Surface cleaning for enhanced adhesion to packaging surfaces: Effect of oxygen and ammonia plasma

The effects of direct plasma chemistries on carbon removal from silicon nitride (SiN{sub x}) and oxynitride (SiO{sub x}N{sub y}) surfaces have been studied by in-situ x-ray photoelectron spectroscopy (XPS) and ex-situ contact angle measurements. The data indicate that O{sub 2} and NH{sub 3} capacitively coupled plasmas are effective at removing adventitious carbon from silicon nitride (SiN{sub x}) and Si oxynitride (SiO{sub x}N{sub y}) surfaces. O{sub 2} plasma treatment results in the formation of a silica overlayer. In contrast, the exposure to NH{sub 3} plasma results in negligible additional oxidation of the SiN{sub x} or SiO{sub x}N{sub y} surface. Ex-situ contact angle measurements show that SiN{sub x} and SiO{sub x}N{sub y} surfaces exposed to oxygen plasma are initially more hydrophilic than surfaces exposed to NH{sub 3} plasma, indicating that the O{sub 2} plasma-induced SiO{sub 2} overlayer is highly reactive toward ambient. At longer ambient exposures (≳10 h), however, surfaces treated by either O{sub 2} or NH{sub 3} plasma exhibit similar steady state contact angles, correlated with rapid uptake of adventitious carbon, as determined by XPS. Surface passivation by exposure to molecular hydrogen prior to ambient exposure significantly retards the increase in contact angle upon exposure to ambient. The results suggest a practical route to enhancing the time available for effective bonding to surfaces in microelectronics packaging applications.

36 MATERIALS SCIENCE↗

Investigation of a Wedge Adhesion Test for Edge Seals

Many photovoltaic (PV) technologies have been found to be sensitive to moisture that diffuses into a PV package. Even with the use of impermeable frontsheets and backsheets, moisture can penetrate from the edges of a module. To limit this moisture ingress pathway from occurring, manufacturers often use a low permeability polyisobutylene (PIB) based edge seal filled with desiccant to further restrict moisture ingress. Moisture ingress studies have shown that these materials are capable of blocking moisture for the 25-year life of a module; but to do so, they must remain well-adhered and free of cracks. This work focuses on adapting the Boeing Wedge test for use with edge seals laminated using glass substrates as part of a strategy to assess the long-term durability of edge seals. The advantage of this method is that it duplicates the residual stresses and strains that a glass/glass module may have when the lamination process results in some residual glass bending that puts the perimeter in tension. Additionally, this method allows one to simultaneously expose the material to thermal stress, humidity, mechanical stress, and ultraviolet radiation. The disadvantage of this method generally is that we are limited by the fracture toughness of the glass substrates that the edge seal is adhered to. However, the low toughness of typical uncrosslinked or sparsely crosslinked PIB makes them suitable for this technique. We present data obtained during the development of the wedge test for use with PV edge seal materials. This includes development of the measuring techniques and evaluation of the test method with relevant materials. We find consistent data within a given experiment, along with the theoretical independence of fracture toughness measurements with wedge thickness. This indicates that the test methodology is reproducible. However, even though individual experimental sets are consistent, the reproducibility between experimental sets is poor. We believe this may be due to inconsistencies in sample history, sample batch, or small changes in sample preparation/assembly from one month to the next. Because the fracture strength of typical edge seal materials is so low, they cannot be relied upon for mechanical strength. A small stress or strain on the edge seal is capable of promoting delamination or tearing causing the edge seal to fail. Because of this, edge seals are very dependent on the processing and construction parameters in the full size PV module such that any long term evaluation of their durability must be conducted on full size modules to be accurate.

14 SOLAR ENERGY↗

Influence of Nitriding on the Wear Resistance and Adhesion of Zinc Coatings on Steel

Chemicothermal treatment of steel is considered: specifically, diffusional zinc coating in a nitrogen-bearing medium; and nitriding of a preformed zinc-filled coating. The structure of the modified layers is investigated. Their microhardness and wear resistance increase as a result of solid-solution hardening by zinc and nitrogen.

36 MATERIALS SCIENCE↗

Nondestructive Characterization of Adhesive Bonds from Guided Wave Data

The critical role played by interface zones in the fracture and failure of composites and other bonded materials is well known. The existing nondestructive evaluation methods are generally not capable of yielding useful quantitative information of the strength of an interface.

developed adhesively bonded joints↗