer layer quality on the dc characteristics of AlGaN/GaN high electron mobility transistors

Here we studied the effect of buffer layer quality on dc characteristics of AlGaN/GaN high electron mobility (HEMTs). AlGaN/GaN HEMT structures with 2 and 5 μm GaN buffer layers on sapphire substrates from two different vendors with the same Al concentration of AlGaN were used. The defect densities of HEMT structures with 2 and 5 μm GaN buffer layer were 7 × 10 9 and 5 × 10 8 cm ₋2 , respectively, as measured by transmission electron microscopy. There was little difference in drain saturation current or in transfer characteristics in HEMTs on these two types of buffer. However, there was no dispersion observed on the nonpassivated HEMTs with 5 μm GaN buffer layer for gate-lag pulsed measurement at 100 kHz, which was in sharp contrast to the 71% drain current reduction for the HEMT with 2 μm GaN buffer layer.

36 MATERIALS SCIENCE↗

Growth of ultrathin Bi 2 Se 3 films by molecular beam epitaxy

Bi 2 Se 3 is a widely studied 3D topological insulator having potential applications in optics, electronics, and spintronics. When the thickness of these films decreases to less than approximately 6 nm, the top and bottom surface states couple, resulting in the opening of a small gap at the Dirac point. In the 2D limit, Bi 2 Se 3 may exhibit quantum spin Hall states. However, growing coalesced ultrathin Bi 2 Se 3 films with a controllable thickness and typical triangular domain morphology in the few nanometer range is challenging. Here, we explore the growth of Bi 2 Se 3 films having thicknesses down to 4 nm on sapphire substrates using molecular beam epitaxy that were then characterized with Hall measurements, atomic force microscopy, and Raman imaging. We find that substrate pretreatment—growing and decomposing a few layers of Bi 2 Se 3 before the actual deposition—is critical to obtaining a completely coalesced film. In addition, higher growth rates and lower substrate temperatures led to improvement in surface roughness, in contrast to what is observed for conventional epitaxy. Altogether, coalesced ultrathin Bi 2 Se 3 films with lower surface roughness enable thickness-dependent studies across the transition from a 3D-topological insulator to one with gapped surface states in the 2D regime.

36 MATERIALS SCIENCE↗

Effect of varying threading dislocation densities on the optical properties of InGaN/GaN quantum wells with intentionally created V-shaped pits

The effect of varying threading dislocation densities on the internal quantum efficiencies (IQEs) of InGaN quantum wells (QWs), with and without intentionally created “V-pits,” is reported here. InGaN QW samples grown on GaN-on-sapphire templates with threading dislocation densities of <1 × 108 and <1 × 109 cm−2 are compared, with and without GaN/InGaN superlattice (SL) layers incorporated to intentionally open up the threading dislocation cores and form large-size “V-pits.” The formation of “V-pits” is confirmed by cross-sectional transmission electron microscopy to initiate from threading dislocations in the SL layers. The densities of the pits are confirmed by plan-view SEM to agree with the substrate threading dislocation densities. The experimental room temperature IQEs of the “V-pit” QW samples are enhanced to 15% ± 1% compared to 6% ± 2% for conventional QW samples. Both conventional and “V-pit” samples show insensitivity to the magnitude of the dislocation densities with respect to IQE performance, while the “V-pit” samples show shifts in the peak emission wavelengths compared to the conventional samples, attributed to strain modulation. This study provides additional understanding of the causes of the observed insensitivity of the IQEs to different threading dislocation densities.

Engineering↗

Toward the origins of binding energy shifts and “satellites” formation during plasma-XPS measurements

In-plasma x-ray photoelectron spectroscopy (plasma-XPS) emerges as a powerful platform for real-time, in situ chemical analysis under conditions relevant to semiconductor processing and other plasma-enabled technologies. This study investigates the origins of binding energy (BE) shifts and the formation of “satellite” peaks observed during plasma-XPS measurements across conductive, dielectric, and gas-phase systems. Using a standard laboratory-based ambient pressure XPS apparatus coupled with an alternating current (AC)-driven capacitively coupled plasma source, we demonstrate that metastable surface species, such as transient Au oxides, can be detected during plasma exposure, revealing chemical states that are hardly accessible using conventional ultrahigh vacuum (UHV) XPS. In dielectric samples (e.g., undoped diamond, sapphire), we observe pressure- and plasma-type-dependent BE shifts of more than 50 eV, attributed to x-ray-induced and plasma-mediated surface charging. These shifts are mitigated at higher pressures/plasmas or in electronegative plasmas (e.g., O 2 ), the latter due to enhanced charge compensation mechanisms involving slow negative ions. For gas-phase species, AC-plasma excitation leads to spectral broadening and the emergence of “satellite” peaks with energy separations of a few electron volts, linked to oscillating local plasma potentials in the probing volume. Furthermore, these findings highlight the complex and important interplay between plasma parameters, surface charging, and local electric fields in shaping XPS spectra. Overall, plasma-XPS emerges as a critical metrological tool for probing transient surface chemistry, with implications for semiconductor processing, material synthesis, and plasma diagnostics.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Subsurface mechanical damage correlations after grinding of various optical materials

Loose abrasive grinding was performed on a wide range of optical workpiece materials [single crystals of Al 2 O 3 (sapphire), SiC, Y 3 Al 5 O 12 (YAG), CaF 2 , and LiB 3 O 5 (LBO); a SiO 2 -Al 2 O 3 -P 2 O 5 -Li 2 O glass-ceramic (Zerodur); and glasses of SiO 2 : TiO 2 (ULE), SiO 2 (fused silica), and P 2 O 5 -Al 2 O 3 -K 2 O-BaO (phosphate)]. Using the magneto rheological finishing (MRF) taper wedge technique (where a wedge was polished on each of the ground workpieces and the resulting samples were appropriately chemically etched), the subsurface mechanical damage (SSD) characteristics were measured. The SSD depth for most of the workpiece materials was found to scale as E1 1/2 / H 1 , where E 1 is the elastic modulus and H 1 is the hardness of the workpiece. This material scaling is the same as that for the growth of lateral cracks, suggesting that lateral cracks are a dominant source for SSD rather than radial/median cracks, as previously proposed. Utilizing the SSD depth data from both this study and others, semiempirical relationships have been formulated, which allows for estimating the SSD depth as a function of workpiece material and important grinding parameters (such as abrasive size and applied pressure).

36 MATERIALS SCIENCE↗

Semiconductor neutron detectors using depleted uranium oxide

This paper reports on recent attempts to develop and test a new type of solid-state neutron detector fabricated from uranium compounds. It has been known for many years that uranium oxide (UO2), triuranium octoxide (U3O8) and other uranium compounds exhibit semiconducting characteristics with a broad range of electrical properties. We seek to exploit these characteristics to make a direct-conversion semiconductor neutron detector. In such a device a neutron interacts with a uranium nucleus, inducing ssion. The ssion products deposit energy-producing, detectable electron-hole pairs. The high energy released in the ssion reaction indicates that noise discrimination in such a device has the potential to be excellent. Schottky devices were fabricated using a chemical deposition coating technique to deposit UO2 layers a few microns thick on a sapphire substrate. Schottky devices have also been made using a single crystal from UO2 samples approximately 500 microns thick. Neutron sensitivity simulations have been performed using GEANT4. Neutron sensitivity for the Schottky devices was tested experimentally using a 252Cf source.

neutron detection, uranium oxide, semiconductor↗

Temperature and Excitation Dependence of Recombination in CIGS Thin Films with High Spatial Resolution

Alkali post-deposition treatments significantly improve the performance of CuInGaSe2 (CIGS) devices, but there is still room for improvement. Here, we investigate the effects of potassium fluoride alkali post-deposition treatment on the defect chemistry and recombination at grain boundaries and grain interiors using temperature- and injection-dependent cathodoluminescence (CL) spectrum imaging. We study CIGS thin films grown on alkali-free sapphire substrates to isolate the effects of alkali treatment from alkali metals that can diffuse from standard soda-lime glass substrates. We find that alkali treatment affects the energy and temperature dependence of the luminescence peaks, as well as the defect activation energies. CL spectrum images reveal that the luminescence transitions at grain boundaries have a distinct power dependence after alkali treatment and substantially different defect chemistry. This work shows that temperatureand injection-dependence CL spectrum images can provide unique insight into the defect chemistry and recombination behavior of CIGS thin films.

14 SOLAR ENERGY↗

Performance of a 512 x 512 Gated CMOS Imager with a 250 ps Exposure Time

We describe the performance of a 512x512 gated CMOS read out integrated circuit (ROIC) with a 250 ps exposure time. A low-skew, H-tree trigger distribution system is used to locally generate individual pixel gates in each 8x8 neighborhood of the ROIC. The temporal width of the gate is voltage controlled and user selectable via a precision potentiometer. The gating implementation was first validated in optical tests of a 64x64 pixel prototype ROIC developed as a proof-of-concept during the early phases of the development program. The layout of the H-Tree addresses each quadrant of the ROIC independently and admits operation of the ROIC in two modes. If “common mode” triggering is used, the camera provides a single 512x512 image. If independent triggers are used, the camera can provide up to four 256x256 images with a frame separation set by the trigger intervals. The ROIC design includes small (sub-pixel) optical photodiode structures to allow test and characterization of the ROIC using optical sources prior to bump bonding. Reported test results were obtained using short pulse, second harmonic Ti:Sapphire laser systems operating at λ~ 400 nm at sub-ps pulse widths.

47 OTHER INSTRUMENTATION↗