Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STARTING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,369 records · Page 76

Facile synthesis of B-type carbonated nanoapatite with tailored microstructure

Nanolime and a phosphate-based chelating agent were used to synthesize B-type carbonated apatite. Developed Rietveld refinement strategies allowed one to determine process yield, product crystallinity as well as structural (unit cell) and microstructural (size, strain) parameters. The effect of synthesis temperature (20–60 °C) as well as Ca/P ratio (1.5–2.5) and solid content (10–30 wt%) of the starting batch on these properties were investigated. FTIR, TEM and gas adsorption data provided supporting evidence. The process yield was 42–60 wt% and found to be governed by the Ca/P ratio. The purified products had high specific surface area (107–186 m{sup 2}/g) and crystallinity (76–97%). The unit cell parameters, correlated to the degree of structural carbonate, were sensitive to the Ca/P ratio. Instead, temperature governed the microstructural parameters. Less strained and larger crystals were obtained at higher temperatures. Long-term aging up to 6 months at 20 °C compensated for higher crystal growth kinetics at higher temperature. - Graphical abstract: Controlled synthesis of carbonated apatite at moderate temperatures using nanolime and sodiumhexametaphosphate as starting reagent. - Highlights: • Chemical synthesis of nano-sized apatite with tailored microstructure was performed. • Colloidal Ca(OH){sub 2} and a phosphorus-based chelating agents were used as reagents. • The method is simple and reproducible which facilitate industrial process scale-up. • Rietveld refinement strategies for product characterization were developed. • Rietveld analyses provided yield, microstructural and structure information.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Bismuth zinc vanadate, BiZn{sub 2}VO{sub 6}: New crystal structure type and electronic structure

We report a combined experimental and computational study of the crystal structure and electronic properties of bismuth zinc vanadate, BiZn{sub 2}VO{sub 6}, known for its visible light photocatalytic activity. The crystal structure has been solved from laboratory powder X-ray diffraction data using the repeated minimisations from random starting values method. BiZn{sub 2}VO{sub 6} adopts a new structure type, based on the following building blocks: corner- and edge-sharing ZnO{sub 4} tetrahedra, ZnO{sub 6} octahedra and VO{sub 4} tetrahedra, and Bi{sub 2}O{sub 12} dimers. It is the only known member of the BiM{sub 2}AO{sub 6} (M=Pb, Ca, Cd, Mn, Zn, Mg, Cu; A=V, P, As) family which does not appear to be structurally closely related to others. The electronic structure of BiZn{sub 2}VO{sub 6}, calculated by DFT methods, shows that it is an indirect gap semiconductor with a calculated band gap of 1.6 eV, which compares favourably to the experimentally measured value of 2.4 eV. - Graphical abstract: The crystal structure of BiZn{sub 2}VO{sub 6}, a new structure type in the BiM{sub 2}AO{sub 6} (M=Mg, Ca, Cd, Cu, Pb, Mn, Zn; A=V, P, As) family. - Highlights: • Structure solution from PXRD data by repeated minimisations from random starting values. • New structure type in the BiM{sub 2}AO{sub 6} (M=Pb, Ca, Cd, Mn, Zn, Mg, Cu; A=V, P, As) family. • Electronic structure calculation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Observation of divergent La{sup 3+} ion dilute effect in two series of 3-D fluorescent lanthanide-MOFs-based molecular alloys RE{sub x}La{sub 1−x}–EBTC (RE{sup 3+}=Eu{sup 3+} or Tb{sup 3+}; EBTC{sup 4−}=1,1′-ethynebenzene-3,3′,5,5′-etracarboxylate)

The lanthanide metal-organic frameworks (MOFs) [Ln{sub 2}(EBTC){sub 1.5}(CH{sub 3}OH){sub 4}]·6H{sub 2}O are isostructural to each other, where EBTC{sup 4−}=1,1′-ethynebenzene-3,3′,5,5′-tetracarboxylate; Ln{sup 3+}=La{sup 3+}, Eu{sup 3+} and Tb{sup 3+}; and the corresponding MOF is abbreviated as Ln–EBTC. MOFs Eu–EBTC and Tb–EBTC emit intense red and green luminescence (visible by bare eyes), respectively. The molecular alloys of Eu{sub x}La{sub 1−x}–EBTC and Tb{sub x}La{sub 1−x}–EBTC have been successfully prepared by mixing Eu{sup 3+}/Tb{sup 3+} and La{sup 3+} salts with the desired molar ratio in the starting material. Two series of Eu{sub x}La{sub 1−x}–EBTC and Tb{sub x}La{sub 1−x}–EBTC molecular alloys are isomorphic to the parent Ln–EBTC MOFs, while exhibit divergent La{sup 3+} ion diluting effect, namely, with increasing the relative amount of La{sup 3+}, the intensity of characteristic emission arising from Tb{sup 3+} ion monotonely increases in Tb{sub x}La{sub 1−x}–EBTC molecular alloys, whereas that of Eu{sup 3+} ion shows non-monotone decrease in Eu{sub x}La{sub 1−x}–EBTC molecular alloys. The possible origin is discussed for such a divergent behavior between Eu{sub x}La{sub 1−x}–EBTC and Tb{sub x}La{sub 1−x}–EBTC molecular alloys. - Graphical abstract: Two series of 3-D fluorescent lanthanide-MOFs-based molecular alloys RE{sub x}La{sub 1−x}–EBTC (RE{sup 3+}=Eu{sup 3+} or Tb{sup 3+}; EBTC{sup 4−}=1,1′-ethynebenzene-3,3′,5,5′-tetracarboxylate) have been successfully prepared by mixing Eu{sup 3+}/Tb{sup 3+} and La{sup 3+} salts with the desired molar ratio in the starting material and showed photoluminescence property with divergent La{sup 3+} ion dilute effect. - Highlights: • 3-D molecular alloys of Eu{sub x}La{sub 1−x}–EBTC and Tb{sub x}La{sub 1−x}–EBTC were prepared. • They are isomorphic to the parent Ln–EBTC MOFs. • They show photoluminescence property with divergent La{sup 3+} ion diluting effect. • The possible origin is discussed for such a divergent behavior.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

HPHT synthesis, structure and electrical properties of type-I clathrates Ba{sub 8}Al{sub x}Si{sub 46−x}

Clathrate compounds Ba{sub 8}Al{sub x}Si{sub 46−x} were successfully synthesized using the method of high-pressure and high-temperature (HPHT). In this process, we used BaSi{sub 2} as one of the starting materials in place of Ba metals, which reduces the complexity of the program caused by the extremely high chemical reactivity. By using this method, the processing time was reduced from few days to an hour. X-ray diffraction and structural refinement indicated this composition crystallized in type-I clathrate phase. Bond length analysis showed the Ba atoms in small dodecahedron had spherical thermal ellipsoids while those in large tetrakaidecahedron displayed anisotropic thermal ellipsoids. The negative Seebeck coefficient indicated transport processes were dominated by electrons as carriers, and increased with the increasing temperature. The electrical properties, including Seebeck coefficient and Power factor, were greatly enhanced by Al substitution. - Graphical abstract: Left: The cavity structure diagram of a China-type large volume cubic high-pressure apparatus, and the Type-I clathrate structure of sample synthesized using HPHT. Middle: X-ray Rietveld refinement profile for Ba{sub 8}Si{sub 46} and element mapping for Ba{sub 8}Al{sub 16}Si{sub 30}. Right: Temperature dependence of Seebeck coefficient for Ba{sub 8}Al{sub x}Si{sub 46−x} prepared by HPHT. - Highlights: • HPHT is a simple and rapid synthetic approach. • We use BaSi{sub 2} as one of the starting materials replacing Ba metals. • The processing time reduces from few days to an hour. • Structure determination is refined by Rietveld analysis of XRD data. • Variable temperature electrical properties are characterized.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Design and syntheses of hybrid metal–organic materials based on K{sub 3}[M(C{sub 2}O{sub 4}){sub 3}]·3H{sub 2}O [M(III)=Fe, Al, Cr] metallotectons

By using K{sub 3}[M(C{sub 2}O{sub 4}){sub 3}]·3H{sub 2}O [M(III)=Fe, Al, Cr] (C{sub 2}O{sub 4}{sup 2−}=oxalate) metallotectons as the starting material, we have synthesized eight novel complexes with formulas [{Fe(C_2O_4)_2(H_2O)_2}{sub 2}]·(H–L{sub 1}){sub 2}·H{sub 2}O 1, [Fe(C{sub 2}O{sub 4})Cl{sub 2}]·(H{sub 2}–L{sub 2}){sub 0.5}·(L{sub 2}){sub 0.5}·H{sub 2}O 2, [{Fe(C_2O_4)_1_._5Cl_2}{sub 2}]·(H–L{sub 3}){sub 4}3, [Fe{sub 2}(C{sub 2}O{sub 4})Cl{sub 8}]·(H{sub 2}–L{sub 4}){sub 2}·2H{sub 2}O 4, K[Al(C{sub 2}O{sub 4}){sub 3}]·(H{sub 2}–L{sub 5})·2H{sub 2}O 5, K[Al(C{sub 2}O{sub 4}){sub 3}]·(H–L{sub 6}){sub 2}·2H{sub 2}O 6, K[Cr(C{sub 2}O{sub 4}){sub 3}]·2H{sub 2}O 7, Na[Fe(C{sub 2}O{sub 4}){sub 3}]·(H–L{sub 6}){sub 2}·2H{sub 2}O 8 (with L{sub 1}=4-dimethylaminopyridine, L{sub 2}=2,3,5,6-tetramethylpyrazine, L{sub 3}=2-aminobenzimidazole, L{sub 4}=1,4-bis-(1H-imidazol-1-yl)benzene, L{sub 5}=1,4-bis((2-methylimidazol-1-yl)methyl)benzene, L{sub 6}=2-methylbenzimidazole). Their structures have been determined by single-crystal X-ray diffraction analyses, elemental analyses, IR spectra and thermogravimetric analyses. Compound 3 is a 2D H-bonded supramolecular architecture. Others are 3D supramolecular structures. Compound 1 shows a [Fe(C{sub 2}O{sub 4}){sub 2}(H{sub 2}O){sub 2}]{sup −} unit and 3D antionic H-bonded framework. Compound 2 features a [Fe(C{sub 2}O{sub 4})Cl{sub 2}]{sup -} anion and 1D iron-oxalate-iron chain. Compound 3 features a [Fe{sub 2}(C{sub 2}O{sub 4}){sub 3}Cl{sub 4}]{sup 4−} unit. Compound 4 features distinct [Fe{sub 2}(C{sub 2}O{sub 4})Cl{sub 8}]{sup 4−} units, which are mutual linked by water molecules to generated a 2D H-bonded network. Compound 5 features infinite ladder-like chains constructed by [Al(C{sub 2}O{sub 4}){sub 3}]{sup 3−} units and K{sup +} cations. The 1D chains are further extended into 3D antionic H-bonded framework through O–H···O H-bonds. Compounds 6–8 show 2D [KAl(C{sub 2}O{sub 4}){sub 3}]{sup 2−} layer, [KCr(C{sub 2}O{sub 4}){sub 3}]{sup 2−} layer and [NaFe(C{sub 2}O{sub 4}){sub 3}]{sup 2−} layer, respectively. - Graphical abstract: We report here eight novel complexes by using [M(C{sub 2}O{sub 4}){sub 3}]{sup 3−} [M(III)=Fe, Al, Cr] metallotectons as the starting materials. These complexes show supramolecular architectures bonded by charge-assisted hydrogen bonds.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Highly regenerable carbon-Fe{sub 3}O{sub 4} core–satellite nanospheres as oxygen reduction electrocatalyst and magnetic adsorbent

We present the synthesis and multifunctional utilization of core-satellite carbon-Fe{sub 3}O{sub 4} nanoparticles to serve as the enabling platform for a range of applications including oxygen reduction reaction (ORR) and magnetic adsorbent. Starting from polydopamine (PDA) nanoparticles and Fe(NO{sub 3}){sub 3}, carbon-Fe{sub 3}O{sub 4} core–satellite nanospheres are synthesized through successive steps of impregnation, ammoniation and carbonization. The synergistic combination of Fe{sub 3}O{sub 4} and N-doped carbon endows the nanocomposite with high electrochemical activity in ORR and mainly four electrons transferred in reaction process. Furthermore, carbon-Fe{sub 3}O{sub 4} nanoparticles used as magnetic adsorbent exhibit the efficient removal of Rhodamine B from an aqueous solution. The recovery and reuse of the adsorbent is demonstrated 5 times without any detectible loss in activity. - Graphical abstract: Starting from polydopamine (PDA) nanoparticles and Fe(NO{sub 3}){sub 3}, carbon-Fe{sub 3}O{sub 4} core–satellite nanospheres are synthesized through successive steps of impregnation, ammoniation and carbonization. The nanocomposites serve as the enabling platform for a range of applications including oxygen reduction reaction (ORR) and magnetic adsorbent. - Highlights: • Carbon-Fe{sub 3}O{sub 4} core–satellite nanospheres are synthesized through successive steps of impregnation, ammoniation and carbonization. • Polydopamine and Fe(NO{sub 3}){sub 3} are precursors for N-doped carbon source and Fe{sub 3}O{sub 4} nanoparticles, respectively. • The nanocomposites exhibit high electrochemical activity in ORR. • The nanocomposites effectively adsorb organic dyes with magnetic recovery and good recycle property.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The effect of chemical composition and austenite conditioning on the transformation behavior of microalloyed steels

In this investigation, by using continuous cooling torsion (CCT) testing, the transformation behavior of four microalloyed steels under two circumstances of austenite conditioning and non-conditioning was studied. A full scale hot-rolling schedule containing a 13-pass deformation was employed for the conditioning of the austenite. The CCT tests were then employed till temperature of {approx} 540 Degree-Sign C and the flow curves obtained from this process were analyzed. The initial and final microstructures of the steels were studied by optical and electron microscopes. Results show that alloying elements would decrease the transformation temperature. This effect intensifies with the gradual increase of Mo, Nb and Cu as alloying elements added to the microalloyed steels. As well, austenite conditioning increased the transformation start temperature due mainly to the promotion of polygonal ferrite formation that resulted from a pancaked austenite. The final microstructures also show that CCT alone would decrease the amount of bainite by inducing ferrite transformation in the two phase region. In addition, after the transformation begins, the deformation might result in the occurrence of dynamic recrystallization in the ferrite region. This could lead to two different ferrite grain sizes at the end of the CCT. Moreover, the Nb bearing steels show no sign of decreasing the strength level after the transformation begins in the non-conditioned situation and their microstructure is a mix of polygonal ferrite and bainite indicating an absence of probable dynamic recrystallization in this condition. In the conditioned cases, however, these steels show a rapid decrease of the strength level and their final microstructures insinuate that ferrite could have undergone a dynamic recrystallization due to deformation. Consequently, no bainite was seen in the austenite conditioned Nb bearing steels. The pancaking of austenite in the latest cases produced fully polygonal ferrite structures. - Highlights: Black-Right-Pointing-Pointer Adding alloying elements would decrease the transformation temperatures. Black-Right-Pointing-Pointer Austenite conditioning increases the transformation start temperature. Black-Right-Pointing-Pointer Deformation could induce the occurrence of dynamic recrystallization in ferrite region.

36 MATERIALS SCIENCE↗

Extrinsic and intrinsic properties in metal–insulator transition of hydrothermally prepared vanadium dioxide crystals

The clear insulator (monoclinic-VO{sub 2}) to metal (rutile-VO{sub 2}) transition (IMT) was observed in electrical conductivity and differential scanning calorimeter (DSC) measurements at around 340 K, which is IMT temperature (T{sub H}), in the hydrothermally prepared VO{sub 2} crystals. The occurrence of metal to insulator transition (MIT) temperature (T{sub C}) was observed below 333 K during the first resistance measurement cycle in the most of cases. The sudden jump of the electrical resistance at IMT and MIT points was amplified several times than that of the first cycle during the repeated successive thermal cycles (heating and cooling across the IMT and MIT temperatures). T{sub C} and T{sub H} shifted to higher temperature by the repeated successive thermal cycles. This shift and the amplified jump might be related to the mechanical stress between the VO{sub 2} crystals, i.e. extrinsic properties. However, the starting point of MIT, T{sub CS} = ∼ 336 K, and the starting point of IMT, T{sub HS} = ∼ 338 K, kept almost constant during the repeated thermal cycles (< 10 times). These two temperatures may be related to the intrinsic properties of the VO{sub 2}: the phase transitions initiated at these temperatures regardless of the number of the repeated thermal cycles. The neat surface of the VO{sub 2} crystals was severely damaged and the average size of particles reduced from 110 nm to 70–90 nm after extensively repeated thermal cycles (> 70 times). The damaged surface and the smaller particles, which would be originated from the mechanical stress caused by crystal volume change during the first order transition of the VO{sub 2}, would weaken the electrical conduction path (loosen grain boundaries) between the VO{sub 2} single crystals and would result in the amplified jump at the following MIT. This report may boost the study for the improved stability and lifetime of the VO{sub 2} based electronic devices. - Highlights: • The sharp phase transition in cluster of VO{sub 2} crystals depends on repeated thermal cycles. • Two intrinsic and two extrinsic temperatures are observed during the phase transition. • The mechanical stress change and surface damage may cause the extrinsic properties in transport measurement.

36 MATERIALS SCIENCE↗

Variation of carbon concentration in proeutectoid ferrite during austenitization in hypoeutectoid steel

The variation of the C concentration in proeutectoid ferrite (α{sub PF}) during austenitization in hypoeutectoid steels was quantitatively investigated using the massive transformation start temperature (T{sub m}) of α{sub PF} to austenite (γ) measured by high-temperature confocal laser scanning microscopy and hardness of α{sub PF}. The C concentration in α{sub PF} at T{sub m} in hypoeutectoid steels increased with increasing total C concentration up to approximately 0.2 wt.% during heating. The hardness of α{sub PF} with isothermal holding time at 775 °C in S20C steel revealed C enrichment in α{sub PF} at the early stage of isothermal holding and its reduction with further holding. These results explain the redistribution of the C in α{sub PF} during austenitization as follows: free C atoms released from cementite during pearlite decomposition diffuse excessively into neighboring α{sub PF} as well as pearlitic ferrite. The supersaturated C concentration in α{sub PF} is reduced during the long-range diffusive transformation of α{sub PF} to γ. However, some of the excess C atoms still remain in α{sub PF} until α{sub PF} starts to massively transform to γ. - Highlights: • Massive transformation of αPF to γ in hypoeutectoid steels was observed using CLSM. • C content in αPF during austenitization was analyzed by measured Tm and hardness. • Tm decreases and C content in αPF at Tm increases with increasing total C. • C atoms released from θ during formation of P to γ diffuse excessively into αPF. • Supersaturated C content in αPF is reduced during transformation of αPF to γ.

36 MATERIALS SCIENCE↗

The metal alloys from the XIX century and weathering action in the Mercado do Ver-o-Peso building, northern Brazil: Identification with the usage of laboratory analysis

The fabrication of metallic buildings started in Europe after the Industrial Revolution in the 18th century. Metallic constructions became very popular, and started being imported by several countries, due to the facility of constructing or assembling. Belém, a northern Brazilian city, holds a great number of buildings entirely made of iron, including the Ver-o-Peso, a fish market which structures were imported from England by the end of the 19th century. This building represents a unique type of architecture and it's an important part of the city's heritage. However, research so far did not focus on its construction materials. Ver-o-Peso building's metal alloys haven't been thoroughly studied concerning physical, chemical and mineralogical characterizations. This paper aims to identify the types of metal alloys used in the building, and also corrosion products' result from weathering actions. The methods used to characterize the materials were scanning electron microscopy and X-ray diffraction. Through this research it was possible to identify four types of iron alloys used in the different parts of the building, characterize the paint coats, and determine types of corrosion. The characterization of the materials in the building allows enrolling basis for restoration processes, documenting the types of metal alloy used in architectural heritage from the 19th century, as well as understanding the advances of corrosion. - Highlights: • Ver-o-peso is a heritage building from the 19th century with unidentified alloys. • Alloy and weathering product characterization was done using SEM/EDS and XRD. • Four metal alloy types were described, indicating different types of foundries. • Weathering products showed distinct mineral phases and physical characteristics. • Original paint coats were found among corrosion products.

36 MATERIALS SCIENCE↗

Formation of less-known structurally complex ζ{sub b} and orthorhombic quasicrystalline approximant ε{sub n} on solidification of selected Al–Pd–Cr alloys

The evolution of phases was investigated on cooling of Al{sub 71}Pd{sub 24}Cr{sub 5}, Al{sub 73}Pd{sub 20}Cr{sub 7}, and Al{sub 73}Pd{sub 23}Cr{sub 4} alloys from 1350 °C down to ambient temperature with the rate of 10 °C·min{sup −1}. To perform the investigation, differential thermal analysis, synchrotron X-ray powder diffraction, and scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy were used. In all the investigated alloys structurally complex phases ε{sub n} (ε{sub 6} + ε{sub 28}) and ζ{sub b}, as well as the δ-phase were identified. Based on the results of differential thermal analysis, sequences of phase transformations were determined. The Al{sub 71}Pd{sub 24}Cr{sub 5} alloy started to solidify at 1031.4 °C through β. Primary dendrites of ζ{sub b} were observed in Al{sub 73}Pd{sub 20}Cr{sub 7} and Al{sub 73}Pd{sub 23}Cr{sub 4} alloys. In the second step of solidification δ and/or ζ{sub b} were formed. The peritectic reaction, liquid + ζ{sub b} + δ → ε{sub n} + ζ{sub b} + δ, leading to the formation of the quasicrystalline approximant ε{sub n} (ε{sub 6} + ε{sub 28}) took place in the final step of solidification at approximately 792 °C. - Highlights: • Structurally complex ε{sub n} (ε{sub 6} + ε{sub 28}), ζ{sub b} and δ-phases were identified. • The Al{sub 71}Pd{sub 24}Cr{sub 5} alloy started to solidify at 1031.4 °C through the primary β phase. • The Al{sub 73}Pd{sub 20}Cr{sub 7} and Al{sub 73}Pd{sub 23}Cr{sub 4} alloys solidified in the same way. • The quasicrystalline approximant ε{sub n} (ε{sub 6} + ε{sub 28}) was formed at approximately 792 °C.

36 MATERIALS SCIENCE↗

Characterisation of Laves phase precipitation and its correlation to creep rupture strength of ferritic steels

The Laves phase precipitation process was characterised by means of field emission scanning electron microscopy to demonstrate its effect on creep rupture strength of steels with a fully ferritic matrix. To eliminate the effects of carbide and carbonitride precipitations so that the creep rupture data can be analysed exclusively in relation to the Laves phase precipitation process, an alloy Fe–9Cr–3Co–3W (wt.%) without C and N additions was used for the study. Creep rupture strengths were measured and volume fraction and particle size of Laves phase precipitates in the ruptured specimens were analysed. It was found that the creep rupture strength started to collapse (or decrease more rapidly) long before the Laves phase precipitation reached equilibrium fraction. This was related to the onset of the coarsening of Laves phase particles, which precipitated only on grain boundaries and hence contributed little to precipitation strengthening. Creep deformation had no effect either on the precipitation kinetics or on the growth kinetics of Laves phase particles. - Highlights: • Laves phase precipitation at 650 °C was characterised for Fe–9Cr–3W–3Co alloy. • Laves phase precipitated predominantly on grain boundaries. • Creep deformation had no effect on Laves phase precipitation and growth kinetics. • Creep strength started to collapse long before Laves phase precipitation is ended. • Collapse of creep strength was attributed to the coarsening of Laves phase particles.

36 MATERIALS SCIENCE↗

First stage of reaction of molten Al with MgO substrate

The Al/MgO couple was produced in vacuum (~ 5 × 10{sup −} {sup 4} Pa) by contact heating from RT up to 1000 °C and holding at that temperature for 1 h of a small 4 × 4 × 4 mm aluminium (5 N) sample placed on the [100] MgO single crystal substrate. TEM observations backed with electron diffraction analysis indicated that the interaction between liquid aluminium and MgO starts from a redox reaction producing a continuous layer of MgAl{sub 2}O{sub 4} spinel on the substrate surface. Its growth is controlled by solid state out-diffusion of magnesium and oxygen towards the surface being in contact with liquid metal. The thickening of spinel layer is accompanied by its cracking and infiltration with aluminium. The above process enables local dissolution of the MgO substrate and formation in it of a thin region of interpenetrating metallic channels walled with spinel. The removal of dissolved magnesium through open aluminium channels towards the drop and to vacuum locally produces areas of aluminium enriched with dissolved oxygen, which results in the nucleation of α-Al{sub 2}O{sub 3} at spinel clad walls. The growth of α-Al{sub 2}O{sub 3} is controlled only by the dissolution rate of MgO by aluminium, liquid state diffusion of Mg to drop/vacuum and oxygen to the front of the of α-Al{sub 2}O{sub 3} crystallites growing into MgO substrate. - Highlights: • New unique evidence of first stages of interaction of liquid Al with MgO substrates • Interaction of liquid Al with MgO starts with the formation of a layer MgAl{sub 2}O{sub 4}. • Growth of MgAl{sub 2}O{sub 4} is slow as controlled by solid state out-diffusion of Mg and O. • MgAl{sub 2}O{sub 4} serves as a nucleation site for Al{sub 2}O{sub 3} and consumed by it soon after. • Growth of Al{sub 2}O{sub 3} is fast as controlled by diffusion in liquid state.

36 MATERIALS SCIENCE↗

Evolution of microstructure, texture and inhibitor along the processing route for grain-oriented electrical steels using strip casting

In the present work, a regular grade GO sheet was produced successively by strip casting, hot rolling, normalizing annealing, two-stage cold rolling with intermediate annealing, primary recrystallization annealing, secondary recrystallization annealing and purification. The aim of this paper was to characterize the evolution of microstructure, texture and inhibitor along the new processing route by comprehensive utilization of optical microscopy, X-ray diffraction and transmission electron microscopy. It was found that a fine microstructure with the ferrite grain size range of 7–12 μm could be obtained in the primary recrystallization annealed sheet though a very coarse microstructure was produced in the initial as-cast strip. The main finding was that the “texture memory” effect on Goss texture started on the through-thickness intermediate annealed strip after first cold rolling, which was not similar to the “texture memory” effect on Goss texture starting on the surface layers of the hot rolled strip in the conventional production route. As a result, the origin of Goss nuclei capable of secondary recrystallization lied in the grains already presented in Goss orientation in the intermediate annealed strip after first cold rolling. Another finding was that fine and dispersive inhibitors (mainly AlN) were easy to be produced in the primary recrystallization microstructure due to the initial rapid solidification during strip casting and the subsequent rapid cooling, and the very high temperature reheating usually used before hot rolling in the conventional production route could be avoided. - Highlights: • A regular grade grain-oriented electrical steel was produced. • Evolution of microstructure, texture and inhibitor was characterized. • Origin of Goss nuclei lied in the intermediate annealed strip. • A fine primary recrystallization microstructure could be produced. • Effective inhibitors were easy to be obtained in the new processing route.

36 MATERIALS SCIENCE↗

Nucleation and growth characteristics of graphite spheroids in bainite during graphitization annealing of a medium carbon steel

The evolution of microstructure in bainite during graphitization annealing at 680 °C of Jominy-quenched bars of an Al-Si bearing medium carbon (0.4C wt%) steel has been studied and compared with that in martensite by using light, scanning and transmission electron microscopy. The results show that the graphitization process in bainite is different from that in martensite in many aspects such as the initial carbon state, the behavior of cementite, the nucleation-growth feature and kinetics of formation of graphite spheroids during graphitization annealing, and the shape, size and distribution of these graphite spheroids. The fact that the graphitization in bainite can produce more homogeneous graphite spheroids with more spherical shape and finer size in a shorter annealing time without the help of preexisting coring particles implies that bainite should be a better starting structure than martensite for making graphitic steel. - Highlights: • This article presents a microstructural characterization of formation of graphite spheroids in bainite. • Nucleation and growth characteristics of graphite spheroids formed in bainite and martensite are compared. • Bainite should be a better starting structure for making graphitic steel as results show.

36 MATERIALS SCIENCE↗

Microstructures and phase transformations of Ti-30Zr-xNb (x = 5, 7, 9, 13 at.%) shape memory alloys

The microstructures, phase transformations and shape memory properties of Ti-30Zr-xNb (x = 5, 7, 9, 13 at.%) alloys were investigated. The X-ray diffraction and transmission electron microscopy observations showed that the Ti-30Zr-5Nb, Ti-30Zr-7/9Nb and Ti-30Zr-13Nb alloys were composed of the hcp α′-martensite, orthorhombic α″-martensite and β phases, respectively. The results indicated the enhanced β-stabilizing effect of Nb in Ti-30Zr-xNb alloys than that in Ti-Nb alloys due to the high content of Zr. The differential scanning calorimetry test indicated that the Ti-30Zr-5Nb alloy displayed a reversible transformation with a high martensitic transformation start temperature of 776 K and a reverse martensitic transformation start temperature (A{sub s}) of 790 K. For the Ti-30Zr-7Nb and Ti-30Zr-9Nb alloys, the martensitic transformation temperatures decreased with the increasing Nb content. Moreover, an ω phase transformation occurred in the both alloys upon heating at a temperature lower than the corresponding A{sub s}, which is prompted by more addition of Nb. Although the critical stress in tension of the three martensitic alloys decreased with increasing Nb content, the Ti-30Zr-9Nb alloy showed a critical stress of as high as 300 MPa. Among all the alloys, the Ti-30Zr-9Nb alloy exhibited the maximum shape memory effect of 1.61%, due to the lowest critical stress for the martensite reorientation. - Highlights: •Ti-30Zr-5Nb alloy is composed of hcp α′-martensite with the M{sub s} of 776 K. •Ti-30Zr-7Nb and Ti-30Zr-9Nb alloys are predominated by orthorhombic α″-martensite. •Ti-30Zr-13Nb alloy consists of a single β phase due to the β-stabilizing effect of Nb. •The martensitic transformation temperatures decrease with increasing Nb content. •Ti-30Zr-9Nb alloy shows the maximum shape memory effect of 1.61%.

36 MATERIALS SCIENCE↗

Chitosan as template for the synthesis of ceria nanoparticles

Graphical abstract: Cerium oxide nanoparticles with cubic fluorite structure were prepared using chitosan as template, cerium nitrate as a starting material and sodium hydroxide as a precipitating agent. Calcinated powders at 350 {sup o}C contain agglomerated particles with average particle size of {approx}4 nm, very high porosity and foam-like morphology formed by open and close pores. Highlights: {yields} Pure CeO{sub 2} nanoparticles can take place using chitosan as template. {yields} A porous material was obtained. {yields} Blueshifts in the ultraviolet absorption spectra have been observed in cerium oxide nanocrystallites. -- Abstract: Cerium oxide (CeO{sub 2}), nanoparticles were prepared using chitosan as template, cerium nitrate as a starting material and sodium hydroxide as a precipitating agent. The resultant ceria-chitosan spheres were calcined at 350 {sup o}C. The synthesized powders were characterized by, XRD, HRTEM, UV-vis, FTIR, and TG-DTA. The average size of the nanoparticles obtained was {approx}4 nm and BET specific surface area {approx}105 m{sup 2} g{sup -1}. Blueshifts in the ultraviolet absorption spectra have been observed in cerium oxide nanocrystallites. The band-gap was found to be 4.5 eV. The blueshifts are well explained for diameters down to less than a few nanometers by the change in the electronic band structure.

60 APPLIED LIFE SCIENCES↗

Preparation of graphene/TiO{sub 2} anode materials for lithium-ion batteries by a novel precipitation method

Graphical abstract: Large-scale preparation of graphene/TiO{sub 2} composites was carried out by precipitation method using graphene oxide nanosheet, Ti(SO{sub 4}){sub 2} and NH{sub 3}H{sub 2}O as starting materials. Highlights: Black-Right-Pointing-Pointer We use cheap graphene oxides, Ti(SO{sub 4}){sub 2} and NH{sub 3}H{sub 2}O as starting materials for preparation of graphene/TiO{sub 2} composites. Black-Right-Pointing-Pointer The reversible capacity and the cycling stability of the TiO{sub 2} are improved by graphene additive. Black-Right-Pointing-Pointer Shorter diffusion length and a larger contact area of graphene/TiO{sub 2} result in excellent electrochemical performance. -- Abstract: This paper reports a large-scale production route for graphene/TiO{sub 2} nanocomposites using water-based in situ precipitation method. In this method, freshly prepared graphene oxides/TiO{sub 2} obtained by precipitating Ti(SO{sub 4}){sub 2} with NH{sub 3}H{sub 2}O was subjected to heat treatment in the presence of N{sub 2}, which resulted in the formation of graphene/TiO{sub 2} nanocomposites. Graphene/TiO{sub 2} composites prepared by our method were found to be suitable as anode materials for lithium ion batteries because of its stable cycling performance and high capacity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗