Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “alloy solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,369 records · Page 76

Characterizing the Use of Ultrasonic Energy in Promoting Uniform Composite Growth in Immiscible Alloys

The results of experimental investigation and mathematical modeling for immiscible alloys subjected to ultrasonic influence are presented. It is known that in inoculated light alloy melts, ultrasonic treatment creates a new type of cast structure with extremely fine grains of uniform composition. This effect is produced across a wide range of freezing rates and technologies. However, it has not been demonstrated that the process can be successfully applied during controlled directional solidification processing. In this work we present the results from a set of directional solidification experiments and suggest describing the droplet size versus ultrasonic frequency and amplitude using an energy approach, followed with a more detailed analysis through numerical modeling of the ultrasonic field.

Grugel, Richard N.↗

Preliminary Investigations of Joining Technologies for Attaching Refractory Metals to Ni-Based Superalloys

In this study, a range of joining technologies has been investigated for creating attachments between refractory metal and Ni-based superalloys. Refractory materials of interest include Mo-47%Re, T-111, and Ta-10%W. The Ni-based superalloys include Hastelloy X and MarM 247. During joining with conventional processes, these materials have potential for a range of solidification and intermetallic formation-related defects. For this study, three non-conventional joining technologies were evaluated. These included inertia welding, electro-spark deposition (ESD) welding, and magnetic pulse welding (MPW). The developed inertia welding practice closely paralleled that typically used for the refractory metals alloys. Metallographic investigations showed that forging during inertia welding occurred predominantly on the nickel base alloy side. It was also noted that at least some degree of forging on the refractory metal side of the joint was necessary to achieve consistent bonding. Both refractory metals were readily weldable to the Hastelloy X material. When bonding to the MarM 247, results were inconsistent. This was related to the higher forging temperatures of the MarM 247, and subsequent reduced deformation on that material during welding. ESD trials using a Hastelloy X filler were successful for all material combinations. ESD places down very thin (5- to 10- m) layers per pass, and interactions between the substrates and the fill were limited (at most) to that layer. For the refractory metals, the fill only appeared to wet the surface, with minimal dilution effects. Microstructures of the deposits showed high weld metal integrity with maximum porosity on the order of a few percent. Some limited success was also obtained with MPW. In these trials, only the T-111 tubes were used. Joints were possible for the T-111 tube to the Hastelloy X bar stock, but the stiffness of the tube (resisting collapse) necessitated the use of very high power levels. These power levels resulted in damage to the equipment (concentrator) during welding. It is of note that the joint made showed the typical wavy bond microstructure associated with magnetic pulse/explosion bond joints. Joints were not possible between the T-111 tube and the MarM 247 bar stock. In this case, the MarM 247 shattered before sufficient impact forces could be developed for bonding.

Gould, Jerry E.↗

Welding of nickel-base superalloys having a nil-ductility range

An article made of a nickel-base superalloy having a nil-ductility range from the solidus temperature of the alloy to about 600.degree. F. below the solidus temperature is welded, as for example in the weld repair of surface cracks, by removing foreign matter from the area to be welded, first stress relieving the article, adjusting the temperature of the article to a welding temperature of from about 1800.degree. F. to about 2100.degree. F., welding a preselected area in an inert atmosphere at the welding temperature, and second stress relieving the article. Welding is preferably accomplished by striking an arc in the preselected area so as to locally melt the alloy in the preselected area, providing a filler metal having the same composition as the nickel-based superalloy of the article, and feeding the filler metal into the arc so that the filler metal is melted and fused with the article to form a weldment upon solidification.

Smashey, Russell W.↗

Additive manufacturing process parameter determination for a new Fe-C-Cu alloy

As a potential replacement for stainless steel alloys commonly used to print parts with laser powder bed fusion, a new Cu precipitation strengthened ferrous alloy, with composition Fe-0.2C-6Cu (wt%), was recently developed. This material is Co- and Ni-free, printable, has mechanical properties comparable to that of high strength stainless steels (approximately 1300 MPa UTS), and is cost-advantaged relative to existing low-alloy steels for additive manufacturing of parts with complex shapes. To gain traction for broader application, optimal laser powder bed fusion (LPBF) processing conditions to produce nearly defect-free parts without compromising mechanical strength are needed. Here, an optimal processing window based upon laser speeds that achieve minimal porosity was quantified via comparisons of measured melt pool penetration, scan speeds, printed material density and laser beam energy density on a commercial LPBF unit operating at 350 W, 80 μm hatch spacing, and 50 μm layer thickness based upon optimal parameters for 17-4PH. Furthermore, the window is 300 to 500 mm/s to achieve >99.8 % dense Fe-0.2C-6Cu (wt%) specimens. Other defects such as burning, spatter, and lack of fusion were also avoided in this window. The window was validated with in-situ synchrotron X-ray imaging that enabled visualization of the vapor cavity, melting, and solidification during a single laser track scan on a miniature powder bed sample. In addition, in-situ infrared imaging provided temperature fields, cooling rate and solidification range, and confirmed minimal printing defects and spatter within the processing window.

36 MATERIALS SCIENCE↗

A study of metal-ceramic wettability in SiC-Al using dynamic melt infiltration of SiC

Pressure-assisted infiltration with a 2014 Al alloy of plain and Cu-coated single crystal platelets of alpha silicon carbide was used to study particulate wettability under dynamic conditions relevant to pressure casting of metal-matrix composites. The total penetration length of infiltrant metal in porous compacts was measured at the conclusion of solidification as a function of pressure, infiltration time, and SiC size for both plain and Cu-coated SiC. The experimental data were analyzed to obtain a threshold pressure for the effect of melt intrusion through SiC compacts. The threshold pressure was taken either directly as a measure of wettability or converted to an effective wetting angle using the Young-Laplace capillary equation. Cu coating resulted in partial but beneficial improvements in wettability as a result of its dissolution in the melt, compared to uncoated SiC.

Asthana, R.↗

The Influence of Galvanizing Parameters on the Structural Development of Zn-Al-Based Coatings

The evolution of some layers’ characteristics, deposited by galvanization, was monitored according to the technological parameters of the process. Two types of alloys from the Zn-Al and Zn-Al-Ti-B systems were used for deposition. The structure of the deposited layers was analyzed by optical and electron microscopy. The chemical composition, phases and compounds in the structures were identified. The mechanical properties of the structural constituents of the layers were determined by nanoindentation. These techniques highlighted the typical non-uniformities in terms of composition and properties in the layers, mainly due to the diffusion and distribution of iron from the steel substrate in the deposited layers. The evaluation of iron diffusion in the deposited layer was done by differential thermal analysis. The values of the critical temperatures (melting temperature, eutectic temperature and solidification temperature) were correlated with the parameters used during deposition. It was observed that the structure of the coatings is layered, with a specific order from the steel substrate to the edge. In these layers, the constituents are mixtures of soft solid solutions of Al in Zn (η and β) and hard intermetallic compounds. Moreover, increasing the immersion time in the galvanizing bath and the bath temperature leads to an increase in iron diffusion in the coating layer, which contributes to lower coating thickness, thus reducing its durability in operation.

36 MATERIALS SCIENCE↗

Morphological Evolution of Directional Solidification Interfaces in Microgravity: An Analysis of Model Experiments Performed on the International Space Station

A series of experiments performed using the Pore Formation and Mobility Investigation (PFMI) apparatus within the glovebox facility (GBX) on board the International Space Station (ISS) has provided video images of the morphological evolution of a three-dimensional interface in a diffusion controlled regime. The experimental samples were prepared on ground by filling glass tubes, 1 cm ID and approximately 30 cm in length, with "alloys" of succinonitrile (SCN) and water in an atmosphere of nitrogen at 450 millibar pressure. The compositions of the samples processed and analyzed are 0.25,0.5 and 1.0 wt% water. Experimental processing parameters of temperature gradient and translation speed, as well as camera settings, were remotely monitored and manipulated from the ground Telescience Center (TSC) at the Marshall !3pace Flight Center. During the experiments, the sample was first subjected to a unidirectional melt back, generally at 10 microns per second, with a constant temperature gradient ahead of the melting interface. Following the melt back, the interface was allowed to stabilize before translation is initiated. The temperatures in the sample were monitored by six in situ thermocouples and the position is monitored by an optical linear encoder. For the experiments performed and analyzed, the gradients ranged from 2.5 - 3.3 K/mm and the initial pulling velocities ranged from 0.7 micron per second to 1 micron per second with subsequent transition velocities of up to 100 microns per second. The data provided by the PFMI for analysis includes near-real-time (NRT) video captured on the ground during the experiment runs, ISS Video Tape Recorder (VTR) data dumped from the VTR at the end of the experiment run and recorded on the ground, telemetry data including temperature and position measurements, and limited flight HI-8 tapes in 2 camera views of experiment runs for which tapes have been returned to the investigators from ISS. Because of limited down mass from the ISS, the majority of the initial analysis has been performed using the NRT and VTR video data but will be supplemented with the HI-8 video as it becomes available. hardware and procedures required to prepare samples for correlation to flight samples is described. Using this ground-based system, a series of experiments have been performed for direct comparison with the flight data. The results of these comparisons as well as implications to future microgravity experiments are presented and discussed. A ground-based thin-sample directional solidification system as well as all associated

Strutzenberg, Louise L.↗

Microstructural Characterization of a Directionally-Solidified Ni-33 (at. %)Al-31Cr-3Mo Eutectic Alloy as a Function of Withdrawal Rate

The Ni-33 (at. %)Al-3lCr-3Mo eutectic alloy was directionally-solidified (DS) at different rates, V(sub I), varying between 2.5 to 508 mm/ h. Detailed qualitative and quantitative metallographic and chemical analyses were conducted on the directionally-solidified rods. The microstructures consisted of eutectic colonies with parallel lamellar NiAl/(Cr,Mo) plates for solidification rates at and below 12.7 mm/ h. Cellular eutectic microstructures were observed at higher solidification rates, where the plates exhibited a radial pattern. The microstructures were demonstrated to be fairly uniform throughout a 100 mm length of the DS zone by quantitative metallography. The average cell size, bar-d, decreased with increasing growth rate to a value of 125 microns at 508 mm/ h according to the relation bar-d (microns) approx. = 465 V(sup -0.22, sub I), where V(sub I) is in mm/ h. Both the average NiAl plate thickness, bar-Delta(sub NiAl), and the interlamellar spacing, bar-lambda, were observed to be constant for V(sub I) less than or = 50.8 mm/ h but decreased with increasing growth rate above this value as 0.93 bar-Delta(sub NiAl)(microns) = 61.2 V(sup -0.93, sub I) and bar-lambda (microns) = 47.7 V(sup -0.64, sub I), respectively. The present results are detailed on a microstructural map. Keywords Optical microscopy, microstructure, compounds intermetallic, directional solidification

Raj, S. V.↗

Microstructures and mechanical properties of a welded CoCrFeMnNi high-entropy alloy

The response of the CoCrFeMnNi high-entropy alloy to weld thermal cycles was investigated to determine its applicability as an engineering structural material. Two processes were used: high-energy-density, low-heat-input electron beam (EB) welding and low-energy-density, high-heat-input gas tungsten arc (GTA) welding. Weldability was determined through comprehensive microstructural and mechanical property characterisation of the welds. The welds did not develop solidification cracking or heat-affected zone cracks. The microstructures in weld fusion zones are similar to that in the as-cast materials, consisting of large columnar grains with dendrite. The dendrite arm spacing and the extent of elemental segregation were less in the welds than in the cast ingot, and also were less pronounced in the EB weld than in the GTA weld. Compositional microsegregation between dendritic cores and interdendritic regions of the welds was insignificant. Both welds exhibited slightly higher yield strengths than the base metal. The EB weld possessed comparable tensile strength and ductility to that of the base metal. In comparison, the GTA weld maintained ∼80% of the base metal's tensile strength and 50% of the ductility.

36 MATERIALS SCIENCE↗

Modeling Macrosegregation in Directionally Solidified Aluminum Alloys under Gravitational and Microgravitational Conditions

This report covers the modeling of seven directionally solidified samples, five under normal gravitational conditions and two in microgravity. A model is presented to predict macrosegregation during the melting phases of samples solidified under microgravitational conditions. The results of this model are compared against two samples processed in microgravity and good agreement is found. A second model is presented that captures thermosolutal convection during directional solidification. Results for this model are compared across several experiments and quantitative comparisons are made between the model and the experimentally obtained radial macrosegregation profiles with good agreement being found. Changes in cross section were present in some samples and micrographs of these are qualitatively compared with the results of the simulations. It is found that macrosegregation patterns can be affected by changing the mold material.

36 MATERIALS SCIENCE↗

The Effect of Weld Metal Composition on Microstructural and Mechanical Properties of Dissimilar Welds Between Monel 400 and Inconel 600

The current work was carried out to characterize welding of Inconel 600 superalloy and Monel 400. In the present study, gas tungsten arc welding (GTAW) with four types of filler metals (ENiCu, ENiCu-7, ENiCr-3 and ENiCrFe-3) was utilized. The filler metals were categorized into two groups based on the presence of Cr and Nb in their chemical composition. This paper describes the selection and application of welding consumables in manufacturing dissimilar metal combinations. It was found that (Nb/Cr) ratio and Fe content can affect on the size and amount of carbides. During solidification of ENiCr-3 and ENiCrFe-3 filler metals, Nb leaves dendritic cores and is rejected to inter-dendritic regions because of its high tendency for segregation. However, No brittle Laves phase was detected in the welds. The interface between weld metal and base metal and gradual changes in alloying elements were also investigated by scanning electron microscopy. EDX analysis was also applied for different samples. Microhardness measurements and tensile test were performed on the joints. The average hardness value in the weld metal obtained from ENiCrFe-3 is higher than the other welds. ENiCu-7 weld exhibited the highest tensile strength of 540 MPa and percent elongation of 53% in contrast to ENiCrFe-3 weld with the lowest tensile strength (518 MPa) and percent elongation (39%).

36 MATERIALS SCIENCE↗

Emergence of complex-regular eutectic patterns in Al–Ge: Observations from correlative nano-imaging

Eutectic solidification exemplifies nonequilibrium pattern formation, making it a well-studied moving boundary problem. Yet the mechanisms behind the formation of complex-regular microstructures – particularly in highly anisotropic systems with a significant volume fraction of a faceted phase – remain poorly understood. Our understanding of such systems is made complicated by the nonlinear interface kinetics and unique growth dynamics characteristic of faceted phases. To address these challenges, we investigate a model Al–Ge eutectic system, where the faceted Ge phase constitutes a substantial volume fraction (~0.35) and where the two solid phases arrange into so-called “fishbone” or “feather” complex-regular patterns. Using synchrotron-based x-ray nano-imaging and nanotomography with high spatial resolution (22 nm per pixel), we capture in real-time the evolution of the solid–liquid interfaces and the resulting three-dimensional microstructures in this faceted/non-faceted eutectic system. By integrating these observations with electron backscattered diffraction, we elucidate the crystallographic biases on the solidification process and the mechanisms driving the formation of such complex-regular microstructures. These findings inform a new growth model for irregular eutectics in (near-)symmetrical phase diagrams, offering insight on advanced microstructural design and processing strategies. More broadly, we demonstrate how interfacial curvature is generated in irregular eutectic alloys and how it depends on the volume fraction of the faceted phase.

36 MATERIALS SCIENCE↗

Growth interactions between icosahedral quasicrystals

We investigate the solidification pathways of a population of icosahedral quasicrystals in a liquid through in situ synchrotron x-ray tomography. The wealth of three-dimensional space- and time-resolved data enables us to test the predictions of various models and theories of crystallization on a quasi-crystal-forming alloy. Remarkably, we find the general evolution equation—that accounts for the competing effects of growth, coalescence, and coarsening—fits well our experimental data on surface area concentration. Furthermore, we quantify the orientation selection, screening length, and coarsening rate of the dodecahedra, and compare these results to that of periodic crystals. The latter is a full order of magnitude smaller than that of elemental metal dendrites in the limit of zero volume fraction, a reflection of the low solid-liquid interfacial energy of the icosahedral phase. Furthermore, our paper provides the critical input data for microstructural models used for integrated computational materials engineering of complex intermetallics, including quasicrystals.

36 MATERIALS SCIENCE↗

MaterialsMap: A CALPHAD-based tool to design composition pathways through feasibility map for desired dissimilar materials, demonstrated with resistance spot welding joining of Ag-Al-Cu

Assembly of dissimilar metals can be achieved by different methods, for example, casting, welding, and additive manufacturing (AM). However, undesired phases formed in liquid-phase assembling processes due to solute segregation during solidification diminish mechanical and other properties of the processed parts. In the present work, an open-source software named MaterialsMap, has been developed based on the CALculation of Phase Diagrams (CALPHAD) approach. The primary objective of MaterialsMap is to facilitate the design of an optimal composition pathway for assembling dissimilar alloys with liquid-phases based on the formation of desired and undesired phases along the pathway. In MaterialsMap, equilibrium thermodynamic calculations are used to predict equilibrium phases formed at slow cooling rate, while Scheil-Gulliver simulations are employed to predict non-equilibrium phases formed during rapid cooling. Additionally, by combining these two simulations, MaterialsMap offers a thorough guide for understanding phase formation in various manufacturing processes, assisting users in making informed decisions during material selection and production. As a demonstration of this approach, a compositional pathway was designed from pure Al to pure Cu through Ag using MaterialsMap. The design was experimentally verified using resistance spot welding (RSW).

36 MATERIALS SCIENCE↗

High-resolution in-situ characterization of laser powder bed fusion via transmission X-ray microscopy at X-ray free electron lasers

In this work, we describe the instrumentation used to perform the first operando transmission X-ray microscopy (TXM) and simultaneous X-ray diffraction of laser melting simulating laser powder bed fusion on the XCS instrument at the Linac Coherent Light Source (LCLS) X-ray free-electron laser (XFEL). Our TXM with 40× magnification in the X-ray regime at 11 keV gave spatial resolutions down to 940 nm per line pair, with effective pixel sizes down to 206 nm, image integration times of <100 fs, and frame rates tunable between 2.1 and 119 ns for two probe frames (0.48 GHz to 8.4 MHz). Images were recorded on Zyla and Icarus (UXI) detectors to trade off between spatial resolution and time dynamics. A 1 kW CW IR laser was coupled into the interaction point to conduct pump–probe studies of laser melting and solidification dynamics. Our temporal and spatial resolution with attenuation-based contrast exceeds that currently possible with synchrotron-based high-speed radiography. This system was sensitive to feature velocities of 10–12000 m s −1 but we did not observe any motion in this range in the laser melting of Al6061 alloy. Shockwaves were not observed and hot cracking proceeded at velocities below the detection limits. Pore accumulation was observed between successive shots, indicating that bubble escape mechanisms were not active. With proper experimental design, the spatial resolution, contrast and field of view could be further improved or modified. The increased brightness and narrower bandwidth of the XFEL allowed for this imaging technique and it lays the groundwork for a wide range of operando techniques to study additive manufacturing.

47 OTHER INSTRUMENTATION↗

Process-dependent anisotropic thermal conductivity of laser powder bed fusion AlSi10Mg: impact of microstructure and aluminum-silicon interfaces

Purpose AlSi10Mg alloy is commonly used in laser powder bed fusion due to its printability, relatively high thermal conductivity, low density and good mechanical properties. However, the thermal conductivity of as-built materials as a function of processing (energy density, laser power, laser scanning speed, support structure) and build orientation, are not well explored in the literature. This study aims to elucidate the relationship between processing, microstructure, and thermal conductivity. Design/methodology/approach The thermal conductivity of laser powder bed fusion (L-PBF) AlSi10Mg samples are investigated by the flash diffusivity and frequency domain thermoreflectance (FDTR) techniques. Thermal conductivities are linked to the microstructure of L-PBF AlSi10Mg, which changes with processing conditions. The through-plane exceeded the in-plane thermal conductivity for all energy densities. A co-located thermal conductivity map by frequency domain thermoreflectance (FDTR) and crystallographic grain orientation map by electron backscattered diffraction (EBSD) was used to investigate the effect of microstructure on thermal conductivity. Findings The highest through-plane thermal conductivity (136 ± 2 W/m-K) was achieved at 59 J/mm 3 and exceeded the values reported previously. The in-plane thermal conductivity peaked at 117 ± 2 W/m-K at 50 J/mm 3 . The trend of thermal conductivity reducing with energy density at similar porosity was primarily due to the reduced grain size producing more Al-Si interfaces that pose thermal resistance. At these interfaces, thermal energy must convert from electrons in the aluminum to phonons in the silicon. The co-located thermal conductivity and crystallographic grain orientation maps confirmed that larger colonies of columnar grains have higher thermal conductivity compared to smaller columnar grains. Practical implications The thermal properties of AlSi10Mg are crucial to heat transfer applications including additively manufactured heatsinks, cold plates, vapor chambers, heat pipes, enclosures and heat exchangers. Additionally, thermal-based nondestructive testing methods require these properties for applications such as defect detection and simulation of L-PBF processes. Industrial standards for L-PBF processes and components can use the data for thermal applications. Originality/value To the best of the authors’ knowledge, this paper is the first to make coupled thermal conductivity maps that were matched to microstructure for L-PBF AlSi10Mg aluminum alloy. This was achieved by a unique in-house thermal conductivity mapping setup and relating the data to local SEM EBSD maps. This provides the first conclusive proof that larger grain sizes can achieve higher thermal conductivity for this processing method and material system. This study also shows that control of the solidification can result in higher thermal conductivity. It was also the first to find that the build substrate (with or without support) has a large effect on thermal conductivity.

Engineering↗

Development of Large Bandgap Materials Using Reactive Growth in Al-SI Eutectic for Optical and RF Applications

Carbon was utilized as reactive element to modify the microstructure using forced mixing during crystallization of the Al-Si alloy by rotation and stirring. We nucleated the material on SiC substrates while the Al-Si melt was rotated with a speed of 30rpm in a graphite crucible. Several experiments were performed and parameters such as time of mixing, soaking temperature, rotation rate of the substrate and rate of cooling during the solidification was changed. We observed dendrite and cell morphologies during the solidification of rotating melt. The microstructure was characterized by optical microscopy and SEM-EDX and compositional spectroscopy. The effect of carbon impurities was studied on the solidifying microstructure. When we used the longer soak time of the melt in presence of carbon impurities we observed the destruction of dendritic morphology and the formation of cellular and colony structures. Similar approach has been used for Ga2O3, a novel large bandgap material also.

Singh, N. B.↗

Structures of immiscible Al-In alloys solidified under microgravity conditions

Four samples of the immiscible Al-In system having monotectic and hypermonotectic compositions were solidified under microgravity during the NASA-SPAR IX flight of January 20th, 1981. The experimental thermal and physico-chemical conditions actually achieved have been analysed. Radiographic and metallographic observations of the samples show a non-regular dispersed primary phase inside the monotectic matrix. These observations are commented on the basis of capillarity and solidification aspects.

Potard, C.↗